JPH06163035A5 - - Google Patents
Info
- Publication number
- JPH06163035A5 JPH06163035A5 JP4-328984A JP32898492A JPH06163035A5 JP H06163035 A5 JPH06163035 A5 JP H06163035A5 JP 32898492 A JP32898492 A JP 32898492A JP H06163035 A5 JPH06163035 A5 JP H06163035A5
- Authority
- JP
- Japan
- Prior art keywords
- furnaces
- heating
- heat treatment
- water vapor
- manganese dioxide
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4328984A JP2700597B2 (ja) | 1992-11-16 | 1992-11-16 | リチウム一次電池用二酸化マンガンの製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4328984A JP2700597B2 (ja) | 1992-11-16 | 1992-11-16 | リチウム一次電池用二酸化マンガンの製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH06163035A JPH06163035A (ja) | 1994-06-10 |
| JPH06163035A5 true JPH06163035A5 (enExample) | 1995-03-17 |
| JP2700597B2 JP2700597B2 (ja) | 1998-01-21 |
Family
ID=18216307
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP4328984A Expired - Lifetime JP2700597B2 (ja) | 1992-11-16 | 1992-11-16 | リチウム一次電池用二酸化マンガンの製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2700597B2 (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP4748760B2 (ja) * | 2003-06-24 | 2011-08-17 | 三井金属鉱業株式会社 | リチウム一次電池用正極活物質およびその製造方法 |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5796467A (en) * | 1980-12-06 | 1982-06-15 | Hitachi Maxell Ltd | Manufacture of anode for organic electrolytic cell |
-
1992
- 1992-11-16 JP JP4328984A patent/JP2700597B2/ja not_active Expired - Lifetime
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| NO156756B (no) | Fremgangsmaate ved forvarming, brenning og avkjoeling av karbonlegemer dannet av pulverformig karbon. | |
| JPH05270834A5 (enExample) | ||
| JPH11312948A5 (enExample) | ||
| MY136966A (en) | Oven | |
| JPH113813A5 (enExample) | ||
| JPH10287733A5 (enExample) | ||
| CA2300247A1 (en) | Anti-bacteria agent made from shell, and methods for purifying and desalinating water and for washing agricultural products with use thereof | |
| JPH10204723A5 (enExample) | ||
| JPH0672826A5 (enExample) | ||
| EP0405018B1 (en) | Process for precooking parboiled rice | |
| RU97118729A (ru) | Способ отжига стекла | |
| JP2000005058A5 (enExample) | ||
| JPH06118838A5 (enExample) | ||
| JPH10189541A5 (enExample) | ||
| JPS5219358A (en) | Portable boiler | |
| JPH09100880A5 (enExample) | ||
| Parent-Simonin et al. | Possibility of Graphitising Annealing at Lower Temperature: Application to Malleable Castings | |
| JPH09108097A5 (enExample) | ||
| JPH07261328A5 (enExample) | ||
| JPH08458A5 (enExample) | ||
| RU2003108597A (ru) | Зпособ термической обработки изделий из низко- и среднеуглеродистых нелегированных и малолегированных сталей | |
| JPH04316983A5 (enExample) | ||
| Tahara et al. | Method of Nitriding Steel and Heat Treatment Furnace Used Therein | |
| JPH08297000A5 (enExample) | ||
| JPH09327378A5 (enExample) |