JPS52144320A - Electrolytic obtaining method of nickel - Google Patents
Electrolytic obtaining method of nickelInfo
- Publication number
- JPS52144320A JPS52144320A JP6129277A JP6129277A JPS52144320A JP S52144320 A JPS52144320 A JP S52144320A JP 6129277 A JP6129277 A JP 6129277A JP 6129277 A JP6129277 A JP 6129277A JP S52144320 A JPS52144320 A JP S52144320A
- Authority
- JP
- Japan
- Prior art keywords
- nickel
- obtaining method
- electrolytic
- electrolytic obtaining
- obtaining
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
- PXHVJJICTQNCMI-UHFFFAOYSA-N Nickel Chemical compound [Ni] PXHVJJICTQNCMI-UHFFFAOYSA-N 0.000 title 2
- 229910052759 nickel Inorganic materials 0.000 title 1
Classifications
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25C—PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- C25C1/00—Electrolytic production, recovery or refining of metals by electrolysis of solutions
- C25C1/06—Electrolytic production, recovery or refining of metals by electrolysis of solutions or iron group metals, refractory metals or manganese
- C25C1/08—Electrolytic production, recovery or refining of metals by electrolysis of solutions or iron group metals, refractory metals or manganese of nickel or cobalt
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Electrolytic Production Of Metals (AREA)
- Manufacture And Refinement Of Metals (AREA)
- Inorganic Compounds Of Heavy Metals (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| CA253,463A CA1062652A (en) | 1976-05-27 | 1976-05-27 | Electrowinning of nickel in diaphragm-free cells |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPS52144320A true JPS52144320A (en) | 1977-12-01 |
Family
ID=4106056
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP6129277A Pending JPS52144320A (en) | 1976-05-27 | 1977-05-27 | Electrolytic obtaining method of nickel |
Country Status (7)
| Country | Link |
|---|---|
| US (1) | US4087338A (enExample) |
| JP (1) | JPS52144320A (enExample) |
| AU (1) | AU2484377A (enExample) |
| CA (1) | CA1062652A (enExample) |
| FI (1) | FI771514A7 (enExample) |
| FR (1) | FR2352896A1 (enExample) |
| NO (1) | NO771814L (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US8980068B2 (en) * | 2010-08-18 | 2015-03-17 | Allen R. Hayes | Nickel pH adjustment method and apparatus |
Family Cites Families (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CA895500A (en) * | 1972-03-14 | Kewanee Oil Company | High speed electrodeposition of nickel | |
| US1754125A (en) * | 1928-03-30 | 1930-04-08 | Smith Stanley Cochran | Electrolytic recovery of metals |
| JPS4218205Y1 (enExample) * | 1964-07-16 | 1967-10-21 | ||
| US3743585A (en) * | 1971-10-12 | 1973-07-03 | Sec Corp | Metal recovery process |
| CA1019278A (en) * | 1974-04-09 | 1977-10-18 | Inco Limited | Electrowinning nickel from sulfate electrolyte |
-
1976
- 1976-05-27 CA CA253,463A patent/CA1062652A/en not_active Expired
-
1977
- 1977-02-22 US US05/770,472 patent/US4087338A/en not_active Expired - Lifetime
- 1977-05-04 AU AU24843/77A patent/AU2484377A/en not_active Expired
- 1977-05-12 FI FI771514A patent/FI771514A7/fi not_active Application Discontinuation
- 1977-05-24 NO NO771814A patent/NO771814L/no unknown
- 1977-05-25 FR FR7715960A patent/FR2352896A1/fr not_active Withdrawn
- 1977-05-27 JP JP6129277A patent/JPS52144320A/ja active Pending
Also Published As
| Publication number | Publication date |
|---|---|
| CA1062652A (en) | 1979-09-18 |
| NO771814L (no) | 1977-11-29 |
| US4087338A (en) | 1978-05-02 |
| FI771514A7 (enExample) | 1977-11-28 |
| FR2352896A1 (fr) | 1977-12-23 |
| AU2484377A (en) | 1978-11-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5363227A (en) | Electroplating method of golddcobalt alloy | |
| JPS535019A (en) | Electrolytic obtaining method of nickel | |
| BG28988A4 (en) | Method of obtaining of 4- halo- dihydropropyrans | |
| JPS5362740A (en) | Electrolytic plating method | |
| BG27754A3 (en) | Method of obtaining of 3- halomethylcephems | |
| JPS531834A (en) | Method of manufacturing nickel electrode | |
| JPS5326740A (en) | Electrolytic method | |
| JPS5297321A (en) | Electrolytic obtaining method of nickel | |
| JPS52144320A (en) | Electrolytic obtaining method of nickel | |
| JPS533904A (en) | Method of manufacturing nickel anode for electroplating | |
| BG27755A3 (en) | Method of obtaining of 7- alkoxy- 3- chlormethilcephems | |
| JPS52111818A (en) | Electrolytic decoppering method | |
| JPS537544A (en) | Nickel plating method | |
| YU102277A (en) | Method of warming up an electrolytic cell | |
| JPS52109438A (en) | Method of aging nonnelectrolytic nickel plating solution | |
| JPS5290429A (en) | Method of electroplating niicuup alloy | |
| JPS52149205A (en) | Method of producing nickel anode for electroplating | |
| JPS5346440A (en) | Nonnelectrolytic nickel plating method | |
| JPS5347945A (en) | Method of manufacturing nickel electrode | |
| JPS5376330A (en) | Method of manufacturing nickel electrode | |
| JPS5360833A (en) | Method of producing currenttsupplying electrode | |
| JPS5368864A (en) | Method of making electrolytic capacitor | |
| JPS5383064A (en) | Method of making electrolytic capacitor | |
| JPS5426428A (en) | Method of making electrolytic solution | |
| JPS52123913A (en) | Method of making aluminiummmagnesium alloy |