JP2001012082A - Floor curing material for construction - Google Patents

Floor curing material for construction

Info

Publication number
JP2001012082A
JP2001012082A JP11183129A JP18312999A JP2001012082A JP 2001012082 A JP2001012082 A JP 2001012082A JP 11183129 A JP11183129 A JP 11183129A JP 18312999 A JP18312999 A JP 18312999A JP 2001012082 A JP2001012082 A JP 2001012082A
Authority
JP
Japan
Prior art keywords
curing material
paper
length
millimeters
curing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP11183129A
Other languages
Japanese (ja)
Inventor
Makoto Ishimaru
誠 石丸
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
KOYO KAGAKU KK
Original Assignee
KOYO KAGAKU KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by KOYO KAGAKU KK filed Critical KOYO KAGAKU KK
Priority to JP11183129A priority Critical patent/JP2001012082A/en
Publication of JP2001012082A publication Critical patent/JP2001012082A/en
Pending legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To provide a floor curing material for construction easy in transportation, execution and the disposal of a waste material after work completion by making thick liner paper an upper layer, making the reinforcing core paper of wave-form structure a lower layer, and sticking them. SOLUTION: The liner paper 2 of weight per m2 of 150-450 g is made an upper layer, reinforcing core paper 3 stuck so that the wave of weight per m2 of 150-450 g, height of 1-5 mm and an interval I of 5-10 mm is orthogonal to the length direction is made a lower layer, and the upper and lower layers are stuck. The curing material 1 is lightweight and excellent in strength, easy in transportation, requires no labor in execution and easy in the disposal of waste after work completion. If the size is a rectangle of 700-850 mm wide and 1700-6800 mm long or a rectangle of 700-1200 mm wide and 200-1500 mm long, it can laid on a standard room, a gallery, a staircase or the like as it is.

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【発明の属する技術分野】本発明は建築中の建物の床、
とくに木質床面の養生材に関するものである。
TECHNICAL FIELD The present invention relates to a floor of a building under construction,
In particular, it relates to curing materials for wooden floors.

【0002】[0002]

【従来の技術】従来の木質床面の養生は、幅が910ミ
リメートルで長さが1820ミリメートル、厚さが1.
75ミリメートルから5ミリメートルの寸法のベニヤ板
や繊維板などの硬質板を床面に敷き詰め、敷き詰められ
た硬質板を覆う形で、ポリエチレンフィルムをラミネー
トし凹凸を付けた段ボール中芯紙からなる養生シートな
どをかぶせ、該養生シートの周囲と継ぎ目を粘着テープ
で密封、固定する工法のほか、幅が900ミリメートル
から910ミリメートルで長さが1800ミリメートル
から1820ミリメートルで下面に厚さが約1ミリメー
トルの発泡ポリエチレンシートをラミネートしたプラス
チック中空板、さらには、上面にプラスチックフィルム
をラミネートし、下面に厚さが約2ミリメートルの発泡
ポリエチレンシートをラミネートした厚さが約1ミリメ
ートルの厚紙を、それぞれ直接床面に敷き詰め粘着テー
プで継ぎ目と周囲を密封、固定する工法が知られてい
る。
2. Description of the Related Art The conventional curing of a wooden floor surface is 910 mm in width, 1820 mm in length, and 1.10 mm in thickness.
A hardened sheet made of corrugated cardboard core paper with a polyethylene film laminated and embossed, covering a hardboard such as plywood or fiberboard with dimensions of 75 mm to 5 mm on the floor and covering the hardboard laid down. In addition to the method of sealing and fixing the periphery and the seam of the curing sheet with adhesive tape, foamed polyethylene with a width of 900 to 910 mm, a length of 1800 to 1820 mm and a thickness of about 1 mm on the lower surface A plastic hollow plate with a laminated sheet, and a plastic film on the upper surface, and a cardboard with a thickness of approximately 1 mm laminated with a foamed polyethylene sheet with a thickness of approximately 2 mm on the lower surface are laid directly on the floor surface. Seam and perimeter with adhesive tape Sealing, method of fixing are known.

