Prior art keywords
gap
molded body
boss
primary
resin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP32389691A
Other languages
Japanese (ja)
Other versions
JPH07119026B2 (en
Inventor
Hiroshi Okutomi
博 奥富
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
KASHIO SEIMITSU KK
Nikko Kogyo KK
Original Assignee
KASHIO SEIMITSU KK
Nikko Kogyo KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by KASHIO SEIMITSU KK, Nikko Kogyo KK filed Critical KASHIO SEIMITSU KK
Priority to JP32389691A priority Critical patent/JPH07119026B2/en
Publication of JPH06270190A publication Critical patent/JPH06270190A/en
Publication of JPH07119026B2 publication Critical patent/JPH07119026B2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Classifications

    • HELECTRICITY
    • H01ELECTRIC ELEMENTS
    • H01HELECTRIC SWITCHES; RELAYS; SELECTORS; EMERGENCY PROTECTIVE DEVICES
    • H01H2229/00Manufacturing
    • H01H2229/044Injection moulding
    • H01H2229/046Multi-colour or double shot injection moulding

Landscapes

  • Moulds For Moulding Plastics Or The Like (AREA)
  • Injection Moulding Of Plastics Or The Like (AREA)
  • Manufacture Of Switches (AREA)

Abstract

PURPOSE:To provide a primary molding which can uniformly transmit light, even with a blocked area present within indicating parts, and to manufacture two-color-products by a simple process. CONSTITUTION:A gap 12 which becomes an indicating part is formed with light-transmitting resin having been poured, and the gap surrounds a blocked area 14 to constitute a key-top, and the peripheral area 16 which surrounds the gap 12 and the blocked area 14 are connected by a boss 30 which crosses the gap.

Description

【発明の詳細な説明】Detailed Description of the Invention

【0001】[0001]

【産業上の利用分野】この発明は、1次モールド成形体
およびこれを用いた2色モールド成形品の製造方法に関
するものである。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a primary molded article and a method for producing a two-color molded article using the same.

【0002】[0002]

【従来の技術】従来から、キーボードやタイプライタの
入力媒体となるキートップのように、入出力情報を目視
によって確認する手段として、文字、数字、符号等の表
示部を表面に有した樹脂モールド成形体である2色モー
ルド成形品が汎用されている。
2. Description of the Related Art Conventionally, a resin mold having a display portion of characters, numbers, symbols, etc. on its surface has been used as a means for visually confirming input / output information like a key top which is an input medium of a keyboard or a typewriter. A two-color molded product that is a molded product is widely used.

【0003】この2色モールド成形品を製造するに際し
ては、先ず、表示部を上面に突出形成した1次モールド
成形体を形成する。次いで、1次モールド成形体の外側
に表示部の天面を露出させるようにして2次モールド成
形体を一体に成形することにより、キートップのような
2色モールド成形品を得ていた。
In manufacturing this two-color molded product, first, a primary molded product having a display portion protruding from the upper surface is formed. Then, the two-color molded product such as a key top was obtained by integrally molding the secondary molded product so that the top surface of the display portion was exposed to the outside of the primary molded product.

【0004】ところで、たとえば数字の「0」、アルフ
ァベットの「D」、符号の「△」のように、表示部の内
側に、表示部によって閉鎖的に囲まれた閉塞領域を有す
るものでは、この閉塞領域に2次モールド成形体の樹脂
を注入する必要がある。そこで、閉塞領域の周辺から表
示部の裏面を通過して当該閉塞領域に至る溝を形成し、
この溝を介して2次モールド成形体の樹脂を閉塞領域に
注入するようにしていた。
By the way, in the case where there is a closed region which is closed and enclosed by the display unit inside the display unit, such as the number "0", the alphabet "D", and the code "Δ", It is necessary to inject the resin of the secondary molded body into the closed area. Therefore, a groove is formed from the periphery of the closed area to the back surface of the display section to reach the closed area,
The resin of the secondary molded body is injected into the closed area through this groove.

