JP2001316647A - Adhesive tape, and application process and device using the same - Google Patents

Adhesive tape, and application process and device using the same

Info

Publication number
JP2001316647A
JP2001316647A JP2000138370A JP2000138370A JP2001316647A JP 2001316647 A JP2001316647 A JP 2001316647A JP 2000138370 A JP2000138370 A JP 2000138370A JP 2000138370 A JP2000138370 A JP 2000138370A JP 2001316647 A JP2001316647 A JP 2001316647A
Authority
JP
Japan
Prior art keywords
adhesive tape
coating
web
adhesive
angle
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2000138370A
Other languages
Japanese (ja)
Other versions
JP4264789B2 (en
Inventor
Nobuo Hamamoto
伸夫 浜本
Kaoru Ishikawa
薫 石川
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Fujifilm Holdings Corp
Original Assignee
Fuji Photo Film Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Fuji Photo Film Co Ltd filed Critical Fuji Photo Film Co Ltd
Priority to JP2000138370A priority Critical patent/JP4264789B2/en
Publication of JP2001316647A publication Critical patent/JP2001316647A/en
Application granted granted Critical
Publication of JP4264789B2 publication Critical patent/JP4264789B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To prevent uneven application caused by a paste squeezed out from the end of adhesive tapes used at joints. SOLUTION: An adhesive tape 26 is used for joining a joint 28 of a web 14 onto which a coating liquid is applied. In order to reduce the squeeze-out of paste from the end of the adhesive tape 26 when running the web 14 on a carrier, the side 46 of the adhesive tape 26 is cut to make the angle between the surface 44 of the adhesive tape 26 without a paste layer 38 and the side 46 of the adhesive tape 26 parallel to the width direction of the web 14 to be within the range of from 45 deg. to 75 deg.. This structure prevents the paste of the adhesive tape 26 from sticking to a carrier roller 30, etc., of a carrier and subsequently being transferred onto a downstream web 14. Consequently, the coating liquid can be uniformly applied onto the web 14 having an adhesive tape 26 at the joint 28.

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【発明の属する技術分野】本発明は接着テープ及び塗布
方法並びに装置に係り、特に、接着テープで接合された
接合部を有する帯状可撓性支持体(以下「ウエブ」とい
う)を搬送路に搬送させながら塗布ヘッドで塗布液を塗
布する塗布方法及び装置に関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to an adhesive tape, a coating method and an apparatus, and more particularly, to a belt-like flexible support (hereinafter, referred to as a "web") having a joint portion joined by an adhesive tape to a transport path. The present invention relates to a coating method and an apparatus for coating a coating liquid with a coating head while performing the coating.

【0002】[0002]

【従来の技術】搬送ローラ等の搬送手段を経由して搬送
するウエブに塗布ヘッドで塗布液を塗布する場合、塗布
を行う現ウエブの後端と次に塗布を行う新ウエブの前端
を接着テープで接合して連続塗布を行うことにより、現
ウエブから新ウエブに切り換わるときに塗布運転を停止
しないようにしている。
2. Description of the Related Art When a coating liquid is applied to a web conveyed through conveyance means such as conveyance rollers by a coating head, an adhesive tape is applied to the rear end of the current web to be coated and the front end of a new web to be coated next. To perform continuous coating, so that the coating operation is not stopped when the current web is switched to a new web.

【0003】しかし、ウエブ同士が接着テープで接合さ
れた接合部では、塗布ムラや塗布スジ等の塗布故障が発
生し易いという問題がある。
[0003] However, there is a problem that a coating failure such as coating unevenness or a coating streak easily occurs at a bonded portion where the webs are bonded with an adhesive tape.

【0004】この為、接合部を有するウエブに塗布液を
塗布する塗布方法では、接合部で発生する塗布故障によ
る損失を軽減するために、以下のような種々の対策がと
られている。
For this reason, in a coating method for applying a coating solution to a web having a joint, various measures as described below are taken in order to reduce a loss due to a coating failure occurring at the joint.

【0005】例えば、特開昭54−62241号公報で
は、接合部の被塗布面に予め疎水性液体を付与すること
が開示されている。また、特開昭58−88074号公
報には、接合部が塗布される直前に、塗布ヘッドを塗布
位置から移動させてウエブから離し、接合部が通過後に
塗布ヘッドを再び元の塗布位置に戻す方法が開示されて
いる。更に、特許2632265号公報では、接合部に
黒色層を設け表面電位を0.5〜2.0kVに荷電させ
る方法が開示されている。
For example, Japanese Patent Application Laid-Open No. 54-62241 discloses that a hydrophobic liquid is applied in advance to a surface to be coated of a joint. Japanese Patent Application Laid-Open No. 58-88074 discloses that immediately before a joint is applied, the application head is moved from the application position to be separated from the web, and after the joint passes, the application head is returned to the original application position again. A method is disclosed. Further, Japanese Patent No. 2632265 discloses a method in which a black layer is provided at a joint portion and the surface potential is charged to 0.5 to 2.0 kV.

【0006】[0006]

【発明が解決しようとする課題】しかしながら、上記し
た従来の塗布方法では、接合部による空気同伴が原因の
塗布ムラや塗布スジ等の塗布故障を軽減することはでき
ても、接合部を接合する接着テープの端部からはみだし
た糊に起因する塗布ムラを解消することはできないとい
う問題がある。即ち、接着テープの端部からはみだした
糊が搬送路の搬送ローラ等に付着し、その付着した糊が
下流側のウエブに転写されると、転写されたウエブ部分
に塗布された塗布膜に塗布ムラが発生する。
However, in the above-mentioned conventional coating method, even if coating defects such as coating unevenness and coating streaks caused by air entrainment by the bonding portion can be reduced, the bonding portion is bonded. There is a problem that it is not possible to eliminate uneven coating caused by glue sticking out from the end of the adhesive tape. In other words, when the glue sticking out from the end of the adhesive tape adheres to the transport roller in the transport path and the glue is transferred to the downstream web, it is applied to the coating film applied to the transferred web portion. Unevenness occurs.

