JP4249880B2 - Labeled container and label mounting method - Google Patents
Labeled container and label mounting method Download PDFInfo
- Publication number
- JP4249880B2 JP4249880B2 JP2000141574A JP2000141574A JP4249880B2 JP 4249880 B2 JP4249880 B2 JP 4249880B2 JP 2000141574 A JP2000141574 A JP 2000141574A JP 2000141574 A JP2000141574 A JP 2000141574A JP 4249880 B2 JP4249880 B2 JP 4249880B2
- Authority
- JP
- Japan
- Prior art keywords
- label
- adhesive
- layer
- container
- main body
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
【0001】
【発明の属する技術分野】
本発明は、ラベルを容器本体に装着するラベル付き容器及びその装着方法に関する。
【0002】
【従来の技術】
従来、例えば、図6(イ)に示すように、例えばプラスチックボトル等の容器本体50には文字,絵柄等が印刷されたラベル51が装着されているのが一般的である。このラベル51は、プラスチックフィルムからなる透明のラベル基材53と、該ラベル基材53の内面に積層された文字や絵柄等の印刷層54と、該印刷層54の内面に積層された白色インキにより形成された隠蔽層55とからラベル本体57が構成されている。尚、隠蔽層55の白インキ印刷層表面は微細な凹凸状に形成されている。そして、ラベル本体57の両端部57a,57bの最内層の隠蔽層55a,55bには、接着剤58a,58bがそれぞれ塗布されている。
【0003】
そして、前記ラベル51の容器本体50への装着に際しては、例えば、ラベル本体57の一端部57aを容器本体50の表面に接着剤58aを介して接着し、該容器本体50を回転させ、ラベル本体57の他端部57bの接着剤58bを一端部57aに接着することにより、ラベル51を容器本体50に巻き付けていた。
【0004】
【発明が解決しようとする課題】
しかしながら、前記ラベル本体の一端部57aの接着剤58aが容器本体50の表面に接着され、他端部57bの接着剤58bは、前記一端部51aの表面に接着され、しかも、両方の接着剤58a,58b同士は重なり合った状態となっていた。
【0005】
このため、前記表面が凹凸状の隠蔽層55に接着剤が塗布されると、乱反射による隠蔽効果がほとんどなくなる。これは、例えば、すりガラスの凹凸面に透明な粘着テープを貼着した状態と同じ現象となり、隠蔽層55が透けやすくなり、ラベルの接着剤を設けた部分が帯状に黒く見える。または、隠蔽層55の色以外に、特に黒、青、赤等の濃色の容器本体50自体の色や、容器本体が透明で内容物の色が濃色である場合に、その内容物の色が透けて黒く見えることもある。
【0006】
そこで、白インキの印刷回数を増やして隠蔽層を厚くすることも考えられるが、かかる場合には、印刷工程が複雑となったり白インキの量が多くなり、製造コストが高くなる欠点がある。
【0007】
本発明の課題は、隠蔽層の印刷工程を複雑にすることなく、製造コストを安くすることができ、しかも、ラベルの貼り合わせ部分が、他の部分に比し、色変わりするのを防止して外観体裁の向上を図ることにある。
【0008】
【課題を解決するための手段】
本発明は、上記の課題を解決するために、ラベル付き容器及びラベルの装着方法としてなされたものであり、ラベル付き容器としての特徴は、透明のラベル基材7に印刷層8と隠蔽層10が積層されてなるラベル本体11の少なくとも一端部に接着剤13aが塗布され、前記ラベル本体11の一端側が接着剤13aを介して容器本体11の表面に接着され、且つ、前記接着剤13aの塗布された一端部に、前記ラベル本体11の他端側に設けられた隠蔽層10が重なり合うように設けられてなることにある。また、該接着剤は基材(透明部分)に塗布されていることが好ましい。
【0010】
