JPH04126838U - Rubber product mold - Google Patents

Rubber product mold

Info

Publication number
JPH04126838U
JPH04126838U JP3103991U JP3103991U JPH04126838U JP H04126838 U JPH04126838 U JP H04126838U JP 3103991 U JP3103991 U JP 3103991U JP 3103991 U JP3103991 U JP 3103991U JP H04126838 U JPH04126838 U JP H04126838U
Authority
JP
Japan
Prior art keywords
plate
mold
rubber
mark
mark plate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP3103991U
Other languages
Japanese (ja)
Inventor
光輝 宮田
Original Assignee
住友ゴム工業株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 住友ゴム工業株式会社 filed Critical 住友ゴム工業株式会社
Priority to JP3103991U priority Critical patent/JPH04126838U/en
Publication of JPH04126838U publication Critical patent/JPH04126838U/en
Pending legal-status Critical Current

Abstract

(57)【要約】 【目的】 ゴム製品の外観を損ねず、マーク用プレート
の製作及び金型への取付・取替作業を容易にかつ短時間
に行ない金型使用の効率化を図る。 【構成】 金型1 の側面等にマーク用プレート嵌着凹部
4 を形成し、該凹部4 にマーク用プレート3 を、ゴム又
は合成樹脂材からなるパッキン8 を介して取替可能に嵌
着し、前記凹部4 とマーク用プレート3 との間に隙間が
生じないようにしてある。
(57) [Summary] [Purpose] To improve efficiency in the use of molds by easily and quickly manufacturing marking plates and attaching/replacing them to molds without damaging the appearance of rubber products. [Configuration] Mark plate fitting recess on the side of mold 1, etc.
4, and a mark plate 3 is replaceably fitted into the recess 4 via a packing 8 made of rubber or synthetic resin, and a gap is created between the recess 4 and the mark plate 3. I have made sure that there is no such thing.

Description

【考案の詳細な説明】[Detailed explanation of the idea]

【0001】0001

【産業上の利用分野】[Industrial application field]

本考案は、タイヤ等のゴム(合成ゴム、混合ゴム等を含む)を主原料とするゴ ム製品の成形金型に関するものである。 This invention applies to tires and other rubber-based rubber (including synthetic rubber, mixed rubber, etc.). This relates to molds for molding products.

【0002】0002

【従来の技術】[Conventional technology]

一般に、ゴム製品、例えばタイヤには、その成型工程において、サイドウォー ル部に人が見て識別できる各種の文字、数字、記号、識別バー等のマークが刻印 されている。 従来、前記マークを刻印する場合、タイヤ成形金型の側面(サイドウォール部 )に、任意の深さで座ぐりを行なってマーク用プレート嵌着凹部を形成し、該凹 部に現物合わせして製作したプレートにマークを彫刻又は刻印した後、前記凹部 にプレートを嵌着する方法と、厚さが 1.5〜2.0 mm程度のプレートにマークを彫 刻したマーク用プレートを、金型に座ぐりした凹部又は凹部のない部分にネジ等 により固着する方法が採用されている。 Generally, rubber products, such as tires, have sidewalls during the molding process. Marks such as various letters, numbers, symbols, identification bars, etc. that can be visually identified by humans are engraved on the main part. has been done. Conventionally, when stamping the above mark, the side surface (sidewall part) of the tire mold ), make a counterbore to an arbitrary depth to form a recess for fitting the mark plate, and then After engraving or engraving a mark on a plate made to match the actual part, the recessed part is How to fit the plate into Insert the engraved mark plate into the recessed or non-recessed part of the mold with a screw, etc. A method of fixing is used.