【0007】本発明は、このような事情に鑑みてなされ
たもので、接合部を接合する接着テープの端部からの糊
はみ出しによる塗布ムラを解消し、接合部を有する帯状
可撓性支持体の塗布品質を向上させることのできる接着
テープ及び塗布方法並びに装置を提供することを目的と
する。
The present invention has been made in view of the above circumstances, and eliminates uneven coating due to adhesive sticking out from an end of an adhesive tape for joining a joint, and a strip-shaped flexible support having a joint. It is an object of the present invention to provide an adhesive tape, a coating method, and an apparatus capable of improving the coating quality of the adhesive tape.

【0008】[0008]

【課題を解決するための手段】本発明は、前記目的を達
成するために、裏面に糊層を有する接着テープにおい
て、前記接着テープの表面と前記接着テープの側面との
なす角度が45°〜75°の範囲になるように前記側面
が裁断されていることを特徴とする。
In order to achieve the above object, the present invention provides an adhesive tape having an adhesive layer on a back surface, wherein the angle between the surface of the adhesive tape and the side surface of the adhesive tape is 45 ° or more. The side surface is cut so as to have a range of 75 °.

【0009】また、本発明は、前記目的を達成するため
に、接着テープで接合された接合部を有する帯状可撓性
支持体を搬送させながら塗布液で塗布する塗布方法であ
って、前記帯状可撓性支持体の接合部が搬送ローラ等の
搬送手段に接触経由して搬送される塗布方法において、
前記接着テープとして、糊層が形成されていない前記接
着テープの表面と前記帯状可撓性支持体の幅方向に平行
な前記接着テープの側面とのなす角度が45°〜75°
の範囲になるように前記側面が裁断されたものを用いる
ことを特徴とする。
In order to achieve the above object, the present invention provides a coating method in which a belt-like flexible support having a joining portion joined by an adhesive tape is applied with a coating solution while being conveyed. In a coating method in which the joint portion of the flexible support is transported via contact with transport means such as a transport roller,
As the adhesive tape, the angle between the surface of the adhesive tape on which no adhesive layer is formed and the side surface of the adhesive tape parallel to the width direction of the strip-shaped flexible support is 45 ° to 75 °.
Characterized in that the side surface is cut so as to fall within the range.

【0010】また、本発明は、前記目的を達成するため
に、接着テープで接合された接合部を有する帯状可撓性
支持体を搬送させながら塗布液で塗布する塗布装置であ
って、前記帯状可撓性支持体の接合部が搬送ローラ等の
搬送手段に接触経由して搬送される塗布装置において、
前記接合部を接合する接着テープの側面を裁断する裁断
手段を設けると共に、該裁断手段は、糊層が形成されて
いない前記接着テープの表面と前記帯状可撓性支持体の
幅方向に平行な前記接着テープの側面とのなす角度が4
5°〜75°の範囲になるように前記側面を裁断するも
のであることを特徴とする。
[0010] In order to achieve the above object, the present invention provides a coating apparatus for coating with a coating liquid while transporting a belt-shaped flexible support having a joint joined with an adhesive tape, In a coating device in which the joint portion of the flexible support is transported via contact with transport means such as a transport roller,
Cutting means for cutting the side surface of the adhesive tape that joins the joining portion is provided, and the cutting means is parallel to the surface of the adhesive tape on which the adhesive layer is not formed and the width direction of the strip-shaped flexible support. The angle between the side of the adhesive tape and the side is 4
The side surface is cut so as to be in a range of 5 ° to 75 °.

【0011】本発明によれば、塗布液が塗布される帯状
可撓性支持体の接合部を接合する接着テープとして、糊
層が形成されていない接着テープの表面と帯状可撓性支
持体の幅方向に平行な接着テープの側面とのなす角度が
45°〜75°の範囲になるように側面が裁断されてい
る接着テープを用いるようにしたので、帯状可撓性支持
体が搬送ローラ等の搬送手段を接触経由する際に、接着
テープの端部から糊がはみ出しにくくできる。これによ
り、接着テープの糊が搬送ローラ等に付着し、その付着
した糊が下流側のウエブに転写されるということを防止
できるので、接合部に接着テープを有する帯状可撓性支
持体に塗布液を塗布した際に塗布ムラや塗布スジが発生
しないようにできる。また、接合部の空気同伴に起因す
る塗布ムラの発生もない。
According to the present invention, the surface of the adhesive tape on which the adhesive layer is not formed and the surface of the band-shaped flexible support are used as the adhesive tape for joining the joints of the band-shaped flexible support to which the coating liquid is applied. Since the adhesive tape whose side surface is cut so that the angle between the side surface of the adhesive tape parallel to the width direction and the side surface of the adhesive tape is in the range of 45 ° to 75 ° is used, the belt-shaped flexible support is used as a transport roller or the like. The adhesive can be prevented from protruding from the end of the adhesive tape when passing through the contact means of the transfer means. As a result, it is possible to prevent the adhesive of the adhesive tape from adhering to the conveying roller and transferring the adhered adhesive to the downstream web, so that the adhesive is applied to the belt-shaped flexible support having the adhesive tape at the joint. It is possible to prevent application unevenness and application streaks from occurring when the liquid is applied. Also, there is no occurrence of coating unevenness due to entrainment of air at the joint.

【0012】[0012]

【発明の実施の形態】以下、添付図面により本発明の接
着テープ及びそれを用いた塗布方法並びに装置の好まし
い実施の形態について詳説する。
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Preferred embodiments of the adhesive tape of the present invention, a coating method and an apparatus using the same will be described in detail with reference to the accompanying drawings.

【0013】図1は、ウエブに塗布液を塗布する塗布装
置10の構成の一例を模式的に示す構成図であり、塗布
ヘッドとしてビード塗布用のスライドホッパー12の例
で説明する。
FIG. 1 is a schematic diagram showing an example of the configuration of a coating apparatus 10 for coating a coating liquid on a web. An example of a slide hopper 12 for bead coating as a coating head will be described.