【0003】階段の養生は両面段ボール紙を素材として
使用し、段鼻と踏み面の境界部分に1本と、踏み面と蹴
込みの境界部分に、2種類の踏み面の長さに対応する2
本の折り曲げのための折り罫が入れられた養生材が用意
され、施工時には踏み面の長さに対応するいずれかの折
り罫を折り曲げて敷設し、周囲を粘着テープで密封、固
定する工法が知られている。
[0003] Curing of stairs uses double-sided corrugated paper as a raw material, one at the boundary between the nose and the tread, and two at the boundary between the tread and the riser, corresponding to two types of tread lengths.
Curing material with creases for book folding is prepared, and at the time of construction, one of the creases corresponding to the length of the tread surface is folded and laid, and the surrounding area is sealed with adhesive tape and fixed. Are known.

【0004】[0004]

【発明が解決しようとする課題】上記硬質板と養生シー
トを併用する場合には、2種の養生材を2層に敷設する
ので手間が1層貼りに比べて余分にかかること、硬質板
は紙やプラスチック中空板に比べ重く運搬に不便である
こと、硬質板を敷き詰めたとき、床面に砂粒がある場合
に硬質板の下面と床面の間で砂粒が転がり、床面に擦り
傷をつけるおそれがあること、廃棄物の処分は紙の場合
のように全国的な回収システムができあがっていないの
で簡単ではないこと、寸法が建材の標準寸法である、幅
が910ミリメートルで長さが1820ミリメートルと
なっているため、廊下や階段など狭い場所を運搬するに
は不便であり、運搬時に堅くとがった角で壁などを傷つ
けやすいことのほか、施工時に裁断するか余分な部分を
重ねて使用することとなり裁断の手間がかかるか、ある
いは、重ね部分に段差が生じ危険であるとともに段差の
部分を粘着テープで密封、固定する場合に、粘着テープ
がはがれやすいなどの問題点を有している。
When the above-mentioned hard plate and curing sheet are used together, two types of curing materials are laid in two layers, so that extra work is required as compared with one-layer pasting. It is heavy and inconvenient to transport compared to paper or plastic hollow boards.When hard boards are laid, if there are sand grains on the floor, the sand grains roll between the lower surface of the hard boards and the floor, causing scratches on the floor There is a danger that the disposal of waste is not easy as there is no national collection system as in the case of paper, the dimensions are the standard dimensions of building materials, the width is 910 mm and the length is 1820 mm It is inconvenient to transport small places such as corridors and stairs, and it is easy to damage walls etc. with hard pointed corners during transportation, and cut or use extra parts at the time of construction This Or it is troublesome next cutting, or sealing with a step is dangerous occurred overlapped portion part of the step with an adhesive tape, when fixed, has a problem such as adhesive tape tends to peel off.

【0005】発泡シートを下面にラミネートしたプラス
チック中空板、あるいは、プラスチックフィルムをラミ
ネートした厚紙を使用する場合の問題点は、比較的高価
な素材を使用していること、あるいは、加工の工程が多
いことからコストがかさみ、落下物などの衝撃による床
面の傷つきに耐えるだけの厚さを持たせることがコスト
的に困難なこと、複合材であることから廃棄物の処分が
容易でないという問題点を有している。
A problem when using a plastic hollow plate having a foam sheet laminated on the lower surface or a cardboard having a plastic film laminated thereon is that a relatively expensive material is used or that there are many processing steps. Therefore, the cost is high, it is difficult to provide a thickness sufficient to withstand the damage to the floor surface due to the impact of falling objects, and the disposal of waste is not easy because of the composite material. have.

【0006】従来の階段養生材で両面段ボール紙を素材
としている場合には、折り曲げ部分については折り罫を
つけなければ折り曲げることができないので各種の踏み
面、あるいは蹴上げの寸法に対応できないという問題点
を有するほか、砂粒が踏み面に入り込んだ場合には擦り
傷が発生しやすいという問題点を有している。
[0006] In the case where the conventional stair curing material is made of double-faced corrugated paper, the folded portion cannot be bent unless it is creased, so that it cannot cope with various tread surfaces or dimensions of rise. In addition, when sand particles enter the tread surface, there is a problem that abrasion easily occurs.

