JP3806708B2 - Compound deterioration accelerator - Google Patents
Compound deterioration accelerator Download PDFInfo
- Publication number
- JP3806708B2 JP3806708B2 JP2003307161A JP2003307161A JP3806708B2 JP 3806708 B2 JP3806708 B2 JP 3806708B2 JP 2003307161 A JP2003307161 A JP 2003307161A JP 2003307161 A JP2003307161 A JP 2003307161A JP 3806708 B2 JP3806708 B2 JP 3806708B2
- Authority
- JP
- Japan
- Prior art keywords
- partition plate
- test
- light source
- water
- salt
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
本発明は、各種外装材等の耐候耐蝕性や耐熱耐水性を試験するために、人工的な環境下で外装材の試験体に複合的な劣化を生じさせる複合劣化促進装置に関する。 The present invention relates to a composite deterioration accelerating device that causes a composite deterioration in a test specimen of an exterior material under an artificial environment in order to test the weather corrosion resistance and heat and water resistance of various exterior materials and the like.
<耐候耐蝕性試験>
建築用の外装材や自動車のボディ等に用いられる金属板は、一般に、耐候性試験や耐食性試験によってその性能が評価されている。
<Weather and corrosion resistance test>
The performance of metal plates used for building exterior materials, automobile bodies, etc. is generally evaluated by weather resistance tests and corrosion resistance tests.
耐候性試験のための装置としては、カーボンアークを光源とするサンシャインウェザーメーター、キセノンランプを光源とするキセノンウェザーメーター、メタルハライドランプを光源とするメタルハライドランプ試験機などがある。それらを用いて、試験体に対し、連続照射、または連続照射と散水を繰り返す方法あるいは装置として、例えばJIS・D0205の「自動車部品の耐候性試験方法」や、特許文献1記載の促進耐候試験装置などが知られている。
As a device for the weather resistance test, there are a sunshine weather meter using a carbon arc as a light source, a xenon weather meter using a xenon lamp as a light source, and a metal halide lamp tester using a metal halide lamp as a light source. As a method or apparatus for repeating continuous irradiation or continuous irradiation and sprinkling with respect to a test body using them, for example, the “weather resistance test method for automobile parts” of JIS D0205 or the accelerated weather resistance test apparatus described in
また、耐食性試験のための装置としては、JIS・Z2371の「塩水噴霧試験方法」に規定された、塩水を連続的に噴霧する塩水噴霧装置がある。また、JASO・M609−91の「自動車用材料腐食試験方法」に規定された、塩水噴霧・乾燥・湿潤を繰り返して行える複合サイクル試験装置がある。また、特許文献2及び3には、塩水噴霧や乾燥、湿潤等のサイクルを変化させて、より忠実に腐食現象を再現しようとした試験方法も提案されている。 Further, as a device for the corrosion resistance test, there is a salt spray device for continuously spraying salt water, which is defined in “Salt spray test method” of JIS Z2371. In addition, there is a combined cycle test apparatus that can repeat salt spraying, drying, and wetting as defined in JASO M609-91 “Automobile Material Corrosion Test Method”. Patent Documents 2 and 3 also propose a test method that attempts to reproduce the corrosion phenomenon more faithfully by changing a cycle such as salt spray, drying, and wetting.
しかし、実際の屋外環境下で使用される金属板には、光線(可視光・紫外線・赤外線)や熱による被膜の劣化と、水分、塩分、酸(酸性雨)および湿潤・乾燥の繰り返しによる鋼板の腐食が、複合的かつ連続的に生じる。上記のような試験方法では、耐候性試験と耐食性試験とが別々に行われることが殆どで、一部の研究では両試験を交互に実施する例があるが、いずれにしても、塗膜の劣化と鋼板の腐食とを同時的かつ複合的に促進させることができない。 However, the metal plates used in the actual outdoor environment are steel plates that are deteriorated by light rays (visible light, ultraviolet rays, infrared rays) and heat, and are repeatedly subjected to moisture, salt, acid (acid rain), and wet / dry conditions. Corrosion occurs in a complex and continuous manner. In the test methods as described above, the weather resistance test and the corrosion resistance test are mostly performed separately, and in some studies, there are examples in which both tests are performed alternately. Deterioration and corrosion of the steel sheet cannot be promoted simultaneously and in combination.
