FR2273277A1 - Dissolved substance concentration determination - by measuring current at anode effect onset during rapid cathode/anode voltage rise - Google Patents
Dissolved substance concentration determination - by measuring current at anode effect onset during rapid cathode/anode voltage riseInfo
- Publication number
- FR2273277A1 FR2273277A1 FR7516625A FR7516625A FR2273277A1 FR 2273277 A1 FR2273277 A1 FR 2273277A1 FR 7516625 A FR7516625 A FR 7516625A FR 7516625 A FR7516625 A FR 7516625A FR 2273277 A1 FR2273277 A1 FR 2273277A1
- Authority
- FR
- France
- Prior art keywords
- anode
- voltage rise
- dissolved substance
- measuring current
- substance concentration
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Links
- 239000000126 substance Substances 0.000 title abstract 3
- PNEYBMLMFCGWSK-UHFFFAOYSA-N Alumina Chemical compound [O-2].[O-2].[O-2].[Al+3].[Al+3] PNEYBMLMFCGWSK-UHFFFAOYSA-N 0.000 abstract 4
- AZDRQVAHHNSJOQ-UHFFFAOYSA-N alumane Chemical compound [AlH3] AZDRQVAHHNSJOQ-UHFFFAOYSA-N 0.000 abstract 1
- 229910052782 aluminium Inorganic materials 0.000 abstract 1
- 239000004411 aluminium Substances 0.000 abstract 1
- 229910052593 corundum Inorganic materials 0.000 abstract 1
- 229910001610 cryolite Inorganic materials 0.000 abstract 1
- 229910001845 yogo sapphire Inorganic materials 0.000 abstract 1
Classifications
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25C—PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- C25C3/00—Electrolytic production, recovery or refining of metals by electrolysis of melts
- C25C3/06—Electrolytic production, recovery or refining of metals by electrolysis of melts of aluminium
- C25C3/20—Automatic control or regulation of cells
-
- G—PHYSICS
- G01—MEASURING; TESTING
- G01N—INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
- G01N27/00—Investigating or analysing materials by the use of electric, electrochemical, or magnetic means
- G01N27/26—Investigating or analysing materials by the use of electric, electrochemical, or magnetic means by investigating electrochemical variables; by using electrolysis or electrophoresis
- G01N27/416—Systems
- G01N27/48—Systems using polarography, i.e. measuring changes in current under a slowly-varying voltage
Landscapes
- Chemical & Material Sciences (AREA)
- Electrochemistry (AREA)
- Life Sciences & Earth Sciences (AREA)
- Health & Medical Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Biochemistry (AREA)
- Pathology (AREA)
- Analytical Chemistry (AREA)
- Molecular Biology (AREA)
- General Health & Medical Sciences (AREA)
- General Physics & Mathematics (AREA)
- Immunology (AREA)
- Physics & Mathematics (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Electrolytic Production Of Metals (AREA)
- Investigating Or Analyzing Materials By The Use Of Electric Means (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| AUPB769074 | 1974-05-28 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| FR2273277A1 true FR2273277A1 (en) | 1975-12-26 |
Family
ID=3765922
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| FR7516625A Withdrawn FR2273277A1 (en) | 1974-05-28 | 1975-05-28 | Dissolved substance concentration determination - by measuring current at anode effect onset during rapid cathode/anode voltage rise |
Country Status (5)
| Country | Link |
|---|---|
| JP (1) | JPS513293A (en:Method) |
| AU (1) | AU8159275A (en:Method) |
| DE (1) | DE2523768A1 (en:Method) |
| FR (1) | FR2273277A1 (en:Method) |
| NO (1) | NO751829L (en:Method) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP0942280A1 (en) * | 1998-03-13 | 1999-09-15 | Eastman Kodak Company | Automatic measuring device for the concentration of a developing agent |
| FR2798467A1 (fr) * | 1999-09-13 | 2001-03-16 | Eastman Kodak Co | Dispositif de mesure automatique de la concentration d'un agent developpateur |
| GB2365023A (en) * | 2000-07-18 | 2002-02-13 | Ionex Ltd | Increasing the surface area of an electrode |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4450063A (en) * | 1983-09-28 | 1984-05-22 | Reynolds Metals Company | Probe for alumina concentration meter |
-
1974
