FR1101314A - Improvement in cast iron treatments - Google Patents
Improvement in cast iron treatmentsInfo
- Publication number
- FR1101314A FR1101314A FR1101314DA FR1101314A FR 1101314 A FR1101314 A FR 1101314A FR 1101314D A FR1101314D A FR 1101314DA FR 1101314 A FR1101314 A FR 1101314A
- Authority
- FR
- France
- Prior art keywords
- improvement
- cast iron
- iron treatments
- treatments
- cast
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21C—PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- C21C1/00—Refining of pig-iron; Cast iron
- C21C1/08—Manufacture of cast-iron
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR1101314T | 1954-04-30 |
Publications (1)
Publication Number | Publication Date |
---|---|
FR1101314A true FR1101314A (en) | 1955-10-05 |
Family
ID=9620979
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR1101314D Expired FR1101314A (en) | 1954-04-30 | 1954-04-30 | Improvement in cast iron treatments |
Country Status (1)
Country | Link |
---|---|
FR (1) | FR1101314A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2453909A1 (en) * | 1979-04-14 | 1980-11-07 | Duisburger Kupferhuette | Grey alloy iron for use at high temps. - contains fine ppte. of carbonitride(s) and nitride(s), and used esp in IC engine exhaust components |
-
1954
- 1954-04-30 FR FR1101314D patent/FR1101314A/en not_active Expired
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2453909A1 (en) * | 1979-04-14 | 1980-11-07 | Duisburger Kupferhuette | Grey alloy iron for use at high temps. - contains fine ppte. of carbonitride(s) and nitride(s), and used esp in IC engine exhaust components |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
FR1137565A (en) | Improvement in syringe-ampoules | |
FR1122726A (en) | Improvements to electromagnetic coils | |
FR1145146A (en) | Improvements in calculating mechanisms | |
FR1101314A (en) | Improvement in cast iron treatments | |
FR1123034A (en) | Contra-angle improvements | |
FR1101665A (en) | Improvements in hydraulic mechanisms | |
FR1109246A (en) | Improvement in valves | |
FR1101283A (en) | Metal casting | |
FR1111614A (en) | Further training in cranes | |
FR1104402A (en) | Advanced training in electromagnetic contactors | |
FR67701E (en) | Metal casting | |
FR1123247A (en) | Improvements in vehicle controls | |
FR1120682A (en) | Further training in cranes | |
FR1150704A (en) | Improvements in nickel-chromium-iron alloys | |
FR1100782A (en) | Furnace for metallurgical treatments | |
FR1092906A (en) | Improvement in magnetic head supports | |
FR1120620A (en) | Improvement in turbo-engines | |
FR1123872A (en) | Improvement in alèzes | |
FR1153262A (en) | Improvements in ovens | |
FR1102538A (en) | Curl enhancement | |
FR1090116A (en) | Improvements in finishing treatments for metal parts | |
FR1073282A (en) | Improvement in ski-skis | |
FR1103011A (en) | Improvements in electromagnetic mechanisms | |
FR1095519A (en) | Improvements to the iron rests | |
FR1104633A (en) | Improvement in valves |