JP2513497B2 - Forming the arc of the cane - Google Patents

Forming the arc of the cane

Info

Publication number
JP2513497B2
JP2513497B2 JP63188078A JP18807888A JP2513497B2 JP 2513497 B2 JP2513497 B2 JP 2513497B2 JP 63188078 A JP63188078 A JP 63188078A JP 18807888 A JP18807888 A JP 18807888A JP 2513497 B2 JP2513497 B2 JP 2513497B2
Authority
JP
Japan
Prior art keywords
vertical
metal plate
forming
rising
hole
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP63188078A
Other languages
Japanese (ja)
Other versions
JPH0237920A (en
Inventor
重治 広浜
寛 鷲塚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HIROHAMA KINZOKU KOGYO KK
Original Assignee
HIROHAMA KINZOKU KOGYO KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HIROHAMA KINZOKU KOGYO KK filed Critical HIROHAMA KINZOKU KOGYO KK
Priority to JP63188078A priority Critical patent/JP2513497B2/en
Publication of JPH0237920A publication Critical patent/JPH0237920A/en
Application granted granted Critical
Publication of JP2513497B2 publication Critical patent/JP2513497B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Description

【発明の詳細な説明】 [産業上の利用分野] 本発明は、罐口金、罐天板等の罐口円弧部の成形方法
に関する。
TECHNICAL FIELD The present invention relates to a method for forming a circular arc portion of a mouthpiece such as a mouthpiece and a cantop plate.

[従来の技術] 従来の罐口円弧部の成形方法は、金属板の一部を平坦
状態から穴を備えた垂直立ち上げ部に形成し、次いで、
垂直立ち上げ部を外側から下方へさらに内方へと円弧部
に形成するものであった。
[Prior Art] A conventional method for forming a circular arc portion is to form a part of a metal plate from a flat state to a vertical rising portion provided with a hole, and then,
The vertical rising portion is formed in the arc portion from the outer side to the lower side and further to the inner side.

なお、実開昭62−45210号公報に罐口金に円弧部を形
成したものが示されている。
Incidentally, Japanese Utility Model Laid-Open No. 62-45210 discloses a canister having an arc portion.

[発明が解決しようとする課題] かかる従来の成形方法では、垂直立ち上げ部を小さな
円弧部に形成することが実際には困難であった。また、
ラミネート材を有する金属板に関するものではなかっ
た。
[Problems to be Solved by the Invention] In such a conventional molding method, it was actually difficult to form the vertical rising portion into a small arc portion. Also,
It was not related to a metal plate having a laminate material.

本発明の目的は、小さな円弧部でも容易に成形できる
ラミネート材を有する罐口円弧部の成形方法を提供する
ことにある。
It is an object of the present invention to provide a method for forming a circular arc portion having a laminate material that can easily form a small circular arc portion.

[課題を解決するための手段] 本発明は、かかる課題を解決するためになされたもの
である。即ち、金属板素材(1)の内面にラミネート材
(2)を有する金属板(3)の一部を平坦状態から穴
(5c)を備えた垂直立ち上げ部(5e)に形成し、次い
で、前記垂直立ち上げ部(5e)を外側から下方へさらに
内方へと小さな円弧部(5f)に形成する罐口円弧部の成
形方法において、前記金属板(3)の平坦部(5a)に円
錐立ち上げ部(5b)を形成し、この円錐立ち上げ部(5
b)の連接部(5d)近傍内側に前記穴(5c)をその側面
(5g)が垂直になるように形成した後、前記円錐立ち上
げ部(5b)の連接部(5d)を含んで垂直立ち上げ部(5
e)を形成し、この垂直立ち上げ部(5e)を外側から下
方へさらに内方へと小さな円弧部(5f)に形成すること
を特徴とする罐口円弧部の成形方法にある。
[Means for Solving the Problems] The present invention has been made to solve the problems. That is, a part of the metal plate (3) having the laminate material (2) on the inner surface of the metal plate material (1) is formed from a flat state to a vertical rising part (5e) having a hole (5c), and then, In the method for forming a canister circular arc portion in which the vertical rising portion (5e) is formed in a small circular arc portion (5f) from the outer side to the lower side, a cone is formed on the flat portion (5a) of the metal plate (3). Forming the rising part (5b), this conical rising part (5b)
After forming the hole (5c) inside the vicinity of the connecting part (5d) of b) so that the side surface (5g) is vertical, the hole is formed vertically including the connecting part (5d) of the conical rising part (5b). Startup section (5
e), and the vertical rising portion (5e) is formed in a small circular arc portion (5f) from the outer side to the lower side and further inward.

[作用] かかる本発明の成形方法によれば、円錐立ち上げ部
(5b)の連接部(5d)が垂直立ち上げ部(5e)内に含ま
れていて外側に変形しやすくなっているので、垂直立ち
上げ部(5e)を外側から下方へさらに内方へと成形する
際に、円弧部(5f)の形成が著しく容易となる。
[Operation] According to the molding method of the present invention, since the connecting portion (5d) of the conical rising portion (5b) is included in the vertical rising portion (5e) and is easily deformed to the outside, When the vertical rising portion (5e) is formed from the outer side to the lower side and further inward, the arc portion (5f) is significantly facilitated to be formed.

