FI873420A - FOERFARANDE FOER REDUKTION AV KROMITMALM. - Google Patents
FOERFARANDE FOER REDUKTION AV KROMITMALM. Download PDFInfo
- Publication number
- FI873420A FI873420A FI873420A FI873420A FI873420A FI 873420 A FI873420 A FI 873420A FI 873420 A FI873420 A FI 873420A FI 873420 A FI873420 A FI 873420A FI 873420 A FI873420 A FI 873420A
- Authority
- FI
- Finland
- Prior art keywords
- chromite
- quartz
- kromitmalm
- reduktion
- alkali metal
- Prior art date
Abstract
The invention relates to a method for reduction of chromite ores in a solid state, whereby a finely distributed chromite ore is heated in an intimate mixture and preferably in agglomerated form with a solid carbonaceous reducing agent, an alkali metal aluminium silicate, quartz and calcium fluoride, to a temperature of principally 1200-1500 degree C and typically at about 1300 degree C in such a way that a liquid flux phase is formed in contact with adjacent solid chromite and reducing agent particles. The alkali metal aluminium silicate, quartz and calcium fluoride are most suitably present in the form of granite and fluorite.
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
ZA865937 | 1986-08-07 | ||
ZA8605937 | 1986-08-07 |
Publications (4)
Publication Number | Publication Date |
---|---|
FI873420A0 FI873420A0 (en) | 1987-08-06 |
FI873420A true FI873420A (en) | 1988-02-08 |
FI87237B FI87237B (en) | 1992-08-31 |
FI87237C FI87237C (en) | 1992-12-10 |
Family
ID=25578507
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FI873420A FI87237C (en) | 1986-08-07 | 1987-08-06 | FOERFARANDE FOER REDUKTION AV KROMITMALM |
Country Status (5)
Country | Link |
---|---|
BR (1) | BR8704022A (en) |
FI (1) | FI87237C (en) |
GR (1) | GR871253B (en) |
IN (1) | IN167768B (en) |
TR (1) | TR23786A (en) |
-
1987
- 1987-07-29 IN IN658/DEL/87A patent/IN167768B/en unknown
- 1987-08-06 BR BR8704022A patent/BR8704022A/en not_active IP Right Cessation
- 1987-08-06 GR GR871253A patent/GR871253B/en unknown
- 1987-08-06 FI FI873420A patent/FI87237C/en not_active IP Right Cessation
- 1987-08-10 TR TR87/0553A patent/TR23786A/en unknown
Also Published As
Publication number | Publication date |
---|---|
FI87237C (en) | 1992-12-10 |
BR8704022A (en) | 1988-04-05 |
TR23786A (en) | 1990-09-13 |
FI873420A0 (en) | 1987-08-06 |
IN167768B (en) | 1990-12-15 |
GR871253B (en) | 1988-01-18 |
FI87237B (en) | 1992-08-31 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES8802605A1 (en) | Forming refractory masses and composition of matter for use in forming such refractory masses | |
NO914352D0 (en) | PROCEDURE FOR TREATMENT OF USED COTTON BOTS | |
ES526482A0 (en) | PROCEDURE FOR OBTAINING A PARTICULATED FUNDENT FOR THE TREATMENT OF CAST METALS | |
DE3473124D1 (en) | Fluxes for casting metals | |
IN162925B (en) | ||
FI873420A (en) | FOERFARANDE FOER REDUKTION AV KROMITMALM. | |
DE3875890D1 (en) | Refractory Oxide Compound / Refractory Hard Metal Composite. | |
JPS526153A (en) | Heat recovery process of melting furnace sediment | |
DE3562668D1 (en) | Method of and apparatus for adding heat to molten metal, and also application of the method | |
EP0099219A3 (en) | Method of producing an agglomerated metallurgical composition | |
YU32683A (en) | Device for the elimination of solid and molten particles from flue gases of metallurgical furnaces | |
IN156686B (en) | ||
Dolinskij | Thermodynamic investigations of conditions of producing the self-decomposing slags in ferrous metallurgy | |
Elliott | Adsorbed Species on Silicate Slag Surfaces as Indicated by Kinetic Measurements | |
ZA827918B (en) | Furnace and method of operating the furnance | |
JPS522809A (en) | Process for prevention of oxidation of molten metal in melting and hol ding furnaces | |
PT77768B (en) | Process for recovering non-ferrous metals by thermal treatment of solutions containing non-ferrous and iron sulphates | |
ES8606829A1 (en) | Continuous prodn. of nodular alkali silicate(s) | |
Tabata et al. | Refractories for Hot Metal Pre-Treatment | |
Garcia | WEAK AREAS IN REFRACTORIES FOR GLASS FURNACES: HOW TO SOLVE THEM | |
Gubenko et al. | The Behaviour of Silicate Inclusions in the Laser Irradiation of Steel | |
ZA816832B (en) | Process for reducing the iron contents of desulphurisation slags and agent suitable for this purpose | |
Landefeld | A Shrinking Core Model of Desulfurization by CaO | |
Bystrov | The Composition of the Matte--Slag Mixture During Smelting in a Liquid Bath | |
Nagata | Literally Advanced Materials--Cast Iron and Metal Composites Are so Close. II |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
MM | Patent lapsed | ||
MM | Patent lapsed |
Owner name: COUNCIL FOR MINERAL TECHNOLOGY |