A method comprises loading into the furnace the charge containing a fluxed sinter in the form of a manganous concentrate and lime and silicomanganese as a reducing agent, melting and releasing the alloy from the furnace, thus the basic capacity of a fluxed sinter makes 2,5-3,5; at a basic capacity 2,5-3,0 of the fluxed sinter, the conversion slag is gained together with the alloy, and at a basic capacity 3,0-3,5 there is a maximum extraction of manganese.
GEAP20060095832006-08-162006-08-16Method for obtaining medium-carbon manganous alloy in ore-thermal electric furnace
GEP20084428B
(en)