JPS4930486A - - Google Patents
Info
- Publication number
- JPS4930486A JPS4930486A JP7167972A JP7167972A JPS4930486A JP S4930486 A JPS4930486 A JP S4930486A JP 7167972 A JP7167972 A JP 7167972A JP 7167972 A JP7167972 A JP 7167972A JP S4930486 A JPS4930486 A JP S4930486A
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Polymerization Catalysts (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7167972A JPS55406B2 (en, 2012) | 1972-07-19 | 1972-07-19 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7167972A JPS55406B2 (en, 2012) | 1972-07-19 | 1972-07-19 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS4930486A true JPS4930486A (en, 2012) | 1974-03-18 |
JPS55406B2 JPS55406B2 (en, 2012) | 1980-01-08 |
Family
ID=13467484
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP7167972A Expired JPS55406B2 (en, 2012) | 1972-07-19 | 1972-07-19 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS55406B2 (en, 2012) |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2320959A1 (fr) * | 1975-08-13 | 1977-03-11 | Exxon Research Engineering Co | Procede pour l'obtention de resines hydrocarbonees a bas point de ramollissement |
JPS5734082A (en) * | 1980-08-08 | 1982-02-24 | Comp Generale Electricite | Method of sintering ceramic tubular member and tubular member thereby |
JPS57205385A (en) * | 1981-06-08 | 1982-12-16 | Sanyo Electric Co | Lithium ion conductive solid electrolyte |
JPH0378974A (ja) * | 1989-08-21 | 1991-04-04 | Ngk Insulators Ltd | ナトリウム―硫黄電池用ベータアルミナ管の焼成方法 |
JPH0388279A (ja) * | 1989-08-31 | 1991-04-12 | Ngk Insulators Ltd | ナトリウム―硫黄電池用ベータアルミナ管の焼成方法 |
-
1972
- 1972-07-19 JP JP7167972A patent/JPS55406B2/ja not_active Expired
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2320959A1 (fr) * | 1975-08-13 | 1977-03-11 | Exxon Research Engineering Co | Procede pour l'obtention de resines hydrocarbonees a bas point de ramollissement |
JPS5734082A (en) * | 1980-08-08 | 1982-02-24 | Comp Generale Electricite | Method of sintering ceramic tubular member and tubular member thereby |
JPS57205385A (en) * | 1981-06-08 | 1982-12-16 | Sanyo Electric Co | Lithium ion conductive solid electrolyte |
JPH0378974A (ja) * | 1989-08-21 | 1991-04-04 | Ngk Insulators Ltd | ナトリウム―硫黄電池用ベータアルミナ管の焼成方法 |
JPH0388279A (ja) * | 1989-08-31 | 1991-04-12 | Ngk Insulators Ltd | ナトリウム―硫黄電池用ベータアルミナ管の焼成方法 |
Also Published As
Publication number | Publication date |
---|---|
JPS55406B2 (en, 2012) | 1980-01-08 |