JP2016159593A - Leather laminated film, leather laminated film molded body, composite resin molded body, and method for producing leather laminated film - Google Patents

Leather laminated film, leather laminated film molded body, composite resin molded body, and method for producing leather laminated film Download PDF

Info

Publication number
JP2016159593A
JP2016159593A JP2015042856A JP2015042856A JP2016159593A JP 2016159593 A JP2016159593 A JP 2016159593A JP 2015042856 A JP2015042856 A JP 2015042856A JP 2015042856 A JP2015042856 A JP 2015042856A JP 2016159593 A JP2016159593 A JP 2016159593A
Authority
JP
Japan
Prior art keywords
leather
laminated film
molded body
film
resin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2015042856A
Other languages
Japanese (ja)
Other versions
JP6632051B2 (en
Inventor
小林 聖一
Seiichi Kobayashi
聖一 小林
鈴木 智之
Tomoyuki Suzuki
智之 鈴木
幸広 村上
Yukihiro Murakami
幸広 村上
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Midori Technopark Co Ltd
Original Assignee
Midori Technopark Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Midori Technopark Co Ltd filed Critical Midori Technopark Co Ltd
Priority to JP2015042856A priority Critical patent/JP6632051B2/en
Publication of JP2016159593A publication Critical patent/JP2016159593A/en
Application granted granted Critical
Publication of JP6632051B2 publication Critical patent/JP6632051B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

PROBLEM TO BE SOLVED: To provide a leather laminated film, a leather laminated film molded body, a composite resin molded body, and a method for producing a leather laminated film, which keep feeling of a natural leather body and can form a coating of a leather with a comparatively simple work.SOLUTION: A leather 2 and a resin film 3 are laminated with an aqueous curable adhesive 4.SELECTED DRAWING: Figure 1

Description

本発明は、皮革と樹脂フィルムとの皮革積層フィルム、これを用いた皮革積層フィルム成形体及び複合樹脂成形体並びに皮革積層フィルムの製造方法に関する。   The present invention relates to a leather laminated film of leather and a resin film, a leather laminated film molded body and a composite resin molded body using the same, and a method for producing a leather laminated film.

従来の自動車等のステアリングホイールは、円形に連続形成されたリング部と、リング部の中心に位置するボス部と、ボス部から放射状に接続された複数のスポーク部とから形成され、運転時の滑り止め、触感向上、高級感を出すなどの目的で、少なくともリング部を天然皮革(以下、単に皮革といい、特に断りの無い限り、皮革は天然皮革をいう)で被覆したものがある。   A conventional steering wheel of an automobile or the like is formed of a ring part continuously formed in a circle, a boss part located at the center of the ring part, and a plurality of spoke parts radially connected from the boss part. For the purpose of preventing slipping, improving touch feeling, and giving a high-class feeling, at least the ring part is coated with natural leather (hereinafter simply referred to as leather, unless otherwise specified, leather refers to natural leather).

また、ステアリングホイールには限定されず、自動車の内装部品、さらには、自動車以外の各種製品において、皮革を貼り付けたものが好まれている。   Further, the present invention is not limited to a steering wheel, and automobile interior parts, and various products other than automobiles that have leather attached thereto are preferred.

従来、ステアリングホイールの皮革での被覆は手縫い方式で行われてきた。手縫い方式は、裁断した皮革をステアリングホイールやシフトノブ等の被覆体に巻き付けた後、人手により皮革端部同士を突き合わせて縫い合わせるものであった。しかしながら、この手縫い作業は作業工数が非常に多く、また、手間がかかるため生産量が限られ、従って、皮革で被覆したステアリングホイールやシフトノブは高価なものとなっていた。   Conventionally, the leather of the steering wheel has been coated by hand sewing. In the hand-sewn method, the cut leather is wrapped around a covering body such as a steering wheel or a shift knob, and then the leather ends are butted together by hand. However, this hand-sewn operation requires a large number of man-hours and is labor-intensive, so the production volume is limited. Therefore, the steering wheel and shift knob covered with leather are expensive.

