JPH03153336A - Method and device for blow-molding hollow vessel - Google Patents

Method and device for blow-molding hollow vessel

Info

Publication number
JPH03153336A
JPH03153336A JP29244589A JP29244589A JPH03153336A JP H03153336 A JPH03153336 A JP H03153336A JP 29244589 A JP29244589 A JP 29244589A JP 29244589 A JP29244589 A JP 29244589A JP H03153336 A JPH03153336 A JP H03153336A
Authority
JP
Japan
Prior art keywords
parison
diameter
pin
mouth
driving
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP29244589A
Other languages
Japanese (ja)
Other versions
JPH0813503B2 (en
Inventor
Takeshi Sugiura
剛 杉浦
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kyoraku Co Ltd
Original Assignee
Kyoraku Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kyoraku Co Ltd filed Critical Kyoraku Co Ltd
Priority to JP1292445A priority Critical patent/JPH0813503B2/en
Publication of JPH03153336A publication Critical patent/JPH03153336A/en
Publication of JPH0813503B2 publication Critical patent/JPH0813503B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

PURPOSE:To flatten a moved parison, and to prevent the generation of a resin reservoir by a method wherein a section regulating the inside diameter of a mouth section and a section reducing the diameter in the drive direction is formed to a drive pin, one part of the parison is moved to the section reducing the diameter in the drive direction on drive, a pressure fluid is blown into the parison and the parison is blown and blistered. CONSTITUTION:A parison 14 is arranged between split molds 5, and the split molds 5 are closed. A drive pin 9 is driven into the mouth section of the parison 14 from the nose of the blowing pin 12 of the pin 9 in mouth-section outside- diameter regulating sections 7, a pressure fluid is blown into the parison 14 from the blowing path 13 of the drive pin 9, and the parison 14 is formed along a cavity 6, thus blow-molding a hollow vessel. Since the drive pin 9 has a section 10 regulating the inside diameter of the mouth section and a section 11 reducing the diameter in the drive direction, a reverse tapered parison is generated in the drive process of the drive pin 9 in the process of blow molding, but the reverse tapered parison is flattened by drive, and the so-called resin reservoir is not generated.

Description

【発明の詳細な説明】 [産業上の利用分野] 本発明は、食品、化粧品、薬品等を収納するプラスチッ
ク製の中空容器をブロー成形によって製造する方法およ
びその実施のために用いる装置に間するものである。
[Detailed Description of the Invention] [Industrial Application Field] The present invention relates to a method for manufacturing hollow plastic containers for storing foods, cosmetics, medicines, etc. by blow molding, and an apparatus used for carrying out the method. It is something.

[従来の技術] 従来、食品、化粧品、薬品等の容器であって、胴部の一
端に筒状の口部を一体に延設した形状のプラスチック製
の容器は、ここに例示するまでもなく知られており、ま
た、この種の容器をブロー成形によって製造することも
知られている(第4図参照)。
[Prior Art] Conventionally, containers for foods, cosmetics, medicines, etc., which are made of plastic and have a cylindrical mouth extending integrally from one end of the body, need not be exemplified here. It is also known to manufacture containers of this type by blow molding (see FIG. 4).

[発明が解決しようとする課題] 胴部の一端に筒状の口部を一体に延設した形状の容器を
ブロー成形するにあたっては、第4図に示すように、分
割金型a、a間にパリスンbを配置した後、分割金型a
、aの上部よりパリスンb内に打込みピンCを打込んで
、口部dの内径を打込みピンCの外径で正確に規制し、
かつ口部dの内面が美麗な平滑面となるように形成する
ことが行われている。
[Problem to be Solved by the Invention] When blow molding a container having a shape in which a cylindrical opening is integrally extended at one end of the body, as shown in FIG. After placing the parison b on the split mold a
, drive a driving pin C into the parison b from the upper part of a, and accurately regulate the inner diameter of the mouth part d with the outer diameter of the driving pin C,
In addition, the inner surface of the mouth portion d is formed to have a beautiful smooth surface.

