JPS49123941A - - Google Patents
Info
- Publication number
- JPS49123941A JPS49123941A JP48083495A JP8349573A JPS49123941A JP S49123941 A JPS49123941 A JP S49123941A JP 48083495 A JP48083495 A JP 48083495A JP 8349573 A JP8349573 A JP 8349573A JP S49123941 A JPS49123941 A JP S49123941A
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C22/00—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals
- C23C22/05—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions
- C23C22/06—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions using aqueous acidic solutions with pH less than 6
- C23C22/34—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions using aqueous acidic solutions with pH less than 6 containing fluorides or complex fluorides
- C23C22/36—Chemical surface treatment of metallic material by reaction of the surface with a reactive liquid, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals using aqueous solutions using aqueous acidic solutions with pH less than 6 containing fluorides or complex fluorides containing also phosphates
Landscapes
- Chemical & Material Sciences (AREA)
- General Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Chemical Treatment Of Metals (AREA)
- Electroplating Methods And Accessories (AREA)
- Coating With Molten Metal (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US00275620A US3839099A (en) | 1972-07-27 | 1972-07-27 | Iron-phosphate coating for tin-plated ferrous metal surfaces |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS49123941A true JPS49123941A (ja) | 1974-11-27 |
JPS5325296B2 JPS5325296B2 (ja) | 1978-07-26 |
Family
ID=23053136
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP8349573A Expired JPS5325296B2 (ja) | 1972-07-27 | 1973-07-23 |
Country Status (5)
Country | Link |
---|---|
US (1) | US3839099A (ja) |
JP (1) | JPS5325296B2 (ja) |
CA (1) | CA980222A (ja) |
FR (1) | FR2194801B1 (ja) |
GB (1) | GB1428857A (ja) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5253739A (en) * | 1975-10-30 | 1977-04-30 | Nippon Steel Corp | Surface treatment of galvanized steel |
JPS52131937A (en) * | 1976-04-05 | 1977-11-05 | Amchem Prod | Solution for coating metal surface |
JPS54100944A (en) * | 1978-01-27 | 1979-08-09 | Toyo Kohan Co Ltd | Electroplating tin plate for seamless can |
JPS5562179A (en) * | 1978-10-30 | 1980-05-10 | Nippon Parkerizing Co Ltd | Chemical treating solution for coating metal surface |
Families Citing this family (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3975215A (en) * | 1973-10-10 | 1976-08-17 | Amchem Products, Inc. | Cleaner for tin plated ferrous metal surfaces |
US4149909A (en) * | 1977-12-30 | 1979-04-17 | Amchem Products, Inc. | Iron phosphate accelerator |
CA1162504A (en) * | 1980-11-25 | 1984-02-21 | Mobuyuki Oda | Treating tin plated steel sheet with composition containing titanium or zirconium compounds |
CA1257527A (en) * | 1984-12-20 | 1989-07-18 | Thomas W. Tull | Cold deformation process employing improved lubrication coating |
US5234509A (en) * | 1984-12-20 | 1993-08-10 | Henkel Corporation | Cold deformation process employing improved lubrication coating |
AU2001243660A1 (en) * | 2000-07-18 | 2002-01-30 | Crown Cork And Seal Technologies Corporation | Tinned iron can for light colored fruits |
WO2018175731A1 (en) | 2017-03-24 | 2018-09-27 | Magna International Inc. | Wax coating over phosphate coating for vehicle components |
Citations (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2312855A (en) * | 1940-09-07 | 1943-03-02 | Parker Rust Proof Co | Method of coating aluminum |
US2327127A (en) * | 1940-02-26 | 1943-08-17 | Frank E Rath | Stain and corrosion resistant tin surface and method of producing the same |
US2657156A (en) * | 1948-07-23 | 1953-10-27 | Parker Rust Proof Co | Phosphate coating composition and process |
US2665231A (en) * | 1949-06-17 | 1954-01-05 | Parker Rust Proof Co | Coating process with alkali metal phosphate and added fluoride salt |
US3152018A (en) * | 1961-11-01 | 1964-10-06 | Wyandotte Chemicals Corp | Room temperature phosphate coating composition |
JPS4928539A (ja) * | 1972-07-12 | 1974-03-14 |
Family Cites Families (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2160061A (en) * | 1936-12-12 | 1939-05-30 | Carbide & Carbon Chem Corp | Vinyl resin coatings and process producing the same |
US2298280A (en) * | 1939-02-02 | 1942-10-13 | Parker Rust Proof Co | Treatment of metal |
US2327885A (en) * | 1939-05-13 | 1943-08-24 | Remington Arms Co Inc | Ammunition manufacture |
US2702768A (en) * | 1948-07-23 | 1955-02-22 | Parker Rust Proof Co | Ferrous surface coating process using alkali metal phosphates and hydroxylamines |
-
1972
- 1972-07-27 US US00275620A patent/US3839099A/en not_active Expired - Lifetime
-
1973
- 1973-06-21 CA CA174,655A patent/CA980222A/en not_active Expired
- 1973-07-23 JP JP8349573A patent/JPS5325296B2/ja not_active Expired
- 1973-07-25 GB GB3536673A patent/GB1428857A/en not_active Expired
- 1973-07-27 FR FR7327643A patent/FR2194801B1/fr not_active Expired
Patent Citations (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2327127A (en) * | 1940-02-26 | 1943-08-17 | Frank E Rath | Stain and corrosion resistant tin surface and method of producing the same |
US2312855A (en) * | 1940-09-07 | 1943-03-02 | Parker Rust Proof Co | Method of coating aluminum |
US2657156A (en) * | 1948-07-23 | 1953-10-27 | Parker Rust Proof Co | Phosphate coating composition and process |
US2665231A (en) * | 1949-06-17 | 1954-01-05 | Parker Rust Proof Co | Coating process with alkali metal phosphate and added fluoride salt |
US3152018A (en) * | 1961-11-01 | 1964-10-06 | Wyandotte Chemicals Corp | Room temperature phosphate coating composition |
JPS4928539A (ja) * | 1972-07-12 | 1974-03-14 |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5253739A (en) * | 1975-10-30 | 1977-04-30 | Nippon Steel Corp | Surface treatment of galvanized steel |
JPS52131937A (en) * | 1976-04-05 | 1977-11-05 | Amchem Prod | Solution for coating metal surface |
JPS5633468B2 (ja) * | 1976-04-05 | 1981-08-04 | ||
JPS54100944A (en) * | 1978-01-27 | 1979-08-09 | Toyo Kohan Co Ltd | Electroplating tin plate for seamless can |
JPS5562179A (en) * | 1978-10-30 | 1980-05-10 | Nippon Parkerizing Co Ltd | Chemical treating solution for coating metal surface |
JPS574708B2 (ja) * | 1978-10-30 | 1982-01-27 |
Also Published As
Publication number | Publication date |
---|---|
GB1428857A (en) | 1976-03-17 |
DE2338290B2 (de) | 1977-05-26 |
US3839099A (en) | 1974-10-01 |
FR2194801A1 (ja) | 1974-03-01 |
FR2194801B1 (ja) | 1975-08-22 |
CA980222A (en) | 1975-12-23 |
JPS5325296B2 (ja) | 1978-07-26 |
DE2338290A1 (de) | 1974-02-07 |