ラベルの装着方法としての特徴は、透明のラベル基材7に印刷層8と隠蔽層10が積層されてなるラベル本体11の少なくとも一端部に接着剤13aを塗布し、前記ラベル本体11の一端側を接着剤13aを介して容器本体11の表面に接着し、前記接着剤13aの塗布された一端部に、前記ラベル本体11の他端側に設けられた隠蔽層10が重なり合うように、ラベル本体11を容器本体11に装着することにある。
【0012】
【発明の実施の形態】
以下、本発明の一実施の形態について図面に従って説明する。
図3において、1は例えばブロー成形された無色透明又は有色不透明のポリエチレンテレフタレート製やポリエチレン製、ガラス製のボトル等の容器本体3に、ラベル(感熱ラベル)5を装着してなる容器を示す。また、内容物としては、コーラ等の飲料、たれ、つゆ等の濃色のものが挙げられる。
【0013】
前記ラベル5は、図1に示す如く長尺状のラベル長尺体1aを所定の位置で切断して形成したもので、透明のラベル基材7と、該ラベル基材7の裏面(内面)に積層され且つ絵柄等が印刷された印刷層8と、更に印刷層8の内面に積層された隠蔽層10とからなる。尚、前記ラベル基材7、印刷層8及び隠蔽層10によりラベル本体11が構成されている。ラベル基材7の透明とは、ラベル基材7を通して印刷層8が目視できる程度をいう。
【0014】
また、隠蔽層10としては、酸化チタンよりなる白色顔料を含有した白色インキにより表面を凹凸状に形成してなる。隠蔽層10は、白色インキの光の乱反射効果によって優れた隠蔽効果を示す。
ラベル基材7としては、例えばポリエチレンテレフタレートやポリプロピレンを二軸延伸したフィルム、ポリ塩化ビニルフィルム、ポリスチレンフィルム等よりなる厚みが20μm〜100 μm程度の合成樹脂製フィルムが挙げられる。
【0015】
該ラベル本体11の長さ(間隔L)は該ラベル1が装着される容器本体3の周長よりも少し長く設けられていると共に、ラベル基材7の両端部には、前記印刷層8及び隠蔽層10が設けられていない接着部分7a,7bが形成されている。そして、その両方の接着部分7a,7bには、加熱することにより活性化するホットメルト接着剤(感熱接着剤)13a,13bがそれぞれ塗布されており、かかる部分は、互いに重なり合わないように完全にずらされている。即ち、ラベル本体11の一方の接着部分(一端側)7aの感熱接着剤13aは、容器本体3の表面に接着され、更に、ラベル本体11の他方の接着部分(他方側)7bの感熱接着剤13bは、前記一方の接着部分7aを通過してラベル基材7の感熱接着剤のない部分7cの表面に接着されている。
【0016】
次に、上記ラベル1を例えばブロー成形された平面視円形の容器本体3に装着する場合について説明する。尚、ラベル1を形成するためのラベル長尺体1aを図1(イ)に示す。そして、ラベル1は、そのラベル長尺体1aに所定の間隔をおいて塗布されている感熱接着剤13の中央(仮想線Aで示す位置)を切断することにより、形成される。
【0017】
更に、ラベル1の両端部に塗布されている感熱接着剤13a,13bをそれぞれ加熱して活性化させる。
【0018】
次に、ラベル1の一端を、一方の感熱接着剤13aを介して容器本体3に接着し、該ラベル1を緊張させた状態で容器本体3を矢印B方向に回転させ(図2(イ)参照)、容器本体3の回転により、ラベル1が順次容器本体3に沿って巻かれる(図2(ロ)参照)。
【0019】
更に、ラベル1を巻き付け、その他端側の感熱接着剤13bを、前記容器本体3にラベル本体11を接着している一方の感熱接着剤13aを通過して基材7の感熱接着剤のない部分7cの表面に接着し、それぞれの感熱接着剤13a,13bの接着部分を、冷却用押圧バー(図示省略)にて感熱接着剤13a,13bが冷えて固化するまで押圧する(図2(ハ)参照)。
【0020】
以上のように形成された容器1は、図1(ロ)に示す如く一方の接着剤13aと他方の感熱接着剤13bの位置をずらせていることから、このラベルの貼り合わせ部分(感熱接着剤13a,13bの位置する部分)が、黒ずんで見えたり等して色変わりすることはない。
【0021】
具体的には、前記隠蔽層10は、その全面にわたって感熱接着剤の影響を受けることなく凹凸状態が維持されていることから、隠蔽層10による隠蔽効果が低下することなく、容器本体3の色、内容物の色等が透けることはない。
