Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NEC Corp
Original Assignee
NEC Corp
Nippon Electric Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NEC Corp, Nippon Electric Co LtdfiledCriticalNEC Corp
Priority to JP50158861ApriorityCriticalpatent/JPS5280499A/en
Publication of JPS5280499ApublicationCriticalpatent/JPS5280499A/en
PURPOSE: The method to obtain La2O3-In2O3-2TiO2 group temperature compensation porcelain dielectric material of dielectric constant of more than 28 and of dielectric constant temperature coefficient within rang of -100W+100 ppm/°C.
COPYRIGHT: (C)1977,JPO&Japio
JP50158861A1975-12-261975-12-26Oxide dielectric material