Application filed by American Cyanamid CofiledCriticalAmerican Cyanamid Co
Priority to ES351429ApriorityCriticalpatent/ES351429A1/en
Publication of ES351429A1publicationCriticalpatent/ES351429A1/en
Process for the polymerization of a glycolide, characterized in that a mixture of an essentially pure glycolide composition, from about 0.05 to 1.5 mole%, based on the moles of said glycolide composition, of an unsaturated free alcohol is heated benzenoid and free of any reactive group other than an alcoholic hydroxy group, and from 0.0005% to about 0.025% by weight, based on the weight of said glycolide composition, of a polymerization catalyst for said glycolide composition, to a temperature that varies between about 205ºc and 235ºc until the equilibrium viscosity is virtually reached. (Machine-translation by Google Translate, not legally binding)
ES351429A1968-03-091968-03-09Procedure for the polymerization of a glycolide. (Machine-translation by Google Translate, not legally binding)
ExpiredES351429A1
(en)
Improvements introduced in the preparation of a thermoplastic polymer, finished in hydroside. (Machine-translation by Google Translate, not legally binding)
A procedure for the preparation of 5-fluor-2-methyl-1- (p-metilsulfinilbenciliden) -3-indenil acetic acid. (Machine-translation by Google Translate, not legally binding)