JPH0716962U - Name plate material for back engraving - Google Patents

Name plate material for back engraving

Info

Publication number
JPH0716962U
JPH0716962U JP5258093U JP5258093U JPH0716962U JP H0716962 U JPH0716962 U JP H0716962U JP 5258093 U JP5258093 U JP 5258093U JP 5258093 U JP5258093 U JP 5258093U JP H0716962 U JPH0716962 U JP H0716962U
Authority
JP
Japan
Prior art keywords
acrylic plate
grooves
nameplate
main surface
paint layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP5258093U
Other languages
Japanese (ja)
Inventor
篤緒 橋本
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to JP5258093U priority Critical patent/JPH0716962U/en
Publication of JPH0716962U publication Critical patent/JPH0716962U/en
Pending legal-status Critical Current

Abstract

(57)【要約】 【目的】 銘板の製造効率を向上させる。 【構成】 対向する第1及び第2の主表面を有する透明
アクリル板32の裏面全域に塗料層34を形成し、第1の主
表面にアクリル板32の縁部に平行に複数の溝40を形成
し、これらに直交するように複数の溝42を形成し、第2
の主表面に溝40、42とほぼ対応する位置に複数の溝36、
38を形成してある。
(57) [Summary] [Purpose] To improve the manufacturing efficiency of nameplates. [Structure] A coating layer 34 is formed on the entire rear surface of a transparent acrylic plate 32 having first and second main surfaces facing each other, and a plurality of grooves 40 are formed on the first main surface in parallel with the edges of the acrylic plate 32. And a plurality of grooves 42 are formed so as to be orthogonal to these,
A plurality of grooves 36, at positions substantially corresponding to the grooves 40, 42 on the main surface of
38 has been formed.

Description

【考案の詳細な説明】[Detailed description of the device]

【0001】[0001]

【産業上の利用分野】[Industrial applications]

本考案は、各種機器に取り付け銘板を作成するために、銘が彫刻される銘板材 に関し、特に裏面から銘を彫刻する裏彫り用の銘板材に関する。 The present invention relates to a nameplate material on which a name is engraved in order to create a nameplate to be attached to various devices, and more particularly, to a nameplate material for engraving a name on the back side.

【0002】[0002]

【従来の技術】[Prior art]

従来、上記のような裏彫り用の銘板材2は、例えば図6に示すように必要とさ れる大きさの透明のアクリル板4の裏面に遮光性の塗料層6を形成したものであ る。このような裏彫り用の銘板材2は、例えば次のようにして製造される。まず 、図7に示すように、比較的大きな大きさの矩形の透明アクリル板8の裏面全域 に、遮光性の塗料例えば白色塗料を塗布して、塗料層10を形成する。次に、ア クリル板8の長辺に沿う仮想の切断線12、12・・・・に沿ってアクリル板8 を鋸で短冊状体8aに切断する。これら短冊状体8aの長辺を鉋で仕上げる。最 後に、これら短冊状体8aを、その短辺に沿う仮想の切断線14、14・・・・ に沿って鋸で切断する。 Conventionally, the nameplate material 2 for back engraving as described above is one in which a light-shielding paint layer 6 is formed on the back surface of a transparent acrylic plate 4 of a required size as shown in FIG. 6, for example. . The nameplate material 2 for such a back engraving is manufactured as follows, for example. First, as shown in FIG. 7, a light-shielding paint such as a white paint is applied to the entire rear surface of a rectangular transparent acrylic plate 8 having a relatively large size to form a paint layer 10. Next, the acrylic plate 8 is cut with a saw along the virtual cutting lines 12, 12 ... Along the long side of the acrylic plate 8 into strips 8a. The long sides of these strips 8a are finished with a plane. Finally, the strip-shaped bodies 8a are sawn along the virtual cutting lines 14, 14 ...