その上、手縫い方式に於いては、皮革の端部同士を縫い合わせる必要からリング部皮革とスポーク部皮革を一体にして皮革を裁断していた。このため、皮革裁断の際の歩留まりが極めて悪いものとなっていた。そして、皮革裁断時の歩留まりを良くすることを優先してスポーク部の形状が決められていた。従って、特に、スポークやシフトノブデザインの自由度が小さく、例えば、スポークやシフトノブの形状を握りやすい形状に設計することすら制約されるといった状況にあった。   In addition, in the hand-sewn method, the leather of the ring part leather and the spoke part leather are cut together because it is necessary to sew the ends of the leather together. For this reason, the yield at the time of leather cutting was extremely bad. And the shape of the spoke part was decided giving priority to improving the yield at the time of leather cutting. Therefore, the degree of freedom in designing the spokes and the shift knob is particularly small, and for example, the design of the spokes and the shift knob is constrained to be designed to be easy to grip.

そこで、作業工数を低減するため、近時、接着方式が提案されている。接着方式は作業工数の低減が可能で、コスト低下を図るため広く採用されるようになってきている(特許文献1参照)。   Therefore, recently, an adhesion method has been proposed to reduce the number of work steps. The bonding method can reduce the number of work steps, and has been widely adopted to reduce the cost (see Patent Document 1).

しかし、接着方式に於いて、皮革が経年変化や環境変化を受けて、皮革が収縮し剥がれ現象が生じるという問題が指摘されている。また、皮革が厚い場合には皮革の柔らかい風合いが残るが、コストダウン等の目的で厚さの薄い皮革を接着すると、皮革本来の柔らかい風合いがなくなってしまうという問題がある。さらに、皮革自体は、成形しても形状が保持できないので、予め所定の形状に成形して接着するという作業ができないという問題もある。   However, a problem has been pointed out that in the bonding method, the leather is subject to secular change and environmental change, and the leather shrinks and peels off. Further, when the leather is thick, the soft texture of the leather remains, but there is a problem that when the leather with a thin thickness is bonded for the purpose of cost reduction or the like, the original soft texture of the leather is lost. Furthermore, since the leather itself cannot retain its shape even if it is molded, there is also a problem that it is not possible to perform an operation of molding and bonding in a predetermined shape in advance.

また、皮革シートと他のシートとの間に熱可塑性樹脂層を介在させた積層シートをプレス加工する技術が開示されている(特許文献2参照)。しかしながら、この技術では、天然皮革の表面が完全にプレスされ、硬化されてしまうので、天然皮革本来の風合いを有するものを得るのは困難であった。   Moreover, the technique which press-processes the lamination sheet which interposed the thermoplastic resin layer between the leather sheet | seat and another sheet | seat is disclosed (refer patent document 2). However, with this technique, the surface of the natural leather is completely pressed and cured, so that it is difficult to obtain one having the natural texture of natural leather.

特開2000−53000号公報JP 2000-53000 A 特開2001−259264号公報JP 2001-259264 A

本発明はこのような事情に鑑み、天然皮革本来の風合いを維持し、比較的簡便な作業で皮革の被覆を設けることができる皮革積層フィルム、皮革積層フィルム成形体及び複合樹脂成形体並びに皮革積層フィルムの製造方法を提供することを課題とする。   In view of such circumstances, the present invention provides a leather laminated film, a leather laminated film molded article, a composite resin molded article, and a leather laminated laminate capable of maintaining the original texture of natural leather and providing a leather coating by a relatively simple operation. It is an object to provide a method for producing a film.

前記課題を解決する本発明の第1の態様は、皮革と、樹脂フィルムとを水性硬化性接着剤で積層したことを特徴とする皮革積層フィルムにある。   A first aspect of the present invention that solves the above-described problems resides in a leather laminated film in which leather and a resin film are laminated with an aqueous curable adhesive.

かかる第1の態様では、水性硬化性接着剤を用いて積層することにより、皮革の本来の風合いを残したまま、樹脂フィルムとの積層体を実現できる。   In such a first aspect, by laminating using an aqueous curable adhesive, it is possible to realize a laminate with a resin film while leaving the original texture of leather.

