JP2005263234A - Paper container - Google Patents

Paper container Download PDF

Info

Publication number
JP2005263234A
JP2005263234A JP2004075354A JP2004075354A JP2005263234A JP 2005263234 A JP2005263234 A JP 2005263234A JP 2004075354 A JP2004075354 A JP 2004075354A JP 2004075354 A JP2004075354 A JP 2004075354A JP 2005263234 A JP2005263234 A JP 2005263234A
Authority
JP
Japan
Prior art keywords
paper
container
container body
opening
varnish
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
JP2004075354A
Other languages
Japanese (ja)
Inventor
Hisakuni Torii
久訓 鳥居
Michiaki Fujita
実智昭 藤田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kao Corp
Original Assignee
Kao Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kao Corp filed Critical Kao Corp
Priority to JP2004075354A priority Critical patent/JP2005263234A/en
Publication of JP2005263234A publication Critical patent/JP2005263234A/en
Withdrawn legal-status Critical Current

Abstract

<P>PROBLEM TO BE SOLVED: To provide a paper container which enhances the adhesiveness of a sealing strip of paper to the opening of a container body. <P>SOLUTION: In the paper container 10, the opening 11E of a container body 11 is sealed by a sealing strip of paper 13. The entire outer periphery on the side of the opening 11E out of the outer peripheries of the container body 11 forms an unvarnished part 22, and the peripheral edge of the sealing strip of paper 13 is adhered to the unvarnished part 22. <P>COPYRIGHT: (C)2005,JPO&NCIPI

Description

本発明は粉体洗剤用紙容器等に用いて好適な紙容器に関する。   The present invention relates to a paper container suitable for use in a powder detergent paper container or the like.

粉体洗剤用紙容器として、特許文献1に記載の如く、内容物の粉体洗剤を流通保管段階で密封するため、容器本体の開口部を封緘紙で密封するものがある。封緘紙は、容器本体の開口部の側の外周の全周に接着される。
特開2001-315767
As a powder detergent paper container, there is a powder detergent paper container in which the opening of the container body is sealed with a sealing paper in order to seal the powder detergent in the contents at the distribution storage stage. The sealing paper is bonded to the entire circumference of the outer periphery of the container body on the opening side.
JP2001-315767

粉体洗剤用紙容器では、一般に、容器本体の外周に印刷を施し、更には、この印刷に光沢や艶消し等のデザイン性を付与したり、この印刷の表面に耐磨耗性を付与するための表面加工として、印刷表面に無色透明又は半透明のニスを施す。   In powder detergent paper containers, in general, printing is performed on the outer periphery of the container main body, and furthermore, design properties such as gloss and matte are given to the printing, and abrasion resistance is given to the surface of the printing. As the surface treatment, a colorless transparent or translucent varnish is applied to the printing surface.

従来の粉体洗剤用紙容器では、特許文献1に記載の如くの封緘紙が接着される容器本体の開口部の側の外周にまで上述の印刷及びニスが付与されており、この印刷及びニスは封緘紙の接着性を阻害する。   In the conventional powder detergent paper container, the above-mentioned printing and varnish are applied to the outer periphery of the opening side of the container body to which the sealing paper as described in Patent Document 1 is bonded. Impairs adhesive properties of sealing paper.

本発明の課題は、紙容器において、容器本体の開口部への封緘紙の接着性を向上することにある。   The subject of this invention is improving the adhesiveness of the sealing paper to the opening part of a container main body in a paper container.

請求項1の発明は、容器本体の開口部を封緘紙で密封した紙容器であって、容器本体の外周のうち、開口部の側の外周の全周をニスが付与されないニス非付与部とし、封緘紙の周縁を上記ニス非付与部に接着したものである。   Invention of Claim 1 is a paper container which sealed the opening part of the container main body with sealing paper, Comprising: The outer periphery of the container main body is made into the varnish non-applied part to which the outer periphery by the side of an opening part is not provided. The periphery of the sealing paper is bonded to the non-varnish portion.

粉体洗剤用紙容器10は、図1に示す如く、容器本体11と蓋12と封緘紙13とからなる。   As shown in FIG. 1, the powder detergent paper container 10 includes a container main body 11, a lid 12, and a sealing paper 13.

