JPH0334615Y2 - - Google Patents

Info

Publication number
JPH0334615Y2
JPH0334615Y2 JP15497886U JP15497886U JPH0334615Y2 JP H0334615 Y2 JPH0334615 Y2 JP H0334615Y2 JP 15497886 U JP15497886 U JP 15497886U JP 15497886 U JP15497886 U JP 15497886U JP H0334615 Y2 JPH0334615 Y2 JP H0334615Y2
Authority
JP
Japan
Prior art keywords
trigger
present
salt solution
metal body
crystallization
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP15497886U
Other languages
Japanese (ja)
Other versions
JPS6360854U (en
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP15497886U priority Critical patent/JPH0334615Y2/ja
Publication of JPS6360854U publication Critical patent/JPS6360854U/ja
Application granted granted Critical
Publication of JPH0334615Y2 publication Critical patent/JPH0334615Y2/ja
Expired legal-status Critical Current

Description

【考案の詳細な説明】 〔産業上の利用分野〕 本考案は、過冷却された塩溶液の結晶化を開始
させる器具、即ちトリガーに関するものである。
DETAILED DESCRIPTION OF THE INVENTION [Industrial Field of Application] The present invention relates to a device or trigger for initiating crystallization of a supercooled salt solution.

〔従来の技術〕[Conventional technology]

過冷却された酢酸ナトリウム等の塩溶液は、結
晶化により熱を放出し、加熱と過冷却とを繰り返
すと、熱の放出を繰り返すので、蓄熱材として利
用されている。
A supercooled salt solution such as sodium acetate releases heat through crystallization, and when heating and supercooling are repeated, heat is released repeatedly, so it is used as a heat storage material.

上記の結晶化を開始させるには、機械的な刺激
を塩溶液に加えれば良く、そのためのトリガー
は、昭和60年特許出願公告第1020号公報、昭和60
特許出願公開第251189号公報、昭和57年特許国内
公表第501414号公報等に提案されている。
In order to initiate the above crystallization, it is sufficient to add mechanical stimulation to the salt solution, and the trigger for this is disclosed in Patent Application Publication No. 1020 of 1985,
It has been proposed in Patent Application Publication No. 251189, Patent National Publication No. 501414 of 1987, etc.

〔考案が解決しようとする問題点〕[Problem that the invention attempts to solve]

しかしながら、従来のトリガーは、何れも、結
晶化の開始に一種のコツを要し、誰にでも容易に
操作できるものではない。
However, all of the conventional triggers require some kind of skill to initiate crystallization, and cannot be easily operated by anyone.

従つて、本考案の目的は、構造が簡易で、塩溶
液の結晶化を容易に生じさせることができ、しか
も繰り返し使用できる新規なトリガーを提供する
ことにある。
Therefore, an object of the present invention is to provide a novel trigger that has a simple structure, can easily cause crystallization of a salt solution, and can be used repeatedly.

〔問題点を解決するための手段〕[Means for solving problems]

本考案は、一対の金属体を螺合させてなること
を特徴とするトリガーを提供することによつて上
記の目的を達成したものである。
The present invention achieves the above object by providing a trigger characterized by a pair of metal bodies screwed together.

〔実施例〕〔Example〕

以下、本考案のトリガーを図面に示す実施例に
ついて説明する。
Hereinafter, an embodiment of the trigger of the present invention shown in the drawings will be described.

第1図は本考案の一実施例の平面図を示すもの
で、同図において、2はボルトよりなる金属体、
3はナツトよりなる金属体で、トリガー1は、こ
れら一対の金属体2,3を螺合させることにより
構成してある。
FIG. 1 shows a plan view of an embodiment of the present invention, in which 2 is a metal body made of a bolt;
Reference numeral 3 denotes a metal body made of a nut, and the trigger 1 is constructed by screwing these pair of metal bodies 2 and 3 together.

金属体2,3には、鉄系材料、特に鋼や鉄を用
いるのが好ましい。又、金属体2,3は、互いに
螺合していれば良く、その数に制限はない。
It is preferable to use a ferrous material, particularly steel or iron, for the metal bodies 2 and 3. Furthermore, the number of metal bodies 2 and 3 is not limited as long as they are screwed together.

また、第2図は本考案の別の実施例の平面図を
示すもので、この実施例の場合、一方の金属体2
に雄ネジ管を用い、又他方の金属体3に雌ネジ管
を用いてある。
Further, FIG. 2 shows a plan view of another embodiment of the present invention, in which one metal body 2
A male threaded pipe is used for the metal body 3, and a female threaded pipe is used for the other metal body 3.

〔作用〕[Effect]

第3図は本考案のトリガー1を蓄熱パツク4内
に塩溶液(蓄熱材)5とともに装填した状態を示
すもので、過冷却された塩溶液5に浸漬されたト
リガー1における一方の金属体2に対して他方の
金属体3を回転させると、これらのネジ部間にお
ける摩擦、擦り合わせ等により機械的な衝撃が発
生し、塩溶液5の結晶化が開始される。結晶化は
速やかに全塩溶液5に波及し、熱が放出される。
FIG. 3 shows the trigger 1 of the present invention loaded together with a salt solution (heat storage material) 5 in a heat storage pack 4. One metal body 2 of the trigger 1 is immersed in the supercooled salt solution 5. When the other metal body 3 is rotated, a mechanical impact is generated due to friction, rubbing, etc. between these threaded parts, and crystallization of the salt solution 5 is started. Crystallization quickly spreads to the entire salt solution 5 and heat is released.

〔考案の効果〕[Effect of idea]

本考案のトリガーは、上述の如く、構造が簡易
で、塩溶液の結晶化を容易に生じさせることがで
き、しかも繰り返し使用できる実用的効果を奏す
るもので、蓄熱パツクに装填して用いるのに極め
て効果的である。
As mentioned above, the trigger of the present invention has a simple structure, can easily crystallize a salt solution, and has a practical effect that can be used repeatedly. Extremely effective.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図は本考案の一実施例の平面図、第2図は
本考案の別の実施例の平面図、第3図は本考案の
トリガーを使用した蓄熱パツクの概略を示す断面
図である。 1……トリガー、2……金属体、3……金属
体。
Fig. 1 is a plan view of one embodiment of the present invention, Fig. 2 is a plan view of another embodiment of the present invention, and Fig. 3 is a sectional view schematically showing a heat storage pack using the trigger of the present invention. . 1...Trigger, 2...Metal body, 3...Metal body.

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] 一対の金属体を螺合させてなることを特徴とす
るトリガー。
A trigger characterized by being made by screwing together a pair of metal bodies.
JP15497886U 1986-10-09 1986-10-09 Expired JPH0334615Y2 (en)