JPH04108909U - Indentation flaw prevention device during temper rolling - Google Patents
Indentation flaw prevention device during temper rollingInfo
- Publication number
- JPH04108909U JPH04108909U JP1133891U JP1133891U JPH04108909U JP H04108909 U JPH04108909 U JP H04108909U JP 1133891 U JP1133891 U JP 1133891U JP 1133891 U JP1133891 U JP 1133891U JP H04108909 U JPH04108909 U JP H04108909U
- Authority
- JP
- Japan
- Prior art keywords
- roll
- nozzle
- temper rolling
- deflector
- respect
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
(57)【要約】
【目的】 調質圧延時に押込み疵を防止すること。
【構成】 押込み疵防止装置は、調質圧延機10の出側
に設けられたアンチクロスブレーキ・ロール3bおよび
デフレクタ・ロール4bにおいて、前記アンチクロスブ
レーキ・ロール3bに対しては鉛直面に対して30度以
下の傾斜角度θ1でロール回転方向に対向して気体を噴
射するノズル31を設け、前記デフレクタ・ロール4b
に対しては鉛直面に対して60度以下の傾斜角度θ2で
ロール回転方向に対向して気体を噴射するノズル41を
設けた構成になっている。
(57) [Summary] [Purpose] To prevent indentation defects during temper rolling. [Structure] The indentation flaw prevention device is provided on the anti-cross brake roll 3b and the deflector roll 4b provided on the exit side of the temper rolling mill 10, with respect to the vertical plane with respect to the anti-cross brake roll 3b. The deflector roll 4b is provided with a nozzle 31 that injects gas at an inclination angle θ 1 of 30 degrees or less and facing the roll rotation direction.
The structure is such that a nozzle 41 for injecting gas is provided facing the roll rotation direction at an inclination angle θ 2 of 60 degrees or less with respect to the vertical plane.
Description
【0001】0001
本考案は、調質圧延時に発生する押込み疵を防止する装置に関するものである 。 The present invention relates to a device for preventing indentation defects that occur during temper rolling. .
【0002】0002
従来、調質圧延時において押込み疵が発生する原因は次のとおりである。 Conventionally, the causes of indentation flaws during temper rolling are as follows.
【0003】 (1)鋼帯からの異物、汚れの持込み (2)圧延機内の汚れ、異物の落下 (3)ロール摩耗 (4)圧延油中の異物 上記(1)の原因に対しては、現在対策がとられていない。上記(4)の原因 に対しては、圧延油を非循環にするか、フィルタ・システムを改善することによ って解消される。0003 (1) Foreign matter and dirt brought in from the steel strip (2) Dirt and foreign matter falling inside the rolling mill (3) Roll wear (4) Foreign matter in rolling oil No countermeasures are currently being taken for the cause of (1) above. Cause of (4) above This can be achieved by making the rolling oil non-circulating or by improving the filter system. It will be resolved.
【0004】 上記(2)、(3)の原因に対しては、従来から種々の対策がとられてきた。 圧延機のワーク・ロールに圧延油ノズルから圧延油を噴射して洗浄する装置(特 開昭61−200606号公報)、またはバックアップ・ロールやワーク・ロー ルにブラシロールを押し付ける洗浄装置が提案されている。0004 Conventionally, various countermeasures have been taken against the causes (2) and (3) above. A device (special equipment) that sprays rolling oil from a rolling oil nozzle onto the work rolls of a rolling mill to clean them. Publication No. 61-200606), or backup role or work row A cleaning device has been proposed in which a brush roll is pressed against a brush roll.
【0005】 しかし、これらの装置では、圧延機内で十分取れなかった異物や汚れが後段ロ ールに付着したり、また、外部からの汚れがロールに付着したものが除去するこ とができず、製品に押込み疵等を発生していた。[0005] However, with these devices, foreign matter and dirt that could not be sufficiently removed in the rolling mill are removed by the subsequent roller. Remove any dirt that may have adhered to the roll or dirt that may have come from outside. This resulted in indentation defects on the product.
