FR2351922B1 - - Google Patents
Info
- Publication number
- FR2351922B1 FR2351922B1 FR7616130A FR7616130A FR2351922B1 FR 2351922 B1 FR2351922 B1 FR 2351922B1 FR 7616130 A FR7616130 A FR 7616130A FR 7616130 A FR7616130 A FR 7616130A FR 2351922 B1 FR2351922 B1 FR 2351922B1
- Authority
- FR
- France
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C15/00—Surface treatment of glass, not in the form of fibres or filaments, by etching
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C8/00—Enamels; Glazes; Fusion seal compositions being frit compositions having non-frit additions
- C03C8/24—Fusion seal compositions being frit compositions having non-frit additions, i.e. for use as seals between dissimilar materials, e.g. glass and metal; Glass solders
Landscapes
- Chemical & Material Sciences (AREA)
- Life Sciences & Earth Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- General Chemical & Material Sciences (AREA)
- Geochemistry & Mineralogy (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Glass Compositions (AREA)
- Surface Treatment Of Glass (AREA)
- Joining Of Glass To Other Materials (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US05/590,651 US3975175A (en) | 1975-06-26 | 1975-06-26 | Process for increasing the strength of sealing glass |
Publications (2)
Publication Number | Publication Date |
---|---|
FR2351922A1 FR2351922A1 (fr) | 1977-12-16 |
FR2351922B1 true FR2351922B1 (US06649357-20031118-C00005.png) | 1980-10-10 |
Family
ID=24363095
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR7616130A Granted FR2351922A1 (fr) | 1975-06-26 | 1976-05-21 | Procede pour ameliorer la resistance d'un verre de scellement |
Country Status (5)
Families Citing this family (13)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4078923A (en) * | 1977-03-08 | 1978-03-14 | Xerox Corporation | Migration imaging with surfactant-modified solvent development |
US4199337A (en) * | 1978-10-06 | 1980-04-22 | International Telephone And Telegraph Corporation | Method of fabricating high strength optical preforms |
US4898777A (en) * | 1989-01-24 | 1990-02-06 | Infrared Fiber Systems | High-strength fluoride glass fibers and process of making |
DE4009602A1 (de) * | 1990-03-26 | 1991-10-02 | Ivoclar Ag | Polymerisierbare dentalmasse |
DE69935070T2 (de) * | 1998-03-31 | 2007-05-31 | Hitachi Ltd. | Anzeigetafel |
DE102010035251B4 (de) * | 2010-02-15 | 2013-09-26 | Schott Ag | Hochtemperatur-Glaslot und dessen Verwendung |
WO2013071021A2 (en) | 2011-11-10 | 2013-05-16 | Corning Incorporated | Acid strengthening of glass |
US10273048B2 (en) | 2012-06-07 | 2019-04-30 | Corning Incorporated | Delamination resistant glass containers with heat-tolerant coatings |
CN104395255A (zh) | 2012-06-07 | 2015-03-04 | 康宁股份有限公司 | 抗脱层的玻璃容器 |
US9034442B2 (en) | 2012-11-30 | 2015-05-19 | Corning Incorporated | Strengthened borosilicate glass containers with improved damage tolerance |
US10117806B2 (en) | 2012-11-30 | 2018-11-06 | Corning Incorporated | Strengthened glass containers resistant to delamination and damage |
US10899659B2 (en) | 2014-09-05 | 2021-01-26 | Corning Incorporated | Glass articles and methods for improving the reliability of glass articles |
KR102273665B1 (ko) * | 2014-11-26 | 2021-07-08 | 코닝 인코포레이티드 | 강화된 및 내구성 있는 유리 용기의 생산 방법 |
Family Cites Families (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
NL217651A (US06649357-20031118-C00005.png) * | 1956-05-29 | 1900-01-01 | ||
US3023139A (en) * | 1957-03-16 | 1962-02-27 | Floris Van Tetterode And Jan D | Method of strengthening sheet glass in agitated liquid fluoride bath |
US3281294A (en) * | 1965-06-08 | 1966-10-25 | Corning Glass Works | Method for etching glass |
NL6817661A (US06649357-20031118-C00005.png) * | 1968-12-10 | 1970-06-12 | ||
BE790476A (fr) * | 1971-10-29 | 1973-04-24 | Champion Spark Plug Co | Procede de preparation d'emaux au plomb |
JPS5130564B2 (US06649357-20031118-C00005.png) * | 1972-10-09 | 1976-09-01 |
-
1975
- 1975-06-26 US US05/590,651 patent/US3975175A/en not_active Expired - Lifetime
-
1976
- 1976-05-19 DE DE19762622141 patent/DE2622141A1/de not_active Withdrawn
- 1976-05-21 FR FR7616130A patent/FR2351922A1/fr active Granted
- 1976-06-11 JP JP51067874A patent/JPS5842139B2/ja not_active Expired
- 1976-06-22 GB GB25778/76A patent/GB1541704A/en not_active Expired
Also Published As
Publication number | Publication date |
---|---|
DE2622141A1 (de) | 1977-01-20 |
FR2351922A1 (fr) | 1977-12-16 |
JPS525815A (en) | 1977-01-17 |
JPS5842139B2 (ja) | 1983-09-17 |
US3975175A (en) | 1976-08-17 |
GB1541704A (en) | 1979-03-07 |
Similar Documents
Legal Events
Date | Code | Title | Description |
---|---|---|---|
ST | Notification of lapse |