【0003】 このようにして製造された銘板材2は、図9に示すように、彫刻機16の真空 吸着テーブル18上に一枚ずつ塗料層6が上面となるように配置、固定される。 なお、図9では、銘板材2を一枚ずつ配置していることを表すために、吸着テー ブル18上に間隔をあけて各銘板材2を配置しているように描いてあるが、実際 には各銘板材2は、間隔をあけずに敷きつめられている。このように配置、固定 された後、カッター部20を矢印X方向に、真空吸着テーブル18を矢印Y方向 に移動させることによって、所望の文字を塗料層6に彫刻する。この際、彫刻さ れる文字は、アクリル板4の表面側から見て、正しく読めるように裏文字とされ ている。この彫刻の終了後、銘板材2の塗料層6に、例えば黒色の塗料を塗布す ることによって、彫刻部分に墨入れし、その後に、不要な黒色塗料を拭き取って 、銘板が完成する。As shown in FIG. 9, the name plate materials 2 thus manufactured are arranged and fixed one by one on the vacuum suction table 18 of the engraving machine 16 so that the paint layers 6 are on the upper surface. In FIG. 9, in order to show that the nameplate materials 2 are arranged one by one, the nameplate materials 2 are illustrated as being arranged on the suction table 18 at intervals. The nameplate materials 2 are laid on each other with no space. After being arranged and fixed in this way, a desired character is engraved on the paint layer 6 by moving the cutter portion 20 in the arrow X direction and moving the vacuum suction table 18 in the arrow Y direction. At this time, the engraved letters are reverse letters so that they can be read correctly when viewed from the front side of the acrylic plate 4. After completion of this engraving, the paint layer 6 of the nameplate material 2 is black-painted, for example, by applying black paint, and then unnecessary black paint is wiped off to complete the nameplate.

【0004】[0004]

【考案が解決しようとする課題】[Problems to be solved by the device]

このような銘板材2では、彫刻を施す際に、彫刻機16の真空吸着テーブル1 8に、一枚ずつ配置しなければならず、その上、一枚ずつ所望通りに文字が彫刻 されているか検査しなければならず、作業効率が低いという問題点があった。 In such a name plate material 2, when engraving, one by one must be arranged on the vacuum suction table 18 of the engraving machine 16, and moreover, one by one, the characters are engraved as desired. It had to be inspected, and there was a problem that work efficiency was low.

【0005】 このような問題点は、例えば図7に示すような各銘板材2に形成する前のアク リル板8に塗料層10を形成しただけの状態で、彫刻、墨入れ、拭き取り、検査 を行ない、その後に各銘板材2となるように切断及び仕上げを行えば、解決でき る。しかし、アクリル板8には塗料層10が形成されているだけであるので、切 断しにくい上に、切断の際に塗料層10の一部が剥離し、商品価値が低下すると いう新たな問題が発生する。Such a problem is engraved, blackened, wiped, and inspected in a state where the paint layer 10 is simply formed on the acrylic plate 8 before being formed on each nameplate material 2 as shown in FIG. 7, for example. The problem can be solved by carrying out the above, and then cutting and finishing so that each nameplate material 2 is obtained. However, since only the paint layer 10 is formed on the acrylic plate 8, it is difficult to cut, and a part of the paint layer 10 peels off at the time of cutting, which reduces the commercial value. Occurs.

【0006】[0006]

【課題を解決するための手段】[Means for Solving the Problems]

上記の問題点を解決するために、本考案は、対向する第1及び第2の主表面を 有する透明アクリル板と、このアクリル板の第1の主表面全域に形成された不透 明塗料層と、第1の主表面に上記アクリル板の縁部に平行に形成された複数の第 1の溝と、第2の主表面に各第1の溝とほぼ対応する位置に形成された複数の第 2の溝とを、具備するものである。 In order to solve the above problems, the present invention provides a transparent acrylic plate having first and second main surfaces facing each other, and an opaque coating layer formed on the entire first main surface of the acrylic plate. A plurality of first grooves formed on the first main surface in parallel to the edge of the acrylic plate, and a plurality of first grooves formed on the second main surface at positions substantially corresponding to the respective first grooves. And a second groove.

【0007】[0007]

【作用】[Action]

本考案によれば、アクリル板の第1及び第2の主表面における対応する位置に 第1及び第2の溝が形成されているので、これら第1及び第2の溝に完全に沿っ て折ることができる。しかも、第1の溝は、塗料層が設けられている第1の主表 面に設けられているので、これら第1の溝には塗料が付着していない。従って、 折った際に、塗料が剥離することはない。 According to the present invention, the first and second grooves are formed at the corresponding positions on the first and second main surfaces of the acrylic plate, so that the first and second grooves are completely folded. be able to. Moreover, since the first groove is provided on the first main surface on which the paint layer is provided, the paint is not attached to these first grooves. Therefore, the paint does not peel off when folded.