このような事情から、本出願人は、特願2002−083394において、ひとつの試験装置内で、日射を想定した任意の温度環境下、任意の時間及びサイクルで、紫外線照射、塩水(中性または酸性)の噴霧、散水(中性または酸性)、湿潤、結露、休止、乾燥等を連続的または断続定に実施することにより、実環境に近い条件で、被膜の劣化と鋼板の腐食を同時的かつ複合的に進行させることのできる複合劣化促進方法を提案している。
<耐熱耐水性試験>
一般に、建築物の屋根や外壁に用いられる外装材は、化粧材(表面材)や下地材、補強材など、異種類の素材を組み合わせて構成されている。これらの外装材は、全体が徐々に温まったり水に浸かったりするわけではなく、日射により表面から急激に加熱されたり、降雨により表面から急激に冷却されたりして、表裏面の間や、表面材と下地材との間で劣化の進行状態や収縮状態に差異が生じる。したがって、この種の外装材の耐久性を正確に評価するためには、構成材料個々の耐熱性や耐水性だけでなく、それらの構成材料を組み合わせた状態での複合的な劣化状態を正確に把握する必要がある。
Under such circumstances, in the Japanese Patent Application No. 2002-083394, the applicant of the present invention applied ultraviolet irradiation, salt water (neutral or neutral) in an arbitrary temperature environment assuming solar radiation in one test apparatus. Acidic spraying, watering (neutral or acidic), wetting, condensation, suspending, drying, etc. are performed continuously or intermittently, so that deterioration of the coating and corrosion of the steel sheet are simultaneously performed under conditions close to the actual environment. In addition, a method for promoting complex deterioration that can be progressed in a complex manner is proposed.
<Heat and water resistance test>
Generally, an exterior material used for a roof or an outer wall of a building is configured by combining different kinds of materials such as a decorative material (surface material), a base material, and a reinforcing material. These exterior materials do not gradually warm or soak in water as a whole, but are heated rapidly from the surface by solar radiation or rapidly cooled from the surface by rainfall, between the front and back surfaces, Differences occur in the deterioration progress state and contraction state between the material and the base material. Therefore, in order to accurately evaluate the durability of this type of exterior material, not only the heat resistance and water resistance of each component material, but also the combined deterioration state in the state where those component materials are combined is accurately determined. It is necessary to grasp.
しかしながら現状では、前記のような複合劣化を実環境に近い条件で人工的に進行させ、その状態を検査する方法は確立していない。例えば代表的な屋根材料のひとつであるアスファルトルーフィングに関して、JIS・A・1436に規定された「建築用被膜材料の下地不連続部における耐疲労性試験方法」があり、また、タイル用接着剤に関して、JIS・A・5548の「陶磁器質タイル用接着剤」に規定された性能規格があるが、これらの試験では、日射熱の影響や、吸湿・乾燥の繰り返しによる形状の変化、表面材と下地材との密着性の低下など、現実的な劣化状態を把握することができない。 However, at present, there is no established method for inspecting the state of the above-mentioned complex deterioration artificially progressing under conditions close to the actual environment. For example, asphalt roofing, one of the typical roofing materials, there is a “Fatigue resistance test method for discontinuous parts of coating materials for buildings” defined in JIS A1436. There are performance standards defined in JIS A. 5548 “Adhesives for Ceramics Tile”, but in these tests, the effects of solar heat, changes in shape due to repeated moisture absorption and drying, surface materials and groundwork A realistic deterioration state such as a decrease in adhesion to the material cannot be grasped.
