JP2923554B2 - Copper tube welding method and gas pressure adjusting tool during welding of copper tube - Google Patents

Copper tube welding method and gas pressure adjusting tool during welding of copper tube

Info

Publication number
JP2923554B2
JP2923554B2 JP30654997A JP30654997A JP2923554B2 JP 2923554 B2 JP2923554 B2 JP 2923554B2 JP 30654997 A JP30654997 A JP 30654997A JP 30654997 A JP30654997 A JP 30654997A JP 2923554 B2 JP2923554 B2 JP 2923554B2
Authority
JP
Japan
Prior art keywords
gas pressure
welding
copper
copper tube
pipe
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP30654997A
Other languages
Japanese (ja)
Other versions
JPH11123593A (en
Inventor
博 杉山
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SUGYAMA KINZOKU KK
Original Assignee
SUGYAMA KINZOKU KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SUGYAMA KINZOKU KK filed Critical SUGYAMA KINZOKU KK
Priority to JP30654997A priority Critical patent/JP2923554B2/en
Publication of JPH11123593A publication Critical patent/JPH11123593A/en
Application granted granted Critical
Publication of JP2923554B2 publication Critical patent/JP2923554B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【発明の属する技術分野】この発明は、冷凍・空調など
の配管時における銅管の溶接方法、及び銅管の溶接時に
おける管内ガス圧の調整用具に関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a method for welding a copper pipe at the time of piping such as refrigeration and air conditioning, and a tool for adjusting the gas pressure in the pipe at the time of welding the copper pipe.

【0002】[0002]

【従来の技術、及び発明が解決しようとする課題】銅管
は、その素材からして加工性、耐食性などが良いうえに
色調も美しく、比較的安価であることとも相まって、冷
凍・空調などの配管材として一般に広く使用されている
ものである。
2. Description of the Related Art Copper tubes have good workability, corrosion resistance, etc., are beautiful in color, and are relatively inexpensive. It is generally widely used as a piping material.

【0003】ところで、かかる銅管を冷凍・空調などの
配管時に溶接して接続せしめるさいには、溶接時の加熱
作用により銅管内部が酸化してスケ−ルを生起せしめ、
種々の弊害を招来せしめるものである。このため、従来
より、かかる銅管内部の酸化を防止せしめるべく、溶接
時に銅管の一端開口部より他端開口部に向けて窒素ガス
を噴出せしめつつ行う溶接方法が一般に広く採られてい
る。しかしながら、かかる銅管の溶接方法は、銅管内部
の酸化を有効に防止せしめることが出来る反面、実際の
配管工事においては非常に重い窒素ボンベの持ち運びや
管理・確認の難しさなどの面から非常に作業性が悪いも
のとなっていた。
By the way, when such a copper tube is welded and connected at the time of piping such as refrigeration and air conditioning, the inside of the copper tube is oxidized by a heating action at the time of welding to produce a scale.
It causes various adverse effects. For this reason, conventionally, in order to prevent such oxidation inside the copper tube, a welding method in which nitrogen gas is ejected from one end opening of the copper tube toward the other end opening thereof at the time of welding has been widely adopted. However, while this copper pipe welding method can effectively prevent oxidation inside the copper pipe, it is very difficult in actual piping work to carry a heavy nitrogen cylinder and to make it difficult to manage and check. Workability was poor.