ところで、第4図に示すように、パリスンbの口部dの
部分に打込みピンCを打込むと、その打込み過程で打込
みピンCの外面に接しているパリスンbが下方に移動し
て、口部dの下端部に厚肉部、いわゆる樹脂溜りeが生
じる。そして、中空容器が透明性の高い樹脂で形成され
ているものでは、樹脂溜りeにより外観が損なわれ、さ
らに、中空容器において樹脂溜りeが口部dと胴部fと
の境に膨出するので、内容物を流出させる際にその流れ
を妨げるものとなり、中空容器内に内容物の残留量を多
くする原因ともなっていた。
By the way, as shown in FIG. 4, when the driving pin C is driven into the opening d of the parison b, the parison b that is in contact with the outer surface of the driving pin C moves downward during the driving process, and the opening d is moved downward. A thick portion, a so-called resin pool e, is formed at the lower end of portion d. If the hollow container is made of a highly transparent resin, the appearance will be impaired by the resin pool e, and furthermore, the resin pool e will bulge out at the boundary between the mouth part d and the body part f of the hollow container. This obstructs the flow of the contents when they are drained, and causes a large amount of the contents to remain inside the hollow container.

本発明は、上記従来のものにおける問題点に鑑み、中空
容器をブロー成形する際に、口部に打込みピンを打込ん
でも、その過程で口部の内端部に樹脂溜りを生じさせず
、胴部と口部が路間−の肉厚の滑らかな面で連続形成さ
れるようにし、もって、中空容器が透明性の高いもので
あっても外観性に優れており、しかも、内容物の流出が
全く妨げられず、その残留量がきわめて少ないプラスチ
ック製の中空容器を得るブロー成形方法およびその方法
を実施するための好適なブロー成形装置を提供すること
を目的とするものである。
In view of the above-mentioned problems with the conventional products, the present invention has been developed to prevent resin accumulation at the inner end of the mouth during blow molding of a hollow container even when a driving pin is driven into the mouth. The body and mouth are formed continuously with a thick and smooth surface between the passages, so that even if the hollow container is highly transparent, it has an excellent appearance and the contents are It is an object of the present invention to provide a blow molding method for obtaining a hollow plastic container in which the outflow is completely unobstructed and the amount of residual plastic is extremely small, and a blow molding apparatus suitable for carrying out the method.

[課題を解決するための手段] 本発明は、上記目的を達成するための技術的手段として
、次の方法を採用し、かつ装置を構成した。すなわち、 分割金型間にパリスンを配置し、次いで分割金型の上部
または下部よりパリスン内に口部内径を規制する打込み
ピンを打込み、パリスン内に加圧流体を吹込んで中空容
器を形成するブロー成形方法において、口部内径を規制
する部分と打込み方向に縮径する部分を有する打込みピ
ンを用い、打込ピンの打込み時に、その打込み方向に縮
径する部分にパリスンの一部を移動させるとともに、打
込みピン内を経てその打込み先端からパリスン内に加圧
流体を吹込んで上記移動したパリスンを吹膨平坦化させ
ることを特徴とする中空容器のブロー成形方法であり、 分割金型間にパリスンを配置し、次いで分割金型の上部
または下部よりパリスン内に口部内径を規制する打込み
ピンを打込み、パリスン内に加圧流体を吹込んで中空容
器を形成するブロー成形装置であって、打込みピンは、
閉じた分割金型の口部外径規制部より口部の肉厚だけ小
径の口部内径を規制する部分と、打込み方向に縮径する
部分と、縮径する部分からさらに延長された小径の吹込
みピンを有し、かつ内部に吹込みピンの先端に通ずる加
圧流体の吹込み通路を形成してなることを特徴とする中
空体のブロー成形装置である。
[Means for Solving the Problems] The present invention employs the following method as a technical means to achieve the above object, and configures an apparatus. That is, a parison is placed between the split molds, a driving pin is driven into the parison from the top or bottom of the split mold to regulate the inner diameter of the opening, and a pressurized fluid is blown into the parison to form a hollow container. In the forming method, a driving pin having a part that regulates the inner diameter of the mouth and a part that reduces in diameter in the driving direction is used, and when the driving pin is driven, a part of the parison is moved to the part that reduces in diameter in the driving direction. , a hollow container blow molding method characterized by blowing pressurized fluid into the parison from the driving tip through the driving pin to blow and flatten the moved parison; A blow molding device that forms a hollow container by blowing pressurized fluid into the parison by driving a driving pin that regulates the inner diameter of the mouth into the parison from the upper or lower part of the split mold, the driving pin is ,
A part that regulates the inner diameter of the mouth which is smaller than the outer diameter regulating part of the mouth of a closed split mold by the wall thickness of the mouth, a part that reduces in diameter in the driving direction, and a part with a small diameter that further extends from the part that reduces the diameter. A blow molding device for a hollow body is characterized in that it has a blowing pin and has a blowing passage for pressurized fluid communicating with the tip of the blowing pin formed therein.