このような事情から、本出願人は、特願2002−083393において、ひとつの試験装置内で、日射を想定した任意の温度環境下、赤外線を含む波長域の光照射、散水(中性または酸性)、湿潤、結露、休止、乾燥等を連続的または断続定に実施することにより、実環境に近い条件で、外装材の表面及び内部における複合的な劣化を進行させることのできる複合劣化促進方法を提案している。
本発明は、上記特願2002−083393及び特願2002−0833944において提案された耐候耐食性試験や耐熱耐水性試験に共通して利用し得る複合劣化促進装置の具体的な構成を提案するものである。 The present invention proposes a specific configuration of a composite deterioration accelerating device that can be commonly used in the weather corrosion resistance test and the heat and water resistance test proposed in the above Japanese Patent Application Nos. 2002-083393 and 2002-0833944. .
かかる装置の開発に際して、本出願人は、従来の各種試験装置の様々な組み合わせを模索し、温湿度を制御しうる試験室内に、試験体を設置するための保持台や、光源、散水装置、塩水噴霧装置等をバランス良く組み込むことを検討した。この検討過程においては、特に、光照射のための光源が高熱を発して試験室内の温湿度制御に影響を及ぼすので、この影響を小さくして、試験室内の温湿度制御を容易にする必要があることや、試験室内に塩水が噴霧されて充満すると、乾燥後に塩分が光源の表面に残存して光照射の妨げになるので、これを防止する必要があるという課題が見出された。 In developing such a device, the present applicant sought various combinations of various conventional test devices, and in a test chamber capable of controlling the temperature and humidity, a holding stand for installing a test body, a light source, a watering device, We considered incorporating a salt spray device in a well-balanced manner. In this examination process, the light source for light irradiation emits high heat and affects the temperature and humidity control in the test room. Therefore, it is necessary to reduce this effect and facilitate the temperature and humidity control in the test room. In addition, when salt water is sprayed and filled in the test chamber, the salt remains on the surface of the light source after drying, which hinders light irradiation, and it has been found that it is necessary to prevent this.
上記した課題のうち、光源が発する高熱の制御に関しては、試験体を保持する試験室と光源とをガラス板等からなる開口部によって仕切り、その開口部を通じて光源を照射することが考えられる。しかし、この場合でも、開口部に取り付けられるガラス板等の表面に塩分が付着する問題が残る。ガラス板への塩分付着を防ぐ方法としては、塩水噴霧時に遮断スクリーンを設けたり、絶えずワイパーでかき落としたりする方法がある。しかし、遮断スクリーンは材質や密閉方法が問題であり、機構的にも複雑になる。またワイパーも駆動部を要するので機構が複雑になり、ガラス面に傷をつけるという問題もある。 Among the above-mentioned problems, regarding the control of high heat generated by the light source, it is conceivable to divide the test chamber holding the test body and the light source by an opening made of a glass plate or the like and irradiate the light source through the opening. However, even in this case, there remains a problem that salt adheres to the surface of a glass plate or the like attached to the opening. As a method for preventing the adhesion of salt to the glass plate, there are a method of providing a blocking screen when spraying salt water, or a method of constantly scraping off with a wiper. However, the material and the sealing method of the shut-off screen are problems, and the mechanism is complicated. Further, since the wiper also requires a drive unit, the mechanism is complicated, and there is a problem that the glass surface is damaged.
本発明は上記のような検討を経てなされたものであり、コストの低い簡単な機構で、効果的に塩分付着を防止することのできる複合劣化促進装置の具体的な構成を提案することを課題としている。 The present invention has been made through the above-described studies, and it is an object to propose a specific configuration of a composite deterioration accelerating device that can effectively prevent the adhesion of salt with a simple mechanism at low cost. It is said.
