JP3132237U - Cutting form correction method tatami - Google Patents

Cutting form correction method tatami Download PDF

Info

Publication number
JP3132237U
JP3132237U JP2006010792U JP2006010792U JP3132237U JP 3132237 U JP3132237 U JP 3132237U JP 2006010792 U JP2006010792 U JP 2006010792U JP 2006010792 U JP2006010792 U JP 2006010792U JP 3132237 U JP3132237 U JP 3132237U
Authority
JP
Japan
Prior art keywords
tatami
shrinkage
tatami mat
polystyrene foam
gap
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP2006010792U
Other languages
Japanese (ja)
Inventor
政典 岸本
Original Assignee
有限会社岸本明商店
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 有限会社岸本明商店 filed Critical 有限会社岸本明商店
Priority to JP2006010792U priority Critical patent/JP3132237U/en
Application granted granted Critical
Publication of JP3132237U publication Critical patent/JP3132237U/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

【課題】畳の部屋の隙間の発生を抑える
【解決手段】畳の部屋の隙間は木材のそりによって生じる場合と畳の縮みによって生じる場合がある。ここでは、畳の縮みによる隙間の発生を抑える為、畳の縮みの原因である断熱材フォームをそのまま使用するのではなく、5cm巾に切断後に縫着し、他の構成品に縮む力が伝わらないようにした。これにより、畳の縮みは最小限となり、部屋に隙間が生じなくなる。
【選択図】図1
To suppress the generation of a gap between tatami rooms, the gap between tatami rooms may be caused by warping of wood or by shrinkage of the tatami. Here, in order to suppress the generation of gaps due to the shrinkage of the tatami mat, the heat insulating foam that causes the shrinkage of the tatami mat is not used as it is, but it is sewn after cutting to a width of 5 cm and the shrinkage force is transmitted to other components. I tried not to. As a result, the shrinkage of the tatami mat is minimized, and no gaps are generated in the room.
[Selection] Figure 1

Description

本考案は、畳の芯材および畳に関する。The present invention relates to a tatami core and a tatami mat.

従来の技術では畳の部屋に生じた隙間は、数年に一度の表替時に手直しをして対処してきた。In the conventional technique, the gap generated in the tatami room has been dealt with by repairing it once every several years.

畳の部屋に生じる隙間は、部屋の木材のそりにより生じる場合と、畳の縮みにより生じる場合があるが、後者が原因の場合は、この考案で解決、改善できる。畳の縮みは縦方向2:横方向1の割合で生じる。これは、畳の構成品の中のポリスチレンフォームが、永年使用することにより縮む為である。本考案は、このポリスチレンフォームの縮む性質を他の構成品に伝えないことで、最終的に畳自体の縮みを防ぐものである。The gap generated in the room of the tatami may be caused by warping of the wood in the room or by shrinkage of the tatami. If the latter is the cause, it can be solved and improved by this device. The shrinkage of the tatami occurs in the ratio of the vertical direction 2: the horizontal direction 1. This is because the polystyrene foam in the components of the tatami mat shrinks when used for many years. In the present invention, the shrinkage property of the polystyrene foam is not transmitted to other components, and finally the shrinkage of the tatami mat itself is prevented.

課題を解決する為の手段Means to solve the problem

本考案は、畳の縮みの原因であるポリスチレンフォームを巾5cmに切断する。その上で同じ状態で並べ置き、上下をインシュレーションボードでサンドイッチ状にはさみ、糸間隔6cmで縫着する。24本の横糸が縦にそれぞれ30ヶ所以上縫い合わさることにより、切断面は安定する。また、切断面に竹炭、活性炭などの粒状炭を挟みこむことにより、キシミ音なしで炭入畳ができる。The present invention cuts polystyrene foam, which is the cause of tatami mat shrinkage, to a width of 5 cm. Then, place them in the same state, sandwich the top and bottom with an insulation board, and sew them at a thread spacing of 6 cm. The cut surface is stabilized when 24 wefts are sewn in the vertical direction at 30 or more locations. In addition, by inserting granular charcoal such as bamboo charcoal or activated carbon into the cut surface, charcoal can be folded without squeaking noise.