【0004】上記従来例の問題点を解決するものとし
て、エステル系エアゾ−ルタイプなど所要の酸化防止剤
を銅管内に吹き付けて行う銅管の溶接方法が提案されて
おり、これを図5及び図6に基づいて説明する。まず、
接続せしめるべき各銅管11の開口部よりエステル系エ
アゾ−ルタイプなど所要の酸化防止剤Aを内部に吹き付
ける(図5参照)。しかるのち、銅製エルボ12を介し
て被接続用銅管11どうしを接続せしめ、接続箇所をガ
ス溶接法やロウ接法など所要の溶接手段13でもって溶
接せしめる(図6参照)。このさい、銅管11内周面に
付着した酸化防止剤Aが溶接時の加熱作用を受けて分解
・ガス化し、銅管11内に充満しつつ還元作用して銅管
11内周面の酸化を防止せしめ、スケ−ルの発生を阻止
せしめるものである。
In order to solve the above-mentioned problems of the prior art, a method of welding a copper pipe by spraying a required antioxidant such as an ester type aerosol into the copper pipe has been proposed. Explanation will be given based on FIG. First,
A required antioxidant A such as an ester-based aerosol type is sprayed from the opening of each copper tube 11 to be connected (see FIG. 5). Thereafter, the copper pipes 11 to be connected are connected to each other via the copper elbow 12, and the connection portions are welded by a required welding means 13 such as a gas welding method or a brazing method (see FIG. 6). At this time, the antioxidant A attached to the inner peripheral surface of the copper tube 11 is decomposed and gasified by the heating action during welding, and is reduced while filling the inside of the copper tube 11 to oxidize the inner peripheral surface of the copper tube 11. To prevent the occurrence of scale.

【0005】ところで、上記の従来例は、その操作を極
めて簡単に行う事が出来る反面、接接せしめるべき銅管
11の両端開口部を開放せしめた状態下にエステル系エ
アゾ−ルタイプなど所要の酸化防止剤Aを吹き付けて溶
接せしめるものであるから、かかる酸化防止剤Aが溶接
時の加熱作用を受けて分解・ガス化し、銅管11両端の
開口部を通して外方に流出しやすいものであって、銅管
11内の還元雰囲気を著しく損いやすく、ひいては、銅
管11内周面が酸化してスケ−ルを発生せしめやすいも
のである。
In the above-mentioned conventional example, the operation can be performed very easily. On the other hand, the required oxidation such as an ester-based aerosol type is performed under the condition that both ends of the copper tube 11 to be brought into contact are opened. Since the antioxidant A is sprayed and welded, the antioxidant A is easily decomposed and gasified by the heating action at the time of welding, and easily flows out through the openings at both ends of the copper pipe 11. In addition, the reducing atmosphere in the copper tube 11 is easily damaged, and the inner peripheral surface of the copper tube 11 is easily oxidized to generate scale.

【0006】かかる従来例の問題点を解決するものとし
て、銅管内部に酸化防止剤を吹き付けたのち両端開口部
を閉塞せしめつつ溶接せしめる方法が考えられるが、か
かる場合には、銅管内周面の酸化を有効に防止せしめる
ことが出来る反面、酸化防止剤の分解・ガス化によって
銅管内のガス圧が異常に高くなり、溶接ロウの浸透に悪
影響を及ぼして溶接不良を生じやすいものである。
In order to solve the problems of the conventional example, a method of spraying an antioxidant into the inside of the copper pipe and then welding while closing the openings at both ends can be considered. While it can effectively prevent oxidation of the surface, the gas pressure inside the copper tube becomes abnormally high due to the decomposition and gasification of the antioxidant, which adversely affects the penetration of the welding braze and easily causes welding defects. is there.

【0007】この発明は、かかる従来例の問題点を一挙
に解決し、銅管内部にエステル系エアゾ−ルタイプなど
所要の酸化防止剤を吹き付け、溶接ロウの浸透などに悪
影響を及ぼすことなく酸化防止機能を確実に発揮せし
め、スケ−ルの発生を有効に防止せしめることが出来る
銅管の溶接方法、及びかかる溶接時に使用するガス圧調
整用具を提供しようとするものである。
The present invention solves the problems of the prior art at a glance, and sprays a required antioxidant such as an ester-based aerosol type into the inside of a copper tube to prevent oxidation without adversely affecting the penetration of a welding wax. An object of the present invention is to provide a method for welding a copper pipe, which can surely exhibit its function and effectively prevent the occurrence of scale, and a gas pressure adjusting tool used at the time of such welding.