【0005】しかながら、1次モールド成形体を透光性
樹脂で成形し、閉塞領域に不透性の2次モールド用樹脂
を注入して表示部を裏から照光させるような場合では、
表示部よりも光透過度の低い2次モールド成形体が表示
部の裏を通過する溝内で成形されるために、その部分が
影となって表示部を均一に照光できないと、いう問題が
あった。
However, in the case where the primary molded body is molded with a light-transmissive resin and the impermeable secondary molding resin is injected into the closed region to illuminate the display section from the back side,
Since the secondary molded body having a lower light transmittance than the display portion is molded in the groove passing through the back of the display portion, that portion becomes a shadow and the display portion cannot be uniformly illuminated. there were.

【0006】そこで、このような問題を解決するため
に、たとえば、特開昭62−279911号では、表示
部の閉塞領域とこの閉塞領域の外側とにおのおの形成さ
れた孔から樹脂を注入、成形し、かつ、これらの孔の間
に形成された表示部の突出部を切断することにより突出
部の下方に一体に成形された外形部材を除去することに
より、表示部内に閉塞領域が存在する場合であっても2
次モールド成形体の影が表示部に投影することなく均一
な表示が可能がキートップ等の2色モールド成形品を得
ることができること、が提案されている。
In order to solve such a problem, for example, in Japanese Patent Laid-Open No. 62-279911, a resin is injected and molded through holes formed in the closed area of the display portion and the outside of the closed area. In addition, by cutting the protruding portion of the display portion formed between these holes to remove the outer shape member integrally molded below the protruding portion, there is a closed area in the display portion. Even 2
It has been proposed that a two-color molded product such as a key top can be obtained by enabling uniform display without the shadow of the next molded product being projected on the display unit.

【0007】[0007]

【発明が解決しようとする課題】しかしながら、前記従
来例では、2色成形の最終段階で、極めて小さい突出部
を切断しなければならず、2色モールド成形品の製造工
程が複雑になるという問題がある。そこで、この発明
は、表示部内に閉塞領域が存在するものであっても、表
示部を均一に照光することができ、しかも簡単な工程で
2色モールド成形品を得ることができる1次モールド成
形体を提供することを第1の目的とし、そして、係る1
次モールド成形体を用いた2色モールド成形品の製造方
法を提供することを第2の目的とする。
However, in the above-mentioned conventional example, an extremely small protruding portion must be cut at the final stage of two-color molding, which complicates the manufacturing process of the two-color molded product. There is. Therefore, according to the present invention, even if a closed area exists in the display unit, the display unit can be uniformly illuminated and a two-color molded product can be obtained by a simple process. The primary purpose is to provide a body and
A second object is to provide a method for producing a two-color molded product using the next molded product.

【0008】[0008]

【課題を解決するための手段】前記第1の目的を達成す
るために、この発明は、透光性樹脂が注入されることに
より表示部となる間隙が形成され、かつこの間隙で囲ま
れた閉塞領域を有する1次モールド成形体において、前
記間隙を跨いで、前記間隙の回りの周辺領域と前記閉塞
領域とを連結するボス、を有してなることを特徴とする
ものである。
In order to achieve the first object, according to the present invention, a gap serving as a display portion is formed by injecting a translucent resin and is surrounded by the gap. The primary molded body having a closed region is characterized by including a boss that straddles the gap and connects the peripheral region around the gap to the closed region.

【0009】そして、前記第2の目的を達成するため
に、この発明は、外側金型と内側金型とを対向させ、当
該外側金型と内側金型の間に形成されたキャビティ内に
樹脂を注入して、表示部となる間隙が形成され、かつこ
の間隙で囲まれた閉塞領域を有し、さらに、前記間隙を
跨いで、前記間隙の回りの周辺領域と前記閉塞領域とを
連結するボス、を有してなる1次モールド成形体を得る
第1の工程と、透光性樹脂を前記間隙内に注入すると共
に、1次モールド成形体に前記透光性樹脂からなる2次
モールド成形体を被着する第2の工程と、を有する2色
モールド成形品の製造方法に係るものである。
In order to achieve the second object, according to the present invention, an outer die and an inner die are opposed to each other, and a resin is placed in a cavity formed between the outer die and the inner die. And a closed region surrounded by the gap is formed, and a peripheral region around the gap is connected to the closed region by straddling the gap. A first step of obtaining a primary molded body having a boss; and a secondary molding of the translucent resin into the primary molded body while injecting a transparent resin into the gap. The present invention relates to a method for producing a two-color molded article, which comprises a second step of applying a body.

