ES236940A1 - A procedure for obtaining aluminum-silicon-iron alloys with carbon content. (Machine-translation by Google Translate, not legally binding)
- Google Patents
A procedure for obtaining aluminum-silicon-iron alloys with carbon content. (Machine-translation by Google Translate, not legally binding)
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hoesch Werke AG
Original Assignee
Hoesch Werke AG
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hoesch Werke AGfiledCriticalHoesch Werke AG
Priority to ES0236940ApriorityCriticalpatent/ES236940A1/en
Publication of ES236940A1publicationCriticalpatent/ES236940A1/en
Procedure for obtaining aluminum-silicon-iron alloys with carbon content, by melt reduction in a closed furnace from low quality fuels, such as ash, etc. Characterized by heating mixtures of aluminum oxide, silicic acid, iron oxide and carbon or minerals containing said materials, at temperatures between 1650º and 1800º c, maintaining at the same time such oxygen-free atmospheric conditions, that at the partial pressure of the oxide of carbon that is formed, is less than 0.1atm. (Machine-translation by Google Translate, not legally binding)
ES0236940A1957-08-021957-08-02A procedure for obtaining aluminum-silicon-iron alloys with carbon content. (Machine-translation by Google Translate, not legally binding)