本発明の第2の態様は、第1の態様の皮革積層フィルムにおいて、前記樹脂フィルムは、前記皮革より大面積であることを特徴とする皮革積層フィルムにある。   According to a second aspect of the present invention, in the leather laminated film of the first aspect, the resin film has a larger area than the leather.

かかる第2の態様では、樹脂フィルムの周囲を金型で挟み込んだ状態で真空圧空成形を行う際に、皮革が無駄にならず、所望の形状の皮革積層フィルム成形体を実現できる。   In the second aspect, when vacuum / pressure forming is performed in a state where the periphery of the resin film is sandwiched between molds, leather is not wasted, and a leather laminated film molded body having a desired shape can be realized.

本発明の第3の態様は、第1又は2の態様の皮革積層フィルムにおいて、前記樹脂フィルムの厚さは0.2〜0.5mmであり、前記皮革の厚さは、0.3〜0.8mmであることを特徴とする皮革積層フィルムにある。   According to a third aspect of the present invention, in the leather laminated film according to the first or second aspect, the resin film has a thickness of 0.2 to 0.5 mm, and the leather has a thickness of 0.3 to 0. It is in a leather laminated film characterized by being 8 mm.

かかる第3の態様では、水性硬化性接着剤を用いて積層することにより、皮革の本来の風合いを残したまま、且つ真空圧空成形で所望の成形が可能な皮革積層フィルムを確実に実現できる。   In the third aspect, by laminating using an aqueous curable adhesive, it is possible to reliably realize a leather laminated film that can be formed by vacuum / pressure forming while keeping the original texture of the leather.

本発明の第4の態様は、第1〜3の何れかの態様の皮革積層フィルムを、真空圧空により所定形状に成形したことを特徴とする皮革積層フィルム成形体にある。   According to a fourth aspect of the present invention, there is provided a leather laminated film molded body in which the leather laminated film according to any one of the first to third aspects is formed into a predetermined shape by vacuum pressure.

かかる第4の態様では、所望の形状を有し、表面に皮革本来の風合いを有する皮革積層フィルム成形体を実現できる。   In the fourth aspect, a leather laminated film molded body having a desired shape and having a leather original texture on the surface can be realized.

本発明の第5の態様は、第4の態様の皮革積層フィルム成形体を一部に備え、当該皮革積層フィルム成形体に樹脂をインサート成形することにより設けられた樹脂成形体を具備することを特徴とする複合樹脂成形体にある。   According to a fifth aspect of the present invention, the leather laminated film molded body according to the fourth aspect is partially provided and a resin molded body provided by insert molding a resin into the leather laminated film molded body. The composite resin molded product is characterized.

かかる第5の態様では、皮革積層フィルム成形体を用いてインサート成形することにより、表面に皮革本来の風合いを有する皮革被覆を具備する複合樹脂成形体を実現できる。   In the fifth aspect, by performing insert molding using a leather laminated film molded body, a composite resin molded body having a leather coating having a leather original texture on the surface can be realized.

本発明の第6の態様は、皮革の一方の面と、樹脂フィルムの一方の面とに水性硬化性接着剤を塗布する工程と、前記皮革の水性硬化性接着剤の塗布層と、前記樹脂フィルムの水性硬化性接着剤の塗布層とを加熱乾燥して活性化する工程と、前記皮革の水性硬化性接着剤の塗布層と、前記樹脂フィルムの水性硬化性接着剤の塗布層とを合わせる工程と、貼り合わせた積層体を圧着する工程と、圧着した積層体を養生して皮革積層フィルムとする工程とを具備することを特徴とする皮革積層フィルムの製造方法にある。   The sixth aspect of the present invention includes a step of applying an aqueous curable adhesive to one side of the leather and one side of the resin film, an application layer of the aqueous curable adhesive of the leather, and the resin. The step of heat-drying and activating the aqueous curable adhesive coating layer of the film is combined with the aqueous curable adhesive coating layer of the leather and the aqueous curable adhesive coating layer of the resin film. A method for producing a leather laminate film comprising: a step, a step of pressure-bonding the bonded laminate, and a step of curing the pressure-bonded laminate to form a leather laminate film.