【0008】[0008]

【課題を解決するための手段】即ち、この出願の請求項
1に係る発明は、銅管どうしを管継手でもって接続せし
めるべく各銅管の内部にエステル系エアゾ−ルタイプな
ど所要の酸化防止剤を吹き付けて溶接せしめるさいに、
上記銅管の各開口端を所要の閉塞部材でもって閉塞せし
めると共に、該閉塞部材の少くとも一個にガス圧調整用
の逃げ孔を設け、該逃げ孔より酸化防止剤の加熱に伴っ
て発生するガスを適宜逃しつつ管内ガス圧を適正に調整
保持せしめることを特徴とする、銅管の溶接方法を要旨
とするものである。
That is, the invention according to claim 1 of the present application provides a required antioxidant, such as an ester-based aerosol type, inside each copper tube in order to connect the copper tubes with a pipe joint. Spraying and welding
Each opening end of the copper pipe is closed with a required closing member, and at least one of the closing members is provided with a relief hole for adjusting gas pressure, and the relief hole is generated by heating the antioxidant from the relief hole. A gist of the present invention is a method for welding a copper pipe, characterized in that the gas pressure in the pipe is appropriately adjusted and held while appropriately releasing gas.

【0009】そして、この発明に係る銅管の溶接方法
は、溶接時に酸化防止剤の分解・ガス化によって発生す
るガスを適宜外方ヘ逃しつつ、銅管内のガス圧を常に適
正に調整保持せしめ、還元雰囲気や溶接ロウの浸透に悪
影響を及ぼすことなく酸化防止機能を確実に発揮せしめ
ることが出来るものである。
In the method for welding a copper pipe according to the present invention, the gas pressure in the copper pipe is always appropriately adjusted and maintained while appropriately releasing gas generated by decomposition and gasification of the antioxidant during welding to the outside. At the very least, the antioxidant function can be reliably exerted without adversely affecting the reducing atmosphere and the penetration of the welding braze.

【0010】さらに、この出願の請求項2に係る発明
は、管継手を介して溶接手段により接続せしめる銅管の
開口端に着脱自在とされた盲状の閉塞用キャップ体と、
同所要径の逃げ孔を有するガス圧調整用キャップ体とよ
りなり、上記各キャップ体を各々接続せしめるべき銅管
の開口端に適宜取付け、溶接時に酸化防止剤の加熱に伴
って発生するガスを適宜逃しつつ管内ガス圧を適正に調
整保持せしめることを特徴とする、銅管の溶接時におけ
る管内ガス圧の調整用具を要旨とするものである。
Further, the invention according to claim 2 of the present application provides a blind closing cap body detachably attached to an open end of a copper pipe connected by welding means via a pipe joint,
A gas pressure adjusting cap body having an escape hole of the same required diameter, which is appropriately attached to the opening end of a copper pipe to be connected to each of the cap bodies, and a gas generated by heating the antioxidant during welding. The gist of the invention is a tool for adjusting the gas pressure in a pipe at the time of welding a copper pipe, which is characterized in that the gas pressure in the pipe is appropriately adjusted and held while being appropriately released.

【0011】そして、この発明に係る管内ガス圧の調整
用具は、溶接せしめるべき一方の銅管の一端部に閉塞用
キャップ体を嵌着せしめると共に、他方の銅管の一端部
にガス圧調整用キャップ体を嵌着せしめて使用に供す
る。そして、各銅管の開口端部より内部にエステル系エ
アゾ−ルタイプなど所要の酸化防止剤を吹き付けると共
に、管継手により接続せしめて溶接を行なうさいには、
酸化防止剤の分解・ガス化によって発生するガスをガス
圧調整用キャップ体の逃げ孔より適宜外方に逃しつつ、
銅管内のガス圧を常に適正に調整保持せしめるものであ
る。
The gas pressure adjusting tool according to the present invention has a capping member fitted to one end of one copper tube to be welded and a gas pressure adjusting device attached to one end of the other copper tube. The cap body is fitted for use. Then, while spraying a required antioxidant such as an ester-based aerosol type from the opening end of each copper tube to the inside, and connecting with a pipe joint to perform welding,
While appropriately releasing gas generated by decomposition and gasification of the antioxidant from the escape hole of the gas pressure adjusting cap body,
The gas pressure in the copper tube is always adjusted and maintained properly.

