JPS50133920A - - Google Patents
Info
- Publication number
- JPS50133920A JPS50133920A JP4096374A JP4096374A JPS50133920A JP S50133920 A JPS50133920 A JP S50133920A JP 4096374 A JP4096374 A JP 4096374A JP 4096374 A JP4096374 A JP 4096374A JP S50133920 A JPS50133920 A JP S50133920A
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4096374A JPS50133920A (en) | 1974-04-15 | 1974-04-15 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4096374A JPS50133920A (en) | 1974-04-15 | 1974-04-15 |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS50133920A true JPS50133920A (en) | 1975-10-23 |
Family
ID=12595126
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP4096374A Pending JPS50133920A (en) | 1974-04-15 | 1974-04-15 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS50133920A (en) |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS52114515A (en) * | 1976-03-24 | 1977-09-26 | Sumitomo Metal Ind Ltd | Heat treatment type high tensile steel of low nitrogen content and containing titanium |
JPS52114514A (en) * | 1976-03-24 | 1977-09-26 | Sumitomo Metal Ind Ltd | Heat treatment type high tensile steel of low nitrogen content, contai ning titanium and having excellent weldability weldability |
JPS5381421A (en) * | 1976-12-28 | 1978-07-18 | Nippon Kokan Kk <Nkk> | Steel for high current mig welding |
JPS55141321A (en) * | 1979-04-24 | 1980-11-05 | Eiichi Nakada | Multilayer metallic material with low temperature toughness |
JPS62151509A (en) * | 1985-12-25 | 1987-07-06 | Sumitomo Metal Ind Ltd | Production of high strength resistance welded pipe having excellent low-temperature toughness |
-
1974
- 1974-04-15 JP JP4096374A patent/JPS50133920A/ja active Pending
Cited By (9)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS52114515A (en) * | 1976-03-24 | 1977-09-26 | Sumitomo Metal Ind Ltd | Heat treatment type high tensile steel of low nitrogen content and containing titanium |
JPS52114514A (en) * | 1976-03-24 | 1977-09-26 | Sumitomo Metal Ind Ltd | Heat treatment type high tensile steel of low nitrogen content, contai ning titanium and having excellent weldability weldability |
JPS5643087B2 (en) * | 1976-03-24 | 1981-10-09 | ||
JPS5643086B2 (en) * | 1976-03-24 | 1981-10-09 | ||
JPS5381421A (en) * | 1976-12-28 | 1978-07-18 | Nippon Kokan Kk <Nkk> | Steel for high current mig welding |
JPS5828028B2 (en) * | 1976-12-28 | 1983-06-13 | 日本鋼管株式会社 | High current MIG welding method |
JPS55141321A (en) * | 1979-04-24 | 1980-11-05 | Eiichi Nakada | Multilayer metallic material with low temperature toughness |
JPS6356060B2 (en) * | 1979-04-24 | 1988-11-07 | Eiichi Nakada | |
JPS62151509A (en) * | 1985-12-25 | 1987-07-06 | Sumitomo Metal Ind Ltd | Production of high strength resistance welded pipe having excellent low-temperature toughness |