しかも、仮に、ラベル本体11の一端部を容器本体3に接着する感熱接着剤13a、及びラベル本体11の一端部を介して容器本体3の色や内容物の色が透けた場合であっても、ラベル本体11の他端部の隠蔽層10が、前記感熱接着剤13a及びラベル本体11の一端部を覆うため、一方の感熱接着剤13aの位置する隠蔽層10や容器本体3の色等によりラベル1が部分的に黒ずんで見えることはない。また、ラベル本体11の他端部の感熱接着剤13bは、ラベル基材7の表面に接着されるが、その感熱接着剤13bが位置するラベル基材7の内面には、凹凸状態が維持された隠蔽層10があるため、ラベルの貼り合わせ部分の隠蔽効果が低下することはない。
【0022】
図4は本発明の他の実施の形態を示す。即ち、前記ラベル長尺体1aに塗布される感熱接着剤13の内、ラベル基材7の一端側は切断線Aの位置まで印刷層8及び隠蔽層10が積層され、その隠蔽層10に一方の感熱接着剤13aが塗布され、且つ、ラベル基材7の他端側は前記実施の形態同様に、ラベル基材7に直接に他方の感熱接着剤13bが塗布されている。
【0023】
従って、かかるラベル長尺体1aを切断線Aで切断することにより、ラベル1を形成し、前記同様に容器本体3にラベル1を装着する。かかる場合、ラベル1の一端側は、一方の感熱接着剤13aが隠蔽層10に密着していることから、隠蔽層10の表面に凹凸がなくなり、隠蔽効果が低下するが、該一端側は、他方の感熱接着剤13bの影響を受けない隠蔽層10に被覆されていることから、ラベル本体7の一端側の隠蔽層10等が黒ずんで見えることはない。
【0024】
また、本発明は、図5に示すように、筒状に形成されたシュリンクラベル1を容器本体3に装着したものにも適用することができる。ここで、シュリンクラベル1は、ラベルの周方向に熱収縮性を有するフィルムからラベル基材7を構成し、前記該ラベル基材7に、前記印刷層8及び隠蔽層10が積層されている。
【0025】
尚、従来では、図6(ロ)に示す如く容器本体50からシュリンクラベル51が不用意に抜けないように、シュリンクラベル51の内面に感熱性の接着剤60を塗布しておいて、その接着剤60でシュリンクラベル51を容器本体50に固定している。従って、かかる場合も、接着剤60が隠蔽層の隠蔽効果を低下させてしまうこととなる。
【0026】
かかるシュリンクラベル1は、容器本体3に熱収縮させて装着すると、前記図1(ロ)または図4(ロ)に示したように、ラベル1を容器本体3に接着させる感熱接着剤13aと、ラベル本体7の他端側をその接着剤の設けられていない部分に接着させる接着剤13bとの位置がずれていることから、前記接着剤13aの塗布された一端部に、前記ラベル本体11の他端側に設けられた隠蔽層10が重なり合うように、ラベル本体11を容器本体11に装着することができる。従って、隠蔽層10や容器本体3内の内容物等が透けて黒ずんで見えるのを防止できる。尚、他端側を接着剤13bを介してラベル本体7の所定位置に接着したが、該接着剤13bは必ず設ける必要はなく、接着剤を使用しない方法として、溶着法や熱融着法などが使用される場合が挙げられる。
【0027】
【発明の効果】
以上のように本発明は、ラベル基材の両方の接着剤は、互いに重なり合わないようにずれた位置に設けられているので、ラベルの貼り合わせ部分が隠蔽層や容器本体等の色により色変わりするのを防止でき、特に、黒、青、赤等の濃色容器や、透明の容器本体に濃色の内容物を充填するのに最適であり、しかも、外観体裁を向上できる。
【0028】
また、隠蔽層の印刷工程を増やして隠蔽層を厚くする必要もないので、製造コストも安くすることができる利点がある。
【図面の簡単な説明】
【図1】本発明の一実施の形態を示し、(イ)はラベル長尺体の断面図、(ロ)はラベルを容器本体に装着した状態の断面拡大図。
【図2】(イ)〜(ハ)は、ラベルの容器本体への巻き付け工程をそれぞれ示す平面断面図。
【図3】同容器を示す斜視図。
【図4】本発明の他の実施の形態を示し、(イ)はラベル長尺体の断面図、(ロ)はラベルを容器本体に装着した状態の断面拡大図。
【図5】シュリンクラベルを装着した容器の斜視図。
【図6】従来例を示し、(イ)はラベルを容器本体に装着した状態の断面拡大図、(ロ)は概略平面図。
【符号の説明】
1…感熱ラベル(ラベル)、3…容器本体、7…ラベル基材、8…印刷層、10…隠蔽層、11…ラベル本体、13a…一方の接着剤、13b…他方の接着剤、10…容器本体[0001]
BACKGROUND OF THE INVENTION
The present invention relates to a labeled container for mounting a label on a container body and a mounting method thereof.
