JP3213383B2 - Pitch impregnation method for refractories - Google Patents

Pitch impregnation method for refractories

Info

Publication number
JP3213383B2
JP3213383B2 JP17998492A JP17998492A JP3213383B2 JP 3213383 B2 JP3213383 B2 JP 3213383B2 JP 17998492 A JP17998492 A JP 17998492A JP 17998492 A JP17998492 A JP 17998492A JP 3213383 B2 JP3213383 B2 JP 3213383B2
Authority
JP
Japan
Prior art keywords
pitch
impregnation
refractory
tank
impregnation tank
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP17998492A
Other languages
Japanese (ja)
Other versions
JPH0624873A (en
Inventor
徹 谷口
Original Assignee
日空工業株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 日空工業株式会社 filed Critical 日空工業株式会社
Priority to JP17998492A priority Critical patent/JP3213383B2/en
Publication of JPH0624873A publication Critical patent/JPH0624873A/en
Application granted granted Critical
Publication of JP3213383B2 publication Critical patent/JP3213383B2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【産業上の利用分野】本発明は、各種耐火物の気孔にピ
ッチを含浸させて、耐火度と耐久力を増大させるピッチ
含有耐火物を形成する過程における耐火物のピッチ含浸
方法に関するものである。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a method for impregnating pitch of refractories in a process of forming pitch-containing refractories for increasing the refractory degree and durability by impregnating the pores of various refractories with pitch. .

【0002】[0002]

【従来の技術】ピッチを含浸させた耐火煉瓦や、ルツボ
などピッチ含有の耐火物を形成するため、耐火材などの
粉末を混和しプレスにより圧縮成形した耐火物の素地の
気孔中に、ピッチを含浸させ、その上で焼成炭化させて
耐火度と耐久力の高いピッチ含有の耐火物を形成する際
の、耐火物中にピッチを含浸させる従来の方法として
は、含浸させる耐火物を、例えば200〜230℃迄加
熱する加熱炉を使用する工程と、加熱された耐火物を含
浸のため加熱状態のピッチを充満した含浸槽に入れる工
程と、そして含浸された耐火物を冷却装置内で冷却する
工程とを、各工程それぞれ別の装置で行なう方式が用い
られていた。
2. Description of the Related Art To form a pitch-containing refractory brick or a refractory containing a pitch such as a crucible, a pitch is impregnated into pores of a refractory base material which is formed by mixing powders such as refractory materials and compression-molding by pressing. A conventional method of impregnating a pitch in a refractory when forming a pitch-containing refractory having high fire resistance and durability by firing and carbonizing on the fired refractory is, for example, a method of impregnating a refractory with a pitch of 200 to Using a heating furnace to heat to ~ 230 ° C, placing the heated refractory into an impregnation bath filled with heated pitches for impregnation, and cooling the impregnated refractory in a cooling device And a process in which each step is performed by a separate apparatus.

【0003】しかしながら、上記の各工程の作業は、い
ずれも衛生状態が悪いため遠隔操作で行なう必要があ
り、排煙をフードで導出し、その排煙による公害の防止
対策のため大がかりな設備を要するので、設備費などが
嵩み、作業性も悪いという問題があった。
[0003] However, the work in each of the above steps must be performed by remote control because of poor hygiene conditions. Smoke exhaust is led out by a hood, and large-scale equipment is required to prevent pollution caused by the smoke exhaust. Therefore, there has been a problem that equipment costs are increased and workability is poor.

【0004】[0004]

【発明が解決しようとする課題】本発明は、前記従来の
問題点を解決するためになされたものであり、耐火物の
ピッチ含浸時の工程を一つの含浸槽内で全て行なうこと
ができ、公害発生が最少限におさえられ、しかも作業性
がよく、経済的な耐火物のピッチ含浸方法を提供するこ
とを目的としている。
DISCLOSURE OF THE INVENTION The present invention has been made to solve the above-mentioned conventional problems, and all steps of pitch impregnation of a refractory can be performed in one impregnation tank. It is an object of the present invention to provide an economical method of pitch impregnation of refractories, in which the occurrence of pollution is minimized and the workability is good.