[作       用  ] 本発明に係る中空容器のブロー成形方法によれば、分割
金型間にパリスンを配置した後、分割金型の上部または
下部よりパリスン内に口部内径を規制する打込みピンを
打込むが、打込みピンは口部内径を規制する部分と打込
み方向に縮径する部分を有しているので、打込みピンの
打込み時に、打込み方向に縮径する部分にパリスンの一
部を移動させることになるが、パリスン内に加圧流体を
吹込んでパリスンを吹膨させることにより、その移動し
たパリスンが平坦化される。このため、口部の打込みピ
ンの打込み方向先端側が厚肉となる膨出部、いわゆる樹
脂溜りが生じない。
[Function] According to the blow molding method for a hollow container according to the present invention, after placing the parison between the split molds, a driving pin for regulating the inner diameter of the opening is driven into the parison from the upper or lower part of the split mold. However, since the driving pin has a part that regulates the inner diameter of the opening and a part that reduces in diameter in the driving direction, when driving the driving pin, a part of the parison must be moved to the part that reduces in diameter in the driving direction. However, by inflating the parison by blowing pressurized fluid into the parison, the moved parison is flattened. For this reason, a bulge in which the leading end side of the mouth portion in the driving direction of the driving pin is thick, that is, a so-called resin pool does not occur.

本発明に係る装置によれば、打込みピンがその打込み方
向に縮径する部分からさらに延長された小径の吹込みピ
ンを有しており、延長された小径の吹込みピンの先端か
らパリスン内の深い部位に加圧流体を吹込むので、前記
のように打込みピンの縮径部によりパリスンが平坦化す
ることに加えて、胴部が口部との境部分を引っ張るよう
に吹膨され、口部の胴部との境に一時的に樹脂溜りが生
じても、それが解消されて平担面に形成される。
According to the device according to the present invention, the driving pin has a small-diameter blowing pin further extended from the part whose diameter decreases in the driving direction, and the small-diameter blowing pin extends from the tip of the extended small-diameter blowing pin into the inside of the parison. Since the pressurized fluid is injected into a deep area, in addition to flattening the parison due to the reduced diameter part of the driving pin as described above, the body is blown up so as to pull the boundary between the mouth and the mouth. Even if a resin pool temporarily forms at the boundary between the part and the body part, it will be eliminated and a flat surface will be formed.

[実   施  例  ] 本発明の実施例を図面を参照して説明する。[Example ] Embodiments of the present invention will be described with reference to the drawings.

第1図には、本発明に係る装置を用いて、本発明に係る
方法の実施により得られたプラスチック製の中空容器の
一例が示されており、1は胴部、2は口部であって、口
部2は胴部lの上端に一体に突出形成されている。口部
2の端面にはフランジ3が形成されている。4は底部で
ある。
FIG. 1 shows an example of a plastic hollow container obtained by implementing the method according to the present invention using the apparatus according to the present invention, where 1 is the body and 2 is the mouth. The mouth portion 2 is integrally formed to protrude from the upper end of the body portion l. A flange 3 is formed on the end surface of the mouth portion 2 . 4 is the bottom.