上記のような課題を解決するため、本発明の複合劣化促進装置の構成は、塩水噴霧装置を具備する温湿度制御可能な試験室に、試験体の保持面が鉛直面に対して20度±10度の仰角をなすように形成された保持台が据え付けられ、上記保持面に正対して設けられた開口部には、透光性の仕切り板を備えた光源ユニットが、該仕切り板を上記保持面と平行にして設置されるとともに、上記仕切り板の室内側の上部付近には、仕切り板の幅方向に延びる樋状の流水溝から溢れさせた水を仕切り板の室内側表面の略全幅にわたって流下させる洗浄装置が設けられたことを特徴とする。 In order to solve the problems as described above, the structure of the composite deterioration accelerating device of the present invention is a test chamber equipped with a salt spray device capable of controlling the temperature and humidity, and the holding surface of the test body is 20 degrees ± with respect to the vertical surface. A holding base formed to make an elevation angle of 10 degrees is installed, and a light source unit provided with a translucent partition plate is provided in an opening provided facing the holding surface. Installed in parallel with the holding surface and near the upper part on the indoor side of the partition plate, the water overflowed from the bowl-shaped water channel extending in the width direction of the partition plate is approximately the full width of the indoor surface of the partition plate. It is characterized in that a cleaning device is provided for flowing down .
この構成によれば、試験体を定置するための試験室と高熱を発する光源ユニットとが透光性の仕切り板を隔てて区画されるので、試験室内の温湿度の制御が容易になる。また、試験室内に塩水が噴霧されて充満しても、光源ユニットが塩分の影響を受けないので、維持管理が容易になる。 According to this configuration, the test chamber for placing the test body and the light source unit that generates high heat are partitioned with the translucent partition plate therebetween, so that the temperature and humidity in the test chamber can be easily controlled. Even if salt water is sprayed and filled in the test chamber, the light source unit is not affected by the salt content, so that maintenance management becomes easy.
さらに、洗浄装置を利用して、仕切り板の表面に付着する塩分を洗浄することにより、常に良好な状態の光照射が得られる。この洗浄は、塩水の噴霧後だけでなく、噴霧の直前にも行うようにすれば、仕切り板の表面に水膜が作られて塩分の付着を少なくすることができるので、噴霧後の洗浄もさらに容易になる。 Furthermore, by using the cleaning device to clean the salt adhering to the surface of the partition plate, it is possible to always obtain light irradiation in a good state. If this washing is performed not only after spraying salt water but also immediately before spraying, a water film is formed on the surface of the partition plate, so that the adhesion of salt can be reduced. It becomes easier.
この洗浄装置は、仕切り板の幅方向に延びる樋状の流水溝を備えており、この流水溝から溢れさせた水を仕切り板の略全幅にわたってカーテン状に流下させることができる。流水溝と仕切り板との間隔は調整可能となされるのが好ましい。この構成によれば、洗浄のための水が試験室内や試験体の表面に跳ね返ることもなく、コストの低い簡単な機構で、効果的に塩分付着を防止することができる。 This cleaning device includes a bowl-shaped flowing water groove extending in the width direction of the partition plate, and the water overflowing from the flowing water groove can flow down in a curtain shape over substantially the entire width of the partition plate. The distance between the running water groove and the partition plate is preferably adjustable. According to this configuration, the water for cleaning does not splash back to the test chamber or the surface of the test body, and it is possible to effectively prevent salt adhesion with a simple mechanism with low cost.
また、本発明の複合劣化促進装置は、試験体の保持面が鉛直面に対して20度±10度の仰角をなすように構成されているので、JIS・Z2371の「塩水噴霧試験方法」に準拠した様々な種類の耐食性試験を行うことができる。当然ながら、光源ユニットも、上記保持面と平行に、つまり、試験室内側の表面が鉛直面に対して上記仰角と等しい20度±10度の俯角をなすように配置される。 Further, the composite deterioration accelerating device of the present invention is configured so that the holding surface of the test body forms an elevation angle of 20 degrees ± 10 degrees with respect to the vertical plane, so that it is in accordance with the “salt spray test method” of JIS / Z2371. Various types of corrosion resistance tests can be performed. Of course, the light source unit is also arranged in parallel with the holding surface, that is, the surface on the test chamber side forms a depression angle of 20 ° ± 10 ° equal to the elevation angle with respect to the vertical surface.