【0014】図1に示すように、ウエブ14に塗布され
る複数(例えば3種類)の塗布液16A、16B、16
Cは、図示しないそれぞれの塗布液タンクから送液量が
可変可能な各送液ポンプによりスライドホッパー12内
の各マニホールド18A、18B、18Cに供給され
る。マニホールド18A、18B、18Cに供給された
各塗布液16A、16B、16Cは所定の幅になるよう
に塗布幅方向に拡流された後、スリット状に形成された
各スロット20A、20B、20Cを通ってスライドホ
ッパー12上面の下方傾斜したスライド面22に押し出
される。スライド面22に押し出された各塗布液16
A、16B、16Cは、多層塗布膜状の多層塗布膜16
となってスライド面22を流下し、スライド面22下端
のリップ先端24に達する。一方、長方形状の接着テー
プ26で接合された接合部28を有するウエブ14は、
搬送路に設けられた搬送ローラ30を経由し、スライド
ホッパー12に対向配置されたバックアップローラ32
に係合支持されて搬送される。そして、リップ先端24
に達した多層塗布液は、リップ先端24と、バックアッ
プローラ32に係合支持されるウエブ14面との間隙に
ビード部34を形成し、このビード部34において、ウ
エブ14はバックアップローラ32の周面に沿って下方
から上方に搬送する。これにより、ビード部34におけ
る多層塗布液は、ウエブ14面の上に引き上げられる作
用を受けて引き伸ばされて薄層化する。この結果、搬送
するウエブ14面上に薄層化した多層塗布膜16を形成
することができる。このとき、ビード部34を安定化さ
せるため、吸引チャンバ36によりビード部34の下側
が減圧される。
As shown in FIG. 1, a plurality (for example, three types) of coating solutions 16A, 16B, 16
C is supplied to each of the manifolds 18A, 18B, and 18C in the slide hopper 12 from each of the coating liquid tanks (not shown) by each of the liquid supply pumps whose liquid supply amount is variable. Each of the coating liquids 16A, 16B, and 16C supplied to the manifolds 18A, 18B, and 18C is expanded in a coating width direction so as to have a predetermined width, and then each of the slit-shaped slots 20A, 20B, and 20C is formed. It is pushed out to the slide surface 22 inclined downward on the upper surface of the slide hopper 12. Each coating solution 16 extruded on the slide surface 22
A, 16B and 16C are multilayer coating films 16 in the form of a multilayer coating film.
As a result, it flows down the slide surface 22 and reaches the lip tip 24 at the lower end of the slide surface 22. On the other hand, the web 14 having the joining portion 28 joined by the rectangular adhesive tape 26 is
A backup roller 32 disposed opposite to the slide hopper 12 via a transport roller 30 provided in the transport path.
And is conveyed while being engaged. And the lip tip 24
Reaches the gap between the lip tip 24 and the surface of the web 14 supported and engaged by the backup roller 32, in which a web 14 is formed around the backup roller 32. It is conveyed upward from below along the surface. Thus, the multilayer coating solution in the bead portion 34 is stretched by the action of being pulled up on the surface of the web 14 to be thinned. As a result, a thin multilayer coating film 16 can be formed on the surface of the web 14 to be conveyed. At this time, in order to stabilize the bead portion 34, the pressure on the lower side of the bead portion 34 is reduced by the suction chamber 36.

【0015】上述したウエブ14への塗布液の塗布にお
いて、図1に示したように、ウエブ14の接合部28が
搬送ローラ30にラップした状態で経由するときに、接
着テープ26の糊層38(図3、図4参照)が搬送ロー
ラ30とウエブ14とで挟圧され、接着テープ26の端
部からはみだした糊38Aが搬送ローラ30に付着し、
その付着した糊38Aが下流側のウエブ14に転写され
ると、図2に示すように糊が転写されたウエブに塗布さ
れた多層塗布膜16に斑点状の塗布ムラが発生してしま
う。この場合、接合部28を接合する接着テープ26の
ウエブ幅方向の側面からはみだす糊38Aは、ウエブ1
4の耳部(ウエブの両端部)に転写されるので影響は小
さいが、接着テープ26のウエブ幅方向と平行な側面か
らはみだす糊はウエブ14の中央部に転写されるので塗
布品質に与える影響が大きい。
In the application of the coating solution to the web 14, as shown in FIG. 1, when the joining portion 28 of the web 14 passes while being wrapped around the transport roller 30, the adhesive layer 38 of the adhesive tape 26 is used. (See FIG. 3 and FIG. 4). The adhesive 38 </ b> A protruding from the end of the adhesive tape 26 adheres to the transport roller 30 while being pressed between the transport roller 30 and the web 14.
When the adhered adhesive 38A is transferred to the downstream web 14, spot-like coating unevenness occurs on the multilayer coating film 16 applied to the web to which the adhesive has been transferred as shown in FIG. In this case, the glue 38A protruding from the side surface in the web width direction of the adhesive tape 26 for joining the joining portion 28 is applied to the web 1
4 is transferred to the ears (both ends of the web), so the influence is small. However, the glue sticking out from the side surface of the adhesive tape 26 parallel to the web width direction is transferred to the center of the web 14, so the influence on the coating quality is affected. Is big.

【0016】ところで、従来の接着テープ26は、図3
に縦断面図を示すように、テープ基材40の裏面に糊層
38(接着剤層)を有し、糊層38に離けい紙42を仮
着して構成され、糊層38が形成されていない接着テー
プ26の表面44と接着テープ26の側面46とのなす
角度αが直角(90°)に形成されている。尚、図3、
図4では、角度αとして、接着テープ26の表面と側面
46との延長線のなす角度で示してある。そして、ウエ
ブ14の端部同士を接合する場合には、接着テープ26
から離けい紙42を剥がして糊層38を露出し、ウエブ
14の端部同士を突き合わせた状態で、突き合わせ部分
に沿って接着テープ26を貼り付ける。以下、糊層38
が形成されていない接着テープ26の表面44と接着テ
ープ26の側面46とのなす角度αを「接着テープ26
の側面角度α」と称す。
The conventional adhesive tape 26 is shown in FIG.
As shown in the vertical cross-sectional view, a glue layer 38 (adhesive layer) is provided on the back surface of the tape base material 40, and a separating paper 42 is temporarily attached to the glue layer 38 to form the glue layer 38. The angle α between the surface 44 of the adhesive tape 26 and the side surface 46 of the adhesive tape 26 is formed at a right angle (90 °). Note that FIG.
In FIG. 4, the angle α is an angle formed by an extension of the surface of the adhesive tape 26 and the side surface 46. Then, when joining the ends of the web 14 together, the adhesive tape 26
The adhesive paper 26 is adhered along the abutting portion in a state where the adhesive layer 38 is exposed by peeling the separation paper 42 from the webbing and exposing the end portions of the web 14 to each other. Hereinafter, the glue layer 38
Is defined as the angle α between the surface 44 of the adhesive tape 26 on which the adhesive tape 26 is not formed and the side surface 46 of the adhesive tape 26.
Side angle α ”.