【0012】[0012]

【発明の実施の形態】以下に、この発明の一実施例を図
面に基づいて説明する。なお、図面中、14は溶接せし
めるべき銅管11の開口端縁に嵌着自在とされた盲状の
閉塞用キャップ体、15は同様に嵌着自在とされたガス
圧調整用キャップ体で、該ガス圧調整用キャップ体15
の中心には小径状の逃げ孔16が形成されている。その
他は従来例と同一であり、同一符号は同一部分を示す。
DESCRIPTION OF THE PREFERRED EMBODIMENTS An embodiment of the present invention will be described below with reference to the drawings. In the drawings, reference numeral 14 denotes a blind closing cap body which can be fitted to the opening edge of the copper tube 11 to be welded, and reference numeral 15 denotes a gas pressure adjusting cap body which can be similarly fitted. The gas pressure adjusting cap body 15
Is formed with a small-diameter relief hole 16 at the center of the hole. Other parts are the same as those of the conventional example, and the same reference numerals indicate the same parts.

【0013】まず、溶接せしめるべき一方の銅管11の
一端部に閉塞用キャップ体14を嵌着せしめると共に、
他方の銅管11の一端部にガス圧調整用キャップ体15
を嵌着せしめたのち、各銅管11の開口端部より内部に
エステル系エアゾ−ルタイプなど所要の酸化防止剤Aを
吹き付ける(図1参照)。しかるのち、エルボ12を介
して銅管11どうしを接続せしめ、銅管11の接続箇所
をロウ接など所要の溶接手段13でもって溶接せしめる
(図2参照)。このさい、銅管11内周面に付着した酸
化防止剤Aが溶接時の加熱作用を受けて分解・ガス化
し、銅管11内に充満してガス圧を生起するも、ガス圧
調整用キャップ体15の逃げ孔16を通して発生ガスを
適宜排出せしめることにより銅管11内のガス圧を常に
一定に調整保持せしめることが出来る。このため、銅管
11内の還元雰囲気や溶接ロウの浸透に悪影響を及ぼす
ことなく酸化防止機能を確実に発揮せしめ、スケ−ルの
発生を有効に防止せしめて常に確実なる溶接を行うこと
が出来るものである。溶接が終了すると、銅管11の両
端より各々閉塞用キャップ体14とガス圧調整用キャッ
プ体15を取外し、溶接作業を完了する。
First, a closing cap body 14 is fitted to one end of one copper tube 11 to be welded,
A gas pressure adjusting cap body 15 is attached to one end of the other copper tube 11.
After that, a required antioxidant A such as an ester-based aerosol type is sprayed from the open end of each copper tube 11 (see FIG. 1). Thereafter, the copper pipes 11 are connected to each other via the elbows 12, and the connection portions of the copper pipes 11 are welded by required welding means 13 such as brazing (see FIG. 2). At this time, the antioxidant A adhering to the inner peripheral surface of the copper tube 11 is decomposed and gasified by the heating action during welding and fills the copper tube 11 to generate a gas pressure. By appropriately discharging the generated gas through the escape hole 16 of the body 15, the gas pressure in the copper tube 11 can be constantly adjusted and maintained. For this reason, the antioxidant function can be reliably exerted without adversely affecting the reducing atmosphere in the copper tube 11 and the penetration of the welding braze, and the occurrence of scale can be effectively prevented, so that reliable welding can always be performed. Things. When the welding is completed, the closing cap body 14 and the gas pressure adjusting cap body 15 are removed from both ends of the copper pipe 11, respectively, and the welding operation is completed.

