JPS51128637A - Method of preventing metal oxidation loss of molten metal bath - Google Patents
Method of preventing metal oxidation loss of molten metal bathInfo
- Publication number
- JPS51128637A JPS51128637A JP5339075A JP5339075A JPS51128637A JP S51128637 A JPS51128637 A JP S51128637A JP 5339075 A JP5339075 A JP 5339075A JP 5339075 A JP5339075 A JP 5339075A JP S51128637 A JPS51128637 A JP S51128637A
- Authority
- JP
- Japan
- Prior art keywords
- oxidation loss
- molten metal
- preventing
- bath
- metal bath
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Manufacture And Refinement Of Metals (AREA)
- Coating With Molten Metal (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP5339075A JPS51128637A (en) | 1975-05-01 | 1975-05-01 | Method of preventing metal oxidation loss of molten metal bath |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP5339075A JPS51128637A (en) | 1975-05-01 | 1975-05-01 | Method of preventing metal oxidation loss of molten metal bath |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS51128637A true JPS51128637A (en) | 1976-11-09 |
Family
ID=12941488
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP5339075A Pending JPS51128637A (en) | 1975-05-01 | 1975-05-01 | Method of preventing metal oxidation loss of molten metal bath |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS51128637A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN115448578A (en) * | 2022-09-16 | 2022-12-09 | 青岛融合新材料科技有限公司 | Top cover for tin bath in float process |
-
1975
- 1975-05-01 JP JP5339075A patent/JPS51128637A/en active Pending
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN115448578A (en) * | 2022-09-16 | 2022-12-09 | 青岛融合新材料科技有限公司 | Top cover for tin bath in float process |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
AU499897B2 (en) | Treatment of molten metal | |
JPS5265800A (en) | Method of treating transition metal compound | |
JPS51138561A (en) | Soldering method of oxidized metal surface | |
JPS5337516A (en) | Desulphurizing method of molten iron | |
JPS5345604A (en) | Method of treating molten metals | |
JPS5345628A (en) | Method of controlling process of continuously casting metal | |
JPS5235722A (en) | One side molten metal plating method | |
JPS5232824A (en) | Method of casting metal melts | |
GB1520937A (en) | Method of continuously casting steel | |
JPS529632A (en) | Method of casting molten metal | |
JPS51128637A (en) | Method of preventing metal oxidation loss of molten metal bath | |
JPS51145455A (en) | Method of metal ingot manufacture | |
JPS52134817A (en) | Casting method of molten metal | |
JPS5240405A (en) | Method of treating molten metal | |
JPS523537A (en) | Method of preventing corrosion of metals | |
JPS5243730A (en) | Method of preventing oxidation of molten aluminium or aluminium alloy | |
JPS5241134A (en) | Molten metal plating method | |
JPS51129820A (en) | Molten metal continuous casting method | |
JPS5440206A (en) | Explosionnpreventive method of molten metal ladle | |
JPS5352240A (en) | Method of continuously casting molten metal | |
ZA781760B (en) | Method of pouring molten metal | |
JPS5226320A (en) | Method of preventing slag from being drained during molten metal supply | |
JPS5274528A (en) | Method of continuous metal casting | |
JPS5344428A (en) | Method of continuously casting molten metal | |
JPS5311834A (en) | Method of continuously casting molten metal |