【0010】[0010]

【作用】間隙に露出するボスの上面に、2次モールド成
形体用透光性樹脂を注入する際の注入圧が付加される
と、ボスを閉塞領域と前記間隙の回りの周辺領域とから
容易に離脱させることができるために、樹脂の注入と表
示部に対して影となるボスの離脱とを一度に行うことが
可能となり、この結果、簡単な工程で2色モールド成形
品を製造できることになる。
When the injection pressure for injecting the translucent resin for the secondary molded body is applied to the upper surface of the boss exposed in the gap, the boss is easily removed from the closed region and the peripheral region around the gap. Since the resin can be removed from the boss, the resin can be injected and the boss that shadows the display can be removed at the same time. As a result, a two-color molded product can be manufactured by a simple process. Become.

【0011】[0011]

【実施例】次に本発明の実施例について説明する。図1
乃至図3は、キートップの1次モールド成形体を示した
ものであり、その表面に数字の「0」が描かれている。
図1はその平面図、図2は図1のII−II断面図、図
3は1次モールド成形体の一部斜視図を示す。
EXAMPLES Next, examples of the present invention will be described. Figure 1
3 to FIG. 3 show a primary molded body of a key top, and a number “0” is drawn on the surface thereof.
1 is a plan view thereof, FIG. 2 is a sectional view taken along line II-II of FIG. 1, and FIG. 3 is a partial perspective view of a primary molded body.

【0012】図1乃至図3において、1次モールド成形
体10は下面が開放され、内部が空洞の一定肉厚の光透
過度が低い不透光色の樹脂で形成され、その表面には表
示部となる「0」を画成する間隙12が形成されてい
る。当該間隙12内には、間隙に囲まれた状態で閉塞領
域14が存在する。
In FIGS. 1 to 3, the primary molded body 10 has an open lower surface, is internally formed of a resin of a non-transmissive color with a low wall thickness and a constant wall thickness, and has a display on the surface thereof. A gap 12 is formed that defines a "0" as a part. Within the gap 12, a closed region 14 exists in a state of being surrounded by the gap.

【0013】閉塞領域14とその周辺領域16の一部
は、その裏側が矩形18に切り欠かれ、切り欠かれた領
域の閉塞領域の裏面20と周辺領域の裏面22には、閉
塞領域14と周辺領域16とを連結する円筒状のボス3
0が前記間隙12を跨ぐ形で、1次モールド体10の内
方に向かって当該1次モールド成形体10と一体に成形
されている。したがって、ボス30を設けることによ
り、閉塞領域14が間隙12に取り囲まれていても、閉
塞領域が脱落することなく当該閉塞領域14を周辺領域
16に支持することができる。尚、ボス30の上面と閉
塞領域の裏面20ないしは周辺領域の裏面22との連結
面積は、ボス30が脱落しない範囲で比較的小さい値に
制限されることが好ましい。
The closed area 14 and a part of the peripheral area 16 are notched on the back side thereof into a rectangle 18, and the back surface 20 of the closed area and the back surface 22 of the peripheral area are covered with the closed area 14. Cylindrical boss 3 that connects to the peripheral region 16
0 extends over the gap 12 and is formed integrally with the primary molded body 10 toward the inside of the primary molded body 10. Therefore, by providing the boss 30, even if the closed region 14 is surrounded by the gap 12, the closed region 14 can be supported by the peripheral region 16 without falling off. The connecting area between the upper surface of the boss 30 and the back surface 20 of the closed area or the back surface 22 of the peripheral area is preferably limited to a relatively small value within a range in which the boss 30 does not fall off.

