JPH02138090U - - Google Patents
Info
- Publication number
- JPH02138090U JPH02138090U JP4645089U JP4645089U JPH02138090U JP H02138090 U JPH02138090 U JP H02138090U JP 4645089 U JP4645089 U JP 4645089U JP 4645089 U JP4645089 U JP 4645089U JP H02138090 U JPH02138090 U JP H02138090U
- Authority
- JP
- Japan
- Prior art keywords
- groove
- surface shape
- smooth
- smooth surface
- welding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
第1図は溶接前の開先形状を示す構造略図、第
2図は溶接後の状態を示す構造略図、第3図は溝
に充填剤を埋設した状態を示す構造略図、第4図
はこの考案を採用したステータ組立体の要部縦断
面図である。
8,9……母材、12……衝合部、13……溝
、16……裏ビート、17……エポキシ系接着剤
(充填剤)。
Figure 1 is a structural diagram showing the groove shape before welding, Figure 2 is a structural diagram showing the state after welding, Figure 3 is a structural diagram showing the state in which the filler is buried in the groove, and Figure 4 is this structural diagram. FIG. 3 is a vertical cross-sectional view of main parts of a stator assembly employing the invention. 8, 9...Base material, 12...Abutting portion, 13...Groove, 16...Back beat, 17...Epoxy adhesive (filler).
Claims (1)
,7において、平滑な面形状が必要な側に溶接ビ
ード16の突出寸法L2以上の深さ寸法L1に設
定された溝13を形成し、溶接後に上記溝部に表
面形状を平滑にするように充填材17を埋設した
ことを特徴とする溶接継手形状。 Welded joints 6 where smooth surface shape is required
, 7, a groove 13 is formed on the side where a smooth surface shape is required, and the groove 13 is set to a depth L1 that is greater than or equal to the protrusion dimension L2 of the weld bead 16, and after welding, the groove is filled to make the surface shape smooth. A welded joint shape characterized by embedding material 17.