FR2322203A1 - Hardening of saw teeth - by selective heat treatment with control of base temp. - Google Patents
Hardening of saw teeth - by selective heat treatment with control of base temp.Info
- Publication number
- FR2322203A1 FR2322203A1 FR7526593A FR7526593A FR2322203A1 FR 2322203 A1 FR2322203 A1 FR 2322203A1 FR 7526593 A FR7526593 A FR 7526593A FR 7526593 A FR7526593 A FR 7526593A FR 2322203 A1 FR2322203 A1 FR 2322203A1
- Authority
- FR
- France
- Prior art keywords
- temp
- saw
- control
- heat treatment
- hardening
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
The saw is pretreated so that the main part of the saw tooth is held at a definite prescribed low temp. During or after the transfer of the tooth in an atmosphere at a definite low temp. the surface layer is heated. On completion of the heating period, the layer loses its heat to the main part of the saw at the low temp. The saw may be moved intermittently or continuously through the heat treatment equipment and temp. control methods may include the use of air or water. By control of the saw temp. the efficiency of the selective hardening process can be assured, independent of changes, e.g. seasonal, in the ambient temp.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7526593A FR2322203A1 (en) | 1975-08-29 | 1975-08-29 | Hardening of saw teeth - by selective heat treatment with control of base temp. |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7526593A FR2322203A1 (en) | 1975-08-29 | 1975-08-29 | Hardening of saw teeth - by selective heat treatment with control of base temp. |
Publications (1)
Publication Number | Publication Date |
---|---|
FR2322203A1 true FR2322203A1 (en) | 1977-03-25 |
Family
ID=9159447
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR7526593A Withdrawn FR2322203A1 (en) | 1975-08-29 | 1975-08-29 | Hardening of saw teeth - by selective heat treatment with control of base temp. |
Country Status (1)
Country | Link |
---|---|
FR (1) | FR2322203A1 (en) |
-
1975
- 1975-08-29 FR FR7526593A patent/FR2322203A1/en not_active Withdrawn
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS51143153A (en) | Method and apparatus for converting relatively low temperature heat into power or energy | |
SE7606068L (en) | FUEL ENRICHMENT AND HEAT START CONTROL DEVICE IN A FUEL CONTROL | |
IT1048481B (en) | Hardening of saw teeth - by selective heat treatment with control of base temp. | |
FR2322203A1 (en) | Hardening of saw teeth - by selective heat treatment with control of base temp. | |
ATA414672A (en) | CONTINUOUS HEAT TREATMENT PROCESS ON ROD-SHAPED, LOW-CARBON STEELS AND DEVICE FOR CARRYING OUT THE PROCESS | |
AT300493B (en) | Process for the treatment of heat exchangers a.ähnl. Apparatus in thermal power plants | |
JPS5325217A (en) | Spheroidizing annealing method for wire by strand method | |
FR2311853A2 (en) | Salt bath heat treatment of metal parts - which are only partially immersed in salt to leave unhardened zones | |
JPS5229410A (en) | Temperature controlling method for continuous annealing and heating ap paratus | |
GB616812A (en) | Method of manufacture of selenium rectifier elements | |
JPS53140646A (en) | High frequency irradiation device | |
GB1528424A (en) | Apparatus for and a method of determination of influenza neuraminidase | |
ES2031824T3 (en) | UNION PERCENTAGE OF SILICONE RUBBER TO METAL. | |
JPS5239511A (en) | Apparatus for treatment of heating members | |
JPS52129605A (en) | Method and equipment for heat treatment of metal | |
JPS51143520A (en) | Heat treatment method of steel wire | |
JPS5217236A (en) | Method and apparatus for micro-wave heating | |
JPS5239510A (en) | Method of operating soaking pits | |
JPS5325218A (en) | Spheroidizing heat treating method for wire by strand method | |
JPS5229415A (en) | Method of heat treatment for saw teeth | |
JPS51131409A (en) | A method and appratus for directly hardening hot rolled wires | |
JPS5237512A (en) | Heat treatment method to improve toughness of steel | |
JPS5350070A (en) | Continuous ion exchange apparatus using thermal regeneration resin | |
JPS52138005A (en) | Continuous heat treatment apparatus for hollow metallic materials | |
JPS5276209A (en) | Heat treatment of meallic pipe of larger diameter |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
ST | Notification of lapse |