また、円錐立ち上げ部(5b)の連接部(5d)近傍内側
に穴(5c)を形成したので、この変形しやすい連接部
(5d)が垂直立ち上げ部(5e)の上部に位置することと
なり、垂直立ち上げ部(5e)を成形する際に、この連接
部(5d)から小さく変形することができ、極めて小さな
円弧部を形成することができる。
Since the hole (5c) is formed inside the conical rising part (5b) near the connecting part (5d), this deformable connecting part (5d) should be located above the vertical rising part (5e). Therefore, when the vertical rising portion (5e) is formed, the connecting portion (5d) can be slightly deformed, and an extremely small arc portion can be formed.

さらには、内面にラミネート材(2)を有する円錐立
ち上げ部(5b)に穴(5c)をその側面(5g)が垂直にな
るように形成するので、ラミネート材(2)が金属板素
材(1)に良好に密着した状態を保ったまま穴(5c)を
成形することができる。そして、垂直立ち上げ部(5e)
が形成された状態で金属板素材(1)の反ラミネート側
が高くなっているので、上型(7)で垂直立ち上げ部
(5e)を変形する際に、この金属板素材(1)の反ラミ
ネート材側が高くなっているので、反ラミネート材側に
変形力が強く加わり、それによりラミネート材(2)を
損傷せずに成形できる。
Furthermore, since the hole (5c) is formed in the conical rising portion (5b) having the laminating material (2) on the inner surface so that the side surface (5g) is vertical, the laminating material (2) is a metal plate material ( The hole (5c) can be formed while maintaining a state of being closely adhered to 1). And vertical launching part (5e)
Since the non-laminating side of the metal plate material (1) is higher in the state where the metal plate material (1) is formed, when the vertical rising part (5e) is deformed by the upper die (7), the metal plate material (1) is Since the laminating material side is high, a deforming force is strongly applied to the anti-laminating material side, whereby the laminating material (2) can be molded without damage.

[実施例] 以下、本発明の一実施例を第1図〜第3図に基いて説
明する。
[Embodiment] An embodiment of the present invention will be described below with reference to FIGS. 1 to 3.

罐口金用金属板3は、ブリキ製金属板素材1とその内
面に貼着されたラミネート材2とより構成されている。
まず、金属板3は平板状態から円筒状側壁部4と上壁部
5とカシメ部6との三部分が所定形状になるように形成
される。上壁部5は、第2図に示すように、平坦部5aの
中央部に円錐立ち上げ部5bが形成され、この円錐立ち上
げ部5bの平坦部5aとの連接部5d近傍内側に穴5cをその側
面5gが垂直になるように形成される。平坦部5aから円錐
立ち上げ部5bが形成されるので、その連接部5dが弱い部
分となっている。また、内面にラミネート材2を有する
円錐立ち上げ部5bに穴5cをその側面5gが垂直になるよう
に形成されるので、ラミネート材2が金属板素材1に良
好に密着した状態を保ったまま穴5cが形成される。
The metal plate 3 for a mouthpiece is composed of a tin metal plate material 1 and a laminating material 2 attached to the inner surface thereof.
First, the metal plate 3 is formed in a flat plate state so that the cylindrical side wall portion 4, the upper wall portion 5, and the crimp portion 6 have three predetermined shapes. As shown in FIG. 2, in the upper wall portion 5, a conical rising portion 5b is formed in the central portion of the flat portion 5a. Is formed so that its side surface 5g is vertical. Since the conical rising part 5b is formed from the flat part 5a, the connecting part 5d is a weak part. Further, since the hole 5c is formed in the conical rising portion 5b having the laminating material 2 on the inner surface so that the side surface 5g becomes vertical, the laminating material 2 is kept in good contact with the metal plate material 1. Hole 5c is formed.

しかる後、円錐立ち上げ部5bの連接部5dを含んで垂直
立ち上げ部5eが第3図に示すように平坦部5aから形成さ
れる。連接部5dは垂直立ち上げ部5eの上部に位置するこ
とになる。
Thereafter, the vertical rising portion 5e including the connecting portion 5d of the conical rising portion 5b is formed from the flat portion 5a as shown in FIG. The connecting portion 5d is located above the vertical rising portion 5e.

