GB394171A - System of separation between the positive and the negative electrodes of electric dry-cells - Google Patents
System of separation between the positive and the negative electrodes of electric dry-cellsInfo
- Publication number
- GB394171A GB394171A GB24243/32A GB2424332A GB394171A GB 394171 A GB394171 A GB 394171A GB 24243/32 A GB24243/32 A GB 24243/32A GB 2424332 A GB2424332 A GB 2424332A GB 394171 A GB394171 A GB 394171A
- Authority
- GB
- United Kingdom
- Prior art keywords
- gelatine
- cup
- cells
- separation
- positive
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
394,171. Batteries. LAURENTI, B., 16, Via Riguccio Galluzzi, Florence, Italy. Aug. 30, 1932, No. 24243. Convention date, Sept. 16, 1931. [Class 53.] The zinc cup a of a dry cell is covered on its interior surface with a layer c of gelatine which is formed by pouring melted gelatine into the cup, distributing it over the surface of the cup and allowing it to cool. The gelatine is rendered insoluble either before or after application to the cup. The Specification as open to inspection under Sect. 91 states that the gelatine layer may be applied to the agglomerate mass of the central electrode instead of to the zinc cup and that gelatine in sheet form may be used. The gelatine may be replaced by glue or other gelatinous or colloid substances. This subjectmatter does not appear in the Specification as accepted.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
IT394171X | 1931-09-16 |
Publications (1)
Publication Number | Publication Date |
---|---|
GB394171A true GB394171A (en) | 1933-06-22 |
Family
ID=11246209
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB24243/32A Expired GB394171A (en) | 1931-09-16 | 1932-08-30 | System of separation between the positive and the negative electrodes of electric dry-cells |
Country Status (4)
Country | Link |
---|---|
BE (1) | BE390925A (en) |
DE (1) | DE617785C (en) |
GB (1) | GB394171A (en) |
NL (1) | NL36090C (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2534336A (en) * | 1944-12-14 | 1950-12-19 | Union Carbide & Carbon Corp | Primary galvanic cell |
WO2000059052A2 (en) * | 1999-03-29 | 2000-10-05 | The Gillette Company | Alkaline cell separator |
-
0
- NL NL36090D patent/NL36090C/xx active
- BE BE390925D patent/BE390925A/xx unknown
-
1932
- 1932-08-30 GB GB24243/32A patent/GB394171A/en not_active Expired
- 1932-09-08 DE DEL81969D patent/DE617785C/en not_active Expired
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2534336A (en) * | 1944-12-14 | 1950-12-19 | Union Carbide & Carbon Corp | Primary galvanic cell |
WO2000059052A2 (en) * | 1999-03-29 | 2000-10-05 | The Gillette Company | Alkaline cell separator |
WO2000059052A3 (en) * | 1999-03-29 | 2001-01-04 | Gillette Co | Alkaline cell separator |
Also Published As
Publication number | Publication date |
---|---|
DE617785C (en) | 1935-08-26 |
NL36090C (en) | |
BE390925A (en) |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB394171A (en) | System of separation between the positive and the negative electrodes of electric dry-cells | |
AU994832A (en) | Improvements in dry cell batteries | |
CA320498A (en) | Dry cell battery | |
CA318183A (en) | Dry cell battery and seal | |
CA220998A (en) | Dry cell battery | |
GB336113A (en) | Improvements in electrical storage batteries or accumulators | |
CA243142A (en) | Dry cell and battery | |
GB250985A (en) | Improvements in or relating to plates for electric accumulators | |
AU2487725A (en) | Improvements in or relating to dry battery cells | |
CA244790A (en) | Dry cell battery | |
CA243144A (en) | Dry cell battery | |
CA305683A (en) | Dry cell battery unit | |
CA273488A (en) | Primary cell and electrolyte | |
CA327581A (en) | Electric storage cell and battery | |
AU110131A (en) | Improvements in or relating to electric storage cells and batteries | |
GB426654A (en) | Improvements in electric batteries | |
CA289026A (en) | Dry cell battery | |
AU110031A (en) | Improvements in or relating to electric storage cells and batteries | |
AU109931A (en) | Improvements in or relating to electric storage cells and batteries | |
CA317006A (en) | Non-spillable primary battery with liquid electrolytes | |
CA318002A (en) | Electric storage cell and battery | |
CA310158A (en) | Container for dry cells | |
AU1514028A (en) | Improvements in or relating to battery separators | |
AU2324229A (en) | Improvements in and relating to electrolytes for electric cells | |
CA262489A (en) | Dry cell battery |