JP2580182B2 - High viscosity material coating device - Google Patents

High viscosity material coating device

Info

Publication number
JP2580182B2
JP2580182B2 JP62161087A JP16108787A JP2580182B2 JP 2580182 B2 JP2580182 B2 JP 2580182B2 JP 62161087 A JP62161087 A JP 62161087A JP 16108787 A JP16108787 A JP 16108787A JP 2580182 B2 JP2580182 B2 JP 2580182B2
Authority
JP
Japan
Prior art keywords
viscosity material
sheet
coated
viscosity
scraping
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP62161087A
Other languages
Japanese (ja)
Other versions
JPS647965A (en
Inventor
久治 荒井
守 関根
健蔵 大木
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Fujikura Rubber Works Ltd
Original Assignee
Fujikura Rubber Works Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Fujikura Rubber Works Ltd filed Critical Fujikura Rubber Works Ltd
Priority to JP62161087A priority Critical patent/JP2580182B2/en
Publication of JPS647965A publication Critical patent/JPS647965A/en
Application granted granted Critical
Publication of JP2580182B2 publication Critical patent/JP2580182B2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

【発明の詳細な説明】 産業上の利用分野 本発明は、金属薄板、布等の被塗布シートの両面にゴ
ム、合成樹脂、高粘度マンガン溶液等の高粘度物を塗布
する塗布装置に係るものであって、この方法により製造
されたシートは、マンガン電池のセパレーター、粘着テ
ープ類、防水シート、ゴムベルトの芯地、その他種々の
目的に使用し得るものである。
Description: BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a coating apparatus for coating a high-viscosity material such as a rubber, a synthetic resin, a high-viscosity manganese solution on both surfaces of a coated sheet such as a thin metal plate or a cloth. The sheet produced by this method can be used for separators of manganese batteries, adhesive tapes, waterproof sheets, rubber belt interlining, and various other purposes.

従来の技術 従来、金属薄板、布等の長尺状の被塗布シートの両面
にゴム、合成樹脂、高粘度マンガン溶液等の高粘度物を
塗布するには、種々の方法が存在した。
2. Description of the Related Art Conventionally, there have been various methods for applying a high-viscosity material such as a rubber, a synthetic resin, or a high-viscosity manganese solution to both surfaces of a long sheet to be applied such as a thin metal plate or cloth.

その一つは、高粘度物を充填した充填槽の中に、被塗
布シートを挿入浸漬して塗布した後、これを、水平方向
に移動させながら、乾燥する方法が知られている。この
方法は、長尺状の被塗布シートの上面に配置する高粘度
物と、下面に配置する高粘度物の密度が、重力によって
異なるものとなるばかりでなく、下面に高粘度物の垂れ
が生じ、均一な塗膜の形成が、困難な欠点を有してい
る。
As one of the methods, a method is known in which a sheet to be coated is inserted and immersed in a filling tank filled with a high-viscosity material, applied, and then dried while moving the sheet horizontally. In this method, the density of the high-viscosity material disposed on the upper surface of the long sheet to be coated and the density of the high-viscosity material disposed on the lower surface differ not only by gravity, but also the dripping of the high-viscosity material on the lower surface. The resulting, uniform coating formation has difficult drawbacks.

また、この欠点を除去するため、被塗布シートの片面
づつ、2回の塗布を行なう事が知られているが、この方
法は極めて多くの手数を要し、効率の悪い欠点を有して
いる。
In order to eliminate this drawback, it is known that the coating is performed twice, one by one, on the sheet to be coated. However, this method requires an extremely large number of steps and has a drawback of being inefficient. .

また、高粘度物を被塗布シートの両面に噴霧して塗布
する方法が知られているが、この方法では、被塗布シー
トが長尺物である場合には適用出来ないとともに薄い塗
膜しか形成することが出来ず、一定厚以上の塗膜を得よ
うとするものには、使用出来ない欠点を有している。
In addition, a method of spraying and applying a high-viscosity material to both surfaces of a sheet to be coated is known, but this method cannot be applied to a case where the sheet to be coated is a long object and forms only a thin coating film. Those which cannot be used and are intended to obtain a coating film having a certain thickness or more have a disadvantage that they cannot be used.