- 1974-05-28 AU AU81592/75A patent/AU8159275A/en not_active Expired
-
1975
- 1975-05-23 NO NO751829A patent/NO751829L/no unknown
- 1975-05-28 FR FR7516625A patent/FR2273277A1/fr not_active Withdrawn
- 1975-05-28 JP JP50063138A patent/JPS513293A/ja active Pending
- 1975-05-28 DE DE19752523768 patent/DE2523768A1/de active Pending
Cited By (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP0942280A1 (en) * | 1998-03-13 | 1999-09-15 | Eastman Kodak Company | Automatic measuring device for the concentration of a developing agent |
| FR2776071A1 (fr) * | 1998-03-13 | 1999-09-17 | Eastman Kodak Co | Dispositif de mesure automatique de la concentration d'un agent developpateur |
| US6228237B1 (en) | 1998-03-13 | 2001-05-08 | Eastman Kodak Company | Automatic measuring device for the concentration of a developing agent |
| FR2798467A1 (fr) * | 1999-09-13 | 2001-03-16 | Eastman Kodak Co | Dispositif de mesure automatique de la concentration d'un agent developpateur |
| EP1085321A1 (en) * | 1999-09-13 | 2001-03-21 | Eastman Kodak Company | Device for the automatic measurement of developing agent concentration |
| GB2365023A (en) * | 2000-07-18 | 2002-02-13 | Ionex Ltd | Increasing the surface area of an electrode |
| GB2365023B (en) * | 2000-07-18 | 2002-08-21 | Ionex Ltd | A process for improving an electrode |
| US7341655B2 (en) | 2000-07-18 | 2008-03-11 | Ionex Limited | Process for improving an electrode |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS513293A (en:Method) | 1976-01-12 |
| AU8159275A (en) | 1976-12-02 |
| NO751829L (en:Method) | 1975-12-01 |
| DE2523768A1 (de) | 1975-12-11 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5529940A (en) | Method and apparatus for determining activity of microorganism | |
| FR2273277A1 (en) | Dissolved substance concentration determination - by measuring current at anode effect onset during rapid cathode/anode voltage rise | |
| DE3274471D1 (en) | Precipitation or depositing of particles from a solution | |
| ES308069A1 (es) | Procedimiento y aparato para la electrolisis ignea de alumina | |
| GB1501893A (en) | Continuous electrolytic colouring of a preanodised aluminium foil or strip | |
| Loucka | The reasons for the loss of activity of titanium-ruthenium dioxide anodes in sulphuric acid media | |
| JPS57181390A (en) | Measuring method for counter electromotive force of aluminum electrolytic cell | |
| Vertes et al. | Oxidation on the nickel hydroxide electrode | |
| US3442779A (en) | Anodic protection of metals | |
| Morris | The rate of electrode oxide formation during chronopotentiograms at a platinum anode | |
| GB1011177A (en) | Improvements in or relating to methods and apparatus for measuring fluoride activity | |
| SU1423627A1 (ru) | Способ контрол концентрации глинозема в криолитглиноземном расплаве | |
| Suzuki | Analytical Studies Using the Convection Electrode. XI. Cathodic Stripping Voltammetry of Chloride Ions with the Pushed-out Mercury Drop Convection Electrode | |
| JPS5687802A (en) | Measuring method for surface area of solid body | |
| Jangg et al. | Investigations Into the Pitting Corrosion of Aluminum | |
| SU739330A1 (ru) | Способ измерени площади поверхности электропроводного объекта | |
| Delahay | Coulostatic Anodic Stripping with a Mercury Electrode. | |
| Azzam et al. | Anodic behaviour and passivation of tin in alkaline—stannate plating solutions | |
| Allen | The photo-electric fatigue of Zinc | |
| Zhu-xian et al. | Studies of Wettability of Carbon Electrodes in Aluminum Electrolysis. Pt. 1 | |
| SU1409895A1 (ru) | Способ определени склонности нержавеющих сталей к межкристаллитной коррозии | |
| Ferguson et al. | STUDIES ON OVERVOLTAGE. IX: The Nature of Cathode and Anode Discharge Potentials at Several Metal Surfaces1, 2 | |
| Sinitsyna | polonium (10-8 moles/liter) in 0.1 N HNO3. They determined the | |
| SU831884A1 (ru) | Способ электрохимическойОбРАбОТКи МиКРОлЕНТы | |
| Shalaevskaya et al. | Kinetics of the Dissolution and Diffusion of Metallic Aluminum in Mercury |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| ST | Notification of lapse |