かかる第6の態様では、水性硬化性接着剤を用いて所定の工程で積層することにより、皮革の本来の風合いを残したまま、樹脂フィルムとの積層体を製造できる。   In this sixth aspect, a laminate with a resin film can be produced while leaving the original texture of leather by laminating in a predetermined step using an aqueous curable adhesive.

以上説明したように、本発明では、水性硬化性接着剤を用いて積層することにより、皮革の本来の風合いを残したまま、樹脂フィルムとの積層体を実現でき、これを用いて、真空圧空することにより、皮革積層フィルム成形体が実現でき、これをさらにインサート成形することにより、複合樹脂成形体が実現できる。   As described above, in the present invention, by laminating using an aqueous curable adhesive, it is possible to realize a laminate with a resin film while leaving the original texture of leather, and using this, vacuum compressed air is used. By doing so, a leather laminated film molded body can be realized, and by further insert molding, a composite resin molded body can be realized.

本発明の一実施形態に係る皮革積層フィルムの斜視図及び側面図である。It is the perspective view and side view of the leather laminated film which concern on one Embodiment of this invention. 皮革積層フィルムの製造工程を説明する図である。It is a figure explaining the manufacturing process of a leather laminated film. 皮革積層フィルムの製造工程を説明する図である。It is a figure explaining the manufacturing process of a leather laminated film. 真空圧空金型の一例を示す断面図である。It is sectional drawing which shows an example of a vacuum pressure mold. 一実施形態の皮革積層フィルム成形体の断面図である。It is sectional drawing of the leather laminated film molded object of one Embodiment. 一実施形態の複合樹脂成形体の断面図である。It is sectional drawing of the composite resin molding of one Embodiment. インサート成形金型の一例を示す断面図である。It is sectional drawing which shows an example of an insert molding die.

以下に本発明を実施形態に基づいて詳細に説明する。   Hereinafter, the present invention will be described in detail based on embodiments.

(実施形態1)
図1(a)、(b)は、本発明の実施形態1に係る皮革積層フィルムの概略を示す斜視図及び側面図である。
(Embodiment 1)
1 (a) and 1 (b) are a perspective view and a side view showing an outline of a leather laminated film according to Embodiment 1 of the present invention.

図1に示すように、本実施形態に係る皮革積層フィルム1は、皮革2と、樹脂フィルム3とを、水溶性硬化性接着剤からなる接着層4で積層したものである。   As shown in FIG. 1, a leather laminated film 1 according to this embodiment is obtained by laminating leather 2 and a resin film 3 with an adhesive layer 4 made of a water-soluble curable adhesive.

皮革2は、厚さ約0.3〜0.8mm程度の天然皮革であり、樹脂フィルム3は、厚さ0.1〜0.5mm、好ましくは、0.15〜0.4mmの樹脂フィルムである。樹脂フィルム3の材質は特に限定されないが、ポリカーボネート、アクリル、塩化ビニールを挙げることができ、ポリカーボネートが特に好ましい。   The leather 2 is a natural leather having a thickness of about 0.3 to 0.8 mm, and the resin film 3 is a resin film having a thickness of 0.1 to 0.5 mm, preferably 0.15 to 0.4 mm. is there. The material of the resin film 3 is not particularly limited, and examples thereof include polycarbonate, acrylic, and vinyl chloride, and polycarbonate is particularly preferable.

接着層4を形成する水溶性硬化性接着剤としては、水性ウレタン系接着剤、水性アクリル系接着剤などを挙げることができ、水性ウレタン系接着剤が好ましい。   Examples of the water-soluble curable adhesive forming the adhesive layer 4 include a water-based urethane adhesive and a water-based acrylic adhesive, and a water-based urethane adhesive is preferable.