また、実公昭50-9328号公報、特開昭51-130442号公
報、特開昭60-166064号公報等には、塗料等の塗布液を
通過した被塗布シートを、上方向に移動させる事が記載
されている。しかしながら、これらの発明はいずれも塗
料等の粘度の低い塗布液を被塗布シートに塗布するもの
であって、ゴム、合成樹脂、高粘度マンガン溶液等の高
粘度物を塗布するには適さないものであった。
In addition, Japanese Utility Model Publication No. 50-9328, Japanese Patent Application Laid-Open No. 51-130442, Japanese Patent Application Laid-Open No. 60-166064, and the like, the sheet to be coated that has passed through a coating solution such as paint is moved upward. Is described. However, all of these inventions apply a low-viscosity coating liquid such as a paint to a sheet to be applied, and are not suitable for applying a high-viscosity material such as rubber, a synthetic resin, and a high-viscosity manganese solution. Met.

発明が解決しようとする問題点 本発明は上述のごとき問題点を解決しようとするもの
であって、必要とされる塗膜厚みを充分に形成する事が
出来るとともに両面共に均一な塗膜を、長尺物に於いて
簡易に形成しようとするものである。
Problems to be Solved by the Invention The present invention is to solve the problems as described above, it is possible to sufficiently form the required coating film thickness and a uniform coating film on both sides, It is intended to be easily formed on a long object.

問題点を解決するための手段 本発明は上述のごとき問題点を解決するため、高粘度
物を充填した充填槽を設け、この充填槽中に浸漬し、外
周に高粘度物を塗布した長尺状の被塗布シートを、連続
的に通過させる対向間隔を設けて、一対の掻落としロー
ルを、充填槽の上面に配置し、この一対の掻落としロー
ルは、螺子棒によりその対向間隔方向に押圧するととも
に対向間隔に発条を介装し、対向間隔を広げる方向に付
勢し、また掻落としロールの両端を角柱とし回転を防止
して成るものである。
Means for Solving the Problems In order to solve the above-mentioned problems, the present invention provides a filling tank filled with a high-viscosity material, immersed in the filling tank, and applied a high-viscosity material to the outer periphery of the long length. A pair of scraping rolls is arranged on the upper surface of the filling tank, with a pair of scraping rolls arranged on the upper surface of the filling tank, and a pair of scraping rolls are pressed by a screw rod in the direction of the facing gap. At the same time, a sprung is interposed at the opposing interval to urge it in the direction to widen the opposing interval, and both ends of the scraping roll are prismatic to prevent rotation.

作用 本発明は上述のごとく構成したものであるから、被塗
布シートに、ゴム、合成樹脂、高粘度マンガン溶液等を
塗布するには、これらの高粘度物を充填した充填槽に、
長尺状の被塗布シートを連続的に挿入して高粘度物中に
浸漬する。そして、この高粘度物を表面に塗布した被塗
布シートを、垂直方向に上昇させながら、掻落としロー
ルの対向間隔を通過し、この掻落としロールにより、被
塗布シートの両側面の余分な高粘度物を一定厚みと成る
ように掻落とす事により、被塗布シートに高粘度物を塗
布する。
Action Since the present invention is configured as described above, in order to apply a rubber, a synthetic resin, a high-viscosity manganese solution or the like to a sheet to be applied, a filling tank filled with these high-viscosity materials is used.
A long sheet to be coated is continuously inserted and immersed in a high-viscosity material. Then, the sheet to which the high-viscosity material is applied on the surface is passed through the facing interval of the scraping rolls while being raised vertically, and the extra high viscosity on both sides of the sheet to be applied is caused by the scraping rolls. A high-viscosity material is applied to the sheet to be coated by scraping the material to a constant thickness.