【0014】なお、上記実施例において、ガス圧調整用
キャップ体15はその中心に小径状の逃げ孔16を形成
するものとされているが、これに限定されるものでな
く、溶接すべき銅管11の径や長さに応じて図3や図4
の如く、逃げ孔26・36の径を所要の大きさに変更せ
しめたガス圧調整用キャップ体25・35に形成せしめ
てもよく、また、場合によっては逃げ孔16・26・3
6に所要の逃し弁を付設せしめてもよいものである。ま
た、銅管11はエルボ12を介して接続せしめつつ溶接
するものとされているが、チ−ズなど他の管継手を介し
て、あるいは、これらの管継手を組合せて所要形状に接
続せしめつつ溶接せしめるさいにも充分適用せしめるこ
とが出来るものであって、かかる場合には複数個のガス
圧調整用キャップ体15・25・35を嵌着せしめて逃
げ孔16・26・36の数を増加せしめてもよいもので
ある。さらに、酸化防止剤として、エステル系エアゾ−
ルタイプのものを示したが、これに限定されるものでな
く、これに類した他の酸化防止剤の使用時にも適用せし
めることが出来るものである。
In the above embodiment, the gas pressure adjusting cap body 15 has a small-diameter relief hole 16 formed at the center thereof. However, the present invention is not limited to this. 3 and 4 according to the diameter and length of the tube 11.
As described above, the diameter of the escape holes 26 and 36 may be changed to a required size and formed on the gas pressure adjusting cap bodies 25 and 35, and in some cases, the escape holes 16 and 26.3 may be formed.
6 may be provided with a required relief valve. The copper pipe 11 is welded while being connected via an elbow 12, but is connected to a required shape through another pipe joint such as a cheese or by combining these pipe joints. It can be applied sufficiently to welding, and in such a case, a plurality of gas pressure adjusting cap bodies 15, 25, 35 are fitted to increase the number of escape holes 16, 26, 36. It is possible to make a mistake. Further, as an antioxidant, ester-based azo-
However, the present invention is not limited to this, and can be applied when other antioxidants similar to this are used.

【0015】[0015]

【発明の効果】この出願に係る請求項1記載の発明は上
述のように構成されているから、銅管溶接時に酸化防止
剤の分解・ガス化によって発生するガスを適宜外方ヘ逃
しつつ、銅管内のガス圧を常に適正に調整保持せしめ、
還元雰囲気や溶接ロウの浸透に悪影響を及ぼすことなく
酸化防止機能を確実に発揮せしめることが出来るもので
あって、常に銅管の溶接を確実に行うことが出来るもの
である。
The invention according to claim 1 of the present application is configured as described above, so that the gas generated by decomposition and gasification of the antioxidant during welding of the copper pipe is appropriately released to the outside while being released. The gas pressure inside the copper tube is always adjusted and maintained properly.
The antioxidant function can be surely exerted without adversely affecting the reducing atmosphere and the penetration of the welding braze, and the copper pipe can always be reliably welded.

【0016】この出願に係る請求項2記載の発明は上述
のように構成されているから、溶接せしめるべき一方の
銅管の一端部に閉塞用キャップ体を嵌着せしめると共
に、他方の銅管の一端部にガス圧調整用キャップ体を嵌
着せしめるという極めて簡単な操作でもって、各銅管の
開口端部より内部にエステル系エアゾ−ルタイプなど所
要の酸化防止剤を吹き付けて管継手により接続せしめつ
つ溶接を行なうさいには、溶接時における酸化防止剤の
分解・ガス化によって発生するガスをガス圧調整用キャ
ップ体の逃げ孔より適宜外方に逃しつつ、銅管内のガス
圧を常に適正に調整保持せしめることが出来るものであ
る。
Since the invention according to claim 2 of the present application is constructed as described above, a closing cap body is fitted to one end of one copper tube to be welded, and the other copper tube is fitted to the other copper tube. With a very simple operation of fitting a cap body for gas pressure adjustment to one end, a required antioxidant such as an ester-based aerosol type is sprayed from the open end of each copper pipe to the inside, and connected by a pipe joint. During welding, the gas generated by the decomposition and gasification of the antioxidant during welding is released to the outside of the gas pressure adjusting cap body appropriately, and the gas pressure in the copper tube is always adjusted appropriately. Can be adjusted and held.

【図面の簡単な説明】[Brief description of the drawings]

【図1】この発明の一実施例を示すもので、接続せしめ
るべき一方の銅管11の一端部に閉塞用キャップ体14
を嵌着せしめると共に、他方の銅管11の一端部にガス
圧調整用キャップ体15を嵌着せしめつつ、各銅管11
の開口端部より酸化防止剤Aを吹き付ける状態を示す縦
断面図である。
FIG. 1 shows an embodiment of the present invention, in which one end of one copper tube 11 to be connected is provided with a closing cap body 14;
While fitting the gas pressure adjusting cap body 15 to one end of the other copper tube 11,
It is a longitudinal cross-sectional view which shows the state which sprays the antioxidant A from the opening end part.

