JP2011178817A5 - - Google Patents

Download PDF

Info

Publication number
JP2011178817A5
JP2011178817A5 JP2010041222A JP2010041222A JP2011178817A5 JP 2011178817 A5 JP2011178817 A5 JP 2011178817A5 JP 2010041222 A JP2010041222 A JP 2010041222A JP 2010041222 A JP2010041222 A JP 2010041222A JP 2011178817 A5 JP2011178817 A5 JP 2011178817A5
Authority
JP
Japan
Prior art keywords
phenolic resin
rosin
modified phenolic
mgkoh
weight
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2010041222A
Other languages
Japanese (ja)
Other versions
JP5482287B2 (en
JP2011178817A (en
Filing date
Publication date
Application filed filed Critical
Priority to JP2010041222A priority Critical patent/JP5482287B2/en
Priority claimed from JP2010041222A external-priority patent/JP5482287B2/en
Publication of JP2011178817A publication Critical patent/JP2011178817A/en
Publication of JP2011178817A5 publication Critical patent/JP2011178817A5/ja
Application granted granted Critical
Publication of JP5482287B2 publication Critical patent/JP5482287B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Description

すなわち、本発明は、(a)ロジン類100重量部、(b)レゾール型フェノール樹脂が30〜90重量部および(c)ポリオールを、酸価が80(mgKOH/g)以下になるまで反応させた後、更に酸触媒を添加する事を特徴とするロジン変性フェノール樹脂の製造方法に関するものである。
That is, the present invention may be prepared by reacting (a) a rosin 100 parts by weight, the (b) resole phenolic resin is 30 to 90 parts by weight (c) a polyol, until an acid value of 80 (mgKOH / g) or less Then, an acid catalyst is further added, and the present invention relates to a method for producing a rosin-modified phenol resin.

Figure 2011178817
Figure 2011178817

Claims (5)

(a)ロジン類100重量部、(b)レゾール型フェノール樹脂が30〜90重量部および(c)ポリオールを、酸価が80(mgKOH/g)以下になるまで反応させた後、更に酸触媒を添加する事を特徴とするロジン変性フェノール樹脂の製造方法。 (A) 100 parts by weight of rosins, (b) 30 to 90 parts by weight of a resol type phenolic resin, and (c) a polyol are reacted until the acid value becomes 80 (mgKOH / g) or less, and then an acid catalyst. A process for producing a rosin-modified phenolic resin characterized by adding 酸価が45〜80(mgKOH/g)になった時、酸触媒を添加することを特徴とする請求項1記載のロジン変性フェノール樹脂の製造方法。   The method for producing a rosin-modified phenolic resin according to claim 1, wherein an acid catalyst is added when the acid value becomes 45 to 80 (mgKOH / g). 請求項1、または2記載の製造方法により合成させてなる事を特徴とするロジン変性フェノール樹脂。   A rosin-modified phenolic resin synthesized by the production method according to claim 1 or 2. 請求項3記載のロジン変性フェノール樹脂を含有する事を特徴とする平版印刷インキ。   A lithographic printing ink comprising the rosin-modified phenolic resin according to claim 3. 請求項4記載の平版印刷インキを印刷してなる印刷物。
A printed matter obtained by printing the lithographic printing ink according to claim 4.
JP2010041222A 2010-02-26 2010-02-26 Method for producing resin for lithographic printing ink and lithographic printing ink Active JP5482287B2 (en)