この高粘度物を塗布した被塗布シートは、垂直方向に
上昇し、乾燥工程等に移動するものである。そのため、
被塗布シートの両面の高粘度物に掛かる重力は、両面と
も同一となり、高粘度物の塗布後に平面移動するものの
ごとく、被塗布シートの上面と下面で異なるような事が
なく、均一な塗布を可能とする。
The sheet to which the high-viscosity material is applied rises in the vertical direction and moves to a drying step or the like. for that reason,
The gravity applied to the high-viscosity material on both sides of the sheet to be coated is the same on both surfaces. Make it possible.

また、被塗布シートに塗布した高粘度物は、掻落とし
ロールの対向間隔を調整することにより、その塗布厚み
を任意に決定することができる。また、被塗布シート
を、垂直方向に移動するものであるから、被塗布シート
を平面移動するものに比し、装置の占有面積を小さなも
のとし、効率的な塗布装置を得ることが出来る。
The thickness of the high-viscosity material applied to the sheet to be applied can be arbitrarily determined by adjusting the facing distance of the scraping roll. Further, since the sheet to be coated is moved in the vertical direction, the area occupied by the apparatus is smaller than that in which the sheet to be coated is moved in a plane, and an efficient coating apparatus can be obtained.

また、掻落としロールは、被塗布シートの垂直方向へ
の上昇に伴なう高粘度物の粘着力で、対向間隔を狭める
方向に力が作用するが、掻落としロールの両端を角柱と
して、回転を防止するとともに発条の復元力よって、対
向間隔を常に一定に保つ事が出来るものである。
In addition, the scraping roll is an adhesive force of a high-viscosity material accompanying the vertical movement of the sheet to be coated, and a force acts in a direction to decrease a facing distance. In addition, the distance between the opposing members can be always kept constant by the restoring force of the firing.

また、高粘度物の被塗布シートへの塗布厚みは、一対
の掻落としロールの対向間隔を大きくすれば、厚く成
り、小さくすれば薄くなるが、この対向間隔の調整は、
螺子棒を対向間隔方向に回動すれば、発条の復元力に抗
して対向間隔は狭められ、螺子棒を上記と反対方向に回
動すれば、発条の復元力で対向間隔は拡大される。
Also, the thickness of the high-viscosity material applied to the sheet to be applied is increased when the interval between the pair of scraping rolls is increased, and is decreased when the interval is decreased.
If the screw rod is rotated in the direction of the opposing interval, the opposing interval is narrowed against the restoring force of the striation, and if the screw rod is rotated in the opposite direction, the opposing interval is enlarged by the restoring force of the striation. .

実施例 以下本発明の一実施例を図面に於いて説明すれば、第
1図は、ゴム、合成樹脂、高粘度物マンガン溶液等の高
粘度物の塗布装置の概略図である。そして、(1)は被
塗布シートで、多数の小孔を設けたステンレススチール
シート、布等により長尺状に形成し、送り出しロール
(2)から連続的に繰り出される。
FIG. 1 is a schematic view of an apparatus for applying a high-viscosity material such as a rubber, a synthetic resin, a high-viscosity manganese solution, and the like. And (1) is a sheet to be coated, which is formed in a long shape with a stainless steel sheet, cloth or the like provided with a large number of small holes, and is continuously fed out from a delivery roll (2).

そして、支持枠(3)に固定し、ゴム、合成樹脂、高
粘度物マンガン溶液等の高粘度物(4)を充填した充填
槽(5)で、両面に高粘度物(4)を塗布された後、垂
直に上昇して乾燥炉(6)に導入され、高粘度物(4)
を乾燥固化した後に、巻き取りロール(7)に巻き取
り、製造を完了する。
The high-viscosity material (4) is applied to both sides in a filling tank (5) fixed to the support frame (3) and filled with a high-viscosity material (4) such as a rubber, a synthetic resin, or a high-viscosity manganese solution. After that, it rises vertically and is introduced into the drying furnace (6), and the high-viscosity material (4)
After being dried and solidified, it is wound up on a winding roll (7) to complete the production.