本発明の皮革積層フィルム1は、水性硬化性接着剤からなる接着層4により、皮革2と樹脂フィルム3とを積層しているので、皮革本来の風合いを維持し、且つ所望の形状に成形できるものである。   Since the leather laminated film 1 of the present invention has the leather 2 and the resin film 3 laminated by the adhesive layer 4 made of an aqueous curable adhesive, the original texture of the leather can be maintained and formed into a desired shape. Is.

なお、本実施形態の皮革積層フィルム1で、樹脂フィルム3が皮革2より大面積となっているのは、後述する真空圧空成形する際に、皮革積層フィルム1の外縁部を固定するために使用するためである。勿論、皮革2が無駄にはなるが、同じ形状の皮革2と樹脂フィルム3とを積層してもよい。   In addition, in the leather laminated film 1 of this embodiment, the resin film 3 has a larger area than the leather 2 when used for fixing the outer edge of the leather laminated film 1 when vacuum / pressure forming described later. It is to do. Of course, although the leather 2 is wasted, the leather 2 and the resin film 3 having the same shape may be laminated.

図2、図3には、皮革積層フィルム1の製造例の一例の概略工程を示す。図に示すように、まず、約0.6mmの厚さの皮革2の接着面と、厚さ0.3mmの厚さのポリカードネートフィルムからなる樹脂フィルム3の接着領域に、水性硬化性接着剤4a、本実施形態では、水溶性ウレタン系接着剤を、例えば、スプレー塗布などにより塗布した(図2(a))。ここで、塗布方法は、接着剤を薄く且つ均一に塗布できる方法であれば、特に限定されず、刷毛塗り、ローラ塗布などで行ってもよいが、特に皮革2への塗布は、皮革本来の風合いを維持するために、スプレー塗布が好ましい。   In FIG. 2, FIG. 3, the outline process of an example of the manufacture example of the leather laminated film 1 is shown. As shown in the figure, first, aqueous curable adhesive is applied to the adhesive surface of the leather 2 having a thickness of about 0.6 mm and the adhesive region of the resin film 3 made of a polycarbonate film having a thickness of 0.3 mm. Agent 4a, in this embodiment, a water-soluble urethane adhesive was applied by, for example, spray coating (FIG. 2A). Here, the application method is not particularly limited as long as the adhesive can be applied thinly and uniformly, and may be performed by brush application, roller application, or the like. In order to maintain the texture, spray coating is preferred.

次いで、このように水溶性硬化性接着剤を塗布した皮革2及び樹脂フィルム3を、乾燥並びに接着剤の活性化処理のために、加熱処理する(図2(b))。   Next, the leather 2 and the resin film 3 to which the water-soluble curable adhesive is thus applied are subjected to heat treatment for drying and activation treatment of the adhesive (FIG. 2B).

乾燥・活性化処理は、加熱処理によって行うが、水分が蒸発し、固形分が加熱活性化されるように行えばよく、その方法は特に限定されないが、好ましくは、遠赤外線ヒーターや近赤外線ヒーターを用いるのがよい。加熱条件は、硬化反応が生じない条件下で行うのがよく、例えば、被処理体が60〜80℃程度になるように加熱処理をするのがよい。本実施形態では、例えば、200℃程度の加熱処理能力を有する、例えば、5台の遠赤外線ヒーター5と、700℃程度の加熱能力を有する近赤外線ヒーター6とを用い、連続的に処理することにより、60〜80℃での処理を行い、最後に瞬間的に80〜120℃程度の高温処理を行い、乾燥・活性化を実施した。   The drying / activation treatment is performed by heat treatment, and it may be carried out so that moisture evaporates and the solid content is heat activated. The method is not particularly limited, but is preferably a far infrared heater or a near infrared heater. Should be used. Heating conditions are preferably performed under conditions that do not cause a curing reaction. For example, heat treatment is preferably performed so that the object to be processed has a temperature of about 60 to 80 ° C. In this embodiment, for example, five far-infrared heaters 5 having a heat treatment capability of about 200 ° C. and a near-infrared heater 6 having a heating capability of about 700 ° C. are used for continuous processing. Then, a treatment at 60 to 80 ° C. was performed, and finally, a high temperature treatment at about 80 to 120 ° C. was instantaneously performed, followed by drying and activation.

