JPS5080941A - - Google Patents
Info
- Publication number
- JPS5080941A JPS5080941A JP13072373A JP13072373A JPS5080941A JP S5080941 A JPS5080941 A JP S5080941A JP 13072373 A JP13072373 A JP 13072373A JP 13072373 A JP13072373 A JP 13072373A JP S5080941 A JPS5080941 A JP S5080941A
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Nonmetallic Welding Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13072373A JPS5080941A (enrdf_load_stackoverflow) | 1973-11-22 | 1973-11-22 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13072373A JPS5080941A (enrdf_load_stackoverflow) | 1973-11-22 | 1973-11-22 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPS5080941A true JPS5080941A (enrdf_load_stackoverflow) | 1975-07-01 |
Family
ID=15041077
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP13072373A Pending JPS5080941A (enrdf_load_stackoverflow) | 1973-11-22 | 1973-11-22 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5080941A (enrdf_load_stackoverflow) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6114097A (ja) * | 1984-06-28 | 1986-01-22 | Kawasaki Steel Corp | 2相ステンレス鋼のサブマ−ジア−ク溶接方法 |
| JPH0299295A (ja) * | 1988-10-04 | 1990-04-11 | Nippon Steel Corp | 高温におけるクリープ破断強度および延性の優れたNi―Crオーステナイト系ステンレス鋼溶接材料 |
| JPH03169497A (ja) * | 1989-11-28 | 1991-07-23 | Nippon Steel Corp | 高温でのクリープ破断延性や強度及び耐脆化性の優れたNi―Crオーステナイト系ステンレス鋼溶接材料 |
| JP2002248598A (ja) * | 2001-02-26 | 2002-09-03 | Nippon Steel Corp | 高耐食ステンレス鋼溶接用被覆アーク溶接棒 |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS493854A (enrdf_load_stackoverflow) * | 1972-05-04 | 1974-01-14 |
-
1973
- 1973-11-22 JP JP13072373A patent/JPS5080941A/ja active Pending
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS493854A (enrdf_load_stackoverflow) * | 1972-05-04 | 1974-01-14 |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6114097A (ja) * | 1984-06-28 | 1986-01-22 | Kawasaki Steel Corp | 2相ステンレス鋼のサブマ−ジア−ク溶接方法 |
| JPH0299295A (ja) * | 1988-10-04 | 1990-04-11 | Nippon Steel Corp | 高温におけるクリープ破断強度および延性の優れたNi―Crオーステナイト系ステンレス鋼溶接材料 |
| JPH03169497A (ja) * | 1989-11-28 | 1991-07-23 | Nippon Steel Corp | 高温でのクリープ破断延性や強度及び耐脆化性の優れたNi―Crオーステナイト系ステンレス鋼溶接材料 |
| JP2002248598A (ja) * | 2001-02-26 | 2002-09-03 | Nippon Steel Corp | 高耐食ステンレス鋼溶接用被覆アーク溶接棒 |