次いで、第3図に示すように円筒状側壁部4内に成形
用下型8を挿入して下型8上に平坦部5aを載置した状態
で、円弧状の成形用凹面を有する成形用上型7を降下さ
せて垂直立ち上げ部5eの上端を上型7の成形用凹面に当
接し、さらに上型7を降下させる。これにより、垂直立
ち上げ部5eは、成形用凹面に案内されて外側から下方へ
と変形し、さらに内方へと変形して小さな円弧部5fが第
1図に示すように形成される。
Then, as shown in FIG. 3, the molding lower die 8 is inserted into the cylindrical side wall portion 4 and the flat portion 5a is placed on the lower die 8, and the molding die having an arcuate molding concave surface is formed. The upper die 7 is lowered to bring the upper end of the vertical rising portion 5e into contact with the molding concave surface of the upper die 7 and further lower the upper die 7. As a result, the vertical rising portion 5e is guided by the molding concave surface, deforms downward from the outside, and further deforms inward to form a small arc portion 5f as shown in FIG.

この際、円錐立ち上げ部5bの連接部5dが垂直立ち上げ
部5e内に含まれていて外側に変形しやすくなっているの
で、著しく容易に変形される。しかも、この変形しやす
い連接部5dが垂直立ち上げ部5eの上部に位置されている
ので、連接部5dから小さく変形され、極めて小さな円弧
部5fが形成される。
At this time, since the connecting portion 5d of the conical rising portion 5b is included in the vertical rising portion 5e and is easily deformed outward, it is remarkably easily deformed. Moreover, since the deformable connecting portion 5d is located above the vertical rising portion 5e, the connecting portion 5d is slightly deformed to form an extremely small arc portion 5f.

上型7の成形用凹面で垂直立ち上げ部5eの変形を開始
する際に、金属板素材1の反ラミネート材側が高くなっ
ているので、反ラミネート材側に変形力が強く加わり、
これによりラミネート材2を損傷せずに成形することが
できる。
When the vertical rising portion 5e starts to be deformed on the molding concave surface of the upper die 7, the anti-laminating material side of the metal plate material 1 is high, and therefore the anti-laminating material side is strongly deformed.
Thereby, the laminate material 2 can be molded without damage.

[発明の効果] 本発明によれば、極めて小さな円弧部を著しく容易に
ラミネート材を損傷することない罐口円弧部の成形方法
を提供することができる。
[Advantages of the Invention] According to the present invention, it is possible to provide a method for forming a mouth arc portion in which an extremely small arc portion does not damage the laminate material very easily.

【図面の簡単な説明】[Brief description of drawings]

第1図〜第3図は本発明の罐口円弧部の成形方法の各工
程断面図である。 1……金属板素材、2……ラミネート材、3……罐口金
用金属板、4……側壁部、5……上壁部、5a……平坦
部、5b……円錐立ち上げ部、5c……穴、5d……連接部、
5e……垂直立ち上げ部、5f……円弧部、5g……側面、6
……カシメ部、7……上型、8……下型。
1 to 3 are cross-sectional views of respective steps of the method for forming a mouthpiece circular arc portion of the present invention. 1 ... Metal plate material, 2 ... Laminated material, 3 ... Metal plate for lip, 4 ... Side wall part, 5 ... Top wall part, 5a ... Flat part, 5b ... Cone rising part, 5c ...... hole, 5d ...... connecting part,
5e …… Vertical rising part, 5f …… Arc part, 5g …… Side, 6
...... Caulking part, 7 ... upper mold, 8 ... lower mold.

Claims (1)

(57)【特許請求の範囲】(57) [Claims] 【請求項1】金属板素材(1)の内面にラミネート材
(2)を有する金属板(3)の一部を平坦状態から穴
(5c)を備えた垂直立ち上げ部(5e)に形成し、次い
で、前記垂直立ち上げ部(5e)を外側から下方へさらに
内方へと小さな円弧部(5f)に形成する罐口円弧部の成
形方法において、前記金属板(3)の平坦部(5a)に円
錐立ち上げ部(5b)を形成し、この円錐立ち上げ部(5
b)の連接部(5d)近傍内側に前記穴(5c)をその側面
(5g)が垂直になるように形成した後、前記円錐立ち上
げ部(5b)の連接部(5d)を含んで前記垂直立ち上げ部
(5e)を形成し、この垂直立ち上げ部(5e)を外側から
下方へさらに内方へと小さな円弧部(5f)に形成したこ
とを特徴とする罐口円弧部の成形方法。
1. A part of a metal plate (3) having a laminate material (2) on the inner surface of a metal plate material (1) is formed from a flat state to a vertical rising part (5e) having a hole (5c). Then, in the method for forming a cantilevered arc portion in which the vertical rising portion (5e) is formed in a small arc portion (5f) from the outer side to the lower side, the flat portion (5a) of the metal plate (3) is formed. ), A cone rising part (5b) is formed, and this cone rising part (5b)
After forming the hole (5c) inside the vicinity of the connecting portion (5d) of b) so that the side surface (5g) is vertical, the hole including the connecting portion (5d) of the conical rising portion (5b) is included. Forming a vertical rising part (5e), and forming this vertical rising part (5e) in a small circular arc part (5f) from the outside toward the bottom and further inward .
JP63188078A 1988-07-29 1988-07-29 Forming the arc of the cane Expired - Fee Related JP2513497B2 (en)