【0005】[0005]

【課題を解決するための手段】上記の目的を達成するた
め、本発明の耐火物のピッチ含浸方法は、含浸させる耐
火物を含浸槽に挿入の後、含浸槽内を所定温度まで加熱
の上で真空状態にして、加熱状態のピッチで含浸槽を充
満し、窒素などの不活性ガスで含浸槽内を所定圧力まで
加圧し、所定時間保持の上、含浸槽内のピッチを排出し
た状態で含浸槽内を徐々に冷却して、ピッチ含有耐火物
を取り出すことを特徴としたものである。
In order to achieve the above object, the method of pitch impregnation of refractories according to the present invention comprises inserting the refractories to be impregnated into the impregnation tank, and then heating the inside of the impregnation tank to a predetermined temperature. Fill the impregnation tank with the pitch in the heated state, pressurize the inside of the impregnation tank with an inert gas such as nitrogen to a predetermined pressure, hold for a predetermined time, and discharge the pitch in the impregnation tank. It is characterized in that the pitch-containing refractory is taken out by gradually cooling the inside of the impregnation tank.

【0006】[0006]

【作用】上記のピッチ含浸方法によれば、含浸槽内に常
温で挿入された耐火物はまず昇温され、加熱状態で槽内
を真空にし、加熱状態のピッチをその槽内に導入充満さ
せた後、所定の圧力迄加圧することにより、耐火物の気
孔内に真空状態でピッチを容易に含浸させることがで
き、またピッチを槽内から排出させ、冷却させること
で、一つの含浸槽内で一連の工程の全てを行なうことが
できる。
According to the pitch impregnation method described above, the refractory inserted into the impregnation tank at normal temperature is first heated, the inside of the tank is evacuated in a heated state, and the heated pitch is introduced and filled in the tank. After that, the pitch can be easily impregnated in a vacuum state into the pores of the refractory by pressurizing to a predetermined pressure, and the pitch is discharged from the tank and cooled, so that the inside of one impregnation tank is cooled. Can perform all of the series of steps.

【0007】[0007]

【実施例】以下図面を参照して本発明の含浸方法を適用
して耐火物のピッチ含浸作業を行なう装置の一実施例を
説明する。図面は、上記含浸装置のフローシートであ
り、含浸させる耐火物は常温で含浸槽1に挿入されるよ
うになっており、この含浸槽1内を加熱するため熱媒ボ
イラー2と、含浸槽1内を徐々に冷却するための水Wを
媒体とした熱交換器3が設けられている。
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS An embodiment of an apparatus for performing a pitch impregnation of a refractory by applying the impregnation method of the present invention will be described below with reference to the drawings. The drawing is a flow sheet of the impregnating apparatus, in which a refractory to be impregnated is inserted into an impregnation tank 1 at normal temperature, and a heating medium boiler 2 for heating the impregnation tank 1 and an impregnation tank 1 A heat exchanger 3 using water W as a medium for gradually cooling the inside is provided.

【0008】また、熱媒ボイラー2からの熱媒体Mとし
て、この実施例では油を使用し、含浸槽1の周囲にはこ
の加熱油が循環する加熱部5が設けられ、またその循環
経路には膨張タンク6を設けている。一方、含浸槽1内
を真空にするために、真空ポンプ7が設けられ、その管
路には、含浸槽1内に不活性ガス、例えば窒素N2 を充
満させるための窒素供給管8が接続されており、真空弁
9および窒素弁10がそれぞれ配設されている。
In this embodiment, an oil is used as the heat medium M from the heat medium boiler 2, and a heating section 5 for circulating the heat oil is provided around the impregnation tank 1. Has an expansion tank 6. On the other hand, a vacuum pump 7 is provided to evacuate the impregnation tank 1, and a nitrogen supply pipe 8 for filling the impregnation tank 1 with an inert gas, for example, nitrogen N 2 , is connected to the vacuum pump 7. A vacuum valve 9 and a nitrogen valve 10 are provided respectively.