上記中空容器は、第2図に示す装置を用いてブロー成形
される。すなわち、5.5は分割金型であって、6.6
はキャビティ、7.7は口部外径規制部、8.8はフラ
ンジ形成部である。9は打込みピンであって、この打込
みピン9は、閉じた分割金型5゜5の口部外径規制部7
.7より口部2の肉厚だけ小径の口部内径を規制する部
分10と、打込み方向に縮径する部分l!を有し、かつ
縮径する部分Uからさらに長く延長された吹込みピン!
2を有するものであって、打込みピン9の内部には吹込
みピン+2の先端に通ずる加圧流体の吹込み通路13が
形成されている。
The hollow container is blow molded using the apparatus shown in FIG. That is, 5.5 is a split mold, and 6.6
is a cavity, 7.7 is a mouth outer diameter regulating portion, and 8.8 is a flange forming portion. Reference numeral 9 denotes a driving pin, and this driving pin 9 is connected to the mouth outer diameter regulating portion 7 of the closed split mold 5°5.
.. 7, a portion 10 that restricts the inner diameter of the mouth portion which is smaller in diameter by the wall thickness of the mouth portion 2, and a portion l whose diameter is reduced in the driving direction! A blow-in pin that has a diameter-reducing portion U and is extended even longer!
A blowing passage 13 for pressurized fluid is formed inside the driving pin 9 and communicating with the tip of the blowing pin +2.

第3図には、上記の装置を用いて中空容器をブロー成形
する態様が例示されており、次にその工程を説明する。
FIG. 3 shows an example of blow molding a hollow container using the above-mentioned apparatus, and the process will be explained next.

分割金型5,5間にパリスン14が配置され、図示のよ
うに分割金型5.5が閉じられる。そして、その状態に
おいて分割金型5.5の口部外径規制部7゜7に打込み
ピン9をその吹込みピン12の先端からパリスン14の
口部に打込み、打込みピン9の吹込み通路!3からパリ
メン14内に加圧流体く例えば圧縮空気)を吹込んでパ
リスン14をキャビティ6.6に沿わせて中空容器をブ
ロー成形する。
A parison 14 is placed between the split molds 5, 5, and the split mold 5.5 is closed as shown. Then, in this state, the driving pin 9 is driven into the opening outer diameter regulating part 7.7 of the split mold 5.5 from the tip of the blowing pin 12 into the mouth of the parison 14, and the driving pin 9 is inserted into the blowing passage. 3, a pressurized fluid such as compressed air is blown into the parison 14 to align the parison 14 along the cavity 6.6 to blow mold a hollow container.

打込みピン9は口部内径を規制する部分10と打込み方
向に縮径する部分11を有しているので、上記ブロー成
形の工程において、打込みピン9の打込み過程では、逆
テーパー状のパリスンが発生するが、吹込みによりこの
逆テーパー吠のパリスンが平坦化して、いわゆる樹脂溜
りが生じない。
Since the driving pin 9 has a portion 10 that regulates the inner diameter of the opening and a portion 11 that decreases in diameter in the driving direction, a reverse tapered parison occurs during the driving process of the driving pin 9 in the blow molding process. However, by blowing, the parisson of this reverse tapered shape is flattened, so that so-called resin pools are not generated.

しかも、打込みピン9の打込み方向に長く延長された吹
込みピン12の先端、からバリメン14内の深い部位に
加圧流体が吹込まれるので、前記のように打込みピン9
0打込み方向に縮径する部分11により樹脂が移動しな
いことに加えて、胴部lが口部2との境部分を引っ張る
ように吹膨され、口部2の胴部lとの境に一時的に樹脂
溜りが生じても、それが解消されて平担面に形成される
Moreover, since the pressurized fluid is blown into a deep part of the bariumen 14 from the tip of the blowing pin 12 which is extended long in the driving direction of the driving pin 9, the driving pin 9
0 In addition to the resin not moving due to the portion 11 whose diameter decreases in the driving direction, the body part l is blown so as to pull the boundary part with the mouth part 2, and the boundary part between the mouth part 2 and the body part l is temporarily inflated. Even if a resin pool occurs, it will be eliminated and a flat surface will be formed.