【0017】そして、本発明者は、接着テープ26から
の糊のはみだしによる塗布ムラ防止について鋭意研究し
た結果、接着テープ26の側面角度αが、糊のはみだし
に大きく影響するという知見を得た。
The inventor of the present invention has conducted intensive studies on the prevention of coating unevenness due to the protrusion of the adhesive from the adhesive tape 26, and as a result, has found that the side angle α of the adhesive tape 26 greatly affects the protrusion of the adhesive.

【0018】本発明の接着テープ26は、上記知見に基
づいて成されたもので、裏面に糊層38を有する接着テ
ープ26において、接着テープ26の側面角度αが45
°〜75°の範囲になるように側面46が裁断されて構
成される。
The adhesive tape 26 of the present invention is based on the above findings. In the adhesive tape 26 having the adhesive layer 38 on the back surface, the side angle α of the adhesive tape 26 is 45.
The side surface 46 is cut so as to be in the range of ° to 75 °.

【0019】本発明の接着テープ26を構成するテープ
基材40としては、アルミ蒸着、黒色層含有、半透明加
工、着色加工等を施された、PETテープ、セロハンテ
ープ、ビニールテープ、布テープ等を使用することがで
きる。
As the tape base material 40 constituting the adhesive tape 26 of the present invention, a PET tape, a cellophane tape, a vinyl tape, a cloth tape, etc., which have been subjected to aluminum deposition, black layer containing, translucent processing, coloring processing, etc. Can be used.

【0020】また、本発明の塗布装置は、本発明の接着
テープをインプラントで用いることができるようにした
もので、図1で説明した塗布装置10に、接着テープ2
6の裁断装置48を組み込むことにより構成される。
The coating device of the present invention is such that the adhesive tape of the present invention can be used for an implant. The coating device 10 described with reference to FIG.
6 by incorporating the cutting device 48.

【0021】図5は、裁断装置48を模式的に示した全
体構成図である。
FIG. 5 is an overall configuration diagram schematically showing the cutting device 48. As shown in FIG.

【0022】供給リール50には、裁断前の接着テープ
26がロール状に巻回され、巻回された接着テープ26
は、カッター台52を経由して巻取リール53に巻き取
られる。尚、55はパスローラである。
On the supply reel 50, the adhesive tape 26 before cutting is wound in a roll shape, and the wound adhesive tape 26 is wound.
Is wound on a take-up reel 53 via a cutter table 52. Incidentally, 55 is a pass roller.

【0023】カッター台52は、図6に示すように、縦
断面が台形な基台54の一対の傾斜側面56、56にそ
れぞれ裁断刃58、58が傾斜に対応して設けられ、ボ
ルト60、60で基台54に固定される。また、この一
対の裁断刃58、58は、図7に示すように、裁断され
る接着テープ26の進行方向61に向かってハの字状に
なるように配置されると共に、接着テープ26の離けい
紙42側が上を向くようにして裁断される。これによ
り、巻取リール53が接着テープ26を巻き取ると、供
給リール50から繰り出された接着テープ26の幅方向
両端部は、カッター台52により図8に示すように裁断
される。この結果、図4で示したように、裁断された帯
状の接着テープ26の幅方向両端は、側面角度αが45
°〜75°の範囲になるように裁断される。側面角度α
を45°〜75°の範囲内で調整するには、傾斜面56
の異なる基台54を複数用意するか、あるいは1台の基
台54の傾斜面56の角度を調整できるような構造にす
るとよい。
As shown in FIG. 6, the cutter base 52 has cutting blades 58, 58 provided on a pair of inclined side surfaces 56, 56 of a base 54 having a trapezoidal longitudinal section corresponding to the inclination, respectively. At 60, it is fixed to the base 54. As shown in FIG. 7, the pair of cutting blades 58, 58 are arranged so as to form a C shape in the traveling direction 61 of the adhesive tape 26 to be cut, and the adhesive tape 26 is separated. The paper 42 is cut so that the side of the paper 42 faces upward. Thus, when the take-up reel 53 takes up the adhesive tape 26, both ends in the width direction of the adhesive tape 26 fed from the supply reel 50 are cut by the cutter table 52 as shown in FIG. As a result, as shown in FIG. 4, both ends of the cut strip-shaped adhesive tape 26 in the width direction have a side surface angle α of 45 degrees.
It is cut so as to be in the range of ° to 75 °. Side angle α
Is adjusted within the range of 45 ° to 75 °, the slope 56
A plurality of bases 54 different from each other may be prepared, or a structure may be employed in which the angle of the inclined surface 56 of one base 54 can be adjusted.