【0008】[0008]

【実施例】【Example】

この実施例による銘板材30は、図1に示すように透明なアクリル板32を有 している。このアクリル板32は、例えば550X700X2mmの大きさの長 方形状のもので、その裏面全面に例えば30乃至40μmの厚さの白色塗料層3 4が形成されている。 The name plate material 30 according to this embodiment has a transparent acrylic plate 32 as shown in FIG. The acrylic plate 32 has a rectangular shape having a size of 550 × 700 × 2 mm, for example, and a white paint layer 34 having a thickness of, for example, 30 to 40 μm is formed on the entire back surface thereof.

【0009】 このアクリル板32の表面には、その一方の辺に平行に複数のV字状の溝36 が形成されている。また、これら溝36に直交するようにV字状の溝38が形成 されている。これらV字状の溝36間の距離、及び同38間の距離は、これら溝 36、38によって区画される各領域が所望の銘板材の大きさとなるように、選 択されている。これらV字状の溝36、38は、例えば深さが約0.7乃至1m mで、図1に示す角度θが約35乃至45度に形成されている。On the surface of the acrylic plate 32, a plurality of V-shaped grooves 36 are formed parallel to one side thereof. Further, a V-shaped groove 38 is formed so as to be orthogonal to these grooves 36. The distance between the V-shaped grooves 36 and the distance between the V-shaped grooves 36 are selected so that each region defined by the grooves 36, 38 has a desired size of a nameplate material. These V-shaped grooves 36 and 38 are, for example, about 0.7 to 1 mm deep and are formed with an angle θ shown in FIG. 1 of about 35 to 45 degrees.

【0010】 また、アクリル板32の裏面には、表面に設けたV字状の溝36と同じ位置に V字状の溝40が形成されており、同様にV字状の溝38と同じ位置にV字状の 溝42が形成されている。これらV字状の溝40、42は、例えば深さが約0. 1mmで、図1に示す角度φが約35乃至45度に形成されている。これらV字 状の溝40、42の形成場所からは、塗料層34の塗料が剥離されている。Further, a V-shaped groove 40 is formed on the back surface of the acrylic plate 32 at the same position as the V-shaped groove 36 provided on the front surface, and similarly at the same position as the V-shaped groove 38. A V-shaped groove 42 is formed in the. These V-shaped grooves 40, 42 have a depth of about 0. 1 mm, the angle φ shown in FIG. 1 is formed to be about 35 to 45 degrees. The paint of the paint layer 34 is peeled off from the places where the V-shaped grooves 40 and 42 are formed.

【0011】 このような銘板材は、例えば次のようにして製造される。先ず、図2(a)に 示すようにアクリル板32を準備し、その裏面側を荒らし、塗料の付着が良好と なる状態として、図2(b)に示すように裏面全域に塗料層34を付着させる。Such a name plate material is manufactured, for example, as follows. First, as shown in FIG. 2 (a), an acrylic plate 32 is prepared, and the back surface side thereof is roughened so that the paint can be adhered well. As shown in FIG. 2 (b), a paint layer 34 is formed over the entire back surface. Attach it.

【0012】 次に、このアクリル板32の隅部の予め定めた位置に、このアクリル板32の 中心線に対称に位置決め用の孔44、44を穿つ。続いて、例えばアクリル板3 2の表面側が上になるように、かつ位置決め用の孔44、44を図2(c)に示 すように切削機上に設けた位置決め用の支柱に挿通することによって、アクリル 板32の位置決めを行い、V字状の溝36、38をそれぞれ切削する。Next, positioning holes 44, 44 are formed at predetermined positions at the corners of the acrylic plate 32 symmetrically with respect to the center line of the acrylic plate 32. Then, for example, insert the positioning holes 44, 44 so that the surface side of the acrylic plate 32 faces upward and the positioning columns provided on the cutting machine as shown in FIG. 2 (c). Then, the acrylic plate 32 is positioned and the V-shaped grooves 36 and 38 are cut.

