JPS5265712A - Two phases stainless steel with inproved corrosion resistance and impr oving method of the corrosion resistance - Google Patents
Two phases stainless steel with inproved corrosion resistance and impr oving method of the corrosion resistanceInfo
- Publication number
- JPS5265712A JPS5265712A JP14268775A JP14268775A JPS5265712A JP S5265712 A JPS5265712 A JP S5265712A JP 14268775 A JP14268775 A JP 14268775A JP 14268775 A JP14268775 A JP 14268775A JP S5265712 A JPS5265712 A JP S5265712A
- Authority
- JP
- Japan
- Prior art keywords
- corrosion resistance
- stainless steel
- inproved
- oving
- impr
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: In order to produce stainless steel with improved surface corrosion resistance and inherent internal strength, nitrogen is diffused on the surface part of two phase stainless steel to form several mm thick austenite alone layer while maintaining internal two phase.
COPYRIGHT: (C)1977,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14268775A JPS5265712A (en) | 1975-11-27 | 1975-11-27 | Two phases stainless steel with inproved corrosion resistance and impr oving method of the corrosion resistance |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14268775A JPS5265712A (en) | 1975-11-27 | 1975-11-27 | Two phases stainless steel with inproved corrosion resistance and impr oving method of the corrosion resistance |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5265712A true JPS5265712A (en) | 1977-05-31 |
JPS5529137B2 JPS5529137B2 (en) | 1980-08-01 |
Family
ID=15321179
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP14268775A Granted JPS5265712A (en) | 1975-11-27 | 1975-11-27 | Two phases stainless steel with inproved corrosion resistance and impr oving method of the corrosion resistance |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5265712A (en) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS60165370A (en) * | 1984-02-07 | 1985-08-28 | Ishikawajima Harima Heavy Ind Co Ltd | Nitriding treatment of stainless steel |
JPS63227790A (en) * | 1987-03-16 | 1988-09-22 | N T T Gijutsu Iten Kk | High strength stainless steel and its production |
US5259935A (en) * | 1991-05-03 | 1993-11-09 | The Boc Group, Inc. | Stainless steel surface passivation treatment |
US20180179606A1 (en) * | 2016-12-23 | 2018-06-28 | Posco | Duplex stainless steel having excellent corrosion resistance and method for manufacturing the same |
-
1975
- 1975-11-27 JP JP14268775A patent/JPS5265712A/en active Granted
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS60165370A (en) * | 1984-02-07 | 1985-08-28 | Ishikawajima Harima Heavy Ind Co Ltd | Nitriding treatment of stainless steel |
JPH0371508B2 (en) * | 1984-02-07 | 1991-11-13 | Ishikawajima Harima Heavy Ind | |
JPS63227790A (en) * | 1987-03-16 | 1988-09-22 | N T T Gijutsu Iten Kk | High strength stainless steel and its production |
US5259935A (en) * | 1991-05-03 | 1993-11-09 | The Boc Group, Inc. | Stainless steel surface passivation treatment |
US20180179606A1 (en) * | 2016-12-23 | 2018-06-28 | Posco | Duplex stainless steel having excellent corrosion resistance and method for manufacturing the same |
Also Published As
Publication number | Publication date |
---|---|
JPS5529137B2 (en) | 1980-08-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
IL52089A (en) | Method of improving the oxidation and corrosion resistance of super alloy bodies and articles so obtained | |
JPS51129328A (en) | Metal baseball bat and method of producing same | |
JPS5265712A (en) | Two phases stainless steel with inproved corrosion resistance and impr oving method of the corrosion resistance | |
JPS54136A (en) | Roller bearing with unsymmetrical crowning track | |
JPS51137611A (en) | High-strength stainless steel | |
JPS5439342A (en) | Method of connecting aluminium material and copper material | |
JPS51112719A (en) | Extra low carbon stainless steel with excellent corrosion resistance | |
JPS52138718A (en) | Pipe joint | |
JPS5236512A (en) | Two phases (ferritic and austenitic) stainless steel of high hardness | |
JPS522838A (en) | Method of preventing corrosion of steel surface in absorption type refrigerator | |
JPS51138733A (en) | Method of coatin g metals | |
JPS51130487A (en) | Method for manufacturing printed decorative metal plates | |
JPS5226537A (en) | Surface treatment of aluminum and aluminum alloy | |
JPS5252691A (en) | Method of determining activity value of leucin amino eptidase | |
JPS52132936A (en) | Ski body | |
JPS53104635A (en) | Coating composition | |
JPS5290160A (en) | Waste water treatment method and its device | |
JPS5280213A (en) | Wear resistance austenite steel for sliding parts in water | |
SU542645A1 (en) | Metal form grease | |
JPS52119414A (en) | Nickel saving type stainless steel having high stretchability | |
JPS5235171A (en) | Resolving method of coagulant | |
Nikiforova et al. | Effect of Cr Content of Steels on Their Corrosion Resistance in High Parameter Water | |
JPS525011A (en) | Pipe joint | |
JPS526325A (en) | Austenite-ferrite stainless steel having acid resistance and wear resi stance | |
JPS51130486A (en) | Method for manufacturing printed decorative metal plates |