【0024】裁断刃58の種類としては、片刃カミソ
リ、両刃カミソリ、カッター刃等を使用することがで
き、また単に先鋭な部分を有する金属、無機物、プラス
チック等でもよい。また、裁断刃58としては、固定刃
が好ましいが、回転刃をも使用することもできる。裁断
する前の接着テープ26の幅は、10mm〜100mm
が一般的である。裁断する接着テープ端部の幅は、0.
5mm〜5mm、好ましくは1mm〜2mmがよい。ま
た、裁断した接着テープ26の表面に塗布液が乗りやす
いように、放電処理や疎水処理を施しても良いし、30
°C以上に加熱してもよい。
As the type of the cutting blade 58, a single-edged razor, a double-edged razor, a cutter blade, or the like can be used. Alternatively, a metal, inorganic substance, plastic, or the like having a sharp portion may be used. Further, as the cutting blade 58, a fixed blade is preferable, but a rotary blade can also be used. The width of the adhesive tape 26 before cutting is 10 mm to 100 mm
Is common. The width of the edge of the adhesive tape to be cut is 0.
5 mm to 5 mm, preferably 1 mm to 2 mm. In addition, a discharge treatment or a hydrophobic treatment may be performed so that the coating liquid can easily be put on the surface of the cut adhesive tape 26.
You may heat above ° C.

【0025】尚、本発明の塗布装置に使用する塗布ヘッ
ド12としては、ビード塗布用のスライドホッパーに限
定されるものではなく、カーテン塗布、エクトルージョ
ン塗布、ロール塗布、エアナイフコーター、ブレードコ
ーター、バーコータ等を使用することができる。
The coating head 12 used in the coating apparatus according to the present invention is not limited to a slide hopper for bead coating, but may be curtain coating, ejection coating, roll coating, air knife coater, blade coater, bar coater. Etc. can be used.

【0026】次に、本発明の塗布装置を用いて接合部2
8に接着テープ26を有するウエブ14に塗布液を塗布
する塗布方法を説明する。
Next, using the coating apparatus of the present invention, the joint 2
A method of applying a coating liquid to the web 14 having the adhesive tape 26 at 8 will be described.

【0027】カッター台52により、側面角度αが45
°〜75°になるように裁断前の接着テープ26を裁断
する。そして、この裁断した接着テープ26を用い、塗
布を行うウエブ14の後端と次に塗布を行うウエブ14
の前端を突き合わせて接合する。この場合、塗布される
ウエブ14の端部同士を接合するために用いられる接着
テープ26としては、上述したように、ウエブ幅方向と
平行な接着テープ26の側面46からはみだす糊38A
はウエブ14の中央部に転写されるので塗布品質に与え
る影響が大きいことから、ウエブ14の幅方向に平行な
側面角度αが45°〜75°の範囲になるように側面4
6を裁断した接着テープ26を用いることが好ましい。
対向する2つの側面46の側面角度αは、両方の側面4
6とも同じ側面角度αであってもよく、異なる側面角度
αでもさしつかえない。また、一方の側面46のみの側
面角度αを45°〜75°の範囲になるようにすること
でも効果が得られる。
The side angle α is 45 by the cutter table 52.
The adhesive tape 26 before cutting is cut so that the angle becomes 75 ° to 75 °. Then, using the cut adhesive tape 26, the rear end of the web 14 to be coated and the web 14
Butt the front ends of In this case, as described above, as the adhesive tape 26 used to join the ends of the web 14 to be applied, the glue 38A protruding from the side surface 46 of the adhesive tape 26 parallel to the web width direction is used.
Is transferred to the central portion of the web 14 and therefore greatly affects the coating quality. Therefore, the side surface 4 is set so that the side angle α parallel to the width direction of the web 14 is in the range of 45 ° to 75 °.
It is preferable to use an adhesive tape 26 obtained by cutting 6.
The side angle α of the two opposing side surfaces 46 is
6 may have the same side angle α, or different side angles α. Also, the effect can be obtained by setting the side surface angle α of only one side surface 46 in the range of 45 ° to 75 °.

【0028】接着テープ26でのウエブ同士の接合は、
塗布を行う前に予め接合しておいてもよく、ウエブ14
の搬送路上に公知の自動接合装置(図示せず)を設け
て、ウエブ14を搬送路に搬送させたまま自動接合して
もよい。
The joining of the webs with the adhesive tape 26 is as follows.
They may be joined in advance before the coating is performed.
A known automatic bonding apparatus (not shown) may be provided on the transfer path of the above, and the web 14 may be automatically bonded while being transferred to the transfer path.

【0029】接着テープ26で接合された接合部28を
有するウエブ14は、図1に示したように、ウエブ14
の接合部28が搬送ローラ30にラップした状態で経由
するときに、接着テープ26の糊層38が搬送ローラ3
0とウエブ14とで挟圧される。
As shown in FIG. 1, the web 14 having the joint 28 joined by the adhesive tape 26 is
When the adhesive layer 38 of the adhesive tape 26 passes through the joint portion 28 of the
0 and the web 14.

【0030】しかし、本発明では、接着テープ26の側
面角度αが45°〜75°の範囲を満足するように裁断
されているので、接着テープ26の端部からの糊のはみ
だしを防止することができる。これにより、従来のよう
に、はみだした糊38Aが、搬送ローラ30に付着し、
その付着した糊が下流側のウエブ14に転写されて塗布
ムラを発生させることがないので、塗布品質を向上させ
ることができる。
However, according to the present invention, the adhesive tape 26 is cut so that the side angle α satisfies the range of 45 ° to 75 °. Therefore, it is necessary to prevent the adhesive from running out from the end of the adhesive tape 26. Can be. As a result, the pasted adhesive 38A adheres to the transport roller 30 as in the related art,
Since the adhered glue is not transferred to the downstream web 14 to cause uneven coating, the coating quality can be improved.