【0014】次に、図1乃至図3に示す1次モールド成
形体10およびこの1次モールド成形体を用いた2色モ
ールド成形品の製造方法について説明する。図4ないし
図6は、その製造工程を示す断面図である。図4におい
て、外側金型41、内側固定金型44、および内側移動
金型42とを対向させ、その際これらの金型間に形成さ
れたキャビティ内に不透光色の樹脂を図示しない注湯口
から注入すると、図1乃至図3に示した1次モールド成
形体10が形成される。外側金型41には、1次モール
ド成形体10に前記間隙部14を形成するための「0」
状の突起46が内方に向かって突設されており、内側移
動金型42には、前記矩形18を形成するための突起4
8と、前記ボス30を形成するための円筒状の凹部50
が形成されている。
Next, a method of manufacturing a primary mold molded body 10 shown in FIGS. 1 to 3 and a two-color molded molded article using this primary mold molded body will be described. 4 to 6 are sectional views showing the manufacturing process. In FIG. 4, the outer mold 41, the inner fixed mold 44, and the inner movable mold 42 are opposed to each other, and the resin of the non-translucent color is not shown in the cavity formed between these molds. When poured from the gate, the primary molded body 10 shown in FIGS. 1 to 3 is formed. The outer mold 41 is provided with “0” for forming the gap portion 14 in the primary molded body 10.
-Shaped projections 46 are provided so as to project inward, and the projections 4 for forming the rectangle 18 are formed on the inner moving mold 42.
8 and a cylindrical recess 50 for forming the boss 30.
Are formed.

【0015】図4の工程が終了すると、図5の工程に移
行する。この工程では、外側金型を前記突起46を有し
ない外側金型41に換えるとともに、内側移動金型42
を僅かに後退させる。この時、内側移動金型42の移動
量に相当する空間51が外側金型41と内側移動金型4
2との間に形成される。次いで、図6に示す工程に移行
し、図示しない注湯口から透光性樹脂の溶融液を前記空
間51に注入する。注入された透光性樹脂52は空間5
1内に充填されて前記1次モールド成形体10の裏面に
被着すると共に、1次モールド成形体10の間隙12内
にも充填される。この時、透光性樹脂の注入圧は、間隙
12に露出する前記ボス30の上面にも付加され、ボス
30が下方に押し込まれるようとする。
When the process of FIG. 4 is completed, the process moves to the process of FIG. In this step, the outer mold is replaced with the outer mold 41 having no protrusion 46, and the inner moving mold 42 is moved.
Back slightly. At this time, the space 51 corresponding to the movement amount of the inner moving mold 42 is formed in the outer mold 41 and the inner moving mold 4.
It is formed between the two. Next, the process proceeds to the step shown in FIG. 6, and the molten liquid of the translucent resin is injected into the space 51 from a pouring port (not shown). The injected translucent resin 52 is the space 5
1 and is applied to the back surface of the primary molded body 10 and is also filled in the gap 12 of the primary molded body 10. At this time, the injection pressure of the transparent resin is also applied to the upper surface of the boss 30 exposed in the gap 12 so that the boss 30 is pushed downward.

【0016】ボス30の上面と閉塞領域の裏面20ない
しは周辺領域の裏面22との連結面積は比較的小さい値
になっていることから、透光性樹脂の注入圧がボス30
の上面に付加されると、ボス30は閉塞領域14および
周辺領域16から離脱して、後退した内側移動金型42
の円筒状の凹部50内に落下する。
Since the connecting area between the upper surface of the boss 30 and the back surface 20 of the closed area or the back surface 22 of the peripheral area has a relatively small value, the injection pressure of the light-transmissive resin is increased.
When it is added to the upper surface of the boss 30, the boss 30 is separated from the closed region 14 and the peripheral region 16 and retracted to the inner moving mold 42.
Falls into the cylindrical recess 50.

【0017】図6の工程を終了することにより、図7に
示すような、不透光性樹脂からなる1次モールド成形体
10と、当該1次モールド成形体10の裏面に被着さ
れ、かつ間隙12内に透光性樹脂が充填され、光が透過
した際数字の「0」を1次モールド成形体10から浮き
立たせる表示部56を有する2次モールド成形体とが一
体になった2色モールド成形品が得られる。
By completing the process of FIG. 6, the primary mold molded body 10 made of an opaque resin as shown in FIG. 7 and the back surface of the primary mold molded body 10 are adhered, and A two-color molding in which a transparent resin is filled in the gap 12 and a secondary molding body having a display portion 56 that makes the numeral “0” stand out from the primary molding body 10 when light is transmitted is integrated. A molded product is obtained.

