JPS53146279A - Corrosion, scale, and stain inhibitor in aqueous system - Google Patents
Corrosion, scale, and stain inhibitor in aqueous systemInfo
- Publication number
- JPS53146279A JPS53146279A JP6162877A JP6162877A JPS53146279A JP S53146279 A JPS53146279 A JP S53146279A JP 6162877 A JP6162877 A JP 6162877A JP 6162877 A JP6162877 A JP 6162877A JP S53146279 A JPS53146279 A JP S53146279A
- Authority
- JP
- Japan
- Prior art keywords
- corrosion
- scale
- stain inhibitor
- aqueous system
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To provide a corrosion, scale and stain inhibitor for slid surfaces in contact with water, which contains a copolymer composed of inorg. phosphoric acids, maleic acid or its acid anhydride and a specified monomer, or water sol. salts of the copolymer as the essential component.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6162877A JPS53146279A (en) | 1977-05-26 | 1977-05-26 | Corrosion, scale, and stain inhibitor in aqueous system |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6162877A JPS53146279A (en) | 1977-05-26 | 1977-05-26 | Corrosion, scale, and stain inhibitor in aqueous system |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS53146279A true JPS53146279A (en) | 1978-12-20 |
JPS6124080B2 JPS6124080B2 (en) | 1986-06-09 |
Family
ID=13176630
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6162877A Granted JPS53146279A (en) | 1977-05-26 | 1977-05-26 | Corrosion, scale, and stain inhibitor in aqueous system |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS53146279A (en) |
Cited By (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5827986A (en) * | 1981-08-13 | 1983-02-18 | Kurita Water Ind Ltd | Corrosion inhibiting agent for metal |
JPS5840199A (en) * | 1981-09-01 | 1983-03-09 | Kurita Water Ind Ltd | Antifouling agent for treating system of hydrogen sulfide-contg. drain in petroleum-refining process |
JPS61153198A (en) * | 1984-12-26 | 1986-07-11 | Nippon Zeon Co Ltd | Anti-scaling agent |
JPS61153199A (en) * | 1984-12-24 | 1986-07-11 | カルゴン コーポレーション | Method and composition of inhibiting scale of calcium oxalate extending over wide ph range |
JPH11502763A (en) * | 1995-03-17 | 1999-03-09 | バックマン・ラボラトリーズ・インターナショナル・インコーポレーテッド | Scale control in aqueous industrial systems. |
WO2005054397A1 (en) * | 2003-12-01 | 2005-06-16 | Shishiai-Kabushikigaisha | Cooling fluid composition |
WO2005054396A1 (en) * | 2003-12-01 | 2005-06-16 | Shishiai-Kabushikigaisha | Cooling fluid composition |
JP4838350B2 (en) * | 2006-05-08 | 2011-12-14 | イーコラブ インコーポレイティド | Acid cleaning agent for metal surfaces |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP5131959B2 (en) * | 2007-05-02 | 2013-01-30 | 株式会社パイロットコーポレーション | Water-based ballpoint pen |
-
1977
- 1977-05-26 JP JP6162877A patent/JPS53146279A/en active Granted
Cited By (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5827986A (en) * | 1981-08-13 | 1983-02-18 | Kurita Water Ind Ltd | Corrosion inhibiting agent for metal |
JPS6119714B2 (en) * | 1981-08-13 | 1986-05-19 | Kurita Water Ind Ltd | |
JPS5840199A (en) * | 1981-09-01 | 1983-03-09 | Kurita Water Ind Ltd | Antifouling agent for treating system of hydrogen sulfide-contg. drain in petroleum-refining process |
JPS6248558B2 (en) * | 1981-09-01 | 1987-10-14 | Kurita Kogyo Kk | |
JPS61153199A (en) * | 1984-12-24 | 1986-07-11 | カルゴン コーポレーション | Method and composition of inhibiting scale of calcium oxalate extending over wide ph range |
JPS61153198A (en) * | 1984-12-26 | 1986-07-11 | Nippon Zeon Co Ltd | Anti-scaling agent |
JPH11502763A (en) * | 1995-03-17 | 1999-03-09 | バックマン・ラボラトリーズ・インターナショナル・インコーポレーテッド | Scale control in aqueous industrial systems. |
WO2005054397A1 (en) * | 2003-12-01 | 2005-06-16 | Shishiai-Kabushikigaisha | Cooling fluid composition |
WO2005054396A1 (en) * | 2003-12-01 | 2005-06-16 | Shishiai-Kabushikigaisha | Cooling fluid composition |
JP4838350B2 (en) * | 2006-05-08 | 2011-12-14 | イーコラブ インコーポレイティド | Acid cleaning agent for metal surfaces |
Also Published As
Publication number | Publication date |
---|---|
JPS6124080B2 (en) | 1986-06-09 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
AU1612676A (en) | Corrosion inhibition in an aqueous system with phosphono- carboxylic acids | |
DE3060877D1 (en) | Use of (meth)acrylic acid and maleic acid copolymers as incrustation inhibitors in detergents | |
ES457440A1 (en) | Corrosion inhibitor for metal surfaces | |
JPS53146279A (en) | Corrosion, scale, and stain inhibitor in aqueous system | |
GB994062A (en) | An antirusting surface treating method for iron and steel products | |
SE8301134D0 (en) | PROCEDURE FOR INHIBITING CORROSION OF IRON-BASED METALS | |
NO792606L (en) | CORROSION INHIBITOR FOR Aqueous SALTS SOLUTIONS | |
DE2860352D1 (en) | Use of corrosion inhibitors in aqueous systems | |
ES439309A1 (en) | Composition and method of inhibiting corosion | |
SE7713717L (en) | INHIBITOR FOR ALUMINUM IN ALKALINE SOLUTIONS | |
HUT77018A (en) | Process for preparing terpolymers | |
IE782443L (en) | Corrosion inhibiitor. | |
DE3063379D1 (en) | Use of alcanol-amine salts of cyclic amidocarboxylic acids as corrosion inhibitors in aqueous systems | |
JPS52116401A (en) | Preparation of carboxylic acid esters | |
JPS542235A (en) | Corrosion inhibitor | |
JPS5230196A (en) | Method of erasing indication in magnetophoresis indicator | |
JPS5288592A (en) | Wetting agent | |
JPS5345860A (en) | Electric hoist | |
JPS5673600A (en) | Preventing method of scale in water | |
JPS53107766A (en) | Utilization of low level energy produced by heat of dissolution | |
JPS5242647A (en) | Method for neutralizing acid or alkaline aqueous solution containing n eutral salt | |
FR2298050A1 (en) | PIPE-LINES CONNECTION PROCEDURE IN UNDERWATER ENVIRONMENT | |
SE8005447L (en) | CORRECTION INHIBITOR IN THE FORM OF ALUMINUM-GLYCONIC ACID COMPLEX | |
JPS53141137A (en) | Method of inhibiting corrosion of metal coming into contact with aqueous calcium chloride solution | |
JPS53132166A (en) | Method of controller ph value |