【0007】そこで本発明は、運搬、施工、ならびに、
廃棄物の処理が容易な建築用床養生材を提供することを
目的としている。
[0007] Accordingly, the present invention provides transport, construction, and
An object of the present invention is to provide an architectural floor curing material that can easily treat waste.

【0008】[0008]

【課題を解決するための手段】上記した目的を達成する
ため、本発明の建築用床養生材は、1平方メートル当た
りの重量が150グラムから450グラムのライナー紙
を上層とし、1平方メートル当たりの重量が150グラ
ムから400グラムで、高さが1ミリメートルから5ミ
リメートルで間隔が5ミリメートルから10ミリメート
ルの波を長さ方向に対して直交するように付けた強化中
芯紙を下層として、上下両層を貼合したことを特徴とし
ている。
In order to achieve the above-mentioned object, a floor curing material for construction according to the present invention comprises a liner paper having a weight per square meter of 150 to 450 grams and a weight per square meter. The upper and lower layers are made of a reinforced core paper having a wave of 150 to 400 grams, a height of 1 to 5 millimeters and a spacing of 5 to 10 millimeters perpendicular to the length direction. It is characterized by pasting.

【0009】また、寸法を幅700ミリメートルから8
50ミリメートル、長さ1700ミリメートルから68
00ミリメートルの長方形とするか、幅700ミリメー
トルから1200ミリメートル、長さが200ミリメー
トルから1500ミリメートルの長方形とすることによ
り、標準的な部屋や廊下あるいは階段にそのまま敷設で
きる幅と長さにできる。
In addition, the size is set to 700 mm to 8 mm.
50 mm, length from 1700 mm to 68
A rectangle of 00 millimeters or a width of 700 to 1200 millimeters and a length of 200 to 1500 millimeters can be as wide and long as it can be laid in a standard room, hallway or staircase.

【0010】[0010]

【発明の実施の形態】以下、本発明を、図面に示す実施
形態例に基づいて、さらに詳細に説明する。養生材1の
構成は、図1に示されるように、上層のライナー紙2と
下層の強化中芯紙3を澱粉糊で貼合してなる。ライナー
紙2は、1平方メートル当たりの重量が150グラム以
下では強度的に不利であるが、450グラムを越すと養
生材1の重量が増加して運搬性に影響する。また、強化
中芯紙3も、1平方メートル当たりの重量が150グラ
ム以上であれば充分な強度を有するが、400グラムを
越すと養生材1の重量が増加して運搬性に影響する。さ
らに、強化中芯紙3の波は、高さHが1ミリメートルか
ら5ミリメートルが養生材1を粘着テープで密封、固定
する上で好ましく、間隔Iが5ミリメートルから10ミ
リメートルが製造上及び耐衝撃強度上好ましい。なお、
上層のライナー紙2、あるいは、下層の強化中芯紙3に
1平方メートル当たりの重量の高いものを用いることに
より、養生材1の耐衝撃強度を向上させることができ
る。
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS The present invention will be described below in more detail based on an embodiment shown in the drawings. As shown in FIG. 1, the configuration of the curing material 1 is obtained by laminating an upper layer liner paper 2 and a lower layer reinforced core paper 3 with a starch paste. If the weight per square meter is 150 g or less, the liner paper 2 is disadvantageous in strength, but if it exceeds 450 g, the weight of the curing material 1 increases and affects the transportability. Further, the reinforced core paper 3 also has sufficient strength if the weight per square meter is 150 g or more, but if it exceeds 400 g, the weight of the curing material 1 increases and affects the transportability. Further, the wave of the reinforced core paper 3 preferably has a height H of 1 mm to 5 mm for sealing and fixing the curing material 1 with an adhesive tape, and an interval I of 5 mm to 10 mm for production and impact resistance. Preferred for strength. In addition,
The impact resistance of the curing material 1 can be improved by using a high weight per square meter for the upper layer liner paper 2 or the lower layer reinforcing core paper 3.

