JPS5289536A - Method of melting at high speed tin to be poured in tin plating bath - Google Patents
Method of melting at high speed tin to be poured in tin plating bathInfo
- Publication number
- JPS5289536A JPS5289536A JP584876A JP584876A JPS5289536A JP S5289536 A JPS5289536 A JP S5289536A JP 584876 A JP584876 A JP 584876A JP 584876 A JP584876 A JP 584876A JP S5289536 A JPS5289536 A JP S5289536A
- Authority
- JP
- Japan
- Prior art keywords
- tin
- poured
- melting
- high speed
- plating bath
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Electroplating And Plating Baths Therefor (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP584876A JPS5289536A (en) | 1976-01-23 | 1976-01-23 | Method of melting at high speed tin to be poured in tin plating bath |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP584876A JPS5289536A (en) | 1976-01-23 | 1976-01-23 | Method of melting at high speed tin to be poured in tin plating bath |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPS5289536A true JPS5289536A (en) | 1977-07-27 |
Family
ID=11622417
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP584876A Pending JPS5289536A (en) | 1976-01-23 | 1976-01-23 | Method of melting at high speed tin to be poured in tin plating bath |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5289536A (ja) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4432844A (en) * | 1982-01-28 | 1984-02-21 | Fujisash Company | Process for regeneration of electrolyte containing tin salts by reducing the same |
| EP0054074B1 (en) * | 1980-06-23 | 1987-05-13 | Fujisash Company | Process for reducing and reclaiming electrolyte containing tin salt |
| EP0570033A1 (fr) * | 1992-04-15 | 1993-11-18 | Recherche et Développement GROUPE COCKERILL SAMBRE | Procédé d'électrodéposition d'étain et/ou d'alliages d'étain sur un support métallique |
| EP1384448A1 (de) * | 2002-07-26 | 2004-01-28 | Heraeus Kulzer GmbH & Co.KG | Vorrichtung zur galvanischen Abscheidung prothetischer, metallischer Dentalformteile |
-
1976
- 1976-01-23 JP JP584876A patent/JPS5289536A/ja active Pending
Cited By (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP0054074B1 (en) * | 1980-06-23 | 1987-05-13 | Fujisash Company | Process for reducing and reclaiming electrolyte containing tin salt |
| US4432844A (en) * | 1982-01-28 | 1984-02-21 | Fujisash Company | Process for regeneration of electrolyte containing tin salts by reducing the same |
| EP0570033A1 (fr) * | 1992-04-15 | 1993-11-18 | Recherche et Développement GROUPE COCKERILL SAMBRE | Procédé d'électrodéposition d'étain et/ou d'alliages d'étain sur un support métallique |
| EP1384448A1 (de) * | 2002-07-26 | 2004-01-28 | Heraeus Kulzer GmbH & Co.KG | Vorrichtung zur galvanischen Abscheidung prothetischer, metallischer Dentalformteile |
| DE10234285B4 (de) * | 2002-07-26 | 2006-12-07 | Heraeus Kulzer Gmbh | Vorrichtung zur galvanischen Abscheidung prothetischer, metallischer Dentalformteile |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| GB2067595B (en) | Method and apparatus for replenishing an electroplating bath with metal to be deposited | |
| JPS5539090A (en) | Method of measuring temperature in molten metal bath | |
| JPS55125214A (en) | Adding of reactive metal to molten metal bath | |
| JPS5289536A (en) | Method of melting at high speed tin to be poured in tin plating bath | |
| JPS571557A (en) | Method of applying flux to molten metal in tubular centrifugal mold | |
| JPS5241132A (en) | Molten plating method | |
| JPS52130433A (en) | Method of plating ironnsteel material with molten leaddtin alloy | |
| JPS51114334A (en) | Method of adjusting quantity of adhesion of plated metal in continuous molten metal plating | |
| JPS54124827A (en) | Imparting of influence to molten metal solidification in continuous casting | |
| GB2001154B (en) | Method of automatically pouring molten metal in continous casting of metal | |
| IT1084755B (it) | Metodo per trattare metallo fuso in getti centrifugati | |
| JPS544248A (en) | Method of selective plating in continuous plating bath | |
| JPS5322126A (en) | Molten metal plating method | |
| JPS52146729A (en) | Members to be dipped in molten aluminum bath | |
| NZ185631A (en) | Float glass process molten metal in bath varies in depth along its length | |
| JPS5314634A (en) | Method of forming refined spangles in molten plating | |
| JPS52124429A (en) | Method of automatically controlling plating speed in nonnelectrolytic plating | |
| JPS52113331A (en) | Method of controlling alloy added for plating in molten zinc plating bath | |
| JPS5388633A (en) | Method of preventing formation of dross floated in continuous melting zinc plating bath and its device | |
| JPS5315228A (en) | Molten plating method of cooler | |
| JPS52126634A (en) | Lusterous plating method and composition for use in galvanizing bath | |
| JPS5381434A (en) | Melting plating method of zinccaluminium alloy | |
| JPS51128633A (en) | Method to control level of molten metal in turndish | |
| JPS5326230A (en) | Method of detecting level of molten metal in mold | |
| JPS5443128A (en) | Method of preventing segregation in molten metal casting |