【0018】このような2色モールド成形品では、2次
モールド成形体の一部斜視図である図8にも示すよう
に、間隙内の閉塞領域14の裏面には2次モールド成形
体である透光性樹脂52が被着されているため、閉塞領
域は当該2次モールド成形体上に支持されている。
In such a two-color molded article, as shown in FIG. 8 which is a partial perspective view of the secondary molded article, the back surface of the closed region 14 in the gap is the secondary molded article. Since the translucent resin 52 is applied, the closed region is supported on the secondary molded body.

【0019】そして、閉塞領域とその周辺領域とを連結
するボス30は、透光性樹脂溶融液の圧入と略同時に離
脱するため、ボスを切断する工程は一切不要にできる。
したがって、樹脂の注入と表示部に対して影となるボス
の離脱を一度に行うことが可能となり、前記従来例と比
較して、製造工程を大幅に簡略にできる。さらに、この
ような2色モールド成形品においては、不透光性の前記
ボス30は離脱されているために、間隙12内の透光性
樹脂に影を投影することなく、表示部56の全体を均一
に照光することができる。
Since the boss 30 connecting the closed region and its peripheral region is released at substantially the same time as the press-in of the transparent resin melt, the step of cutting the boss can be eliminated.
Therefore, it becomes possible to inject the resin and remove the boss that shadows the display portion at a time, and the manufacturing process can be greatly simplified as compared with the conventional example. Further, in such a two-color molded product, the non-translucent boss 30 is separated, so that the entire display portion 56 can be formed without projecting a shadow on the translucent resin in the gap 12. Can be illuminated uniformly.

【0020】本実施例において、ボス30が閉塞領域1
4とその周辺領域16とから離脱するように、1次モー
ルド成形体の材質、ボス30と閉塞領域14および周辺
領域16との連結面積、透光性樹脂の注入圧、透光性樹
脂の注入時温度等の少なくとも一つが適宜調整されるこ
とが好ましい。
In this embodiment, the boss 30 has the closed area 1
4 so as to be separated from the peripheral region 16 and the peripheral region 16, the material of the primary molded body, the connection area between the boss 30 and the closed region 14 and the peripheral region 16, the injection pressure of the transparent resin, the injection of the transparent resin. At least one of the hour temperature and the like is preferably adjusted appropriately.

【0021】本実施例において、図3に示すように、前
記2次モールド成形体用の透光性樹脂を注入する際、こ
の透光性樹脂が前記間隙12内を互いに反対方向に進む
ようにし、反対方向の樹脂流60A,Bがそれぞれボス
30の側面に到達した後この側面に沿って上昇し、次い
でボスの丁度上面にて衝突するようにすると、衝突した
樹脂流がボス30に向かって略垂直に下降しボスの上面
により大きな圧力を付加しようとするため、ボスの離脱
が確実となって好ましい。
In this embodiment, as shown in FIG. 3, when the translucent resin for the secondary molded body is injected, the translucent resin advances in the gaps 12 in mutually opposite directions. , And the resin flows 60A and B in the opposite directions reach the side surface of the boss 30 and then rise along the side surface, and then collide with each other just on the upper surface of the boss. It is preferable that the boss is surely detached because it is lowered substantially vertically to apply a larger pressure to the upper surface of the boss.

【0022】尚、前記実施例では、1次モールド成形体
の裏面に2次モールド成形体を被着した構成としたが、
1次モールド成形体の表面に2次モールド成形体を被着
する構成でも良い。また、ボスは1箇所のみに形成した
構成となっているが、閉塞領域が脱落しないように、ボ
スを2箇所以上形成することもできる。さらに、前記実
施例では、閉塞領域を有する表示部として数字の「0」
を例示したが、閉塞領域を有する文字、記号、符号等で
あれば全て本発明を適用することができることは勿論で
ある。さらにまた、前記実施例では、ボスを1次モール
ド成形体の裏面に形成したが、ボスを1次モールド成形
体の表面側に形成することもできる。
In the above embodiment, the back surface of the primary molded body is covered with the secondary molded body.
A configuration in which the secondary mold molded body is adhered to the surface of the primary mold molded body may be used. Further, although the boss is formed only at one place, it is also possible to form the boss at two or more places so that the closed region does not fall off. Further, in the above embodiment, the number "0" is used as the display unit having the closed area.
However, it goes without saying that the present invention can be applied to any character, symbol, code or the like having a closed region. Furthermore, in the above embodiment, the boss is formed on the back surface of the primary molded body, but the boss can be formed on the front surface side of the primary molded body.

