JPH0716590Y2 - Paper liquid container - Google Patents
Paper liquid containerInfo
- Publication number
- JPH0716590Y2 JPH0716590Y2 JP1988010834U JP1083488U JPH0716590Y2 JP H0716590 Y2 JPH0716590 Y2 JP H0716590Y2 JP 1988010834 U JP1988010834 U JP 1988010834U JP 1083488 U JP1083488 U JP 1083488U JP H0716590 Y2 JPH0716590 Y2 JP H0716590Y2
- Authority
- JP
- Japan
- Prior art keywords
- spout
- folding piece
- adhesive layer
- cut
- adhesive
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Description
【考案の詳細な説明】 [産業上の利用分野] この考案は、牛乳やジュース等を収納する容器であっ
て、特にゲーベルトップと称される紙製液体容器に関す
るものである。DETAILED DESCRIPTION OF THE INVENTION [Industrial field of application] The present invention relates to a container for storing milk, juice and the like, and particularly to a liquid container made of paper called a gobel top.
[従来の技術] この種の液体収納容器は、頂部が切妻型の屋根のように
形成されており、開口するときにはその合掌状態に接合
された封着部の一方の端部の合わせ目を剥すと共に、封
着部の中央部まで引き剥がして折込片を平面状態に押し
拡げ、更にその折込片の上部の両端部を後方に押しなが
ら上縁の中央を押し出すように剥離させ、引き続き折込
片の両端部まで剥離させて折込片の接着層を完全に剥す
共に、その折込片の両端部を窄めるようにして中央部を
三角形に突出させて注出口を形成出来るようにしてあ
る。[Prior Art] This type of liquid storage container has a top portion formed like a gable-shaped roof, and when the liquid storage container is opened, the seam at one end of the sealing portion joined to the gas palm is removed. At the same time, peel off to the central part of the sealing part and push the folding piece into a flat state, and further push back both ends of the upper part of the folding piece to push it out so that the center of the upper edge is pushed out, and then continue to Both ends are peeled off to completely peel off the adhesive layer of the folded piece, and both ends of the folded piece are closed so that the center portion is triangularly projected to form a spout.
[考案が解決しようとする課題] 前記のような液体容器の開口に際しては、封着部の引き
剥しを中央部まで完全に行わないと、折込片の上縁の中
央を押し出す剥離作業が円滑にいかず、指を引っ掛けて
強引にこじあけることが往々にしてある。これは不衛生
であるばかりでなく、折込片の上縁中央部が破れて注出
作業がし難くなる。また、折込片の剥離が円滑にいった
としても、その折込片の上縁に剥がれた接着層の一部が
付着しているので不潔な感じを与える。[Problems to be Solved by the Invention] When opening the liquid container as described above, the peeling work of pushing out the center of the upper edge of the folding piece should be smooth unless the sealing portion is completely peeled off to the central portion. It is often the case that people use their fingers to force them to pry open. This is not only unsanitary, but also the center part of the upper edge of the folding piece is torn, which makes the pouring work difficult. Even if the folded piece is smoothly peeled off, a part of the peeled adhesive layer is attached to the upper edge of the folded piece, which gives a feeling of being unclean.
このような欠点を防止するために注出口となる折込片の
上部にスリットを設けたもの(例えば、実開昭52-62224
号公報、実公昭45-32525号公報)があるが、スリットが
不連続であったり、スリットの位置が不適当であったり
して必ずしも満足すべき結果が得られるものではない。In order to prevent such a defect, a slit is provided on the upper part of the folding piece serving as the spout (for example, Japanese Utility Model Laid-Open No. 52-62224).
However, the slits are discontinuous and the positions of the slits are not appropriate, so that satisfactory results cannot always be obtained.
本考案は、以上のような従来の種々の問題点を技術的に
解決することを課題として成されたものである。The present invention has been made with the object of technically solving the above-described various conventional problems.
[課題を解決するための手段] その課題を解決する手段として、本考案は、開閉自在の
注出口を有する頂部を切妻型とした熱接着性プラスチッ
クフィルムラミネート紙製容器において、前記注出口と
なる折込片4の上端部の外面側は両端部が接着層4aでそ
の間に挟まれた部分は非接着層4bに形成され、この非接
着層4bには注出口の上縁となるほぼ横長U字型の半切L
が表側から形成され、前記折込片4の上端部の内面側は
一定の幅で接着層4cが形成され、その下縁に沿って半切
Mが前記半切Lに関連させて若干位置をずらして裏側か
ら形成されたことを要旨とするものである。[Means for Solving the Problem] As a means for solving the problem, the present invention provides a thermal adhesive plastic film laminated paper container having a gable top with an openable and closable spout serving as the spout. On the outer surface side of the upper end portion of the folding piece 4, both ends are sandwiched between the adhesive layers 4a and the non-adhesive layer 4b is formed, and the non-adhesive layer 4b has a substantially horizontal U-shape serving as the upper edge of the spout. Mold half-cut L
Is formed from the front side, and an adhesive layer 4c is formed on the inner surface side of the upper end portion of the folding piece 4 with a constant width, and the half cut M is displaced along the lower edge thereof in relation to the half cut L and the back side is formed. It is made up of the following.