考案を実施する為の最良の形態Best mode for carrying out the invention

本考案の実施の形態を図面を参照して例をあげながら説明する。〔図1〕はポリスチレンフォーム(2)をインシュレーションボード(1)でサンドイッチ状にはさみ、糸(3)で縫着した畳の断面図である。〔図2〕は〔図1〕が数年経過し縮みが生じた断面である。真ん中のポリスチレンフォームは、明らかに段差となって、縮んでいるが、この縮む力は上下のインシュレーションボードにも縫着されているため伝わり、畳全体にも縮みが生じている。〔図5〕は8畳が敷きこまれた平面図で、隙間が生じる場所をあらわす。〔図3〕は、本考案である、ポリスチレンフォームを巾5cmに切断し、糸でインシュレーションボードと縫着した畳の断面図である。〔図4〕は〔図3〕が数年経過し、ポリスチレンフォームに縮みが発生した断面図であるが、縮みは内部に隙間を生じさせるものの、糸の縫着間隔のほうが大きい為、インシュレーションボードに対し、縮みの力を与えないので、畳の縮みの発生を最小限に抑えることができたことをあらわした図である。〔図6〕は、さらに竹炭、活性炭(5)を切断したポリスチレンフォームの間に入れたものである。Embodiments of the present invention will be described with reference to the drawings. [FIG. 1] is a cross-sectional view of a tatami mat in which polystyrene foam (2) is sandwiched between insulation boards (1) and sewn with thread (3). [FIG. 2] is a cross section in which [FIG. 1] shrinks after several years. The polystyrene foam in the middle is clearly stepped and shrunk, but this shrinking force is transmitted to the upper and lower insulation boards, and the entire tatami mat is shrunk. [FIG. 5] is a plan view in which 8 tatami mats are laid, and represents a place where a gap is generated. FIG. 3 is a sectional view of a tatami mat according to the present invention, in which a polystyrene foam is cut to a width of 5 cm and sewn to an insulation board with a thread. [FIG. 4] is a cross-sectional view in which the shrinkage occurs in the polystyrene foam after several years in [FIG. 3]. Although the shrinkage causes a gap in the interior, the thread sewing interval is larger, so the insulation It is a diagram showing that the generation of tatami mat shrinkage can be minimized because no contraction force is applied to the board. [FIG. 6] shows a case where bamboo charcoal and activated carbon (5) are further placed between the cut polystyrene foams.

考案の効果Effect of device

本考案を利用すれば、畳の部屋に生じる隙間を最小限にし、ゴミやホコリなどがたまる不衛生な環境をなくすことができる。さらに竹炭や活性炭の効果により健康的な住空間を保つことができる。If this invention is used, the gap which arises in a tatami room can be minimized, and the unsanitary environment where dust, dust, etc. can accumulate can be eliminated. Furthermore, a healthy living space can be maintained by the effect of bamboo charcoal and activated carbon.

インシュレーションボードでポリスチレンフォームをはさみ、糸で縫着した畳の仕上がり断面図である。It is a finished sectional view of a tatami mat sandwiched with polystyrene foam with an insulation board and sewn with thread. 図1のものが数年経過した時点で縮んだ断面図である。It is sectional drawing shrunk when the thing of FIG. 1 passed several years. ポリスチレンフォームを切断した畳の仕上がり断面図である。It is the finishing sectional drawing of the tatami which cut | disconnected the polystyrene foam. 図3のものが数年経過した時点で縮んだ断面図である。It is sectional drawing shrunk when the thing of FIG. 3 passed several years. 一般的な敷き方をした8畳間の平面図である。It is a top view between 8 tatami mats in a general manner. ポリスチレンフォームの切断面に竹炭、活性炭を入れたものの断面図である。It is sectional drawing of what put bamboo charcoal and activated carbon in the cut surface of a polystyrene foam.

符号の説明Explanation of symbols

1 インシュレーションボード
2 ポリスチレンフォーム
3 縫着糸
4 縮みによって生じた隙間
5 粒状の竹炭、活性炭
DESCRIPTION OF SYMBOLS 1 Insulation board 2 Polystyrene foam 3 Sewing thread 4 Crevice produced by shrinkage 5 Granular bamboo charcoal, activated carbon

Claims (2)

断熱材であり、畳の芯材であるポリスチレンフォームを巾5cmに切断し、再び成型することにより、断熱性を生かしながら、他の構成品(インシュレーションボードなど)に縮む力を与えず、畳全体の縮みを最小限に抑えた畳By cutting the polystyrene foam, which is a heat insulating material and the core material of the tatami mat, into a width of 5 cm, and then remolding it, the tatami mat does not give shrinkage to other components (insulation board, etc.) while taking advantage of the heat insulating properties. Tatami with minimal overall shrinkage 切断したポリスチレンフォームを再び成型する断面に竹炭、活性炭などの粒状炭を入れることにより、さらに住環境を改善することができる請求項1の畳The tatami mat according to claim 1, wherein the living environment can be further improved by putting granular charcoal such as bamboo charcoal and activated carbon into the cross section for re-molding the cut polystyrene foam.
JP2006010792U 2006-12-12 2006-12-12 Cutting form correction method tatami Expired - Fee Related JP3132237U (en)