また、本発明の複合劣化促進装置は、試験体の保持台が、光源ユニットからの照射光の光軸方向に沿って移動することにより、照射距離を調整可能となされるのが好ましい。これによると、例えば光源の出力が使用時間とともに低下しても、その出力に応じて、試験体表面の照度分布や温度分布を適正に維持することができる。また、試験室内に噴霧される塩水の流動性等に応じて試験体の位置を変化させることもできる。 The composite deterioration acceleration device of the present invention, holder of the test body, by moving along the optical axis direction of the irradiation light from the light source unit, preferably Ru made adjustable irradiation distance. According to this, even if the output of the light source decreases with the use time, for example, the illuminance distribution and temperature distribution on the surface of the specimen can be properly maintained according to the output. Moreover, the position of the test body can be changed according to the fluidity of salt water sprayed into the test chamber.
また、本発明の複合劣化促進装置は、外形寸法の共通化された複数種類の光源ユニットが交換可能となされるのが好ましい。これにより、種類の異なる光線の影響を一台の装置で試験することが可能になり、装置の調達コストや運用コストを節約することができる。光源の種類は、耐候耐蝕性試験用としてはメタルハライドランプやキセノンランプ等の紫外線光源が好適であり、耐熱耐水性試験用としては赤外線ランプ等のランプ型可視・赤外光源が好適であるが、試験の目的等に応じて他の種類の光源を利用することも可能である。 The composite deterioration acceleration device of the present invention is preferably common to the plurality of types of light source unit external dimensions Ru made interchangeable. This makes it possible to test the influence of different types of light beams with a single device, and to save device procurement costs and operation costs. As the type of the light source, an ultraviolet light source such as a metal halide lamp or a xenon lamp is suitable for a weather corrosion resistance test, and a lamp-type visible / infrared light source such as an infrared lamp is suitable for a heat and water resistance test. It is possible to use other types of light sources depending on the purpose of the test.
また、本発明の複合劣化促進装置には、試験体の保持台の裏面に向かって冷却水を散布しうる冷却装置が設けられてもよい。これにより、試験体の裏面温度を制御しやすくなる。 Moreover, the composite deterioration promoting device of the present invention may be provided with a cooling device capable of spraying cooling water toward the back surface of the holding base of the test specimen. Thereby, it becomes easy to control the back surface temperature of the test body.
本発明の複合劣化促進装置は、試験室と光源ユニットとが仕切り板を隔てて区画されるので、光源の種類に関わらず、様々な条件下での試験が可能になり、試験室内の温湿度の制御も容易になる。また、試験室内に塩水が噴霧されて充満しても、光源ユニットが塩分の影響を受けないので、光源の維持管理も容易になる。さらに、仕切り板の表面を洗浄し得る洗浄装置を試験室内に設けることにより、常に良好な状態の光照射が得られる。 In the composite deterioration accelerating device of the present invention, the test chamber and the light source unit are partitioned with a partition plate therebetween, so that tests under various conditions are possible regardless of the type of light source, and the temperature and humidity in the test chamber are It becomes easy to control. Moreover, even if salt water is sprayed and filled in the test chamber, the light source unit is not affected by the salt content, so that the light source can be easily maintained and managed. Further, by providing a cleaning device in the test chamber that can clean the surface of the partition plate, light irradiation in a good state can always be obtained.
洗浄装置は、仕切り板の幅方向に延びる樋状の流水溝から溢れさせた水を仕切り板の略全幅にわたって流下させるように構成されているので、洗浄のための水が試験室内や試験体の表面に跳ね返ることもなく、コストの低い簡単な機構で、効果的に塩分付着を防止することができる。流水溝と仕切り板との間隔は調整可能となされるのが好ましい。 The cleaning device is configured to allow the water overflowing from the bowl-shaped flowing water groove extending in the width direction of the partition plate to flow down over almost the entire width of the partition plate. It is possible to effectively prevent salt adhesion with a simple mechanism with low cost without rebounding to the surface. The distance between the running water groove and the partition plate is preferably adjustable.