【0031】接着テープ26の側面角度αが45°〜7
5°の範囲を満足することにより、糊のはみだしが防止
される理由としては、図9に示すように、接着テープ2
6の側面46が適度に傾斜していることにより、ウエブ
14が糊層38のみでなく接着テープ26の側面46に
も密着し易くなる。この結果、接着テープ26の側面4
6とウエブ14との間に隙間62が形成されなくなるた
めに、接着テープ26の端部からの糊のはみだしが防止
されるものと考察される。特に、ウエブ14が搬送ロー
ラ30にラップすると、ウエブ14が接着テープ26の
側面46に一層密着し易くなるので、糊層38がウエブ
14と搬送ローラ30とで挟圧されても、その挟圧力が
逆に接着テープ26の側面46とウエブ14との間の隙
間62をなくす方向に作用するためと考察される。
The side angle α of the adhesive tape 26 is 45 ° to 7
The reason why the glue is prevented from running out by satisfying the range of 5 ° is as shown in FIG.
Since the side surface 46 of the sixth taper 6 is appropriately inclined, the web 14 can easily adhere to not only the adhesive layer 38 but also the side surface 46 of the adhesive tape 26. As a result, the side surface 4 of the adhesive tape 26
Since the gap 62 is not formed between the web 6 and the web 14, it is considered that the adhesive is prevented from running out from the end of the adhesive tape 26. In particular, when the web 14 wraps around the transport roller 30, the web 14 more easily adheres to the side surface 46 of the adhesive tape 26. Therefore, even if the adhesive layer 38 is Is considered to act in a direction to eliminate the gap 62 between the side surface 46 of the adhesive tape 26 and the web 14.

【0032】これに対し、従来の接着テープ26のよう
に、側面角度αが90°の場合には、図10に示すよう
に、ウエブ14が接着テープ26の側面46に密着し難
いために、接着テープ26の側面46とウエブ14との
間に隙間62が形成され、特に搬送ローラ30を経由す
る際に接着テープ26の端部からはみだした糊38Aが
搬送ローラ30に付着するものと考察される。
On the other hand, when the side surface angle α is 90 ° as in the conventional adhesive tape 26, as shown in FIG. 10, since the web 14 is hard to adhere to the side surface 46 of the adhesive tape 26, It is considered that a gap 62 is formed between the side surface 46 of the adhesive tape 26 and the web 14, and that the adhesive 38 </ b> A protruding from the end of the adhesive tape 26 particularly adheres to the transport roller 30 when passing through the transport roller 30. You.

【0033】また、接着テープ30の側面角度αが45
°未満の場合には、ウエブ14が接着テープ26の側面
46に密着し易いという点では同様であるが、側面角度
αが小さすぎると、カッター台52で裁断する際に、接
着テープ26が裁断刃58に引っ掛かって裁断が不能に
なると共に、裁断されたとしても裁断面、即ち側面46
が凸凹になり糊がはみだし易くなる。
The side angle α of the adhesive tape 30 is 45
When the side angle α is too small, the adhesive tape 26 is cut off when the side surface angle α is too small. The blade 58 is caught by the blade 58 and cannot be cut.
Becomes uneven, and the glue is easily protruded.

【0034】このように、本発明の塗布方法及び塗布装
置によれば、塗布液が塗布されるウエブ14の接合部2
8を接合する接着テープ26として、ウエブ14の幅方
向に平行な接着テープ26の側面角度が45°〜75°
の範囲になるように側面46が裁断されたものを用いる
ようにしたので、ウエブ14が搬送ローラ30を経由す
る際にも接着テープ26の端部から糊がはみ出しにくく
することができる。これにより、接着テープ26の糊が
搬送ローラ30等に付着し、その付着した糊が下流側の
ウエブ14に転写されるということを防止できるので、
接合部28に接着テープ26を有するウエブ14に塗布
液を塗布した際に塗布ムラや塗布スジが発生しないよう
にでき、塗布品質を向上させることができる。
As described above, according to the coating method and the coating apparatus of the present invention, the bonding portion 2 of the web 14 to which the coating liquid is coated
8, the side angle of the adhesive tape 26 parallel to the width direction of the web 14 is 45 ° to 75 °.
Is used, so that the adhesive can be prevented from protruding from the end of the adhesive tape 26 even when the web 14 passes through the transport roller 30. As a result, it is possible to prevent the adhesive of the adhesive tape 26 from adhering to the transport roller 30 and the like, and preventing the adhered adhesive from being transferred to the downstream web 14.
When the application liquid is applied to the web 14 having the adhesive tape 26 on the joint portion 28, application unevenness and application streaks can be prevented from occurring, and application quality can be improved.

【0035】また、接着テープ26の側面角度を45°
〜75°の範囲になるようにすることで接合部28の空
気同伴に起因した塗布ムラの発生もない。
The side angle of the adhesive tape 26 is 45 °.
By setting the angle in the range of up to 75 °, there is no occurrence of coating unevenness due to entrainment of air in the joint portion 28.

【0036】[0036]

【実施例】次に、本発明の実施例を説明する。 (実施例1)図5の裁断装置を用いて、幅50mmのア
ルミ蒸着PETテープの両端部2mmを100mに渡っ
て裁断し、側面角度αが75°の接着テープを作成し
た。この接着テープでウエブ同士の接合部を接合し、接
合部に接着テープを有するウエブを、図1に示した搬送
路を200m/分で搬送させ、スライドホッパーとバッ
クアップローラとによるビード塗布を行った。多層塗布
膜は3層であり、塗布液の総塗布量を80cc/m2
最下層の塗布液量を12cc/m2 、最下層のゼラチン
濃度を5重量%、最下層の10(l/s)における粘度
を27mPas、ウエブの表面温度を32°Cとした。
また、ウエブは、ゼラチン下引き層を表面に有するTA
Cフィルムを使用した。 (実施例2)図5の裁断装置で接着テープの側面角度α
を60°に裁断した以外は、実施例1と同様とした。 (実施例3)図5の裁断装置で接着テープの側面角度α
を45°に裁断した以外は、実施例1と同様とした。 (比較例1)側面角度αが90°の従来の接着テープを
そのまま使用した以外は、実施例1と同様とした。 (比較例2)図5の裁断装置で接着テープの側面角度α
を30°に設定して裁断した。 (比較例3)図5の裁断装置で接着テープの側面角度α
を90°に裁断した以外は、実施例1と同様とした。 (比較例4)図5の裁断装置で接着テープの側面角度α
を135°に裁断した以外は、実施例1と同様とした。
Next, embodiments of the present invention will be described. Example 1 Using a cutting apparatus shown in FIG. 5, an aluminum-deposited PET tape having a width of 50 mm was cut at both ends 2 mm over 100 m to prepare an adhesive tape having a side surface angle α of 75 °. The joining portions of the webs were joined with the adhesive tape, the web having the adhesive tape at the joining portions was transported at a speed of 200 m / min through the transport path shown in FIG. 1, and the beads were applied by a slide hopper and a backup roller. . The multilayer coating film has three layers, and the total coating amount of the coating solution is 80 cc / m 2 ,
The coating amount of the lowermost layer was 12 cc / m 2 , the gelatin concentration of the lowermost layer was 5% by weight, the viscosity of the lowermost layer at 10 (l / s) was 27 mPas, and the surface temperature of the web was 32 ° C.
The web is made of TA having a gelatin subbing layer on the surface.
C film was used. (Embodiment 2) Side angle α of the adhesive tape by the cutting device shown in FIG.
Was cut to 60 °, and the same as in Example 1. (Embodiment 3) Side angle α of the adhesive tape by the cutting device shown in FIG.
Was cut to 45 ° and the same as in Example 1. (Comparative Example 1) Example 1 was the same as Example 1 except that a conventional adhesive tape having a side surface angle α of 90 ° was used as it was. (Comparative Example 2) Side angle α of the adhesive tape with the cutting device of FIG.
Was set at 30 ° and cut. (Comparative Example 3) Side angle α of the adhesive tape with the cutting device of FIG.
Was cut to 90 °, and the same as in Example 1 was performed. (Comparative Example 4) Side angle α of the adhesive tape with the cutting device of FIG.
Was cut to 135 °, and the same as in Example 1 was performed.

