ES288508A1 - Procedure for obtaining a glass composition of high chemical stability (Machine-translation by Google Translate, not legally binding)
- Google Patents
Procedure for obtaining a glass composition of high chemical stability (Machine-translation by Google Translate, not legally binding)
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by IndividualfiledCriticalIndividual
Priority to ES288508ApriorityCriticalpatent/ES288508A1/en
Publication of ES288508A1publicationCriticalpatent/ES288508A1/en
"PROCEDURE FOR OBTAINING A GLASS COMPOSITION OF HIGH CHEMICAL STABILITY", characterized in that it essentially consists of: (see graphic) varying the combined amounts of Li2O, Na2O and K2O, between 2 and 7%. (Machine-translation by Google Translate, not legally binding)
ES288508A1963-05-291963-05-29Procedure for obtaining a glass composition of high chemical stability (Machine-translation by Google Translate, not legally binding)