[0002]
[Prior art]
Conventionally, for example, as shown in FIG. 6A, a
[0003]
When the
[0004]
[Problems to be solved by the invention]
However, the adhesive 58a of the one end portion 57a of the label body is adhered to the surface of the
[0005]
For this reason, when the adhesive is applied to the concealed
[0006]
Therefore, it is conceivable to increase the number of times of printing with white ink to increase the thickness of the concealing layer. However, in such a case, there is a disadvantage that the printing process becomes complicated or the amount of white ink increases, resulting in an increase in manufacturing cost.
[0007]
The object of the present invention is to reduce the manufacturing cost without complicating the printing process of the concealing layer, and to prevent the bonded portion of the label from changing color compared to other portions. The purpose is to improve the appearance.
[0008]
[Means for Solving the Problems]
In order to solve the above problems, the present invention has been made as a container with a label and a method for attaching the label. The feature as a container with a label is that a printed
[0010]
The label mounting method is characterized in that an adhesive 13a is applied to at least one end of a
[0012]
DETAILED DESCRIPTION OF THE INVENTION
Hereinafter, an embodiment of the present invention will be described with reference to the drawings.
In FIG. 3,
[0013]
The
[0014]
Moreover, as the
Examples of the
[0015]
The length (interval L) of the label
[0016]
Next, the case where the
[0017]
Furthermore, the heat-
[0018]
Next, one end of the
[0019]
Furthermore, the
[0020]
Since the
[0021]
Specifically, since the
Moreover, even if the color of the
[0022]
FIG. 4 shows another embodiment of the present invention. That is, among the heat-
[0023]
Therefore, the
[0024]
Further, as shown in FIG. 5, the present invention can also be applied to a case where a
[0025]
Conventionally, as shown in FIG. 6 (b), a heat-
[0026]
When the
[0027]
【The invention's effect】
As described above, according to the present invention, since both the adhesives of the label base material are provided at positions shifted so as not to overlap each other, the bonded portion of the label changes color depending on the color of the concealing layer, the container body, and the like. In particular, it is optimal for filling dark colored containers such as black, blue, and red, and a transparent container main body with dark colored contents, and can improve the appearance.
[0028]
In addition, since it is not necessary to increase the thickness of the masking layer by increasing the masking layer printing process, there is an advantage that the manufacturing cost can be reduced.
[Brief description of the drawings]
1A and 1B show an embodiment of the present invention, in which FIG. 1A is a cross-sectional view of a long label body, and FIG. 1B is an enlarged cross-sectional view of a state where a label is mounted on a container body.
FIGS. 2A to 2C are cross-sectional plan views illustrating steps of winding a label around a container body.
FIG. 3 is a perspective view showing the container.
FIGS. 4A and 4B show another embodiment of the present invention, in which FIG. 4A is a cross-sectional view of a long label body, and FIG. 4B is an enlarged cross-sectional view of a state in which the label is mounted on a container body.
FIG. 5 is a perspective view of a container equipped with a shrink label.
6A and 6B show a conventional example, in which FIG. 6A is an enlarged cross-sectional view of a state in which a label is mounted on a container body, and FIG.
[Explanation of symbols]
DESCRIPTION OF
Claims (2)