容器本体11は、紙だけ、もしくは紙を主材料としてプラスチックフィルムをラミネートされた素材を折り曲げて組立てたものであり、正面板11A、背面板11B(不図示)、両側板11C、11C、底板11D(不図示)を有する。   The container body 11 is assembled by folding only a paper or a material laminated with a plastic film using paper as a main material, and includes a front plate 11A, a back plate 11B (not shown), both side plates 11C, 11C, and a bottom plate 11D. (Not shown).

容器本体11は、正面板11A、背面板11B、両側板11C、11Cの上端部により開口部11Eを囲み形成し、正面板11A、背面板11B、両側板11C、11Cの開口部11Eの側の縁部である各開口縁部11Fに、実公平2-32567と同様の外側から設けた半切り線を介して折返し片11Gを連設し、この半切り線を開くように折返し片11Gをそれらの正面板11A、背面板11B、両側板11C、11Cの内側に折返している。半切り線の深さは、折返し片11Gを折返したときに、半切り線を開くことによって相並ぶ正面板11A、背面板11B、両側板11C、11Cの各開口縁部11Fと、それらに対応する折返し片11Gの上端部とが面一をなす平坦面を形成するように、容器本体11の板厚の2/3〜1/2とすることが好ましい。折返し片11Gは、本実施例では正面板11A、背面板11B、両側板11C、11Cの内面に接着するが、必ずしも接着することを要しない。これにより、容器本体11の正面板11A、背面板11B、両側板11C、11Cの各開口縁部11Fと、それらに対応する折返し片11Gの上端部は、図2に示す如く、面一をなして相並ぶ平坦面状縁部(巾w)を形成する。   The container body 11 surrounds and forms an opening 11E with upper ends of the front plate 11A, the back plate 11B, and the side plates 11C and 11C, and is located on the side of the opening 11E of the front plate 11A, the back plate 11B, and the side plates 11C and 11C. Folding pieces 11G are continuously connected to each opening edge portion 11F, which is an edge portion, through a half cut line provided from the outside similar to that of actual fair 2-332567, and the folded pieces 11G are arranged so as to open this half cut line. The front plate 11A, the back plate 11B, and both side plates 11C and 11C are folded back. The depth of the half-cut line corresponds to the opening edge portions 11F of the front plate 11A, the back plate 11B, the side plates 11C, 11C, which are aligned by opening the half-cut line when the folded piece 11G is folded back, and to them. It is preferable that the thickness of the container body 11 be 2/3 to 1/2 so that a flat surface that is flush with the upper end of the folded piece 11G is formed. The folded piece 11G adheres to the inner surfaces of the front plate 11A, the back plate 11B, and the side plates 11C, 11C in this embodiment, but it does not necessarily need to be bonded. As a result, the opening edge 11F of the front plate 11A, the back plate 11B, the side plates 11C, 11C of the container body 11 and the upper end of the folded piece 11G corresponding to them are flush with each other as shown in FIG. To form a flat planar edge (width w).

蓋12は、紙だけ、もしくは紙を主材料としてプラスチックフィルムをラミネートされた素材を折り曲げて組立てたものであり、前板12A、後板12B(不図示)、両側板12C、12C、天板12Dを有する。蓋12は、前板12Aにつまみ部12Eを備え、後板12Bにヒンジ結合部12F(不図示)を備える。   The lid 12 is assembled by folding only a paper or a material laminated with a plastic film using paper as a main material, and includes a front plate 12A, a rear plate 12B (not shown), both side plates 12C and 12C, and a top plate 12D. Have The lid 12 includes a knob 12E on the front plate 12A, and a hinge coupling portion 12F (not shown) on the rear plate 12B.

紙容器10は、容器本体11の背面板11Bに蓋12のヒンジ結合部12Fをヒンジ結合して構成される。このとき、紙容器10は、容器本体11の開口部11Eを封緘紙13で密封し、内容物の粉体洗剤を流通保管段階で密封可能にする。   The paper container 10 is configured by hinge-joining a hinge coupling portion 12F of the lid 12 to a back plate 11B of the container body 11. At this time, the paper container 10 seals the opening 11E of the container main body 11 with the sealing paper 13 so that the powder detergent of the contents can be sealed at the distribution storage stage.

