JP2003320474A - Method for welding metallic thin film - Google Patents
Method for welding metallic thin filmInfo
- Publication number
- JP2003320474A JP2003320474A JP2002170702A JP2002170702A JP2003320474A JP 2003320474 A JP2003320474 A JP 2003320474A JP 2002170702 A JP2002170702 A JP 2002170702A JP 2002170702 A JP2002170702 A JP 2002170702A JP 2003320474 A JP2003320474 A JP 2003320474A
- Authority
- JP
- Japan
- Prior art keywords
- thin film
- metal thin
- welding
- frame
- camber
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
【001】[001]
【発明の属する技術分野】本発明は、金属薄膜を各種用
途に利用する際金属薄膜に張力及び歪み逃げを設けて枠
フレーム本体部品に溶接固定する方法。BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a method of welding and fixing a metal thin film to a frame body part by providing tension and strain relief to the metal thin film when it is used for various purposes.
【002】[002]
【従来の技術】従来は、金属薄膜を溶接固定することが
難しかった。そのため金属薄膜を厚い板によって物理的
にサンドイッチする構造であり電鋳のような一体の成型
品などを使用してきた。2. Description of the Related Art Conventionally, it was difficult to weld and fix a metal thin film. Therefore, a structure in which a metal thin film is physically sandwiched by a thick plate has been used, and an integrally molded product such as electroforming has been used.
【003】[003]
【発明が解決しようとする課題】金属薄膜の溶接技術が
限られており溶接歪みも考えて実現難しい状況であっ
た。金属薄膜の溶接もシーム溶接にて各種材質に対して
溶接可能となり採用してみた。The technique for welding a metal thin film is limited, and it has been difficult to realize due to welding distortion. We also tried using metal thin film welding because it can be welded to various materials by seam welding.
【004】[004]
【課題を解決するための手段】単純に溶接固定した場合
溶接熱による縮み特性溶接物相互のヒートバランスの相
違による歪みなどが発生する。これを解決する方法とし
て溶接前に金属薄膜に張力を加えた状態にしてシーム溶
接する。また溶接部付近に溶接歪み逃げを設ける。[Means for Solving the Problems] When simply fixed by welding, shrinkage characteristics due to welding heat Distortion occurs due to the difference in heat balance between welded products. As a method of solving this, seam welding is performed with tension applied to the metal thin film before welding. Weld strain relief is provided near the weld.
【005】[0095]
【発明の実施の形態】張力の加え方は、溶接物形状によ
り異なってくる。図−1のごとく金属薄膜とキャンバを
付けた状態の枠フレームをシーム溶接固定する。この場
合溶接治具より取り外された時点で枠フレームの復帰力
にて金属薄膜に張力が与えられ歪み取りされた状態にな
る。図−2のごとく本体部品にキャンバを加えられない
場合の方法として張った状態にした金属薄膜に溶接する
本体部品を押しつけあるいは、逆に金属薄膜の方を押し
つけこの押しつけ圧力を調整してシーム溶接する。そし
て溶接時の歪みを逃がす処理方法として図−3に示すよ
うに溶接部近くに多孔穴加工スリット加工切り込みの加
工処理を加える。BEST MODE FOR CARRYING OUT THE INVENTION How to apply tension depends on the shape of the welded material. As shown in Fig. 1, the frame and frame with the metal thin film and camber attached are fixed by seam welding. In this case, when the metal thin film is removed from the welding jig, tension is applied to the metal thin film by the restoring force of the frame and the metal thin film is distorted. As shown in Fig. 2, when the camber cannot be added to the body part, the body part to be welded is pressed against the thin metal film in the stretched state, or conversely, the metal thin film side is pressed to adjust the pressing pressure and seam welding. To do. Then, as a processing method for releasing the distortion during welding, as shown in Fig. 3, processing processing such as perforation slit processing and cutting is added near the welded portion.
【006】[0096]
【発明の効果】金属薄膜の溶接方法そのものが新しいた
め金属薄膜と枠フレーム本体部品の用途活用が少ない。
しかし溶接法が簡単なため用途拡大が見込める。更に用
途拡大してくると金属薄膜と枠フレーム本体部品の形状
によりヒートバランス調整が必要になり更に多くの加工
方法が必要になることありそうである。EFFECTS OF THE INVENTION Since the welding method of the metal thin film itself is new, the metal thin film and the frame frame body parts are less utilized.
However, since the welding method is simple, it can be expected to expand its applications. As the applications are further expanded, it is likely that heat balance adjustment will be required depending on the shapes of the metal thin film and the frame and frame body parts, and more processing methods will be required.
【図1】枠フレームにキャンバを付けてシーム溶接する
場合。FIG. 1 shows a case where a camber is attached to a frame and seam welding is performed.
【図2】金属薄膜側に張力を加えてシーム溶接する場
合。[Fig. 2] When seam welding is performed by applying tension to the metal thin film side.
【図3】枠フレームを金属薄膜側に張力を加えて歪み逃
げ加工を処理した場合。FIG. 3 shows a case where strain relief processing is performed by applying tension to the metal thin film side of the frame.
【図4】金属薄膜を溶接するシーム溶接機例[Fig. 4] Example of seam welding machine for welding metal thin films
1 金属薄膜 2 枠フレーム 3 本体部品 4 キャンバ 5 スリット加工 1 metal thin film 2 frame 3 body parts 4 camber 5 slit processing
Claims (2)
リーンメッシュ薄膜壁などを固定する場合に金属薄膜溶
接部付近に切り込み多孔穴加工スリット加工などの歪み
逃げ機能を設けてシーム溶接固定する。1. When fixing a screen mesh thin film wall of a metal thin film to a frame frame body part or the like, a seam welding fixing is performed by providing a strain relief function such as a slit perforation and a slit processing near the metal thin film welding portion.
ーム溶接しキャンバの復元力にて歪み取りする。あるい
は、枠フレーム本体部品を金属箔に押しつけて金属薄膜
に張力を与えシーム溶接する。2. A frame is provided with a camber on a frame body part and seam-welded to remove distortion by the restoring force of the camber. Alternatively, the frame body member is pressed against the metal foil to apply tension to the metal thin film and perform seam welding.