したがって、中空容器が透明性の高いものであっても外
観性に優れたものとなり、しかも、容器内に収容した内
容物の流出が口部2で全く妨げられることがなく、内容
物の残留量がきわめて少ない中空容器を得ることができ
る。
Therefore, even if the hollow container is highly transparent, it has an excellent appearance.Moreover, the outflow of the contents stored in the container is not obstructed at all by the mouth part 2, and the remaining amount of the contents is It is possible to obtain a hollow container with extremely low

[発明の効果] 本発明に係る中空容器のブロー成形方法は、分割金型間
にパリスンを配置し、次いで分割金型の上部または下部
よりパリスン内に口部内径を規制する打込みピンを打込
み、パリスン内に加圧流体を吹込んで中空容器を形成す
るブロー成形方法において、口部内径を規制する部分と
打込み方向に縮径する部分を有する打込みピンを用い、
打込ピンの打込み時に、その打込み方向に縮径する部分
にパリスンの一部を移動させるとともに、打込みピン内
を経てその打込み先端からパリスン内に加圧流体を吹込
んで上記移動したパリスンを吹膨平坦化させるものであ
り、また、本発明に係る中空容器のブロー成形装置は、
分割金型間にパリスンを配置し、次いで分割金型の上部
または下部よりパリスン内に口部の内径を規制する打込
みピンを打込み、パリスン内に加圧流体を吹込んで中空
容器を形成するブロー成形装置であって、打込みピンは
、閉じた分割金型の口部外径規制部より口部の肉厚だけ
小径の口部内径を規制する部分と、打込み方向に縮径す
る部分と、縮径部からさらに延長された小径の吹込みピ
ンを有し、かつ内部に吹込みピンの先端に通ずる加圧流
体の吹込み通路を形成してなるものであるから、口部に
打込みピンを打込んでも、その過程で口部の内端部に樹
脂溜りが生ぜず、中空容器が透明性の高いものであって
も外観を妨げる樹脂溜りがないところから外観性に優れ
、しかも、樹脂溜りがないところから内容物の流出が全
く妨げられず、内容物の残留量がきわめて少ないプラス
チック製の中空容器を得ることができる。
[Effects of the Invention] The method for blow molding a hollow container according to the present invention includes arranging a parison between split molds, then driving a driving pin for regulating the inner diameter of the opening into the parison from the upper or lower part of the split mold, In a blow molding method in which a pressurized fluid is blown into a parison to form a hollow container, a driving pin having a part that regulates the inner diameter of the opening and a part that decreases in diameter in the driving direction is used.
When driving the driving pin, a part of the parison is moved to the part whose diameter decreases in the driving direction, and pressurized fluid is blown into the parison from the driving tip through the driving pin to blow up the moved parison. The hollow container blow molding apparatus according to the present invention flattens the hollow container.
Blow molding involves placing a parison between split molds, then driving a driving pin into the parison from the top or bottom of the split mold to regulate the inner diameter of the mouth, and blowing pressurized fluid into the parison to form a hollow container. The driving pin has a part that regulates the inner diameter of the mouth which is smaller by the wall thickness of the mouth than the outer diameter regulating part of the mouth of the closed split mold, a part that reduces the diameter in the driving direction, and a part that reduces the diameter. It has a small-diameter blowing pin that extends further from the opening, and has a pressurized fluid blowing passage that leads to the tip of the blowing pin inside, so it is easy to drive the driving pin into the opening. However, in the process, there is no resin accumulation at the inner end of the mouth, and even if the hollow container is highly transparent, there is no resin accumulation that interferes with the appearance, giving it an excellent appearance.Moreover, there is no resin accumulation. Therefore, it is possible to obtain a plastic hollow container in which the outflow of the contents is not obstructed at all and the amount of residual contents is extremely small.