【0011】本実施形態例では、ライナー紙2に、1平
方メートル当たりの重量が280グラムのものを用い、
強化中芯紙3に、1平方メートル当たりの重量が200
グラムで、長さ方向に対して直交するように付けた波の
高さHを約2ミリメートル、波の間隔Iを約6ミリメー
トルとしたものを用いた。
In this embodiment, a liner paper 2 having a weight per square meter of 280 grams is used.
The reinforced core paper 3 has a weight per square meter of 200
In grams, a wave having a height H of about 2 mm and a wave interval I of about 6 mm was used so as to be orthogonal to the length direction.

【0012】養生材1の寸法は、幅700ミリメートル
から850ミリメートル、長さ1700ミリメートルか
ら6800ミリメートルの長方形が好ましい。例えば、
図2に示される部屋用では、1畳を単位とした寸法とさ
れており、幅Wを850ミリメートル、長さLを幅Wの
2倍の1700ミリメートルとし、該寸法の養生材1を
部屋の中央部に敷き詰め、周囲と養生材同士の突き合わ
せ部分を粘着テープで密封、固定する。該寸法の養生材
1を6畳間に敷設すると、一般的な住宅の壁の厚さは、
通常約90ミリメートルであり、6畳間の短辺1.5間
の部分の長さは1820ミリメートルの1.5倍の27
30ミリメートルから上記壁の厚さ約90ミリメートル
を差し引いた約2640ミリメートルであり、一方養生
材の幅4は850ミリメートルの3倍、2550ミリメ
ートルであるので、差し引き両側に約45ミリメートル
の粘着テープで密封、固定するための余地が生ずる。こ
れより半間長くなるごとに片側にそれぞれ約30ミリメ
ートルの余地が加わる。従って6畳間の長辺については
約45ミリメートルに約30ミリメートルを加えた約7
5ミリメートルの余地が片側にそれぞれ生じ、通常の寸
法の部屋では養生材を裁断せずに施工することができ
る。
The size of the curing material 1 is preferably a rectangle having a width of 700 mm to 850 mm and a length of 1700 mm to 6800 mm. For example,
In the room shown in FIG. 2, the size is set in units of 1 tatami, the width W is 850 mm, the length L is 1700 mm which is twice the width W, and the curing material 1 of the size is used for the room. Spread in the center and seal the butted part between the surrounding and the cured material with adhesive tape. When the curing material 1 of this size is laid between 6 tatami mats, the thickness of the wall of a general house becomes
It is usually about 90 mm and the length between the short sides 1.5 between 6 tatami mats is 1.5 times 1820 mm 27
30 mm minus about 90 mm of the wall thickness, about 2640 mm, while the width 4 of the curing material is 3 times 850 mm, 2550 mm, so seal on both sides with about 45 mm of adhesive tape This leaves room for fixing. Each half-length adds about 30 millimeters of space on each side. Therefore, the long side between 6 tatami mats is about 45 mm plus about 30 mm plus about 7 mm.
A room of 5 millimeters is created on each side, so that a room of normal dimensions can be applied without cutting the curing material.

【0013】裁断する必要が生じた場合には、カッター
などを使用して硬質板などに比べて比較的容易に裁断で
きる。また本実施例では、上記寸法の養生材12枚を直
径約300ミリメートルの円筒状に巻いたものを一つの
梱包とすることにより周囲の壁などを傷つけることなく
容易に搬入される。使用後も同様の形状にして容易に搬
出される。
When it is necessary to perform cutting, cutting can be performed relatively easily using a cutter or the like as compared with a hard plate or the like. Further, in this embodiment, 12 curing materials having the above dimensions are wound into a cylindrical shape having a diameter of about 300 mm to form a single package, so that they can be easily carried in without damaging surrounding walls and the like. After use, it is easily carried out in the same shape.