【0006】 一般の調質圧延機においては、図1に示すように、ワーク・ロール1、バック アップ・ロール2からできている。調質圧延機10の入側・出側にはクリッピン グ・ロール3a、アンチクロスブレーキ・ロール3b、デフレクタ・ロール4a ,4b、ブライドル・ロール5a,5bがそれぞれ設けられている。[0006] In a general temper rolling mill, as shown in Fig. 1, work roll 1, back It is made up of up roll 2. Clip pins are installed on the entry and exit sides of the temper rolling mill 10. brake roll 3a, anti-cross brake roll 3b, deflector roll 4a , 4b, and bridle rolls 5a, 5b, respectively.
【0007】 テンション・ロール3a,3bおよびデフレクタ・ロール4a,4bは取替え 周期が長く、また、クリッピング・ロール3a、アンチクロスブレーキ・ロール 3bが鋼帯6の下に配置されているので洗浄が困難である。また、デフレクタ・ ロール4a,4bの付近はスペースがなく、洗浄が困難である。[0007] Tension rolls 3a, 3b and deflector rolls 4a, 4b are replaced. The cycle is long, and clipping roll 3a, anti-cross brake roll 3b is located below the steel strip 6, making it difficult to clean. Also, the deflector There is no space near the rolls 4a and 4b, making cleaning difficult.
【0008】 従来、需要者側の品質意識はさほど厳しくなかったので、クリッピング・ロー ル3a、アンチクロスブレーキ・ロール3b、デフレクタ・ロール4a,4bの 洗浄はさほど問題になっていなかった。[0008] In the past, quality awareness on the part of consumers was not so strict, so clipping rollers roll 3a, anti-cross brake roll 3b, deflector roll 4a, 4b. Cleaning wasn't much of a problem.
【0009】[0009]
本考案が解決しようとする課題は、調質圧延時にテンション・ロールやデフレ クタ・ロールによる押込み疵を防止することにある。 The problem that this invention aims to solve is the need for tension rolls and deflation during temper rolling. The objective is to prevent indentation scratches caused by the cutter roll.
【0010】0010
本考案の調質圧延時の押込み疵防止装置は、調質圧延機の出側に設けられたア ンチクロスブレーキ・ロールおよびデフレクタ・ロールにおいて、前記アンチク ロスブレーキ・ロールに対しては鉛直面に対して30度以下の傾斜角度でロール 回転方向に対向して気体を噴射するノズルを設け、前記デフレクタ・ロールに対 しては鉛直面に対して60度以下の傾斜角度でロール回転方向に対向して気体を 噴射するノズルを設けた手段によって、上記課題を解決している。 The device for preventing indentation flaws during skin pass rolling of the present invention is installed on the exit side of the skin pass rolling mill. In anti-cross brake rolls and deflector rolls, For loss brake rolls, roll at an angle of inclination of 30 degrees or less relative to the vertical plane. A nozzle is provided that injects gas in opposition to the direction of rotation, and Then, the gas is directed opposite the direction of roll rotation at an angle of inclination of 60 degrees or less to the vertical plane. The above problem is solved by a means provided with a nozzle for spraying.
【0011】 前記各ノズルに隣接して別のノズルを設けることもできる。[0011] Another nozzle may also be provided adjacent to each of the nozzles.
【0012】 前記デフレクタ・ロールに対向して設けるノズルに昇降機構を連結し、該ノズ ルを選択的に上下位置を変更できるようにすることもできる。0012 A lifting mechanism is connected to a nozzle provided opposite to the deflector roll, and the nozzle It is also possible to selectively change the vertical position of the screen.
【0013】[0013]
【作用】 本考案の調質圧延時の押込み疵防止装置は、ノズルから噴出する加圧気体がア ンチクロスブレーキ・ロールおよびデフレクタ・ロールに衝突し、ロール表面に 付着している異物および汚れを吹き飛ばす。[Effect] The device for preventing indentation flaws during skin pass rolling of the present invention prevents pressurized gas ejected from the nozzle from collision with the cross-brake roll and deflector roll, causing damage to the roll surface. Blow off any foreign objects and dirt that may have adhered to it.
【0014】 調質圧延機の入側にある各ロールに対しては、洗浄を行わない。これは、調質 圧延機の出入側で通常の圧延油による洗浄が行われているからである。[0014] The rolls on the entry side of the temper rolling mill are not cleaned. This is tempering This is because cleaning with normal rolling oil is performed on the entry and exit sides of the rolling mill.
【0015】[0015]
図1−5を参照して、本考案の調質圧延時の押込み疵防止装置の実施例につい て説明する。 Referring to Figure 1-5, an example of the device for preventing indentation flaws during skin pass rolling according to the present invention will be explained. I will explain.