そして、ゴム、合成樹脂、高粘度マンガン溶液等の高
粘度物(4)を充填した充填槽(5)は、第2図に示す
ごとく、被塗布シート(1)を強制的に高粘度物(4)
中に浸漬する為の浸漬ロール(10)を、下底方向に複数
設けている。
A filling tank (5) filled with a high-viscosity material (4) such as a rubber, a synthetic resin, or a high-viscosity manganese solution forcibly removes the coated sheet (1) from the high-viscosity material (4) as shown in FIG. 4)
There are provided a plurality of immersion rolls (10) for immersion in the lower bottom direction.

また、充填槽(5)の上面には、一対の掻落としロー
ル(11)(12)を、一対の固定枠(13)(14)によって
固定配置している。この掻落としロール(11)(12)
は、充填槽(5)中に浸漬し、外周に高粘度物(4)を
塗布した被塗布シート(1)を、通過させる対向間隔
(15)を設けて配置する。
A pair of scraping rolls (11) and (12) are fixedly arranged on the upper surface of the filling tank (5) by a pair of fixed frames (13) and (14). This scraping roll (11) (12)
Is disposed with an opposing interval (15) through which the coated sheet (1), which is immersed in the filling tank (5) and coated with the high-viscosity material (4) on the outer periphery, passes therethrough.

また、掻落としロール(11)(12)は、固定枠(13)
(14)に螺着した螺子棒(16)により、両端を、その対
向間隔(15)方向に押圧している。そして、この対向間
隔(15)の両端に、第3図に示すごとく発条(17)(1
8)を介装し、掻落としロール(11)(12)の対向間隔
(15)を広げる方向に付勢している。
The scraping rolls (11) and (12) are fixed frame (13)
Both ends are pressed in the direction of the opposing interval (15) by a screw rod (16) screwed to (14). Then, at both ends of the facing space (15), as shown in FIG.
8) is interposed to urge the scraping rolls (11) and (12) in a direction to widen the facing distance (15).

上述のごとく構成したものに於いて、被塗布シート
(1)に、ゴム、合成樹脂、高粘度マンガン溶液等を塗
布するには、高粘度物(4)を充填した充填槽(5)
に、長尺状の被塗布シート(1)を挿入して高粘度物
(4)中に連続的に浸漬する。
In the apparatus configured as described above, in order to apply a rubber, a synthetic resin, a high-viscosity manganese solution or the like to the sheet (1) to be applied, a filling tank (5) filled with a high-viscosity material (4)
, A long sheet to be coated (1) is inserted and continuously immersed in a high-viscosity material (4).

そして、この高粘度物(4)を表面に塗布した被塗布
シート(1)を、垂直方向に上昇させながら、掻落とし
ロール(11)(12)の対向間隔(15)を通過させる。す
ると、第4図に示すごとく、掻落としロール(11)(1
2)により、被塗布シート(1)の両側面の余分な高粘
度物(4)を、一定厚みと成るように掻落とす事がで
き、予め設定された規定厚みで、被塗布シート(1)に
高粘度物(4)を連続的に塗布することができる。
Then, the coated sheet (1) having the surface coated with the high-viscosity material (4) is passed through the facing interval (15) of the scraping rolls (11) and (12) while being raised in the vertical direction. Then, as shown in FIG. 4, the scraping roll (11) (1
According to 2), the excess high-viscosity material (4) on both sides of the coated sheet (1) can be scraped off to have a constant thickness. , A high-viscosity material (4) can be applied continuously.

また、高粘度物(4)の被塗布シート(1)への塗布
厚みは、一対の掻落としロール(11)(12)の対向間隔
(15)を大きくすれば、厚く成り、小さくすれば薄くな
る。また、この対向間隔(15)の調整は、螺子棒(16)
を対向間隔(15)方向に回動すれば、発条(17)(18)
の復元力に抗して対向間隔(15)は狭められる。また、
螺子棒(16)を上記と反対方向に回動すれば、発条(1
7)(18)の復元力で対向間隔(15)は拡大される。
The thickness of the high-viscosity material (4) applied to the sheet (1) is increased by increasing the distance (15) between the pair of scraping rolls (11) and (12), and is decreased by decreasing the distance. Become. The adjustment of the facing distance (15) is performed by adjusting the screw rod (16)
Is turned in the direction of the opposing interval (15), the firing (17) (18)
The opposing interval (15) is narrowed against the restoring force of. Also,
If the screw rod (16) is turned in the opposite direction to the above,
7) The opposing interval (15) is enlarged by the restoring force of (18).