【0003】0003

【考案が解決しようとする課題】[Problem that the idea aims to solve]

ところで、上記従来技術の前者にあっては、マーク用プレートと金型の凹部と の隙間へのオーバースピュー等ゴムのはみ出しもなく外観が良好であるが、現物 合わせによりプレートを製作するので、マーク用プレートを追加する際にも加工 期間中金型を必要とし、金型使用時間に制約があり、金型凹部に嵌込んだプレー トが固着状態で、プレート交換時に、プレートを外しにくくなり、無理に取外す とプレートが変形して再使用不能になるなどの問題がある。また、従来技術の後 者にあっては、マーク用プレートを金型と別個に単独製作でき、金型への取付け 作業は現物合わせを必要としないため比較的容易であるが、マーク用プレートが 金型に完全に沿わないうえ、長期使用によって変形が生じ、マーク用プレートと 金型間の隙間からゴムのはみ出しが発生し、タイヤの外観不良をきたす等の問題 がある。 By the way, in the former of the above conventional techniques, the mark plate and the recess of the mold Although the appearance is good with no overspew or other rubber protruding into the gaps, the actual Since plates are manufactured by matching, processing is also required when adding marking plates. The mold is required during the period, the mold usage time is limited, and the mold is stuck in the mold recess. If the plate is stuck, it will be difficult to remove the plate when replacing it, and you may have to remove it by force. There are problems such as the plate deforming and becoming unusable. Also, after the conventional technology If you are a manufacturer, you can manufacture the mark plate separately from the mold, and you can attach it to the mold. The work is relatively easy as it does not require actual alignment, but the marking plate is It does not fit perfectly with the mold, and due to long-term use, it becomes deformed and the marking plate Problems such as rubber protruding from the gap between the molds, causing poor appearance of the tire. There is.

【0004】 本考案は、上述のような実状に鑑みてなされたもので、その目的とするところ は、マーク用プレートの製作及び金型への取付が容易で、金型への取付作業時間 を可及的に少なくして金型使用の効率化を図り、マーク用プレートの取替作業が 容易で迅速に行ないうると共に、ゴム製品の外観を損ねることのないゴム製品成 形金型を提供するにある。0004 This invention was made in view of the above-mentioned circumstances, and its purpose is to , it is easy to manufacture the mark plate and attach it to the mold, and it takes less time to attach it to the mold. We aim to make the use of molds more efficient by minimizing the amount of damage that occurs, and the work of replacing marking plates is reduced. Rubber product manufacturing that is easy and quick and does not damage the appearance of the rubber product. We provide molds and molds.

【0005】[0005]

【課題を解決するための手段】[Means to solve the problem]

本考案では、上記目的を達成するために、次の技術的手段を講じた。 即ち、本考案は、側面等にマーク用プレートを取替可能に取付けたゴム製品成 形金型において、前記マーク用プレートの外周端縁部にゴム又は合成樹脂材から なるパッキンを介装したことを特徴としている。 In order to achieve the above object, the present invention takes the following technical measures. In other words, the present invention is a rubber product with a mark plate replaceably attached to the side surface, etc. In the mold, the outer peripheral edge of the mark plate is made of rubber or synthetic resin material. It is characterized by the inclusion of a packing.

【0006】[0006]

【作用】[Effect]

本考案によれば、マーク用プレートの外周端縁部と金型表面の間にゴム又は合 成樹脂材からなるパッキンが介装されているので、前記プレートと金型との間に 隙間がなくなり、ゴム等がはみ出さず、製品の外観を損ねることはない。また、 マーク用プレート嵌着凹部は、マーク用プレートの大きさよりも若干大きく加工 されるので、マーク用プレートの製作を、金型とは別個に単独製作でき、金型と の現物合わせ作業が不要である。さらに、マーク用プレートの交換に際しては、 金型にマーク用プレートを固定している固定ねじを緩め外すことにより、マーク 用プレートを変形させることなく容易に取外すことができ、交換用プレートは別 個に製作し準備しておけばよい。 According to the present invention, there is a rubber or composite material between the outer peripheral edge of the marking plate and the mold surface. Since a packing made of plastic material is interposed, there is no space between the plate and the mold. There are no gaps, rubber, etc. do not protrude, and the appearance of the product is not impaired. Also, The mark plate fitting recess is machined to be slightly larger than the mark plate size. As a result, the mark plate can be manufactured separately from the mold, and can be manufactured separately from the mold. There is no need for actual matching work. Furthermore, when replacing the mark plate, Marking can be done by loosening and removing the fixing screw that fixes the marking plate to the mold. The replacement plate can be easily removed without deforming the replacement plate. You can make and prepare them individually.