【0037】そして、実施例1〜3及び比較例1〜3に
ついて、ウエブが搬送ローラを経由した後の接着テープ
端部からの糊のはみだしの有無を光学顕微鏡により観察
すると共に、塗布された塗布膜の塗布ムラを目視にて観
察した。塗布ムラについては、接着テープの端部からの
糊のはみだしに起因するものと、接合部の空気同伴に起
因する塗布ムラとを分けて観察した。結果を表1に示
す。
In Examples 1 to 3 and Comparative Examples 1 to 3, the presence or absence of glue extruding from the end of the adhesive tape after the web passed through the transport roller was observed with an optical microscope, and the applied coating was observed. The coating unevenness of the film was visually observed. Regarding the coating unevenness, the coating unevenness caused by the protrusion of the adhesive from the end of the adhesive tape and the coating unevenness caused by the air entrainment of the joining portion were separately observed. Table 1 shows the results.

【0038】[0038]

【表1】 表1の、実施例1〜3の結果から分かるように、接着テ
ープの側面角度αが45°〜75°の範囲に入っている
場合には、接着テープの端部からの糊のはみだしがなか
った。これにより、糊のはみだしに起因した塗布ムラが
ないだけでなく、空気同伴に起因した塗布ムラもなく、
安定した塗布を行うことができた。
[Table 1] As can be seen from the results of Examples 1 to 3 in Table 1, when the side angle α of the adhesive tape falls within the range of 45 ° to 75 °, no glue protrudes from the end of the adhesive tape. Was. As a result, not only there is no coating unevenness due to the protrusion of the glue, but also there is no coating unevenness due to air entrainment,
Stable coating could be performed.

【0039】これに対し、従来の接着テープをそのまま
使用した比較例1の場合には、空気同伴に起因した塗布
ムラはないものの、接着テープの端部からの糊のはみだ
しに起因する塗布ムラが発生した。側面角度αを30°
に設定した裁断装置で裁断を試みた比較例2の場合に
は、裁断を5m実施したところで接着テープが裁断刃に
引っ掛かって裁断が不能になってしまった。接着テープ
の側面角度αを90°に裁断した比較例3は、比較例1
と同様の結果であった。また、接着テープの側面角度α
を135°に裁断した比較例4は、糊のはみだしに起因
した塗布ムラと、空気同伴に起因した塗布ムラの両方が
発生した。
On the other hand, in the case of Comparative Example 1 in which the conventional adhesive tape was used as it was, although there was no coating unevenness due to entrainment of air, the coating unevenness due to sticking out of the adhesive from the end of the adhesive tape did not. Occurred. 30 ° side angle
In the case of Comparative Example 2 in which cutting was attempted using the cutting device set in the above, the adhesive tape was caught on the cutting blade when cutting was performed for 5 m, and the cutting became impossible. Comparative Example 3 in which the side angle α of the adhesive tape was cut to 90 ° was Comparative Example 1
It was the same result as. Also, the side angle α of the adhesive tape
Was cut to 135 °, both coating unevenness caused by sticking out of the adhesive and coating unevenness caused by air entrainment occurred.

【0040】[0040]

【発明の効果】以上説明したように、本発明によれば、
接合部を接合する接着テープの端部からの糊はみだしを
防止することができる。
As described above, according to the present invention,
The glue can be prevented from running out from the end of the adhesive tape joining the joining portions.

【0041】これにより、接着テープで接合した接合部
を有する帯状可撓性支持体に塗布液を塗布する場合に、
糊のはみだしに起因する塗布ムラを解消することがで
き、更には接合部の空気同伴に起因する塗布ムラも発生
しない。従って、接合部を有する帯状可撓性支持体の塗
布品質を向上させることができる。
Thus, when the coating liquid is applied to the belt-shaped flexible support having the joints joined by the adhesive tape,
The coating unevenness caused by the protrusion of the glue can be eliminated, and the coating unevenness caused by the air entrainment of the joint does not occur. Therefore, the coating quality of the belt-shaped flexible support having the joint can be improved.

【図面の簡単な説明】[Brief description of the drawings]

【図1】塗布装置の一例を模式的に説明する説明図FIG. 1 is an explanatory view schematically illustrating an example of a coating apparatus.

【図2】接着テープの糊のはみだしに起因する塗布ムラ
を説明する説明図
FIG. 2 is an explanatory diagram illustrating coating unevenness caused by sticking out of an adhesive tape.

【図3】従来の接着テープの断面図FIG. 3 is a cross-sectional view of a conventional adhesive tape.

【図4】本発明の接着テープの断面図FIG. 4 is a sectional view of the adhesive tape of the present invention.