また、掻落としロール(11)(12)は、被塗布シート
(1)の垂直方向への上昇に伴なう高粘度物(4)の粘
着力で、対向間隔(15)を狭める方向に力が作用する
が、掻落としロール(11)(12)の両端を角柱(19)と
して、回転を防止するとともに発条(17)(18)の復元
力によって、対向間隔(15)を常に一定に保つ事が出来
るものである。
In addition, the scraping rolls (11) and (12) use the adhesive force of the high-viscosity material (4) as the sheet (1) to be applied rises in the vertical direction, and apply force in a direction to decrease the facing distance (15). Works, but both ends of the scraping rolls (11) and (12) are square prisms (19) to prevent rotation and to keep the facing distance (15) constant at all times by the restoring force of the springs (17) and (18) Things that can do things.

また、高粘度物(4)を塗布した被塗布シート(1)
は垂直方向に上昇し、乾燥工程等に移動するものである
から、被塗布シート(1)の両面の高粘度物(4)に掛
かる重力は、両面とも同一となり、高粘度物(4)の塗
布後に平面移動するもののごとく、被塗布シート(1)
の上面と下面で密度が異なるような事がなく、均一な塗
布を可能とする。また、被塗布シート(1)を平面移動
するものに比し、装置の占有床面積を小さなものとし、
効率的な塗布装置を得ることが出来るものである。
Further, a coated sheet (1) coated with a high-viscosity material (4)
Rises in the vertical direction and moves to the drying step, etc., the gravitational force applied to the high-viscosity material (4) on both surfaces of the coated sheet (1) becomes the same on both surfaces, and the high-viscosity material (4) Sheet to be coated (1) as if it moves in a plane after coating
The density does not differ between the upper surface and the lower surface, and uniform application is possible. Further, the occupied floor area of the apparatus is smaller than that of the apparatus in which the coated sheet (1) is moved in a plane,
An efficient coating device can be obtained.

発明の効果 本発明は上述のごとく構成したものであるから、充填
槽に長尺状の被塗布シートを連続的に浸漬して、高粘度
物を表面に塗布し、これを垂直方向に上昇させながら、
掻落としロールの対向間隔を通過するのみで、被塗布シ
ートの両側面の余分な高粘度物は、一定厚みと成るよう
掻落とされ、簡易な高粘度物の塗布を可能とする。
Effect of the Invention Since the present invention is configured as described above, a long sheet to be coated is continuously immersed in the filling tank, a high-viscosity material is applied to the surface, and this is raised vertically. While
Excessive high-viscosity material on both side surfaces of the sheet to be coated is scraped off to have a constant thickness only by passing through the opposing interval of the scraping rolls, so that simple high-viscosity material can be applied.

また高粘度物を塗布した被塗布シートは、垂直方向に
上昇するものであるから、被塗布シートの両面の高粘度
物に掛かる重力は、両面とも同一となる。そのため、高
粘度物の塗布後に平面移動するもののごとく、被塗布シ
ートの上面と下面で密度が異なるような事がなく、均一
な塗布を可能とする。
Further, since the coated sheet on which the high-viscosity material is applied rises in the vertical direction, the gravity applied to the high-viscosity material on both surfaces of the applied sheet is the same on both surfaces. For this reason, the density does not differ between the upper surface and the lower surface of the sheet to be applied, as in the case where the high-viscosity material moves in a plane after the application, and uniform application is possible.