【0007】[0007]

【実施例】【Example】

以下、本考案の実施例を図面に基づき説明する。 図1は、本考案をタイヤ成形金型に採用した実施例を示し、成形金型1 には半 割状のタイヤ成形部2 が形成されると共に、マーク成形部分即ちサイドウォール 部には、マーク用プレート 3 (型板) を面一に埋設するためのプレート嵌着凹部 4 が形成されている。(図2,図3,図4参照)このプレート嵌着凹部4 は、プ レート3 の厚さと同じ深さ(1.5〜3.0 mm程度) とされ、その長さ及び幅はプレー ト3 の長さ及び幅よりも若干 (夫々約 1.0〜3.0 mm程度) 大きくされている。 Hereinafter, embodiments of the present invention will be described based on the drawings. Figure 1 shows an example in which the present invention is applied to a tire molding mold. The split tire molding part 2 is formed, and the mark molding part, that is, the sidewall There is a plate fitting recess in which the mark plate 3 (template) is buried flush. 4 is formed. (See Figures 2, 3, and 4) This plate fitting recess 4 The depth is the same as the thickness of rate 3 (approximately 1.5 to 3.0 mm), and its length and width are determined by the thickness of the plate. The length and width of G3 are slightly larger (approximately 1.0 to 3.0 mm each).

【0008】 前記プレート3 は、厚さが 1.5〜3.0 mmの鋼板又はステンシル板に、所要のマ ーク5 を彫刻したもので、マーク5 が各種の文字、数字、記号、識別バー等から なり、必要なもので同形同寸のものが多数準備され、必要に応じて交換可能とな っており、長さ方向両端部に固定ねじ孔6 が設けられている。そして、該プレー ト3 の外周端縁7 には、裏面側寄りに面取りが施され、表面側の厚さが夫々1.0 〜3.0 mm程度で外周面が表面に対して略直角になるように、ゴム (例えば配合ゴ ム) 又は軟質合成樹脂材からなるパッキン8 が貼着されている。なお、該パッキ ン8 は、前記プレート3 の裏面から 0.5mm以下の突出部8Aができるようにしてあ る。したがって、成形金型1 の前記プレート嵌着凹部4 に、マーク用プレート3 を嵌合させてねじ孔6 に固定ねじ9 を挿入し、該プレート3 を締付け固定すると 、パッキン8 の突出部8Aが、プレート外周端縁7 の面取り部により、金型1 の前 記凹部4 周壁に押付けられて弾性変形し、前記凹部4 周壁と前記プレート外周端 縁7 に密着して、両者3,4 間の隙間10がパッキン8 により完全に閉塞される。[0008] The plate 3 is made of a steel plate or a stencil plate with a thickness of 1.5 to 3.0 mm with the required marking. Mark 5 is carved from various letters, numbers, symbols, identification bars, etc. As a result, many necessary items of the same shape and size are prepared and can be replaced as necessary. Fixing screw holes 6 are provided at both lengthwise ends. And the play The outer peripheral edge 7 of the plate 3 is chamfered toward the back side, and the thickness of the front side is 1.0 mm. Rubber (for example, compound rubber) so that the outer circumferential surface is approximately perpendicular to the surface at a distance of ~3.0 mm. A packing 8 made of aluminum or soft synthetic resin material is attached. In addition, the packing The pin 8 is designed so that a protrusion 8A of 0.5 mm or less is formed from the back surface of the plate 3. Ru. Therefore, the mark plate 3 is placed in the plate fitting recess 4 of the molding die 1. , insert the fixing screw 9 into the screw hole 6, and tighten and fix the plate 3. , the protruding part 8A of the packing 8 is located in front of the mold 1 due to the chamfered part of the outer peripheral edge 7 of the plate. The recessed portion 4 is pressed against the peripheral wall and elastically deforms, and the recessed portion 4 is pressed against the peripheral wall and the outer peripheral end of the plate. The packing 8 is in close contact with the edge 7, and the gap 10 between the two 3 and 4 is completely closed.

