JPS496470A - - Google Patents
Info
- Publication number
- JPS496470A JPS496470A JP4621772A JP4621772A JPS496470A JP S496470 A JPS496470 A JP S496470A JP 4621772 A JP4621772 A JP 4621772A JP 4621772 A JP4621772 A JP 4621772A JP S496470 A JPS496470 A JP S496470A
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4621772A JPS496470A (en) | 1972-05-09 | 1972-05-09 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4621772A JPS496470A (en) | 1972-05-09 | 1972-05-09 |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS496470A true JPS496470A (en) | 1974-01-21 |
Family
ID=12740925
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP4621772A Pending JPS496470A (en) | 1972-05-09 | 1972-05-09 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS496470A (en) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH02501718A (en) * | 1986-07-21 | 1990-06-14 | マイクロ・モーション・インコーポレーテッド | Method for brazing corrosion-resistant nickel-based thin-walled tubing to stainless steel base members |
US4973366A (en) * | 1987-11-19 | 1990-11-27 | The Agency Of Industrial Science And Technology | Insert material for solid phase diffusion welding for nickel base superalloy and method therefor |
JPH04504982A (en) * | 1990-01-26 | 1992-09-03 | サンドストランド・コーポレイション | Method for manufacturing a combustor that can be repaired by welding |
WO2020195792A1 (en) * | 2019-03-26 | 2020-10-01 | 株式会社荏原製作所 | Canned motor and pump driven by same, and rocket engine system and liquid fuel rocket employing same |
-
1972
- 1972-05-09 JP JP4621772A patent/JPS496470A/ja active Pending
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH02501718A (en) * | 1986-07-21 | 1990-06-14 | マイクロ・モーション・インコーポレーテッド | Method for brazing corrosion-resistant nickel-based thin-walled tubing to stainless steel base members |
JPH0372382B2 (en) * | 1986-07-21 | 1991-11-18 | Maikuro Mooshon Inc | |
US4973366A (en) * | 1987-11-19 | 1990-11-27 | The Agency Of Industrial Science And Technology | Insert material for solid phase diffusion welding for nickel base superalloy and method therefor |
JPH04504982A (en) * | 1990-01-26 | 1992-09-03 | サンドストランド・コーポレイション | Method for manufacturing a combustor that can be repaired by welding |
WO2020195792A1 (en) * | 2019-03-26 | 2020-10-01 | 株式会社荏原製作所 | Canned motor and pump driven by same, and rocket engine system and liquid fuel rocket employing same |