【0013】 次に、アクリル板32を裏返して、即ち、塗料層34が上側になるようにして 、位置決め用の孔44、44を位置決め用の支柱に挿通する。そして、V字状の 溝36、38を切削したときと同様に切削機を動作させることによって、V字状 の溝42、44を切削する。これによって、V字状の溝36と42、V字状の溝 38と44とは、アクリル板32の表裏における同じ位置に形成される。なお、 位置決め用の孔44をアクリル板32に穿ったが、図2(c)に点線で示すよう に、切削機に当たりを形成し、これを用いてもよい。Next, the acrylic plate 32 is turned upside down, that is, the paint layer 34 is on the upper side, and the positioning holes 44, 44 are inserted into the positioning columns. Then, the V-shaped grooves 42 and 44 are cut by operating the cutting machine in the same manner as when cutting the V-shaped grooves 36 and 38. As a result, the V-shaped grooves 36 and 42 and the V-shaped grooves 38 and 44 are formed at the same positions on the front and back of the acrylic plate 32. Although the positioning hole 44 is formed in the acrylic plate 32, a contact may be formed in the cutting machine as shown by the dotted line in FIG. 2C, and this may be used.

【0014】 このようにして製造された銘板材30は、図3に示すように彫刻機16の真空 吸着テーブル18上に、塗料層34が上面となるように配置され、V字状の溝4 2、44で区画された領域を1単位領域として、各単位領域ごとに文字を彫刻す る。この彫刻は、カッター部20をX方向に、真空吸着テーブル18をY方向に それぞれ移動させることによって行われる。The name plate material 30 manufactured as described above is arranged on the vacuum suction table 18 of the engraving machine 16 so that the paint layer 34 is on the upper surface as shown in FIG. Characters are engraved in each unit area with the area divided by 2, 44 as one unit area. This engraving is performed by moving the cutter unit 20 in the X direction and the vacuum suction table 18 in the Y direction.

【0015】 各単位領域への彫刻がそれぞれ終了すると、真空吸着テーブル18から銘板材 30を取り外し、各単位領域の彫刻部分それぞれに黒色塗料を塗布することによ って、墨入れを行う。その後、塗料層34の面から不要な黒色塗料を拭き取る。When the engraving on each unit area is completed, the nameplate material 30 is removed from the vacuum suction table 18, and black paint is applied to each engraved portion of each unit area to carry out inking. After that, unnecessary black paint is wiped off from the surface of the paint layer 34.

【0016】 次に、図4(a)に示すように銘板材30の塗料層34側に両面接着テープ4 6を貼着し、この両面接着テープ46に溝40、42に沿って筋48を入れ、こ れら筋48に沿って銘板材30を折る。これによって、銘板が完成する。Next, as shown in FIG. 4 (a), a double-sided adhesive tape 46 is attached to the paint layer 34 side of the name plate material 30, and the double-sided adhesive tape 46 is provided with streaks 48 along the grooves 40 and 42. Insert and fold the nameplate material 30 along these lines 48. This completes the nameplate.

【0017】 銘板材30の表面側だけでなく、裏面側にも溝42、44が、表面側の溝36 、38と同じ位置に設けられているので、折る際には容易に折れるし、その折っ た面が荒れることはない。しかも、裏面側の溝42、44には塗料が付着してい ないので、塗料が剥離することもない。Since the grooves 42, 44 are provided not only on the front surface side of the nameplate material 30 but also on the back surface side thereof at the same positions as the grooves 36, 38 on the front surface side, they easily break when folded, and The folded surface does not get rough. Moreover, since the coating material is not attached to the grooves 42 and 44 on the rear surface side, the coating material does not peel off.

【0018】 なお、この折る際に、図5に示すように、先ず各銘板の短辺に対応する溝36 、40に沿って折り、各銘板の短辺が一列に連なった状態にすれば、各銘板それ ぞれにばらばらにした後では鉋掛けのしにくい、各短辺部分も容易に鉋掛けを行 うことができる。At the time of folding, as shown in FIG. 5, first, by folding along the grooves 36, 40 corresponding to the short sides of each nameplate, the short sides of each nameplate are arranged in a line. It is difficult to hook each name plate into pieces, and each short side can be hooked easily.

【0019】 上記の実施例では、アクリル板の表面側は、露出した状態のままとしたが、彫 刻、墨入れ、拭き取り等の作業中に、アクリル板の表面に傷がつかないように、 薄膜のマスク材をアクリル板の表面に圧着してもよい。また、上記の実施例では 、アクリル板32の表側には溝36、38を、裏面側には溝40、42をそれぞ れ形成したが、例えばアクリル板32の表側には溝36だけを、裏面側には溝4 0だけを設けてもよいし、アクリル板32の表側には溝38だけを、裏面側には 溝42だけを設けてもよい。In the above embodiments, the surface side of the acrylic plate was left exposed, but during the work such as engraving, inking, wiping, etc., the surface of the acrylic plate should not be scratched. A thin film mask material may be pressed onto the surface of the acrylic plate. Further, in the above embodiment, the grooves 36 and 38 are formed on the front side of the acrylic plate 32, and the grooves 40 and 42 are formed on the back surface side, respectively. However, for example, only the groove 36 is formed on the front side of the acrylic plate 32. Only the groove 40 may be provided on the back side, only the groove 38 may be provided on the front side of the acrylic plate 32, and only the groove 42 may be provided on the back side.