次いで、乾燥・活性化処理を施した皮革2及び樹脂フィルム3を、接着面同士を合わせて積層した(図3(a))。続いて、ローラ7などを用いて両者を圧着した(図3(b))。   Next, the leather 2 and the resin film 3 that had been subjected to drying / activation treatment were laminated with the adhesive surfaces thereof aligned (FIG. 3A). Then, both were pressure-bonded using the roller 7 etc. (FIG.3 (b)).

圧着する条件は、特に限定されないが、例えば、5〜20kg/cm程度の圧力で行う。これにより、皮革積層フィルム1が製造される(図3(c))。 Although the conditions for crimping are not particularly limited, for example, the pressure is about 5 to 20 kg / cm 2 . Thereby, the leather laminated film 1 is manufactured (FIG. 3C).

このような皮革積層フィルム1は、水性ウレタン系接着剤などの水性硬化性接着剤を用いて積層することにより、塗布した接着剤が皮革の繊維内に含浸せずに硬化するためか、皮革の本来の風合いを残したままであった。   Such a leather laminated film 1 is laminated by using a water-based curable adhesive such as a water-based urethane adhesive, so that the applied adhesive is cured without impregnating the fibers of the leather, or the leather The original texture was left.

また、皮革2だけでは所望の形状に成形できないが、皮革積層フィルム1は、樹脂フィルム3との積層体となっているので、所望の形状に成形が可能である。   Moreover, although it cannot be shape | molded in a desired shape only with the leather 2, since the leather laminated | multilayer film 1 is a laminated body with the resin film 3, it can be shape | molded in a desired shape.

このような皮革積層フィルム1の形成は、プレス成形などによっても可能であるが、皮革の本来の風合いをできるだけ維持したまま成形するためには、真空圧空成形を行うのがよい。   The leather laminated film 1 can be formed by press molding or the like, but in order to mold the leather while maintaining the original texture as much as possible, it is preferable to perform vacuum / pressure forming.

真空圧空成形は、所定の金型を用い、皮革積層フィルム1の一方面から真空引きすると同時に、他方面から空気などの気体で加圧することにより行う。加圧する面は、皮革2の面であり、気体での加圧なので、皮革本来の風合いを維持することができる。   Vacuum / pressure forming is performed by using a predetermined mold and evacuating from one surface of the leather laminated film 1 and simultaneously applying pressure from the other surface with a gas such as air. The surface to be pressed is the surface of the leather 2 and is pressurized with gas, so that the original texture of the leather can be maintained.

具体的な真空圧空成形の概略を図5に示す。図5に示す真空圧空金型20は、下型21を有する。下型21は、所望の形状の凸部22を具備し、凸部22の成形面に開口し、真空引きするための複数の貫通孔23を具備する。また、皮革積層フィルム1の外縁部、図5の皮革積層フィルム1では、樹脂フィルム3のみを部分を固定する固定部24を具備する。一方、上型25は、下型21との間に所定の空間26を画成する凹部27を有し、また、空間26に加圧気体を導入するための複数の加圧孔28を具備するものである。   A specific vacuum / pressure forming process is schematically shown in FIG. The vacuum pressure mold 20 shown in FIG. 5 has a lower mold 21. The lower mold 21 includes a convex portion 22 having a desired shape, and includes a plurality of through holes 23 that open to the molding surface of the convex portion 22 and are evacuated. Moreover, in the outer edge part of the leather laminated film 1, and the leather laminated film 1 of FIG. 5, the fixing | fixed part 24 which fixes only the resin film 3 is comprised. On the other hand, the upper die 25 has a concave portion 27 that defines a predetermined space 26 between the upper die 25 and a plurality of pressurizing holes 28 for introducing pressurized gas into the space 26. Is.