紙容器10は、図3に示す如く、容器本体11の正面板11A、背面板11B、両側板11C、11Cが構成する外周の概ね全部を印刷部21とするものの、開口部11Eの側の外周についてはその全周を一定巾のニス非付与部22(巾h)とする。印刷部21では、正面板11A、背面板11B、両側板11C、11Cの外面に印刷を施し、更には、この印刷に光沢や艶消し等のデザイン性を付与したり、この印刷の表面に耐磨耗性を付与するための表面加工として、印刷表面に無色透明又は半透明のopニス等のニスを施す。ニス非付与部22では、印刷及びニスが施されない。   As shown in FIG. 3, the paper container 10 has a printing unit 21 as a whole of the outer periphery formed by the front plate 11 </ b> A, the back plate 11 </ b> B, and the both side plates 11 </ b> C and 11 </ b> C of the container body 11, but the outer periphery on the opening 11 </ b> E side. The whole circumference is defined as a varnish non-applied portion 22 (width h) having a constant width. The printing unit 21 performs printing on the outer surfaces of the front plate 11A, the back plate 11B, and the both side plates 11C and 11C, and further gives design such as gloss and matte to the print, and provides resistance to the surface of the print. As a surface treatment for imparting abrasion, a varnish such as a colorless transparent or translucent op varnish is applied to the printing surface. In the varnish non-applying portion 22, printing and varnishing are not performed.

但し、本発明では、ニス非付与部22に、印刷は施し、ニスは施さないものとしても良い。   However, in the present invention, the varnish non-applied portion 22 may be printed but not varnished.

紙容器10は、容器本体11の開口部11Eに被した封緘紙13の四角枠状接着部13Aを、容器本体11の正面板11A、背面板11B、両側板11C、11Cの各開口縁部11Fと、それらに対応する折返し片11Gの上端部とが形成する巾wの平坦面状縁部に接着するとともに、封緘紙13の接着部13Aより外周側の周縁であって容器本体11の各開口縁部11Fの周囲に突出する周縁に定めた接着部13Bを、容器本体11の正面板11A、背面板11B、両側板11C、11Cに設けたニス非付与部22に接着する。   In the paper container 10, the rectangular frame-shaped adhesive portion 13A of the sealing paper 13 that covers the opening portion 11E of the container body 11 is connected to the opening edge portions 11F of the front plate 11A, the back plate 11B, and the side plates 11C, 11C of the container body 11. And the upper end of the folded piece 11G corresponding to them are bonded to the flat surface edge of width w, and are the peripheral edge on the outer peripheral side from the bonding portion 13A of the sealing paper 13 and each opening of the container body 11 The adhesion part 13B defined on the periphery protruding around the edge part 11F is adhered to the varnish non-applied part 22 provided on the front plate 11A, the back plate 11B, and the side plates 11C, 11C of the container body 11.

紙容器10の製造手順は例えば以下の如くである(図4)。
(1)容器本体11の各開口縁部11Fと、折返し片11Gの上端部が形成する平坦面状縁部(巾w)と、容器本体11のニス非付与部22(巾h)のそれぞれに接着剤を塗布する。接着剤としては、例えば水性エマルジョン系接着剤を使用できる。
The manufacturing procedure of the paper container 10 is, for example, as follows (FIG. 4).
(1) Each opening edge portion 11F of the container body 11, the flat surface edge portion (width w) formed by the upper end portion of the folded piece 11G, and the varnish non-applied portion 22 (width h) of the container body 11 Apply adhesive. As the adhesive, for example, an aqueous emulsion adhesive can be used.

(2)封緘紙13における、容器本体11への接着剤塗布箇所に対応する箇所(接着部13A、13B)に、容器本体11への接着剤塗布巾より広い巾で接着剤を塗布する。接着剤としては、例えば水性エマルジョン系接着剤を使用できる。   (2) The adhesive is applied to a location (adhesive portions 13A, 13B) corresponding to the location where the adhesive is applied to the container body 11 in the sealing paper 13 with a width wider than the width of the adhesive applied to the container body 11. As the adhesive, for example, an aqueous emulsion adhesive can be used.