【0014】また、幅の狭い廊下などにも適合できるよ
う、図3に示されるように、養生材1の幅を700ミリ
メートルとし、さらに接続の手間を省くため長さを34
00ミリメートルとして2間用としてもよく、この場合
には、廊下の木質床板10に敷き詰めれば、標準的な幅
の廊下であれば、養生材1の周囲に粘着テープ11で密
封、固定するための余地が生ずる。この寸法は、部屋の
1辺が2間の部屋にも使用できる。3間用あるいは4間
用を用意して同様に使用できるが、このように巻き長さ
を長く取ると接続の手間が省けるが、部屋の長さより大
きくなり過ぎると巻き直径が大きくなり端末部の切断が
困難となるので、部屋の寸法に見合ったものを用意する
ことが好ましい。
In addition, as shown in FIG. 3, the width of the curing material 1 is set to 700 mm so as to be adaptable to a narrow corridor or the like, and the length is set to 34 in order to save the trouble of connection.
It may be used for two spaces as 00 mm. In this case, if it is laid on the wooden floorboard 10 of the corridor, if it is a corridor of a standard width, it is sealed and fixed around the curing material 1 with the adhesive tape 11. There is room for This dimension can also be used for rooms where one side of the room is between two. It can be used in the same way by preparing for three or four rooms, but taking a long winding length in this way can save the trouble of connection, but if it becomes too long than the room length, the winding diameter becomes large and the terminal part Since cutting becomes difficult, it is preferable to prepare one that matches the size of the room.

【0015】さらに、階段部分に用いる養生材1は、そ
の寸法を幅700ミリメートルから1200ミリメート
ル、長さが200ミリメートルから1500ミリメート
ルの長方形が好ましい。例えば、図4及び図5に示され
る養生材1は、幅を700ミリメートル、長さを680
ミリメートルとし、下層方向への折り曲げをさらに容易
とするために折り罫を段鼻12と踏み面13の境界に設
けるとともに、折り罫から下方向へ踏み板14の厚さに
相当する約30ミリメートルの位置で折り返して踏み面
11前部に約60ミリメートルの幅の波状の滑り止め1
5を設け、周囲を粘着テープ11で密封、固定してい
る。
Further, the curing material 1 used for the stairs is preferably a rectangle having a width of 700 mm to 1200 mm and a length of 200 mm to 1500 mm. For example, the curing material 1 shown in FIGS. 4 and 5 has a width of 700 millimeters and a length of 680.
Millimeters, and a folding rule is provided at the boundary between the nosing 12 and the tread surface 13 in order to further facilitate bending in the lower direction, and at a position of about 30 millimeters corresponding to the thickness of the tread plate 14 downward from the folding rule. Fold it back and set a wavy antislip 1 with a width of about 60 mm on the front of the tread surface 11.
5 are provided, and the periphery is sealed and fixed with an adhesive tape 11.

【0016】また、蹴上げ16の部分の養生が不要な場
合には、踏み面13の養生に必要な長さにとどめる。さ
らに、階段に曲がり部分がある場合には蹴上げ16面か
ら養生材1を立ち上げ、蹴込み17、段鼻12、踏み面
13の養生に必要な長さとし、踏み面13と次の蹴上げ
16との境界、あるいは、側板との境界に沿って裁断し
たものを用意する。曲がりの一部では、直線部に比べ幅
が広く踏み面11の長さが長いものを用意する。また、
曲がり部分で滑り止め15を設ける場合には蹴上げ16
の下部で折り返しても良いが、別途裁断したものを用意
して貼り付けることでも良い。裏返して2層となった滑
り止め15の部分は、踏み面13と段鼻12の部分の保
護の強化に役立つ。滑り止め15は踏み面13の全面に
設けても良い。
When curing of the riser 16 is not necessary, the length of the tread 13 is required to be sufficient. Further, when the stairs have a bent portion, the curing material 1 is set up from the riser 16 surface, and the riser 17, the nose 12 and the tread surface 13 are set to the necessary length for curing. Prepare one cut along the border or the border with the side plate. For a part of the bend, a bend that is wider than the straight portion and has a longer tread surface 11 is prepared. Also,
If a non-slip 15 is provided at the bend, raise 16
May be folded back at the bottom, or may be separately cut and prepared and pasted. The two-layered non-slip portion 15 which is turned upside down serves to enhance the protection of the tread surface 13 and the nose 12 portion. The non-slip 15 may be provided on the entire surface of the tread surface 13.