【0009】次に、貯溜槽11の周囲にはピッチPを加
熱するため、熱媒ボイラー12から熱媒Nを循環させる
加熱部13が設けられ、この貯溜槽11にピッチPを供
給する受入れ槽14もこの熱媒ボイラー12からの熱媒
体Nで熱交換により加熱されるようになっており、ま
た、加熱したピッチPを含浸槽1内に充満する際には貯
溜槽11内に不活性ガス、例えば窒素ガスN2 を供給す
るため窒素供給管8と窒素弁10が設けられている。
Next, a heating section 13 for circulating a heating medium N from a heating medium boiler 12 is provided around the storage tank 11 for heating the pitch P. A receiving tank for supplying the pitch P to the storage tank 11 is provided. 14 is also heated by heat exchange with the heat medium N from the heat medium boiler 12, and when the heated pitch P is filled in the impregnation tank 1, an inert gas is stored in the storage tank 11. For example, a nitrogen supply pipe 8 and a nitrogen valve 10 for supplying nitrogen gas N 2 are provided.

【0010】なお、図中の15で示すのはそれぞれフィ
ルターであり、16で示すのは開閉弁である。次に、上
記の構成からなるこの実施例の含浸装置により耐火物を
含浸する工程について説明すると、まず、含浸させる耐
火物をパレットなどに積んで常温で含浸槽1に挿入の
後、含浸槽1を熱媒ボイラー2からの約340℃の熱媒
体Mで加熱し、被含浸物である耐火物を約200から2
30℃まで昇温させる。
In the figure, reference numeral 15 denotes a filter, and reference numeral 16 denotes an on-off valve. Next, the step of impregnating the refractory with the impregnating apparatus of this embodiment having the above configuration will be described. First, the refractory to be impregnated is loaded on a pallet or the like and inserted into the impregnation tank 1 at room temperature. Is heated with a heating medium M at about 340 ° C. from the heating medium boiler 2 to remove the refractory as an impregnated substance from about 200 to 2
Raise the temperature to 30 ° C.

【0011】上記の加熱を約10時間行なった後、含浸
槽1内の空気を排除するため、真空弁9を開けて真空ポ
ンプ7により真空として、貯溜槽11内の約200から
230℃まで加熱されたピッチPを約2kg/cm2 圧の窒
素N2 で加圧し、窒素弁10を開けることで含浸槽1内
に充満させる。ピッチPが充満した含浸槽1内に窒素弁
10を開けることで窒素供給管8からの不活性ガスであ
る窒素N2 により16kg/cm2 まで加圧するが、この加
圧する圧は、被含浸物や加圧時間により適宜決定される
ものであり、この状態で所定時間保持することにより、
被含浸物である耐火物の気孔内にピッチを浸入させるこ
とができるが、この含浸時間にはこの実施例では約4時
間を要している。
After the above heating is performed for about 10 hours, the vacuum valve 9 is opened and the vacuum pump 7 is evacuated to remove the air in the impregnation tank 1 to heat the storage tank 11 from about 200 to 230 ° C. The pitch P is pressurized with nitrogen N 2 at a pressure of about 2 kg / cm 2 , and the impregnation tank 1 is filled by opening the nitrogen valve 10. By opening the nitrogen valve 10 in the impregnation tank 1 filled with the pitch P, the pressure is increased to 16 kg / cm 2 by nitrogen N 2 which is an inert gas from the nitrogen supply pipe 8. And the pressurizing time are appropriately determined, and by holding in this state for a predetermined time,
The pitch can be penetrated into the pores of the refractory material to be impregnated, but this impregnation time takes about 4 hours in this embodiment.