(3)封緘紙13の接着部13Aを、容器本体11の各開口縁部11Fと、折返し片11Gの上端部が形成する平坦面状縁部に位置合せして被せる。   (3) The adhesive portion 13A of the sealing paper 13 is placed in alignment with each opening edge portion 11F of the container body 11 and the flat surface edge portion formed by the upper end portion of the folded piece 11G.

(4)蓋12を封緘紙13の上から容器本体11の正面板11A、背面板11B、両側板11C、11Cが構成する外周に嵌着する。このとき、蓋12の前板12A、後板12B、両側板12C、12Cにより、容器本体11の各開口縁部11Fの周囲に突出した封緘紙13の周縁を、容器本体11の正面板11A、背面板11B、両側板11C、11Cの外面に向けて折り込む。そして、蓋12の天板12Dに加える圧力により、封緘紙13の接着部13Aを容器本体11の各開口縁部11Fと、折返し片11Gの上端部が形成する平坦面状縁部に圧着するとともに、蓋12の前板12A、後板12B、両側板12C、12Cに加える圧力により、封緘紙13の接着部13Bを容器本体11のニス非付与部22に圧着する。   (4) The lid 12 is fitted on the outer periphery formed by the front plate 11A, the back plate 11B, and the side plates 11C, 11C of the container body 11 from the top of the sealing paper 13. At this time, the front plate 12A, rear plate 12B, and both side plates 12C, 12C of the lid 12 are used to connect the peripheral edge of the sealing paper 13 protruding around each opening edge 11F of the container body 11 to the front plate 11A of the container body 11. Fold toward the outer surface of the back plate 11B and the side plates 11C, 11C. Then, with the pressure applied to the top plate 12D of the lid 12, the adhesive portion 13A of the sealing paper 13 is pressure-bonded to each opening edge portion 11F of the container body 11 and the flat planar edge portion formed by the upper end portion of the folded piece 11G. The adhesive portion 13B of the sealing paper 13 is pressure-bonded to the varnish non-applied portion 22 of the container body 11 by pressure applied to the front plate 12A, the rear plate 12B, and the side plates 12C and 12C of the lid 12.

尚、封緘紙13は、蓋12に積極的に加える外的圧力により容器本体11の側に接着されるものに限らず、蓋12を容器本体11に嵌着すると同時に容器本体11の側に接着されるものであっても良い。   Note that the sealing paper 13 is not limited to the one that is adhered to the container body 11 by external pressure positively applied to the lid 12, but is simultaneously adhered to the container body 11 while the lid 12 is fitted to the container body 11. It may be.

(5)蓋12の前後のつまみ部12Eとヒンジ結合部12Fが、容器本体11の正面板11A、背面板11Bのそれぞれに接着される。   (5) The front and rear knob portions 12E and the hinge coupling portion 12F of the lid 12 are bonded to the front plate 11A and the back plate 11B of the container body 11, respectively.

本実施例によれば、以下の作用効果を奏する。
(請求項1)
a 封緘紙13が接着される容器本体11の開口部11Eの側の外周の全周がニス非付与部22とされる。ニス非付与部22は、容器本体11の外周の全周に一定の広巾h(例えば5mm巾)をなして延在し、封緘紙13を確実に接着するに必要十分な接着面積を提供する。これにより、封緘紙13により、容器本体11の開口部11Eを簡易にして確実に密封可能として、併せて洗剤等の内容物の防湿性を向上する。
According to the present embodiment, the following operational effects can be obtained.
(Claim 1)
a The entire circumference of the outer periphery on the side of the opening 11E of the container body 11 to which the sealing paper 13 is bonded is the varnish non-applying portion 22. The varnish non-applying portion 22 extends around the entire circumference of the outer periphery of the container main body 11 with a certain wide width h (for example, 5 mm width), and provides a necessary and sufficient bonding area for securely bonding the sealing paper 13. Thereby, the opening 11E of the container main body 11 can be simply and reliably sealed by the sealing paper 13, and the moisture resistance of the contents such as the detergent is improved.