【0016】 本考案が適用される調質圧延設備は、図1に最もよく示すように、供給リール 7から巻も戻された鋼帯6がデフレクタ・ロール4aとブライドル・ロール5a この間を通り、クリッピング・ロール3aを通過して、調質圧延機10のワーク ・ロール1間を通り、調質圧延をされる。調質圧延をされた鋼帯6は、アンチク ロスブレーキ・ロール3bを通過し、デフレクタ・ロール4bとブライドル・ロ ール5bとの間を通って巻取リール8に巻き取られる。[0016] As best shown in Figure 1, the skin pass rolling equipment to which the present invention is applied is equipped with a supply reel. The steel strip 6 which has been unwound from 7 is a deflector roll 4a and a bridle roll 5a. The workpiece of the temper rolling mill 10 passes through this gap and passes the clipping roll 3a. - Passes between rolls 1 and undergoes temper rolling. The steel strip 6 that has been temper rolled is It passes through the loss brake roll 3b, then deflector roll 4b and bridle roll. It passes between the winding reel 5b and the winding reel 8 and is wound up on the winding reel 8.
【0017】 本考案の調質圧延時の押込み疵防止装置は、図1に示すように調質圧延機10 の出側に設けられたアンチクロスブレーキ・ロール3bおよびデフレクタ・ロー ル4bにおいて、アンチクロスブレーキ・ロール3bに対しては鉛直面に対して 30度以下の傾斜角度θ1(図2)でロール回転方向に対向して気体を噴射する ノズル31を設け、またデフレクタ・ロール4bに対しては鉛直面に対して60 度以下の傾斜角度θ2(図4(A))でロール回転方向に対向して気体を噴射する ノズル41を設けたことを特徴としている。[0017] As shown in FIG. 1, the indentation flaw prevention device during temper rolling of the present invention prevents anti-cross brake rolls 3b and deflector rolls 4b provided on the exit side of the temper rolling mill 10. The brake roll 3b is provided with a nozzle 31 that injects gas at an inclination angle θ 1 (FIG. 2) of 30 degrees or less with respect to the vertical plane, and is opposed to the roll rotation direction. is characterized in that a nozzle 41 that injects gas is provided facing the roll rotation direction at an inclination angle θ 2 (FIG. 4(A)) of 60 degrees or less with respect to the vertical plane.
【0018】 ノズル31,41から噴射される気体は空気または不活性ガス等が好ましい。 また、気体の圧力は約2kg/cm2以上が好ましい。The gas injected from the nozzles 31 and 41 is preferably air or an inert gas. Further, the pressure of the gas is preferably about 2 kg/cm 2 or more.
【0019】 ノズル31,41は、図3に例示するように、ヘッダ311に複数の噴出口3 12を等間隔に並列に設けたようなものでよい。スペースが小さいときには噴出 口312を広幅薄厚に成形することが好ましい。[0019] The nozzles 31 and 41 have a plurality of ejection ports 3 in a header 311, as illustrated in FIG. 12 may be arranged in parallel at equal intervals. Erupts when space is small It is preferable that the opening 312 be formed wide and thin.
【0020】 図4の(B)に例示するように、ノズル31に隣接して、別のノズル31を設 けてもよい。これは、ノズル41についても同様である。このとき、一方のノズ ルには水等のジェット流を噴出させ、他方のノズルには高温気体を噴射させるこ とにより、洗浄効果を一層高めることができる。[0020] As illustrated in FIG. 4(B), another nozzle 31 is installed adjacent to the nozzle 31. You can leave it. This also applies to the nozzle 41. At this time, one nozzle One nozzle is used to eject a jet stream of water, and the other nozzle is used to eject high-temperature gas. Accordingly, the cleaning effect can be further enhanced.
【0021】 さらに、図4の(C)に示すように、ブライドル・ロール5bを使用するよう な場合には、デフレクタ・ロール4bに対向して設けるノズル41に昇降機構4 3を連結し、ノズル41を選択的に上下位置を変更できるようにすることもでき る。[0021] Furthermore, as shown in FIG. 4(C), a bridle roll 5b is used. In such a case, the lifting mechanism 4 is installed in the nozzle 41 provided opposite to the deflector roll 4b. 3 can be connected to each other so that the vertical position of the nozzle 41 can be selectively changed. Ru.