【0017】このように、養生材1は、耐荷重・耐衝撃
強度に特に優れた厚手のライナー紙2と波形構造の強化
中芯紙3を貼合してなる高強度の片面段ボール紙を使用
しているので、軽量で、強度に優れ、しかも、廃棄物の
回収システムの整っている紙のみを素材としているか
ら、廃棄処理が容易である。また、1枚あるいは複数枚
を円筒状に巻くことができ、運搬が容易で、1層だけの
施工である。さらに、下層を波形構造とすることによ
り、養生材1の下面に入り込んだ砂粒等の転がりによる
擦り傷を防ぐことができる。また、耐水性が必要な場合
には、上面のライナー紙2にワックスなどを塗布するこ
ともできる。
As described above, as the curing material 1, a high-strength single-sided corrugated paper made by laminating a thick liner paper 2 particularly excellent in load resistance and impact resistance and a corrugated reinforced core paper 3 is used. As a result, since only paper having a lightweight and excellent strength and a waste collection system is used as a material, disposal processing is easy. In addition, one or a plurality of sheets can be wound in a cylindrical shape, so that they can be easily transported, and only one layer is applied. Further, by forming the lower layer into a corrugated structure, it is possible to prevent abrasion caused by rolling of sand particles or the like that have entered the lower surface of the curing material 1. When water resistance is required, wax or the like can be applied to the liner paper 2 on the upper surface.

【0018】また、養生材1の寸法を、標準的な部屋、
廊下あるいは階段にそのまま敷設できる幅と長さとする
とともに、厚さは密封、固定に使用する粘着テープ11
がはがれない程度にとどめる。階段用に関しては、下層
を波形構造とすることにより、上層方向へ任意の箇所で
折り曲げることのできる。
Further, the dimensions of the curing material 1 are set in a standard room,
Adhesive tape 11 used for sealing and fixing while having a width and length that can be laid directly in a corridor or stairs
Keep to the extent that it does not come off. For the staircase, the lower layer has a corrugated structure so that it can be bent at an arbitrary position in the upper layer direction.

【0019】使用後の養生材1の廃棄物は古紙回収業者
により、古紙の市況が高い場合には有償で買い上げら
れ、古紙の市況が低い場合には無償で、あるいは逆有償
で回収されて製紙工場に運搬され製紙原料とされる。
The waste of the curing material 1 after use is purchased by a waste paper collection company for a fee when the market condition of the waste paper is high, and is collected free of charge or reversely when the market condition of the waste paper is low. It is transported to the factory and used as papermaking raw material.

【0020】[0020]

【発明の効果】以上説明したように、本発明の養生材
は、厚手のライナー紙を上層とし、波形構造の強化中芯
紙を下層にして両者を貼合した構成なので、軽量で、強
度に優れ、運搬が容易で壁などを傷つけにくく、1層だ
けの施工ですむので、2層の施工に比べ手間が掛からな
い。また、掃除が不十分で床面に砂粒が残っている場合
でも、砂粒が波の間の空間に集まるので擦り傷がつきに
くい。さらに、廃棄物の回収システムのある、紙のみを
原料として使用しているので廃棄物の処分が容易であ
る。また、上面のライナー紙にワックスなどを塗布し耐
水性を持たせることもできる。しかも、上層のライナー
紙と下層の強化中芯紙の1平方メートル当たり重量を選
択することにより希望する耐衝撃・耐圧強度の養生材が
比較的低コストで得られる。
As described above, the curing material of the present invention is composed of a thick liner paper as an upper layer and a corrugated reinforced core paper as a lower layer, and is laminated to each other. Excellent, easy to transport, hard to damage walls, etc. Only one layer construction is required, so it takes less time than two layers construction. Further, even when the cleaning is insufficient and the sand particles remain on the floor surface, the sand particles are gathered in the space between the waves, so that they are not easily scratched. Further, since only a paper having a waste recovery system is used as a raw material, disposal of the waste is easy. In addition, wax or the like can be applied to the liner paper on the upper surface to impart water resistance. In addition, by selecting the weight per square meter of the upper layer liner paper and the lower layer reinforced core paper, a curing material having a desired impact resistance and pressure resistance can be obtained at a relatively low cost.