【0023】[0023]

【発明の効果】以上説明したように、本発明は、透光性
樹脂が注入されることにより表示部となる間隙の回りの
周辺領域とこの間隙で囲まれた閉塞領域とを前記間隙を
跨いで連結するボス、を有する構成となっているため、
表示部内に閉塞領域が存在しても、表示部を均一に照光
することができ、しかも簡単な工程で製造可能な2色モ
ールド成形品を得ることができる、という優れた効果を
達成することができる。
As described above, according to the present invention, the translucent resin is injected so that the peripheral region around the gap to be the display portion and the closed region surrounded by the gap straddle the gap. Since it has a boss that connects with,
Even if there is a closed region in the display unit, the excellent effect that the display unit can be uniformly illuminated and a two-color molded product that can be manufactured by a simple process can be obtained. it can.

【図面の簡単な説明】[Brief description of drawings]

【図1】本発明の一実施例に係わるキートップの1次モ
ールド成形体を示した平面図である。
FIG. 1 is a plan view showing a primary molded body of a key top according to an embodiment of the present invention.

【図2】図1のII−II断面図である。FIG. 2 is a sectional view taken along line II-II of FIG.

【図3】図1の一部斜視図である。FIG. 3 is a partial perspective view of FIG.

【図4】1次モールド成形体の製造工程を示す断面図で
ある。
FIG. 4 is a cross-sectional view showing a manufacturing process of the primary molded body.

【図5】図4の次の工程に来る、2色モールド成形品の
製造工程を示す断面図である。
FIG. 5 is a cross-sectional view showing a manufacturing process of a two-color molded product that comes in the next process of FIG.

【図6】図5の次の工程に来る、2色モールド成形品の
製造工程を示す断面図である。
FIG. 6 is a cross-sectional view showing a manufacturing process of a two-color molded product that comes in the next process of FIG.

【図7】図4ないし図6の工程により得られた2色モー
ルド成形品の断面図である。
FIG. 7 is a cross-sectional view of a two-color molded product obtained by the steps of FIGS.

【図8】2次モールド成形体の一部斜視図である。FIG. 8 is a partial perspective view of a secondary molded body.

【符号の説明】[Explanation of symbols]

10 1次モールド成形体 12 間隙 14 閉塞領域 16 周辺領域 30 ボス 10 Primary Molded Body 12 Gap 14 Closure Area 16 Peripheral Area 30 Boss

Claims (2)

【特許請求の範囲】[Claims] 【請求項1】 透光性樹脂が注入されることにより表示
部となる間隙が形成され、かつこの間隙で囲まれた閉塞
領域を有する1次モールド成形体において、前記間隙を
跨いで、前記間隙の回りの周辺領域と前記閉塞領域とを
連結するボス、を有してなる1次モールド成形体。
1. A primary molded body having a gap serving as a display portion formed by injecting a translucent resin, and having a closed region surrounded by the gap, and the gap extending across the gap. A primary molded body comprising a boss that connects a peripheral region around the skirt and the closed region.
【請求項2】 外側金型と内側金型とを対向させ、当該
外側金型と内側金型の間に形成されたキャビティ内に樹
脂を注入して、表示部となる間隙が形成され、かつこの
間隙で囲まれた閉塞領域を有し、さらに、前記間隙を跨
いで、前記間隙の回りの周辺領域と前記閉塞領域とを連
結するボス、を有してなる1次モールド成形体を得る第
1の工程と、透光性樹脂を前記間隙内に注入すると共
に、1次モールド成形体に前記透光性樹脂からなる2次
モールド成形体を被着する第2の工程と、を有する2色
モールド成形品の製造方法。
2. An outer mold and an inner mold are opposed to each other, and a resin is injected into a cavity formed between the outer mold and the inner mold to form a gap serving as a display portion, and A primary molded body having a closed region surrounded by the gap, and further comprising a boss that straddles the gap and connects the peripheral region around the gap to the closed region; 2 colors including a step 1 and a second step of injecting a translucent resin into the gap and depositing a secondary molded body made of the translucent resin on the primary molded body. Manufacturing method of molded article.
JP32389691A 1991-11-12 1991-11-12 Primary molding product and method for producing two-color molding product using the same Expired - Lifetime JPH07119026B2 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP32389691A JPH07119026B2 (en) 1991-11-12 1991-11-12 Primary molding product and method for producing two-color molding product using the same

