JPH01128022U - - Google Patents
Info
- Publication number
- JPH01128022U JPH01128022U JP2394088U JP2394088U JPH01128022U JP H01128022 U JPH01128022 U JP H01128022U JP 2394088 U JP2394088 U JP 2394088U JP 2394088 U JP2394088 U JP 2394088U JP H01128022 U JPH01128022 U JP H01128022U
- Authority
- JP
- Japan
- Prior art keywords
- inner circumferential
- hollow portion
- circumferential surface
- hollow
- hardening
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
第1図イは本発明の一実施例の縦断面図、第1
図ロは第1図イの応力分布図、第2図イは本考案
の開発過程での中空円筒ころの縦断面図、第2図
ロは第2図イの応力分布図である。
10……中空ころ、11……外周面、12……
端面、13……硬化部分、14……中空部、15
……内周面、16……周段部。
FIG. 1A is a longitudinal cross-sectional view of one embodiment of the present invention;
Figure B is a stress distribution diagram of Figure 1A, Figure 2A is a longitudinal cross-sectional view of the hollow cylindrical roller during the development process of the present invention, and Figure 2B is a stress distribution diagram of Figure 2A. 10...Hollow roller, 11...Outer peripheral surface, 12...
End face, 13... Hardened portion, 14... Hollow part, 15
...Inner circumferential surface, 16... Circumferential stepped portion.
Claims (1)
ともに、前記中空部内周面の両端部に端面の硬化
厚みtよりも大きい幅t1を有する周段部を形成
し、前記中空部内周面及び前記周段部表面に軟質
部分を残存させていることを特徴とする中空ころ
。 A hardening treatment is applied to the surfaces other than the inner circumferential surface of the hollow portion, and circumferential step portions having a width t1 larger than the hardening thickness t of the end surfaces are formed at both ends of the inner circumferential surface of the hollow portion, and the inner circumferential surface of the hollow portion and the A hollow roller characterized by a soft portion remaining on the surface of the circumferential step.