- JPS50360B1 JPS50360B1 JP9662470A JP9662470A JPS50360B1 JP S50360 B1 JPS50360 B1 JP S50360B1 JP 9662470 A JP9662470 A JP 9662470A JP 9662470 A JP9662470 A JP 9662470A JP S50360 B1 JPS50360 B1 JP S50360B1
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Ceramic Products (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9662470A JPS50360B1 (ja) | 1970-11-02 | 1970-11-02 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9662470A JPS50360B1 (ja) | 1970-11-02 | 1970-11-02 |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS50360B1 true JPS50360B1 (ja) | 1975-01-08 |
Family
ID=14169980
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP9662470A Pending JPS50360B1 (ja) | 1970-11-02 | 1970-11-02 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS50360B1 (ja) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0289580A1 (en) * | 1986-10-23 | 1988-11-09 | Arch Development Corporation | Sintering aid for lanthanum chromite refractories |
US5397657A (en) * | 1991-01-28 | 1995-03-14 | Ngk Insulators, Ltd. | Method for increasing the electrical conductivity of a thermal sprayed interconnector for a solid electrolyte fuel cell |
-
1970
- 1970-11-02 JP JP9662470A patent/JPS50360B1/ja active Pending
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0289580A1 (en) * | 1986-10-23 | 1988-11-09 | Arch Development Corporation | Sintering aid for lanthanum chromite refractories |
US5397657A (en) * | 1991-01-28 | 1995-03-14 | Ngk Insulators, Ltd. | Method for increasing the electrical conductivity of a thermal sprayed interconnector for a solid electrolyte fuel cell |