[作用] 注出口の形成において、折込片を拡げてその両端部を窄
めると半切に沿って層間剥離が生じ、その部分が切れて
注出口を形成することができ、かつ注出口の上縁は接着
層のカスが付着せずに綺麗な状態となる。[Function] In forming the spout, if the folding piece is expanded and both ends thereof are closed, delamination occurs along the half-cut, and the part can be cut to form the spout, and The edges are in a clean state without the dust of the adhesive layer attached.
[実施例] 以下、図示の実施例によって本考案を具体的に説明す
る。[Embodiment] Hereinafter, the present invention will be described in detail with reference to the illustrated embodiment.
1は容器本体を構成する側板であり、横に4枚並設され
ると共にそれらの上縁には容器の頂部を形成する一対の
天板2、3と折込片4、5が交互に連設されている。こ
のようなブランクは、従来と同様に熱接着性プラスチッ
クフィルムラミネート紙で一体成形される。6は一方の
端縁に設けられた糊代である。前記天板2、3の上縁に
は互いに合掌状態に接着される封止片2a、3aが形成さ
れ、前記折込片4の上端部の外面は両端部が接着層4aに
形成されると共に、その接着層に挟まれた部分は剥離ニ
スを塗布することによって非接着層4bに形成され、この
非接着層の部分に注出口の上縁となるほぼ横長U字型の
半切Lが表側から形成されている。また、この折込片4
の上端部の内面側は、一定の幅で接着層4cが形成され、
その下縁に沿って半切Mが前記半切Lに関連させて若干
位置をずらせて裏側(内面側)から形成されている。Reference numeral 1 is a side plate that constitutes the container body. Four side plates are arranged side by side, and a pair of top plates 2 and 3 and folding pieces 4 and 5 that form the top of the container are alternately arranged at their upper edges. Has been done. Such a blank is integrally molded with a heat-adhesive plastic film laminated paper as in the conventional case. 6 is a glue margin provided on one edge. Sealing pieces 2a and 3a are formed on the upper edges of the top plates 2 and 3 so as to be bonded to each other in a palm-like manner. The part sandwiched between the adhesive layers is formed on the non-adhesive layer 4b by applying a release varnish, and a substantially horizontal U-shaped half-cut L which is the upper edge of the spout is formed on the non-adhesive layer part from the front side. Has been done. Also, this folding piece 4
On the inner surface side of the upper end of the adhesive layer 4c is formed with a constant width,
A half-cut M is formed along the lower edge thereof from the back side (inner surface side) with a slight displacement in relation to the half-cut L.
本考案に係る紙製容器は上記のように形成され、前記糊
代6をその糊代と反対側の側板1の端部に接着して角筒
状の容器本体を形成すると共に、前記折込片4、5を折
り込み、前記天板2、3の封止片2a、3aを合掌状態に接
着することによって切妻型の頂部を形成できるようにな
っている。このとき、前記折込片4の上端部の外面側
は、前記接着層4aにより両端部のみが相互に自己接着さ
れる。The paper container according to the present invention is formed as described above, and the gluing margin 6 is adhered to the end of the side plate 1 on the opposite side of the gluing margin to form a rectangular tube-shaped container body, and the folding piece is also provided. The gabled tops can be formed by folding in 4 and 5 and adhering the sealing pieces 2a and 3a of the top plates 2 and 3 in a palmed-up state. At this time, only the both ends of the outer surface of the upper end of the folding piece 4 are self-bonded to each other by the adhesive layer 4a.