また、試験体の保持台を移動可能にして光源ユニットからの距離を拡縮させることにより、光源の出力に応じて、試験体表面の照度分布や温度分布を適正に維持することができる。試験体の保持台に20度±10度の仰角を付与して、その角度を調整できるようにすれば、JIS・Z2371の「塩水噴霧試験方法」に準拠した耐食性試験を行うことができる。 In addition, the illuminance distribution and the temperature distribution on the surface of the test body can be appropriately maintained according to the output of the light source by making the holding base of the test body movable and expanding and reducing the distance from the light source unit. If an elevation angle of 20 ° ± 10 ° is given to the holding base of the test body so that the angle can be adjusted, a corrosion resistance test based on the “salt spray test method” of JIS / Z2371 can be performed.
さらに、複数種類の光源ユニットの外形寸法を共通化して交換可能とすることにより、活用範囲が拡大し、装置の調達コストや運用コストを節約することができる。 Furthermore, by making the external dimensions of a plurality of types of light source units common and exchangeable, the range of utilization can be expanded, and the procurement cost and operation cost of the apparatus can be saved.
また、試験体の保持台の裏面を冷却し得る冷却装置を試験室内に設けることにより、試験体の裏面温度を制御しやすくなる。 Moreover, it becomes easy to control the back surface temperature of a test body by providing the cooling device which can cool the back surface of the holding stand of a test body in a test chamber.
以下、本発明の実施の形態について図を参照して説明する。 Hereinafter, embodiments of the present invention will be described with reference to the drawings.
図1〜図3は本発明の複合劣化促進装置の実施形態を示す。図1は平面図、図2は正面図、図3はA−A断面図である。 1 to 3 show an embodiment of the composite deterioration promoting apparatus of the present invention. 1 is a plan view, FIG. 2 is a front view, and FIG. 3 is an AA cross-sectional view.
この複合劣化促進装置1の本体は、一辺が2m弱程度の直方体形状で、正面から見て左側の上部に試験室11が設けられ、試験室11の背面側に光源室12、試験室11の右側に制御室13がそれぞれ設けられている。また、本体の外側には、電源供給ユニット14が接続されている。
The main body of the composite
試験室11内には、ガラリ状の通気部15によって区画された冷却室16が設けられ、この冷却室16に設置された冷却コイル17やファン18、試験室11の下側に設置された空冷式冷凍機19、制御室13内に設置された攪拌装置20、光源室12の下部に設置されたチラーユニット21や加湿器22等によって、温湿度を制御しうるようになっている。これらの制御は、本体の正面右側に設けられた制御パネル23を通じて操作される。また、冷却室16の上部と光源室12の上部には、排熱や換気のためのダクト24,25が接続されている。なお、上記装置類の構成や位置関係は単なる一例であり、全体の大きさや形状に応じて適宜、変更可能である。
In the
試験室11内には、試験体を定置するための保持台30が据え付けられている。保持台30は、ステンレス鋼やチタン等の高耐蝕性金属により形成され、試験体の保持面が背面側に向かって20度±10度の仰角θをなすように設置されている。この保持台30は、正面側から見て傾斜角θの登り勾配となるように設けられた基台31上に設置され、この基台31が適宜の角度調整手段によって傾斜角θを変更できるように取り付けられるとともに、保持台30が基台31上を前後方向に摺動しうるように保持されている。
In the
