FR1309587A - Nickel-chromium-molybdenum alloy with high resistance to corrosion, especially intercrystalline corrosion - Google Patents

Nickel-chromium-molybdenum alloy with high resistance to corrosion, especially intercrystalline corrosion

Info

Publication number
FR1309587A
FR1309587A FR882932A FR882932A FR1309587A FR 1309587 A FR1309587 A FR 1309587A FR 882932 A FR882932 A FR 882932A FR 882932 A FR882932 A FR 882932A FR 1309587 A FR1309587 A FR 1309587A
Authority
FR
France
Prior art keywords
corrosion
chromium
nickel
high resistance
molybdenum alloy
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
FR882932A
Other languages
French (fr)
Inventor
Erich Scheil
Immanuel Class
Hubert Graefen
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
BASF SE
Original Assignee
BASF SE
Badische Anilin and Sodafabrik AG
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BASF SE, Badische Anilin and Sodafabrik AG filed Critical BASF SE
Priority to FR882932A priority Critical patent/FR1309587A/en
Application granted granted Critical
Publication of FR1309587A publication Critical patent/FR1309587A/en
Expired legal-status Critical Current

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C22METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
    • C22CALLOYS
    • C22C19/00Alloys based on nickel or cobalt
    • C22C19/03Alloys based on nickel or cobalt based on nickel
    • C22C19/05Alloys based on nickel or cobalt based on nickel with chromium
    • C22C19/051Alloys based on nickel or cobalt based on nickel with chromium and Mo or W
    • C22C19/055Alloys based on nickel or cobalt based on nickel with chromium and Mo or W with the maximum Cr content being at least 20% but less than 30%
FR882932A 1961-12-22 1961-12-22 Nickel-chromium-molybdenum alloy with high resistance to corrosion, especially intercrystalline corrosion Expired FR1309587A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
FR882932A FR1309587A (en) 1961-12-22 1961-12-22 Nickel-chromium-molybdenum alloy with high resistance to corrosion, especially intercrystalline corrosion

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
FR882932A FR1309587A (en) 1961-12-22 1961-12-22 Nickel-chromium-molybdenum alloy with high resistance to corrosion, especially intercrystalline corrosion

Publications (1)

Publication Number Publication Date
FR1309587A true FR1309587A (en) 1962-11-16

Family

ID=8769343

Family Applications (1)

Application Number Title Priority Date Filing Date
FR882932A Expired FR1309587A (en) 1961-12-22 1961-12-22 Nickel-chromium-molybdenum alloy with high resistance to corrosion, especially intercrystalline corrosion

Country Status (1)

Country Link
FR (1) FR1309587A (en)

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
FR2416956A1 (en) * 1978-02-09 1979-09-07 Cabot Corp NICKEL, CHROME, MOLYBDENE BASED ALLOY, CORROSION AND CRACK RESISTANCE FOR TUBULAR PRODUCTS
FR2491094A1 (en) * 1980-09-29 1982-04-02 Mitsubishi Steel Mfg LOW CROSS-RESISTIVITY ROLLER FOR ELECTROLYTIC DEPOSITION
FR2493343A1 (en) * 1980-07-10 1982-05-07 Cabot Corp CORROSION RESISTANT NICKEL ALLOY
FR2507629A1 (en) * 1981-06-10 1982-12-17 Sumitomo Metal Ind ALLOY WITH HIGH RESISTANCE TO TENSIO N CORROSION CRACKING, ESPECIALLY FOR THE REALIZATION OF TUBULAR PRODUCTS FOR DEEP WELLS
FR2508930A1 (en) * 1981-07-03 1983-01-07 Sumitomo Metal Ind PROCESS FOR MANUFACTURING HIGH MECHANICAL RESISTANCE PIPES AND PIPES FOR DEEP WELLS
EP0092397A1 (en) * 1982-04-20 1983-10-26 Huntington Alloys, Inc. Nickel-chromium-molybdenum alloy

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
FR2416956A1 (en) * 1978-02-09 1979-09-07 Cabot Corp NICKEL, CHROME, MOLYBDENE BASED ALLOY, CORROSION AND CRACK RESISTANCE FOR TUBULAR PRODUCTS
FR2493343A1 (en) * 1980-07-10 1982-05-07 Cabot Corp CORROSION RESISTANT NICKEL ALLOY
FR2491094A1 (en) * 1980-09-29 1982-04-02 Mitsubishi Steel Mfg LOW CROSS-RESISTIVITY ROLLER FOR ELECTROLYTIC DEPOSITION
FR2507629A1 (en) * 1981-06-10 1982-12-17 Sumitomo Metal Ind ALLOY WITH HIGH RESISTANCE TO TENSIO N CORROSION CRACKING, ESPECIALLY FOR THE REALIZATION OF TUBULAR PRODUCTS FOR DEEP WELLS
FR2508930A1 (en) * 1981-07-03 1983-01-07 Sumitomo Metal Ind PROCESS FOR MANUFACTURING HIGH MECHANICAL RESISTANCE PIPES AND PIPES FOR DEEP WELLS
EP0092397A1 (en) * 1982-04-20 1983-10-26 Huntington Alloys, Inc. Nickel-chromium-molybdenum alloy

Similar Documents

Publication Publication Date Title
BE612240A (en) Improvements to steel alloys.
FR1280924A (en) Creep resistant alloys
CH415068A (en) Steel alloy
BE591665A (en) High strength alloy that can be used at high temperatures
BE608907A (en) Improvements in the assembly of metal sheets.
FR1309587A (en) Nickel-chromium-molybdenum alloy with high resistance to corrosion, especially intercrystalline corrosion
BE604924A (en) Improvements at the junction of metals
CH410439A (en) Niobium alloy
CH410438A (en) Niobium alloy
FR1264974A (en) Alloy
CH400579A (en) Niobium alloy
FR1314540A (en) Stainless steel alloy
CH450734A (en) Heat resistant alloy, nickel-chromium-cobalt-molybdenum
FR1492538A (en) High corrosion resistance nickel alloy
BE611099A (en) Stainless steel alloy
FR1397741A (en) High corrosion resistance cobalt-chromium-wolfram alloys
WALLBAUM IMPROVEMENT OF THE CORROSION BEHAVIOR OF COPPER BASED MATERIALS BY SMALL ALLOY ADDITIONS
FR1259886A (en) Corrosion resistant alloys
GRAND Corrosion behavior under tension of aluminum alloy sections and forged parts(Aluminum alloy corrosion and fracture under tension showing relation to intergranular corrosion)
FR1412853A (en) High corrosion resistance cobalt-chromium-tungsten alloys
FR1343084A (en) Improvements concerning the coating of alloys, in particular based on columbium
DK96484C (en) Copper alloy with two-phase structure.
FR1279509A (en) Low alloy steel
FR1259271A (en) High strength alloy intended for use at high temperatures
FR1336078A (en) Bilame with good corrosion resistance