【0021】また、標準的な部屋、廊下あるいは階段に
そのまま敷設できる寸法とすることにより、裁断の手間
を省くとともに、重ね合わせによる段差が発生しないよ
うにすることができる。さらに、階段用に関しては踏み
面の長さに対応した箇所で折り曲げることのできる構造
であるので、多様な階段の踏み面の寸法に対応できると
ともに、一部分を折り返すだけで滑り止めを設けること
ができる。
Further, by setting the dimensions so as to be able to be laid directly in a standard room, corridor or stairs, it is possible to save time and effort for cutting and to prevent a step due to overlapping. Furthermore, as for stairs, since it is a structure that can be bent at a position corresponding to the length of the tread surface, it can correspond to various dimensions of the tread surface of the stairs and can be provided with a non-slip simply by folding a part thereof. .

【図面の簡単な説明】[Brief description of the drawings]

【図1】 本発明の養生材の一実施形態例を示す断面図
である。
FIG. 1 is a cross-sectional view showing one embodiment of a curing material of the present invention.

【図2】 同じく一部断面平面図である。FIG. 2 is a partially sectional plan view of the same.

【図3】 半間幅で2間長さの廊下での敷設平面図であ
る。
FIG. 3 is a plan view of installation in a corridor having a half width and a length of two spaces.

【図4】 滑り止めを設けた階段での養生材の敷設斜視
図である。
FIG. 4 is a perspective view of laying of a curing material on a stair provided with a non-slip.

【図5】 階段での養生材の敷設断面図である。FIG. 5 is a cross-sectional view of laying a curing material on stairs.

【符号の説明】[Explanation of symbols]

1…養生材、2…上層のライナー紙、3…下層の強化中
芯紙、10…木質床板、11…粘着テープ、12…段
鼻、13…踏み面、14…踏み板、15…滑り止め、1
6…蹴上げ、17…蹴込み、W…幅、L…長さ、H…波
の高さ、I…波の間隔
DESCRIPTION OF SYMBOLS 1 ... Curing material, 2 ... Upper layer liner paper, 3 ... Lower layer reinforced core paper, 10 ... Wood floor board, 11 ... Adhesive tape, 12 ... Nose, 13 ... Tread surface, 14 ... Tread plate, 15 ... Non-slip, 1
6 ... kick, 17 ... kick, W ... width, L ... length, H ... wave height, I ... wave interval

Claims (3)

【特許請求の範囲】[Claims] 【請求項1】 1平方メートル当たりの重量が150グ
ラムから450グラムのライナー紙を上層とし、1平方
メートル当たりの重量が150グラムから400グラム
で、高さが1ミリメートルから5ミリメートルで間隔が
5ミリメートルから10ミリメートルの波を長さ方向に
対して直交するように付けた強化中芯紙を下層として、
上下両層を貼合したことを特徴とする建築用床養生材。
An upper layer of liner paper weighing from 150 to 450 grams per square meter, weighing from 150 to 400 grams per square meter, having a height of from 1 to 5 millimeters, and having a spacing of from 5 to 5 millimeters. As a lower layer, a reinforced core paper with 10 mm waves attached so as to be orthogonal to the length direction,
Floor curing material for construction characterized by laminating both upper and lower layers.
【請求項2】 寸法が幅700ミリメートルから850
ミリメートル、長さ1700ミリメートルから6800
ミリメートルの長方形の請求項1記載の建築用床養生
材。
2. Dimensions ranging from 700 mm to 850 in width
Millimeters, length from 1700 millimeters to 6800
The architectural floor curing material according to claim 1, which is a millimeter-shaped rectangle.
【請求項3】 寸法が幅700ミリメートルから120
0ミリメートル、長さが200ミリメートルから150
0ミリメートルの長方形の請求項1記載の建築用床養生
材。
3. The dimensions range from 700 mm to 120 mm wide.
0mm, length from 200mm to 150mm
2. The building floor curing material according to claim 1, which is a rectangle of 0 mm.
JP11183129A 1999-06-29 1999-06-29 Floor curing material for construction Pending JP2001012082A (en)