【0020】[0020]

【考案の効果】[Effect of device]

以上のように、本考案によれば、透明アクリル板の第1の主表面全域に不透明 塗料層を形成し、第1の主表面にアクリル板の縁部に平行に複数の第1の溝を形 成し、第1の主表面に対向する第2の主表面に各第1の溝とほぼ対応する位置に 複数の第2の溝を形成してあるので、銘板を作成するために折った場合にも、折 りやすい上に、その折り面が荒れることが少ない。しかも、折った際に、塗料層 から塗料が剥離することがなく、銘板の商品価値が低下することもない。その上 、彫刻、拭き取り、検査を一枚の大きな板の状態の銘板材に対して行った後、各 溝に沿って折ることによって、各銘板を作成することができるので、製造効率を 向上させることができる。 As described above, according to the present invention, the opaque paint layer is formed on the entire area of the first main surface of the transparent acrylic plate, and the plurality of first grooves are formed on the first main surface parallel to the edge of the acrylic plate. Formed and formed with a plurality of second grooves at positions substantially corresponding to the respective first grooves on the second main surface opposite to the first main surface. Therefore, the second main surface was folded to form a nameplate. In that case, it is easy to fold and the fold surface is not rough. Moreover, the paint does not peel off from the paint layer when it is folded, and the commercial value of the nameplate does not decrease. In addition, after engraving, wiping, and inspecting the nameplate material in the state of one large plate, each nameplate can be created by folding it along each groove, improving manufacturing efficiency. be able to.

【図面の簡単な説明】[Brief description of drawings]

【図1】本考案による銘板材の1実施例の部分省略斜視
図である。
FIG. 1 is a partially omitted perspective view of an embodiment of a nameplate material according to the present invention.

【図2】同実施例の製造工程を示す図である。FIG. 2 is a diagram showing a manufacturing process of the embodiment.

【図3】同実施例の銘板材に彫刻をしている状態の斜視
図である。
FIG. 3 is a perspective view showing a state where a nameplate material of the embodiment is engraved.

【図4】同実施例の銘板材を折るための準備段階の工程
図である。
FIG. 4 is a process drawing of a preparatory stage for folding the name plate material of the same example.

【図5】同実施例の銘板材を折った状態の斜視図であ
る。
FIG. 5 is a perspective view showing a state in which the nameplate material of the embodiment is folded.

【図6】従来の銘板材の斜視図である。FIG. 6 is a perspective view of a conventional nameplate material.

【図7】従来の銘板材の製造の1過程を示す図である。FIG. 7 is a diagram showing one process of manufacturing a conventional nameplate material.

【図8】従来の銘板材の製造の他の過程を示す図であ
る。
FIG. 8 is a diagram showing another process of manufacturing a conventional nameplate material.

【図9】従来の銘板材に彫刻をしている状態の斜視図で
ある。
FIG. 9 is a perspective view showing a state in which a conventional nameplate material is engraved.

【符号の説明】[Explanation of symbols]

32 アクリル板 34 塗料層 36 38 第2の溝 40 42 第1の溝 32 acrylic plate 34 paint layer 36 38 second groove 40 42 first groove

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] 【請求項1】 対向する第1及び第2の主表面を有する
透明アクリル板と、このアクリル板の第1の主表面全域
に形成された不透明塗料層と、第1の主表面に上記アク
リル板の縁部に平行に形成された複数の第1の溝と、第
2の主表面に各第1の溝とほぼ対応する位置に形成され
た複数の第2の溝とを、具備する裏彫り用銘板材。
1. A transparent acrylic plate having first and second main surfaces facing each other, an opaque paint layer formed on the entire area of the first main surface of the acrylic plate, and the acrylic plate on the first main surface. Having a plurality of first grooves formed parallel to the edges of the first groove and a plurality of second grooves formed on the second main surface at positions substantially corresponding to the respective first grooves. Name plate material.
JP5258093U 1993-09-01 1993-09-01 Name plate material for back engraving Pending JPH0716962U (en)