JPH0440769U - - Google Patents
Info
- Publication number
- JPH0440769U JPH0440769U JP8264890U JP8264890U JPH0440769U JP H0440769 U JPH0440769 U JP H0440769U JP 8264890 U JP8264890 U JP 8264890U JP 8264890 U JP8264890 U JP 8264890U JP H0440769 U JPH0440769 U JP H0440769U
- Authority
- JP
- Japan
- Prior art keywords
- lead
- insoluble anode
- matrix
- weight
- dioxide powder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
図面は本考案の一実施例を示し、第1図は不溶
性陽極の縦断面図、第2図はその一部分を拡大し
て示した説明図である。
1は不溶性陽極、2は鉛合金、3は二酸化鉛粉
末粒子。
The drawings show an embodiment of the present invention, and FIG. 1 is a longitudinal cross-sectional view of an insoluble anode, and FIG. 2 is an explanatory view showing an enlarged part of the anode. 1 is an insoluble anode, 2 is a lead alloy, and 3 is a lead dioxide powder particle.
Claims (1)
のマトリツクス中に二酸化鉛粉末を20〜50重
量%の割合で複合化し成形したことを特徴とする
電気分解用不溶性陽極。 (2) 二酸化鉛粉末の粒径が0.1〜1.0mmで
あることを特徴とする請求項1記載の電気分解用
不溶性陽極。 (3) 鉛合金がIn,Sb,Sn,Teのうち少
なくとも1種を5〜15重量%含むことを特徴と
する請求項1記載の電気分解用不溶性陽極。[Claims for Utility Model Registration] (1) An insoluble anode for electrolysis, characterized in that the matrix is made of lead or a lead alloy, and lead dioxide powder is composited into the matrix in a proportion of 20 to 50% by weight. (2) The insoluble anode for electrolysis according to claim 1, wherein the lead dioxide powder has a particle size of 0.1 to 1.0 mm. (3) The insoluble anode for electrolysis according to claim 1, wherein the lead alloy contains 5 to 15% by weight of at least one of In, Sb, Sn, and Te.