【図2】同溶接状態を示す一部拡大縦断面図である。FIG. 2 is a partially enlarged longitudinal sectional view showing the welding state.

【図3】他のガス圧調整用キャップ体25を示す斜視図
である。
FIG. 3 is a perspective view showing another gas pressure adjusting cap body 25. FIG.

【図4】他のガス圧調整用キャップ体35を示す斜視図
である。
FIG. 4 is a perspective view showing another cap body 35 for adjusting gas pressure.

【図5】従来例を示すもので、接続せしめるべき銅管1
1内に酸化防止剤Aを吹き付ける状態を示す縦断面図で
ある。
FIG. 5 shows a conventional example, and a copper tube 1 to be connected.
1 is a longitudinal sectional view showing a state in which an antioxidant A is sprayed into 1.

【図6】同溶接状態を示す一部拡大縦断面図である。FIG. 6 is a partially enlarged longitudinal sectional view showing the welding state.

【符号の説明】[Explanation of symbols]

11 銅管 12 エルボ 13 溶接手段 14 閉塞用キャップ体 15・25・35 ガス圧調整用キャップ体 16・26・36 逃げ孔 DESCRIPTION OF SYMBOLS 11 Copper pipe 12 Elbow 13 Welding means 14 Closure cap body 15.25.35 Gas pressure adjustment cap body 16.26.36 Escape hole

───────────────────────────────────────────────────── フロントページの続き (58)調査した分野(Int.Cl.6,DB名) B23K 37/00 301 B23K 9/028 B23K 9/23 ──────────────────────────────────────────────────続 き Continued on the front page (58) Field surveyed (Int. Cl. 6 , DB name) B23K 37/00 301 B23K 9/028 B23K 9/23

Claims (2)

(57)【特許請求の範囲】(57) [Claims] 【請求項1】銅管どうしを管継手でもって接続せしめる
べく各銅管の内部にエステル系エアゾ−ルタイプなど所
要の酸化防止剤を吹き付けて溶接せしめるさいに、上記
銅管の各開口端を所要の閉塞部材でもって閉塞せしめる
と共に、該閉塞部材の少くとも一個にガス圧調整用の逃
げ孔を設け、該逃げ孔より酸化防止剤の加熱に伴って発
生するガスを適宜逃しつつ管内ガス圧を適正に調整保持
せしめることを特徴とする、銅管の溶接方法。
An opening end of each of the copper tubes is required to be welded by spraying a required antioxidant such as an ester-based aerosol type into each of the copper tubes so as to connect the copper tubes with a pipe joint. At least one of the closing members is provided with a relief hole for gas pressure adjustment, and the gas generated in the pipe along with the heating of the antioxidant is appropriately released from the relief hole to reduce the gas pressure in the pipe. A method for welding copper pipes, characterized by appropriately adjusting and holding.
【請求項2】管継手を介して溶接手段により接続せしめ
る銅管の開口端に着脱自在とされた盲状の閉塞用キャッ
プ体と、同所要径の逃げ孔を有するガス圧調整用キャッ
プ体とよりなり、上記各キャップ体を各々接続せしめる
べき銅管の開口端に適宜取付け、溶接時に酸化防止剤の
加熱に伴って発生するガスを適宜逃しつつ管内ガス圧を
適正に調整保持せしめることを特徴とする、銅管の溶接
時における管内ガス圧の調整用具。
2. A blind closing cap body detachably attached to an open end of a copper pipe connected by welding means via a pipe joint, and a gas pressure adjusting cap body having an escape hole of the same required diameter. The above-mentioned cap bodies are appropriately attached to the open ends of the copper tubes to be connected, and the gas pressure generated during heating of the antioxidant during welding is appropriately released and the gas pressure in the tubes is appropriately adjusted and held. A tool for adjusting the gas pressure in a pipe when welding a copper pipe.
JP30654997A 1997-10-20 1997-10-20 Copper tube welding method and gas pressure adjusting tool during welding of copper tube Expired - Fee Related JP2923554B2 (en)