【図5】本発明の塗布装置に設けられた裁断装置を模式
的に説明する説明図
FIG. 5 is an explanatory diagram schematically illustrating a cutting device provided in the coating device of the present invention.

【図6】裁断装置におけるカッター台の側面図FIG. 6 is a side view of a cutter table in the cutting device.

【図7】裁断装置におけるカッター台の上面図FIG. 7 is a top view of a cutter table in the cutting device.

【図8】裁断装置で接着テープを裁断している上面図FIG. 8 is a top view of cutting the adhesive tape by the cutting device.

【図9】本発明の接着テープを用いた塗布装置の作用を
説明する説明図
FIG. 9 is an explanatory view for explaining the operation of a coating apparatus using the adhesive tape of the present invention.

【図10】従来の接着テープを用いた塗布装置の作用を
説明する説明図
FIG. 10 is an explanatory view for explaining the operation of a coating apparatus using a conventional adhesive tape.

【符号の説明】[Explanation of symbols]

10…塗布装置、12…スライドホッパー、14…ウエ
ブ、16…多層塗布膜、22…スライド面、26…接着
テープ、28…接合部、30…搬送ローラ、32…バッ
クアップローラ、34…ビード部、38…接着テープの
糊層、40…接着テープのテープ基材、42…接着テー
プの離けい紙、44…接着テープの表面、46…接着テ
ープの側面、48…裁断装置、50…供給リール、52
…カッター台、53…巻取リール、54…カッター台の
基台、56…カッター台の傾斜面、58…カッター台の
裁断刃、62…ウエブと搬送ローラとの間の隙間
DESCRIPTION OF SYMBOLS 10 ... Coating apparatus, 12 ... Slide hopper, 14 ... Web, 16 ... Multilayer coating film, 22 ... Slide surface, 26 ... Adhesive tape, 28 ... Joint part, 30 ... Transport roller, 32 ... Backup roller, 34 ... Bead part 38: adhesive tape adhesive layer, 40: adhesive tape tape base material, 42: adhesive tape release paper, 44: adhesive tape surface, 46: adhesive tape side surface, 48: cutting device, 50: supply reel, 52
... Cutter stand, 53 ... Take-up reel, 54 ... Cutter stand base, 56 ... Cutter stand inclined surface, 58 ... Cutter stand cutting blade, 62 ... Gap between web and transport roller

フロントページの続き Fターム(参考) 4D075 AC72 AC97 CA47 DA04 DB31 4F041 AA12 AB01 BA07 BA19 BA56 BA59 CA06 CA13 CA22 CA28 4F042 AA22 BA08 BA25 DC00 4J004 CA06 CC03 CC08 Continued on front page F term (reference) 4D075 AC72 AC97 CA47 DA04 DB31 4F041 AA12 AB01 BA07 BA19 BA56 BA59 CA06 CA13 CA22 CA28 4F042 AA22 BA08 BA25 DC00 4J004 CA06 CC03 CC08

Claims (4)

【特許請求の範囲】[Claims] 【請求項1】裏面に糊層を有する接着テープにおいて、 前記接着テープの表面と前記接着テープの側面とのなす
角度が45°〜75°の範囲になるように前記側面が裁
断されていることを特徴とする接着テープ。
1. An adhesive tape having an adhesive layer on a back surface, wherein the side surface is cut so that an angle between a surface of the adhesive tape and a side surface of the adhesive tape is in a range of 45 ° to 75 °. Adhesive tape characterized by the following.
【請求項2】接着テープで接合された接合部を有する帯
状可撓性支持体を搬送させながら塗布液で塗布する塗布
方法であって、前記帯状可撓性支持体の接合部が搬送ロ
ーラ等の搬送手段に接触経由して搬送される塗布方法に
おいて、 前記接着テープとして、糊層が形成されていない前記接
着テープの表面と前記帯状可撓性支持体の幅方向に平行
な前記接着テープの側面とのなす角度が45°〜75°
の範囲になるように前記側面が裁断されたものを用いる
ことを特徴とする塗布方法。
2. A coating method of applying a coating liquid while transporting a belt-shaped flexible support having a bonding portion bonded by an adhesive tape, wherein the bonding portion of the belt-shaped flexible support is a transport roller or the like. The coating method in which the adhesive tape is parallel to a surface of the adhesive tape on which an adhesive layer is not formed and a width direction of the band-shaped flexible support as the adhesive tape. 45 ° to 75 ° angle with the side
Wherein the side surface is cut so as to fall within the range of.
【請求項3】前記接合部は、前記帯状可撓性支持体の端
部同士を突き合わせた状態で前記接着テープで接合され
ていることを特徴とする請求項2の塗布方法。
3. The coating method according to claim 2, wherein said bonding portion is bonded with said adhesive tape in a state where ends of said flexible belt-shaped support are abutted with each other.
【請求項4】接着テープで接合された接合部を有する帯
状可撓性支持体を搬送させながら塗布液で塗布する塗布
装置であって、前記帯状可撓性支持体の接合部が搬送ロ
ーラ等の搬送手段に接触経由して搬送される塗布装置に
おいて、 前記接合部を接合する接着テープの側面を裁断する裁断
手段を設けると共に、該裁断手段は、糊層が形成されて
いない前記接着テープの表面と前記帯状可撓性支持体の
幅方向に平行な前記接着テープの側面とのなす角度が4
5°〜75°の範囲になるように前記側面を裁断するも
のであることを特徴とする塗布装置。
4. A coating device for applying a coating liquid while transporting a belt-shaped flexible support having a joining portion joined by an adhesive tape, wherein the joining portion of the belt-shaped flexible support is a transport roller or the like. In the coating apparatus transported via contact with the transporting means, a cutting means for cutting the side surface of the adhesive tape to join the joining portion is provided, and the cutting means, the adhesive tape of the adhesive tape is not formed The angle between the surface and the side surface of the adhesive tape parallel to the width direction of the strip-shaped flexible support is 4
The coating device, wherein the side surface is cut so as to be in a range of 5 ° to 75 °.
JP2000138370A 2000-05-11 2000-05-11 Application method and apparatus Expired - Fee Related JP4264789B2 (en)