真空圧空成形は、上述した真空圧空金型20を用い、下型21の貫通孔23から、例えば、−1kg/cm程度で真空引きしながら皮革積層フィルム1を凸部22に被せ、固定部24を用いて、皮革積層フィルム1を下型21に固定する。この状態で上型25を閉め、皮革積層フィルム1と上型25との間の空間26に、加圧孔28から加圧気体、例えば、空気を導入する。これにより、皮革積層フィルム1の皮革2からなる表面を0〜300kg/cm程度の力Fで加圧する。また、下型21は、必要に応じて、60〜80℃程度に加熱しても良い。 Vacuum / pressure forming uses the above-described vacuum / pressure air mold 20 and covers the leather laminated film 1 on the convex portion 22 while evacuating from the through hole 23 of the lower die 21 at, for example, about −1 kg / cm 2 , and fixing portion 24, the leather laminated film 1 is fixed to the lower mold 21. In this state, the upper mold 25 is closed, and a pressurized gas, for example, air is introduced into the space 26 between the leather laminated film 1 and the upper mold 25 from the pressure hole 28. Thereby, the surface which consists of the leather 2 of the leather laminated film 1 is pressurized with the force F of about 0-300 kg / cm < 2 >. Moreover, you may heat the lower mold | type 21 to about 60-80 degreeC as needed.

これにより、図4(a)に示すような、皮革積層フィルム成形体10を製造することができる。この際、皮革2の表面は、気体で加圧されるので、皮革本来の風合いを維持することができる。   Thereby, the leather laminated film molded object 10 as shown to Fig.4 (a) can be manufactured. At this time, since the surface of the leather 2 is pressurized with gas, the original texture of the leather can be maintained.

また、皮革積層フィルム成形体10は、不要な部位を切断して、皮革積層フィルム成形体11とすることができる。   Moreover, the leather laminated film molded object 10 can cut | disconnect an unnecessary site | part, and can be set as the leather laminated film molded object 11.

このような皮革積層フィルム成形体11は、例えば、スマートフォンのケースなど、各種用途に用いることができるが、さらに、皮革積層フィルム成形体11を用いてインサート成形し、複合樹脂成形体とすることができる。   Such a leather laminated film molded body 11 can be used for various applications such as a smartphone case, and further, insert molding using the leather laminated film molded body 11 to form a composite resin molded body. it can.

図6には、複合樹脂成形体の一例の断面を示す。図示するように、この複合樹脂成形体30は、皮革積層フィルム成形体11の樹脂フィルム側に、樹脂成形部31を一体的に形成したものである。   In FIG. 6, the cross section of an example of a composite resin molding is shown. As shown in the figure, the composite resin molded body 30 is obtained by integrally forming a resin molded portion 31 on the resin film side of the leather laminated film molded body 11.

このような複合樹脂成形体30の製造方法の一例の概略を図7に示す。図7は、複合樹脂成形体30を成形するインサート成形金型の一例を示す。インサート成形金型40は、上型41を備える。上型41は、皮革積層フィルム成形体11を保持するための凹部42と、凹部42の内面に開口する複数の貫通孔43とを具備し、貫通孔43を介して吸引することにより皮革積層フィルム成形体11を凹部42に保持できるようになっている。また、インサート成形金型40は、下型45を備える。下型45は、上型41との間で、樹脂成形部31を成形する成形凹部46を有し、成形凹部46に連通する樹脂流入路47を具備し、樹脂流入路47の成形凹部46とは反対側には、射出成形機48のノズル49が接続されている。   An outline of an example of a method for producing such a composite resin molded body 30 is shown in FIG. FIG. 7 shows an example of an insert molding die for molding the composite resin molded body 30. The insert molding die 40 includes an upper die 41. The upper die 41 includes a concave portion 42 for holding the leather laminated film molded body 11 and a plurality of through holes 43 opened in the inner surface of the concave portion 42, and the leather laminated film is sucked through the through holes 43. The molded body 11 can be held in the recess 42. Further, the insert molding die 40 includes a lower die 45. The lower mold 45 has a molding recess 46 that molds the resin molding portion 31 between the lower mold 45 and a resin inflow passage 47 that communicates with the molding recess 46. The nozzle 49 of the injection molding machine 48 is connected to the opposite side.