特に、本発明に係る装置によれば、打込みピンが打込み
方向に縮径する部分からさらに延長された小径の吹込み
ピンを有しており、しかも、延長された吹込みピンの先
端からパリスン内の深い部位に加圧流体を吹込むので、
前記のように打込みピンの打込み方向に縮径する部分に
よりパリスンが平坦化されることに加えて、胴部が口部
との境部分を引っ張るように吹膨され、口部のtiIN
3との境に成形過程で一時的に樹脂溜りが生じてもそれ
が解消され、−層良好なプラスチック製の中空容器を得
ることができる。
In particular, according to the device according to the present invention, the driving pin has a small-diameter blowing pin that is further extended from the portion whose diameter decreases in the driving direction, and furthermore, the driving pin has a small diameter blowing pin that is further extended from the tip of the extended blowing pin into the parison. Pressurized fluid is injected into the deep parts of the body, so
In addition to flattening the parison by the portion whose diameter decreases in the driving direction of the driving pin as described above, the body is blown up to pull the boundary between the mouth and the mouth.
Even if resin stagnation occurs temporarily at the boundary between 3 and 3 during the molding process, it is eliminated, and a plastic hollow container with good layer quality can be obtained.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図ないし第3図は本発明の実施例を示し、第1図は
一部を破断して示す中空容器の全体正面図、第2図はブ
ロー成形装置の要部を示す縦断面図、第3図はブロー成
形工程を示す要部の縦断面図である。 第4図は従来のブロー成形工程を示す要部の縦断面図で
ある。 l・・・胴部、2・・・口部、5.5・・・分割金型、
6.6・・・キャビテも 7.7・・・口部外径規制部
、9・・・打込みピン、lO・・・口部内径を規制する
部分、11・・・打込み方向に縮径する部分、12・・
・吹込みピン、13・・・吹込み通路、14・・・パリ
スン
1 to 3 show embodiments of the present invention, FIG. 1 is an overall front view of a partially cutaway hollow container, and FIG. 2 is a vertical sectional view showing the main parts of a blow molding device. FIG. 3 is a longitudinal cross-sectional view of the main parts showing the blow molding process. FIG. 4 is a vertical sectional view of the main parts showing a conventional blow molding process. l... body part, 2... mouth part, 5.5... split mold,
6.6... Cavity too 7.7... Mouth outer diameter regulating part, 9... Driving pin, lO... Portion regulating mouth inner diameter, 11... Diameter reduced in driving direction Part 12...
・Blowing pin, 13...Blowing passage, 14...Parison

Claims (2)

【特許請求の範囲】[Claims] (1)分割金型間にパリスンを配置し、次いで分割金型
の上部または下部よりパリスン内に口部内径を規制する
打込みピンを打込み、パリスン内に加圧流体を吹込んで
中空容器を形成するブロー成形方法において、口部内径
を規制する部分と打込み方向に縮径する部分を有する打
込ピンを用い、打込ピンの打込み時に、その打込み方向
に縮径する部分にパリスンの一部を移動させるとともに
、打込みピン内を経てその打込み先端からパリスン内に
加圧流体を吹込んで上記移動したパリスンを吹膨平坦化
させることを特徴とする中空容器のブロー成形方法。
(1) Place a parison between the split molds, then drive a driving pin that regulates the inner diameter of the opening into the parison from the top or bottom of the split mold, and blow pressurized fluid into the parison to form a hollow container. In the blow molding method, a driving pin that has a part that regulates the inner diameter of the mouth and a part that reduces in diameter in the driving direction is used, and when the driving pin is driven, a part of the parison is moved to the part that reduces in diameter in the driving direction. A method for blow molding a hollow container, characterized in that the moved parison is blown and flattened by blowing pressurized fluid into the parison from the driving tip of the driving pin through the inside of the driving pin.
(2)分割金型間にパリスンを配置し、次いで分割金型
の上部または下部よりパリスン内に口部内径を規制する
打込みピンを打込み、パリスン内に加圧流体を吹込んで
中空容器を形成するブロー成形装置であって、打込みピ
ンは、閉じた分割金型の口部外径規制部より口部の肉厚
だけ小径の口部内径を規制する部分と、打込み方向に縮
径する部分と、縮径部からさらに延長された小径の吹込
みピンを有し、かつ内部に吹込みピンの先端に通ずる加
圧流体の吹込み通路を形成してなることを特徴とする中
空容器のブロー成形装置。
(2) Place a parison between the split molds, then drive a driving pin to regulate the inner diameter of the mouth into the parison from the top or bottom of the split mold, and blow pressurized fluid into the parison to form a hollow container. In the blow molding device, the driving pin has a portion that regulates the inner diameter of the mouth portion which is smaller in diameter than the mouth outer diameter regulating portion of the closed split mold by the wall thickness of the mouth portion, and a portion that reduces in diameter in the driving direction. A blow molding device for a hollow container, characterized by having a small diameter blowing pin further extended from the reduced diameter part, and forming therein a pressurized fluid blowing passage leading to the tip of the blowing pin. .
JP1292445A 1989-11-13 1989-11-13 Blow molding method and apparatus for hollow container Expired - Fee Related JPH0813503B2 (en)