【0009】 そこで、マーク用プレート3 を交換する場合、予じめ単独に製作されたプレー ト3 を準備し、タイヤ成形金型1 のマーク用プレート嵌着凹部4 に螺入されてい る固定ねじ9 を緩めて取外すと、パッキン8 の弾力によって若干プレート3 が浮 き上がるので、プレート3 を簡単に取外すことができ、交換するプレート3 を、 前記凹部4 に嵌入し、固定ねじ9 によりタイヤ成形金型1 に固定すればよく、容 易にかつ迅速に交換でき、マーク用プレート3 の交換時間は短かく、タイヤ成形 金型1 の休止時間を大幅に短縮することができる。[0009] Therefore, when replacing the mark plate 3, use a separately manufactured plate in advance. Prepare the plate 3 and screw it into the mark plate fitting recess 4 of the tire mold 1. When the fixing screw 9 is loosened and removed, the plate 3 will be slightly lifted due to the elasticity of the packing 8. Plate 3 can be easily removed, and the plate 3 to be replaced can be All you have to do is fit it into the recess 4 and fix it to the tire mold 1 with the fixing screw 9. It can be easily and quickly replaced, and the time required to replace the marking plate 3 is short, making it easier to mold the tire. The downtime of mold 1 can be significantly reduced.

【0010】 上記実施例では、パッキン8 がマーク用プレート3 の外周端縁7 に貼着されて いるが、タイヤ成形金型1 に設けたプレート嵌着凹部4 の周壁にパッキン8 を嵌 着 (接着又は嵌入のみ) することができ、上記実施例と同等の効果を期待するこ とができる。 なお、上記実施例に代えて、図6,図7,図8に示すように、プレート3とプ レート嵌着凹部4の側面間に隙間10がなく、プレート3をプレート嵌着凹部4に 密接に嵌合した構造としてもよく、また、図9,図10,図11に示すようにプ レート嵌着凹部4を形成せずに、金型表面に直接マーク用プレート3を取付ける ことができる。0010 In the above embodiment, the packing 8 is attached to the outer peripheral edge 7 of the marking plate 3. However, the packing 8 is fitted to the peripheral wall of the plate fitting recess 4 provided in the tire mold 1. (adhesion or insertion only), and the same effect as the above example can be expected. I can do that. In addition, instead of the above embodiment, as shown in FIGS. 6, 7, and 8, the plate 3 and plate There is no gap 10 between the sides of the plate fitting recess 4, and the plate 3 is inserted into the plate fitting recess 4. A close-fitting structure may also be used, or a plug-in structure may be used as shown in FIGS. 9, 10, and 11. Attaching the mark plate 3 directly to the mold surface without forming the rate fitting recess 4 be able to.

【0011】 本考案は、上記実施例に限定されるものではなく、例えば、タイヤ成形金型以 外の合成樹脂製品成形金型にも採用することができる。[0011] The present invention is not limited to the above-mentioned embodiments, but includes, for example, tire molding molds, etc. It can also be used in molds for molding other synthetic resin products.