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP32389691A JPH07119026B2 (en) 1991-11-12 1991-11-12 Primary molding product and method for producing two-color molding product using the same

Publications (2)

Publication Number Publication Date
JPH06270190A true JPH06270190A (en) 1994-09-27
JPH07119026B2 JPH07119026B2 (en) 1995-12-20

Family

ID=18159822

Family Applications (1)

Application Number Title Priority Date Filing Date
JP32389691A Expired - Lifetime JPH07119026B2 (en) 1991-11-12 1991-11-12 Primary molding product and method for producing two-color molding product using the same

Country Status (1)

Country Link
JP (1) JPH07119026B2 (en)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2002018895A (en) * 2000-07-03 2002-01-22 Lion Corp Two-color molding
JP2010158339A (en) * 2009-01-07 2010-07-22 Sanshin Kako Kk Patterned two-color mold dish and method for manufacturing the same
WO2010101021A1 (en) * 2009-03-03 2010-09-10 Terauchi Tadayori Process for producing molded resin, molded resin, and molded-resin unit

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2002018895A (en) * 2000-07-03 2002-01-22 Lion Corp Two-color molding
JP2010158339A (en) * 2009-01-07 2010-07-22 Sanshin Kako Kk Patterned two-color mold dish and method for manufacturing the same
WO2010101021A1 (en) * 2009-03-03 2010-09-10 Terauchi Tadayori Process for producing molded resin, molded resin, and molded-resin unit
JP2010201745A (en) * 2009-03-03 2010-09-16 Tadayori Terauchi Method of manufacturing resin molded product, resin molded product, resin molded product unit

Also Published As

Publication number Publication date
JPH07119026B2 (en) 1995-12-20

Similar Documents

Publication Publication Date Title
US4990077A (en) Injection mold
US4155972A (en) Multiple-shot method of molding plastic products
US4676941A (en) Method of manufacture of plastic molding
US3443005A (en) Plural part molding
KR860002403A (en) Container closures, parts and manufacturing methods
JPH07118178B2 (en) Magnetic tape cassette manufacturing method
JPH06270190A (en) Primary molding and manufacture of two-color molded product in use of the molding
KR860001702A (en) Injection Molding Method
JP3101859B2 (en) Manufacturing method of key top plate
JPS62279911A (en) Manufacture of key top
KR0130038B1 (en) Dovble injection moulding method and from transparent plastic opaque or coloured plastic
JP2535308B2 (en) Key top
KR19980086852A (en) Insert molding bezel and its manufacturing method
JP2003094484A (en) Two-color molding method and mold device
JPH09174599A (en) Two-color molding of panel
JP4638269B2 (en) Molding method of resin product and molding apparatus used for molding method
JPS6274615A (en) Manufacture of molded body of different materials
JP3338104B2 (en) Key top two-color molding method
GB2277475A (en) Moulding display device from opaque and light transmitting resins
JP2672707B2 (en) Key top
JP2682853B2 (en) Manufacturing method of button with illumination display
CN100345232C (en) Push-button forming method and push-button manufactured through the method
KR20050022849A (en) Shape-formed article of synthetic resin sheet and process for producing the same
JPH071506A (en) Two-color molding method for key top
JPH0655579A (en) Injection molding method and injection molding die