(請求項2)
b 容器本体11の上述aのニス非付与部22が、印刷及びニスを付与されないことにより、容器本体11の他の部分がいか様に印刷及びニスを付与されていても、封緘紙13をそのニス非付与部22に確実に接着できる。
(Claim 2)
b Since the varnish non-applying portion 22 of the above-mentioned a of the container main body 11 is not provided with printing and varnish, no matter how the other parts of the container main body 11 are printed and varnished, the sealing paper 13 is It is possible to securely adhere to the varnish non-applied portion 22.

(請求項3)
c 容器本体11の開口部11Eの側の縁部11Fに、外側から設けた半切り線を介して折返し片11Gを連設し、折返し片11Gを容器本体11の内側に折返した。容器本体11と折返し片11Gの上端部は、面一をなして相並ぶ平坦面状縁部を形成するものになり、容器本体11の開口部11Eの側の縁部11Fが単に折返された丸味状縁部を形成する場合に比して、封緘紙13をその平坦面状縁部にも安定的に接着できる。この平坦面状縁部は、比較的狭巾w(例えば1.4mm)であり、広巾化により封緘紙13の接着面積の拡大を図ることは困難であるものの、前述aのニス非付与部22の存在に相伴うことにより、封緘紙13による密封性を一層向上可能にする。
(Claim 3)
c The folded piece 11G was continuously connected to the edge portion 11F on the opening 11E side of the container body 11 via a half-cut line provided from the outside, and the folded piece 11G was folded inside the container body 11. The container body 11 and the upper end of the folded piece 11G form a flat planar edge that is flush with each other, and the edge 11F on the side of the opening 11E of the container body 11 is simply folded. The sealing paper 13 can be stably adhered to the flat surface edge as compared with the case where the edge is formed. Although this flat planar edge has a relatively narrow width w (eg, 1.4 mm) and it is difficult to increase the adhesive area of the sealing paper 13 by widening, By being accompanied by the presence, the sealing performance by the sealing paper 13 can be further improved.

図1は紙容器の開蓋状態を示す模式斜視図である。FIG. 1 is a schematic perspective view showing the open state of the paper container. 図2は紙容器の要部を示す模式断面図である。FIG. 2 is a schematic cross-sectional view showing the main part of the paper container. 図3は紙容器の容器本体を示す模式斜視図である。FIG. 3 is a schematic perspective view showing the container body of the paper container. 図4は紙容器の製造手順を示す工程図である。FIG. 4 is a process diagram showing a procedure for manufacturing a paper container.

符号の説明Explanation of symbols

10 紙容器
11 容器本体
11B 開口部
11F 開口縁部
11G 折返し片
13 封緘紙
22 ニス非付与部
DESCRIPTION OF SYMBOLS 10 Paper container 11 Container main body 11B Opening part 11F Opening edge part 11G Folding piece 13 Sealing paper 22 Varnish non-giving part

Claims (3)

容器本体の開口部を封緘紙で密封した紙容器であって、
容器本体の外周のうち、開口部の側の外周の全周をニスが付与されないニス非付与部とし、封緘紙の周縁を前記開口部又は/及び前記ニス非付与部に接着した紙容器。
A paper container in which the opening of the container body is sealed with a sealing paper,
The paper container which made the outer periphery of the container main body the outer periphery by the side of an opening part as the varnish non-applied part to which a varnish is not provided, and adhere | attached the periphery of the sealing paper on the said opening part and / or the said varnish non-applied part.
前記ニス非付与部が、印刷及びニスを付与されない請求項1に記載の紙容器。   The paper container according to claim 1, wherein the varnish non-applied portion is not applied with printing and varnish. 前記容器本体の開口部の側の縁部に、外側から設けた半切り線を介して折返し片を連設し、該折返し片を容器本体の内側に折返し、前記封緘紙を容器本体と折返し片の上端部にも接着してなる請求項1又は2に記載の紙容器。   Folding pieces are continuously connected to the edge of the opening side of the container body through a half-cut line provided from the outside, the folding pieces are folded back to the inside of the container body, and the sealing paper is folded to the container body. The paper container of Claim 1 or 2 formed by adhere | attaching also on the upper end part.
JP2004075354A 2004-03-16 2004-03-16 Paper container Withdrawn JP2005263234A (en)