【0022】 平均寸法が0.86mm厚×1178mm幅の冷延鋼帯に対して本考案を適用 した調質圧延ラインにおいて調質圧延を実施した結果を図5に示す。本考案の実 施により、押込み疵が著しく減少していることがわかる。[0022] The present invention was applied to a cold-rolled steel strip with average dimensions of 0.86 mm thick x 1178 mm wide. Figure 5 shows the results of temper rolling carried out in the temper rolling line. The fruits of this invention It can be seen that the number of indentation flaws is significantly reduced by applying this method.
【0023】[0023]
本考案によれば、わずかな設備改善によって、押込み疵を著しく低減すること ができる。 According to the present invention, indentation scratches can be significantly reduced with slight equipment improvements. I can do it.
【図1】本考案を適用した調質圧延機の概略説明図。FIG. 1 is a schematic explanatory diagram of a temper rolling mill to which the present invention is applied.
【図2】アンチクロスブレーキ・ロールの洗浄例を示す
概略説明図。FIG. 2 is a schematic explanatory diagram showing an example of cleaning an anti-cross brake roll.
【図3】図2のIII−III線からみた正面図。FIG. 3 is a front view taken from line III-III in FIG. 2;
【図4】各種ロールの洗浄例の説明図。FIG. 4 is an explanatory diagram of an example of cleaning various rolls.
【図5】本考案の効果を示すグラフ。FIG. 5 is a graph showing the effects of the present invention.
1:ワーク・ロール 2:バックアップ・ロール 3a:クリッピングロール 4a,4b:デフレクタ・ロール 5a,5b:ブライドル・ロール 6:鋼帯 7:供給リール 8:巻取リール 10:調質圧延機 31,41:ノズル 43:昇降機構 1: Work role 2: Backup role 3a: Clipping roll 4a, 4b: Deflector roll 5a, 5b: Bridle roll 6: Steel strip 7: Supply reel 8: Take-up reel 10: Temper rolling mill 31, 41: Nozzle 43: Lifting mechanism
───────────────────────────────────────────────────── フロントページの続き (72)考案者 神崎 信治 茨城県鹿島郡鹿島町大字光3番地 住友金 属工業株式会社鹿島製鉄所内 (72)考案者 佐藤 時夫 茨城県鹿島郡鹿島町大字光3番地 住友金 属工業株式会社鹿島製鉄所内 ──────────────────────────────────────────────── ─── Continuation of front page (72) Creator Shinji Kanzaki Sumitomo Metal, 3 Hikari, Kashima-machi, Kashima-gun, Ibaraki Prefecture Inside the Kashima Steel Works of Betsu Kogyo Co., Ltd. (72) Creator Tokio Sato Sumitomo Metal, 3 Hikari, Kashima-machi, Kashima-gun, Ibaraki Prefecture Inside the Kashima Steel Works of Betsu Kogyo Co., Ltd.
Claims (3)
ロスブレーキ・ロールおよびデフレクタ・ロールにおい
て、前記アンチクロスブレーキ・ロールに対しては鉛直
面に対して30度以下の傾斜角度でロール回転方向に対
向して気体を噴射するノズルを設け、前記デフレクタ・
ロールに対しては鉛直面に対して60度以下の傾斜角度
でロール回転方向に対向して気体を噴射するノズルを設
けたことを特徴とした調質圧延時の押込み疵防止装置。1. In an anti-cross brake roll and a deflector roll provided on the exit side of a temper rolling mill, the anti-cross brake roll is rolled at an inclination angle of 30 degrees or less with respect to the vertical plane. The deflector is provided with nozzles that inject gas in opposite directions in the direction of rotation.
A device for preventing indentation flaws during skin pass rolling, characterized in that a nozzle is provided on the roll to inject gas at an angle of inclination of 60 degrees or less with respect to the vertical plane and facing the roll rotation direction.
けたことを特徴とした請求項1記載の装置。2. The apparatus according to claim 1, further comprising another nozzle adjacent to each of said nozzles.
るノズルに昇降機構を連結し、該ノズルを選択的に上下
位置を変更できるようにしたことを特徴とした請求項1
記載の装置。3. Claim 1, characterized in that an elevating mechanism is connected to a nozzle provided opposite to the deflector roll, so that the vertical position of the nozzle can be selectively changed.
The device described.