【0012】その後、含浸槽1内に窒素N2 を供給する
ことにより充満したピッチPを貯溜槽11側に戻した
後、水Wを媒体とした熱交換器3により熱媒体Mを介し
て徐々に含浸槽1を冷却させるが、この場合の冷却に、
この実施例では約8時間を要しており、冷却後は含浸槽
1からピッチ含有耐火物を取り出し、その後ベーキング
炉などによりさらにそれを炭化させて耐火物の耐火度と
耐久力を増大させる工程に入る。
Thereafter, the filled pitch P is returned to the storage tank 11 by supplying nitrogen N 2 into the impregnation tank 1, and then gradually through the heat medium M by the heat exchanger 3 using water W as a medium. The impregnation tank 1 is cooled in this case.
In this embodiment, about 8 hours are required. After cooling, a step of removing the pitch-containing refractory from the impregnation tank 1 and thereafter further carbonizing it with a baking furnace or the like to increase the refractory and durability of the refractory. to go into.

【0013】なお、上記の含浸装置には、含浸槽1、貯
溜槽11、熱交換器3、熱媒ボイラー2および受入れ槽
14をそれぞれ複数基分設けて、それぞれ配管により接
続して効率よく含浸作業を行なうことが望ましく、例え
ばこの実施例では3基分の各機器を組合せて設けてい
る。
The impregnating apparatus is provided with a plurality of impregnating tanks 1, storage tanks 11, heat exchangers 3, heat medium boilers 2, and receiving tanks 14, each of which is connected by a pipe and efficiently impregnated. It is desirable to carry out the work. For example, in this embodiment, three devices are provided in combination.

【0014】[0014]

【発明の効果】以上に説明した本発明の耐火物のピッチ
含浸方法によれば、従来、加熱、含浸および冷却の三つ
の工程を別々の装置で行なっていた全工程を、本発明で
は一つの含浸槽で全て行なうことになり、公害発生を最
少限におさえることができ、しかも作業性が向上して経
済的な含浸作業ができるという効果がある。
According to the method for impregnating pitch of refractories of the present invention described above, all steps in which three steps of heating, impregnation and cooling are conventionally performed by separate apparatuses are now replaced by one in the present invention. Since all the operations are performed in the impregnation tank, the generation of pollution can be minimized, and the workability is improved and the economic impregnation operation can be performed.

【図面の簡単な説明】[Brief description of the drawings]

【図1】本発明の耐火物の含浸方法を適用した含浸装置
の一実施例のフローシートである。
FIG. 1 is a flow sheet of one embodiment of an impregnation apparatus to which a method for impregnating a refractory according to the present invention is applied.

【符号の説明】[Explanation of symbols]

1 含浸槽 2 熱媒ボイラ
ー 3 熱交換器 7 真空ポンプ 8 窒素供給管 11 貯溜槽 N2 窒素 P ピッチ
1 impregnation vessel 2 heat medium boiler 3 heat exchanger 7 vacuum pump 8 nitrogen feed pipe 11 the reservoir N 2 nitrogen P Pitch

Claims (1)

(57)【特許請求の範囲】(57) [Claims] 【請求項1】 含浸させる耐火物を含浸槽に挿入の後、
含浸槽内を所定温度まで加熱し、真空状態にして、加熱
状態のピッチで含浸槽を充満し、不活性ガスで含浸槽内
を所定圧力まで加圧し、所定時間保持の上、含浸槽内の
ピッチを排出した状態で含浸槽内を冷却する耐火物のピ
ッチ含浸方法。
After the refractory to be impregnated is inserted into the impregnation tank,
The inside of the impregnation tank is heated to a predetermined temperature, vacuumed, the impregnation tank is filled with a pitch in a heated state, the inside of the impregnation tank is pressurized to a predetermined pressure with an inert gas, and maintained for a predetermined time, and then the inside of the impregnation tank is maintained. A pitch impregnation method for a refractory in which the inside of an impregnation tank is cooled with the pitch discharged.
JP17998492A 1992-07-07 1992-07-07 Pitch impregnation method for refractories Expired - Lifetime JP3213383B2 (en)