このようなインサート成形金型40を用い、上型41の凹部42に皮革積層フィルム成形体11を保持した状態で、樹脂をインサート成形することにより、複合樹脂成形体30を製造できる。   The composite resin molded body 30 can be manufactured by insert molding the resin using such an insert molding die 40 while holding the leather laminated film molded body 11 in the recess 42 of the upper mold 41.

このように、皮革積層フィルム成形体11を用いてインサート成形することにより製造された複合樹脂成形体30は、表面に皮革本来の風合いを有する皮革被覆を具備するものである。   Thus, the composite resin molded body 30 manufactured by insert molding using the leather laminated film molded body 11 is provided with a leather coating having a leather original texture on the surface.

1 皮革積層フィルム
2 皮革
3 樹脂フィルム
4 接着層
10、11 皮革積層フィルム成形体
20 真空圧空金型
30 複合樹脂成形体
31 樹脂成形部
40 インサート成形金型
DESCRIPTION OF SYMBOLS 1 Leather laminated film 2 Leather 3 Resin film 4 Adhesive layer 10, 11 Leather laminated film molded body 20 Vacuum pressure air mold 30 Composite resin molded body 31 Resin molded part 40 Insert mold

Claims (6)

皮革と、樹脂フィルムとを水性硬化性接着剤で積層したことを特徴とする皮革積層フィルム。   A leather laminated film comprising a leather and a resin film laminated with an aqueous curable adhesive. 請求項1の皮革積層フィルムにおいて、前記樹脂フィルムは、前記皮革より大面積であることを特徴とする皮革積層フィルム。   The leather laminated film according to claim 1, wherein the resin film has a larger area than the leather. 請求項1又は2の皮革積層フィルムにおいて、前記樹脂フィルムの厚さは0.2〜0.5mmであり、前記皮革の厚さは、0.3〜0.8mmであることを特徴とする皮革積層フィルム。   The leather laminated film according to claim 1 or 2, wherein the resin film has a thickness of 0.2 to 0.5 mm, and the leather has a thickness of 0.3 to 0.8 mm. Laminated film. 請求項1〜3の何れか一項記載の皮革積層フィルムを、真空圧空により所定形状に成形したことを特徴とする皮革積層フィルム成形体。   A leather laminate film molded body, wherein the leather laminate film according to any one of claims 1 to 3 is formed into a predetermined shape by vacuum pressure air. 請求項4記載の皮革積層フィルム成形体を一部に備え、当該皮革積層フィルム成形体に樹脂をインサート成形することにより設けられた樹脂成形体を具備することを特徴とする複合樹脂成形体。   5. A composite resin molded body comprising a leather multilayer film molded body according to claim 4 in a part, and comprising a resin molded body provided by insert molding a resin in the leather multilayer film molded body. 皮革の一方の面と、樹脂フィルムの一方の面とに水性硬化性接着剤を塗布する工程と、
前記皮革の水性硬化性接着剤の塗布層と、前記樹脂フィルムの水性硬化性接着剤の塗布層とを加熱乾燥して活性化する工程と、
前記皮革の水性硬化性接着剤の塗布層と、前記樹脂フィルムの水性硬化性接着剤の塗布層とを合わせる工程と、
貼り合わせた積層体を圧着する工程と、
圧着した積層体を養生して皮革積層フィルムとする工程と
を具備することを特徴とする皮革積層フィルムの製造方法。
Applying an aqueous curable adhesive to one side of the leather and one side of the resin film;
A step of heat-drying and activating the aqueous curable adhesive coating layer of the leather and the aqueous curable adhesive coating layer of the resin film;
Combining the aqueous curable adhesive coating layer of the leather with the aqueous curable adhesive coating layer of the resin film;
A step of pressure-bonding the laminated body,
A method for producing a leather laminate film comprising: curing a pressure-bonded laminate to form a leather laminate film.
JP2015042856A 2015-03-04 2015-03-04 Leather laminated film for vacuum pressure forming, leather laminated film molded product, composite resin molded product, and method for producing leather laminated film Active JP6632051B2 (en)