【0012】0012

【考案の効果】[Effect of the idea]

本考案は、上述のように、側面等にマーク用プレートを取替可能に嵌着したゴ ム製品成形金型において、前記マーク用プレートの外周端縁部と金型表面との間 にゴム又は合成樹脂材からなるパッキンを介装したことを特徴とするものである から、はみ出しゴム等によって成形製品の外観を損ねることがなく、マーク用プ レートの取付、取外し、交換等の作業を簡単かつ短時間でしかも精度よく行なう ことができ、マーク用プレートの製作を金型とは別個に単独で行なえるので、金 型休止時間を大幅に短縮して使用の効率化を図ることができ、また、金型のマー ク用加工作業を比較的簡単に行なえ、マーク用プレート交換に際して、マーク用 プレートを変形させることもない。 As mentioned above, the present invention is based on a rubber plate with a mark plate attached to the side surface etc. in a replaceable manner. In a mold for molding a product, the space between the outer peripheral edge of the marking plate and the mold surface. It is characterized by having a packing made of rubber or synthetic resin interposed between the Because of this, the appearance of the molded product is not spoiled by protruding rubber, etc., and the marking plate is Perform work such as attaching, removing, and replacing plates easily, quickly, and accurately. Since the marking plate can be manufactured separately from the mold, the marking plate can be manufactured separately from the mold. It can significantly reduce mold down time, improve usage efficiency, and reduce mold markings. It is relatively easy to perform mark processing work, and when replacing the mark plate, it is possible to It does not deform the plate.

【図面の簡単な説明】[Brief explanation of drawings]

【図1】本考案の第1実施例を示す平面図である。FIG. 1 is a plan view showing a first embodiment of the present invention.

【図2】図1のA−A線断面図である。FIG. 2 is a sectional view taken along the line AA in FIG. 1;

【図3】第1実施例のマーク用プレートの拡大平面図で
ある。
FIG. 3 is an enlarged plan view of the mark plate of the first embodiment.

【図4】図3のB−B線に沿う断面図である。FIG. 4 is a sectional view taken along line BB in FIG. 3;

【図5】図3のC−C線断面図である。FIG. 5 is a sectional view taken along line CC in FIG. 3;

【図6】本考案の第2実施例のマーク用プレートの拡大
平面図である。
FIG. 6 is an enlarged plan view of a marking plate according to a second embodiment of the present invention.

【図7】図6のD−D線断面図である。7 is a sectional view taken along line DD in FIG. 6. FIG.

【図8】図6のE−E線断面図である。8 is a cross-sectional view taken along the line E-E in FIG. 6. FIG.

【図9】本考案の第3実施例のマーク用プレートの拡大
平面図である。
FIG. 9 is an enlarged plan view of a mark plate according to a third embodiment of the present invention.

【図10】図9のF−F線断面図である。FIG. 10 is a sectional view taken along line FF in FIG. 9;

【図11】図9のG−G線断面図である。11 is a sectional view taken along line GG in FIG. 9. FIG.

【符号の説明】[Explanation of symbols]

1 タイヤ成形金型 3 マーク用プレート 7 プレートの外周端縁 8 パッキン 1 Tire mold 3 Mark plate 7 Outer edge of plate 8 Packing

───────────────────────────────────────────────────── フロントページの続き (51)Int.Cl.5 識別記号 庁内整理番号 FI 技術表示箇所 B29L 30:00 4F ──────────────────────────────────────────────── ─── Continued from front page (51) Int.Cl. 5 Identification code Internal reference number FI Technical display location B29L 30:00 4F

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] 【請求項1】 側面等にマーク用プレートを取替可能に
取付けたゴム製品成形金型において、前記マーク用プレ
ートの外周端縁部にゴム又は合成樹脂材からなるパッキ
ンを介装したことを特徴とするゴム製品成形金型。
1. A mold for molding a rubber product having a mark plate replaceably attached to the side surface, etc., characterized in that a packing made of rubber or synthetic resin is interposed on the outer peripheral edge of the mark plate. A mold for molding rubber products.
JP3103991U 1991-05-07 1991-05-07 Rubber product mold Pending JPH04126838U (en)