また、被塗布シートに塗布した高粘度物は、掻落とし
ロールの対向間隔を調整することにより、その塗布厚み
を任意に決定することができる。また被塗布シートを垂
直方向に移動するものであるから、被塗布シートを平面
移動するものに比し、装置の占有床面積を小さなものと
し、効率的な塗布装置を得ることが出来る。
The thickness of the high-viscosity material applied to the sheet to be applied can be arbitrarily determined by adjusting the facing distance of the scraping roll. In addition, since the sheet to be coated is moved in the vertical direction, the occupied floor area of the apparatus can be made smaller than that in which the sheet to be coated is moved in a plane, and an efficient coating apparatus can be obtained.

また、掻落としロールは、被塗布シートの垂直方向へ
の上昇に伴なう高粘度物の粘着力で、対向間隔を狭める
方向に力が作用するが、掻落としロールの両端を角柱と
して、回転を防止するとともに発条の復元力によって、
対向間隔を常に一定に保つ事が出来る。
In addition, the scraping roll is an adhesive force of a high-viscosity material accompanying the vertical movement of the sheet to be coated, and a force acts in a direction to decrease a facing distance. To prevent
The facing distance can always be kept constant.

また、高粘度物の被塗布シートへの塗布厚みは、一対
の掻落としロールの対向間隔を大きくすれば、厚く成
り、小さくすれば薄くなるが、この対向間隔の調整は、
螺子棒を対向間隔方向に回動すれば、発条の復元力に抗
して対向間隔は狭められ、螺子棒を上記と反対方向に回
動すれば、発条の復元力で対向間隔は拡大され、正確な
間隔調整を簡易に行う事ができるものである。
Also, the thickness of the high-viscosity material applied to the sheet to be applied is increased when the interval between the pair of scraping rolls is increased, and is decreased when the interval is decreased.
If the screw rod is rotated in the opposing interval direction, the opposing interval is narrowed against the restoring force of the striation, and if the screw rod is rotated in the opposite direction, the opposing interval is enlarged by the restoring force of the striation, Accurate interval adjustment can be easily performed.

【図面の簡単な説明】[Brief description of the drawings]

図面は本発明の一実施例を示すものであって、第1図は
概略正面図、第2図は充填槽部分の拡大断面図、第3図
は掻落としロール部分の拡大平面図、第4図は掻落とし
ロールと被塗布シートに塗布した高粘度物の関係を示す
拡大断面図である。 (1)……被塗布シート (4)……高粘度物 (5)……充填槽 (11)(12)……掻落としロール (15)……対向間隔 (16)……螺子棒 (17)(18)……発条
1 is a schematic front view, FIG. 2 is an enlarged sectional view of a filling tank portion, FIG. 3 is an enlarged plan view of a scraping roll portion, FIG. The figure is an enlarged sectional view showing the relationship between a scraping roll and a high-viscosity object applied to a sheet to be applied. (1) Sheet to be coated (4) High viscosity material (5) Filling tank (11) (12) Scrapping roll (15) Opposing distance (16) Screw rod (17) ) (18) ……

Claims (1)

(57)【特許請求の範囲】(57) [Claims] 【請求項1】高粘度物を充填した充填槽を設け、この充
填槽中に浸漬し、外周に高粘度物を塗布した長尺状の被
塗布シートを、連続的に通過させる対向間隔を設けて、
一対の掻落としロールを、充填槽の上面に配置し、この
一対の掻落としロールを、螺子棒によりその対向間隔方
向に押圧するとともに対向間隔に発条を介装し、対向間
隔を広げる方向に付勢し、また掻落としロールの両端を
角柱とし回転を防止した事を特徴とする高粘度物の塗布
装置。
A filling tank filled with a high-viscosity material is provided, and an opposing interval is provided to continuously pass a long sheet to be coated, which is immersed in the filling tank and coated with a high-viscosity material on the outer periphery. hand,
A pair of scraping rolls are arranged on the upper surface of the filling tank, and the pair of scraping rolls are pressed in the direction of the opposing interval by a screw bar, and a sprung is interposed at the opposing interval, and is attached in the direction of increasing the opposing interval. A high-viscosity material coating apparatus characterized in that both ends of a scraping roll are made prismatic and rotation is prevented.
JP62161087A 1987-06-30 1987-06-30 High viscosity material coating device Expired - Lifetime JP2580182B2 (en)