試験室11と光源室12との間には、保持台30の保持面と正対するようにして開口部が設けられ、この開口部の外側(光源室12側)に光源ユニット33が設置されている。光源ユニット33の表面には、透明の耐熱ガラス等からなる仕切り板32が取り付けられ、光源ユニット33からの照射光が仕切り板32を通じて保持台30の保持面を照射する。光源ユニット33及び仕切り板32は、保持台30に向かって俯角θの傾斜をなすように取り付けられ、この俯角θも適宜の調整手段によって変更できるようになっている。光源ユニット33は、例えばメタルハライドランプやキセノンランプ等の紫外線光源、あるいは赤外線ランプ等のランプ型可視・赤外光源を略箱型のユニット筐体に収容したもので、発光特性の異なる複数種類の光源ユニット33が共通の外形寸法に形成され、本体の背面側に設けられた着脱自在の取替口34を通じて簡単に交換できるようになっている。
An opening is provided between the
試験室11内における保持台30の裏面(正面)側には塩水噴霧装置40が設置され、噴霧ノズル41が上方に向けて突設されている。この塩水噴霧装置40には、外部に接続された塩水タンク42から塩水が供給される。また、塩水噴霧装置40の近傍からホース43が引き出されて保持台30の裏面に取り付けられ、このホース43から保持台30の裏面に冷却水が散布されるようになっている。
A
また、仕切り板32の上部付近には、仕切り板32の表面に水を流下させる流水溝44を備えた洗浄装置が設置されている。
In addition, near the upper portion of the
流水溝44は、仕切り板32の幅方向に延びる断面U字形ないし凹形の樋のような溝で、両端が閉じられ、その中にホース等を介して上方から水が流し込まれるようになっている。これにより、流水溝44から溢れた水が、仕切り板32の略全幅にわたって、仕切り板32の表面をカーテン状に流下する。流水溝44は、仕切り板32の上縁部から数ミリの距離に取り付けられて、仕切り板32までの距離を調整できるように保持されている。これにより、仕切り板32の俯角θを変化させた場合でも、仕切り板32の表面に良好な状態で水を流下させることができる。
The flowing
さらに、本体の正面から見て左側面には、試験室11内に試験体を出し入れするための開閉扉50が設けられている。この開閉扉50は、正面側を吊元として外開きになるように取り付けられている。このようにして開閉扉50を取り付けると、例えば紫外線等の照射中、作業者が照度を確認したりする必要から開閉扉50を開けた場合でも、光源が直接、作業者の目に入らず、作業者を強力な光照射から保護することができる。
Furthermore, an opening / closing
さらに、この開閉扉50の内側には、開閉扉50の開口面の一部を遮蔽しうる遮蔽板51が取り付けられ、開閉扉50の枠部から出し入れ可能に保持されている。この遮蔽板51には、試験室11内に照度計その他の計器類を挿入しうる小さな窓穴(図示せず)が形成されている。このような遮蔽板51を取り付けることにより、紫外線等の照射中であっても、試験室11内の状態をより安全に計測することが可能になる。
Further, a shielding
本発明の複合劣化促進装置は上記のように構成されているので、例えば、塩水(中性または酸性)噴霧→紫外線または赤外線を含む波長域の光照射→散水(中性または酸性)→高温高湿状態→冷却による結露→休止→乾燥、といったサイクルで、様々な劣化因子に対する複合的な試験を実施することができる。 Since the composite deterioration accelerating device of the present invention is configured as described above, for example, salt water (neutral or acidic) spray → light irradiation in a wavelength region including ultraviolet rays or infrared rays → water spray (neutral or acidic) → high temperature and high A combined test for various deterioration factors can be performed in a cycle of wet state → condensation due to cooling → resting → drying.
本発明の複合劣化促進装置は、建築物や車両の他、屋外に設けられる各種の設備・機械類の外装材として使用される材料の耐久性試験に幅広く利用することができる。 The composite deterioration accelerating device of the present invention can be widely used for durability tests of materials used as exterior materials for various facilities and machinery provided outdoors in addition to buildings and vehicles.
1 複合劣化促進装置
11 試験室
30 保持台
40 塩水噴霧装置
32 仕切り板
33 光源ユニット
44 流水溝
50 開閉扉
51 遮蔽板
DESCRIPTION OF
Claims (2)