この紙製容器を開口するには、従来と同様にまず合掌状
態に接合された封着部の一方の端部の合わせ目及び折込
片4の合わせ目を剥すと共に、封着部の中央部まで引き
剥がして折込片4を平面状態に押し拡げる。次に、折込
片4の両端部を窄めてその中央部を押し出すようにする
と、第7図に示すように前記表裏の半切L、Mにより折
込片4の上端部に層間剥離が生じ、半切Lを上縁とする
三角形の注出口を形成することができる。この注出口の
上縁は、表裏いずれも接着層が全然付着していないので
極めて清潔である。In order to open this paper container, first remove the seam of one end of the sealing part and the seam of the folding piece 4 which are joined in a palm-like state as in the conventional case, and reach the center of the sealing part. It is peeled off and the folding piece 4 is pushed and spread in a flat state. Next, when both ends of the folding piece 4 are narrowed and the central portion thereof is pushed out, as shown in FIG. 7, delamination occurs at the upper end of the folding piece 4 due to the half cuts L and M on the front and back sides, and the half cut is made. A triangular spout with L as the top edge can be formed. The upper edge of this spout is extremely clean because no adhesive layer is attached to either the front or back.
また、折込片4の非接着層4bの部分は、その内面側が前
記封止片2a、3aの内面側に接着されているので、前記の
ように注出口を形成した際に層間剥離が生じた部分と共
にそのまま残留することになる。尚、内容物である液体
の注出後に再封するには、従来と同様に注出口を折り込
むようにして折込片4を元の状態に戻せば良い。Further, since the inner surface side of the non-adhesive layer 4b of the folding piece 4 is adhered to the inner surface side of the sealing pieces 2a and 3a, delamination occurs when the spout is formed as described above. It will remain as it is with the part. In addition, in order to reseal the liquid as the content after being poured out, the folding piece 4 may be returned to the original state by folding the pouring port as in the conventional case.
[考案の効果] 以上説明したように、この考案によれば、ゲーベルトッ
プ型の紙製液体容器を開口する際に、注出口となる折込
片の両端部を窄めることにより半切を上縁とする注出口
が形成されるようにしたので、開口作業が非常に簡単で
あると共に、注出口の上縁には接着層の剥離カスが付着
しないので、極めて清潔である等の優れた効果を奏す
る。[Effects of the Invention] As described above, according to the present invention, when opening a Gobel-top type liquid container made of paper, both ends of the folding piece serving as a spout are closed so that the upper edge of the half-section is cut off. Since the spout to be formed is formed, the opening work is very easy, and since the peeling residue of the adhesive layer does not adhere to the upper edge of the spout, it has an excellent effect such as being extremely clean. Play.
第1図は本考案に係る紙製容器の要部の展開図、第2図
は組み立てられた紙製容器の頂部の斜視図、第3図はそ
の頂部の接着状態を示す説明図、第4図は折込片を拡げ
た状態での頂部の斜視図、第5図はそのときの頂部の状
態を示す説明図、第6図は同じく折込片の正面図、第7
図は注出口を形成したときの頂部の斜視図、第8図はそ
のときの頂部の状態を示す説明図である。 1……側板、2、3……天板 4……折込片、4a……接着層 4b……非接着層、4c……接着層 5……折込片、6……糊代 L、M……半切FIG. 1 is a development view of essential parts of a paper container according to the present invention, FIG. 2 is a perspective view of a top part of an assembled paper container, and FIG. 3 is an explanatory view showing a bonding state of the top part. FIG. 5 is a perspective view of the top portion when the folding piece is expanded, FIG. 5 is an explanatory view showing the state of the top portion at that time, and FIG. 6 is a front view of the folding piece, and FIG.
The figure is a perspective view of the top when the spout is formed, and FIG. 8 is an explanatory view showing the state of the top at that time. 1 ... Side plate, 2, 3 ... Top plate 4 ... Folding piece, 4a ... Adhesive layer 4b ... Non-adhesive layer, 4c ... Adhesive layer 5 ... Folding piece, 6 ... Glue margin L, M ... … Half cut
Claims (1)
した熱接着性プラスチックフィルムラミネート紙製容器
において、前記注出口となる折込片4の上端部の外面側
は両端部が接着層4aでその間に挟まれた部分は非接着層
4bに形成され、この非接着層4bには注出口の上縁となる
ほぼ横長U字型の半切Lが表側から形成され、前記折込
片4の上端部の内面側は一定の幅で接着層4cが形成さ
れ、その下縁に沿って半切Mが前記半切Lに関連させて
若干位置をずらして裏側から形成されたことを特徴とす
る紙製液体容器。1. A thermo-adhesive plastic film laminated paper container having a gable top with an openable / closable spout, and both ends of the outer surface of the upper end of the folding piece 4 serving as the spout are adhesive layers 4a. The part sandwiched between is the non-adhesive layer
The non-adhesive layer 4b is formed with a substantially horizontal U-shaped half-cut L as the upper edge of the spout from the front side, and the inner surface side of the upper end of the folding piece 4 has a constant width. 4c is formed, and a half cut M is formed along the lower edge thereof from the back side with a slight shift in relation to the half cut L.