ES2044820T3 - Procedimiento para unir piezas de fundicion de hierro nodular con acero o fundicion de acero. - Google Patents
Procedimiento para unir piezas de fundicion de hierro nodular con acero o fundicion de acero.Info
- Publication number
- ES2044820T3 ES2044820T3 ES93102364T ES93102364T ES2044820T3 ES 2044820 T3 ES2044820 T3 ES 2044820T3 ES 93102364 T ES93102364 T ES 93102364T ES 93102364 T ES93102364 T ES 93102364T ES 2044820 T3 ES2044820 T3 ES 2044820T3
- Authority
- ES
- Spain
- Prior art keywords
- steel
- welding
- casting
- joining
- procedure
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
PARA LOGRAR UNA UNION DE PIEZAS DE HIERRO FUNDIDO DE GRAFITO ESFEROIDAL CON EXTREMO EN FORMA TUBULAR, CON PIEZAS PRESOLDADAS DE ACERO O ACERO FUNDIDO EN FORMA TUBULAR, MEDIANTE SOLDADURA POR PRESION CON UN DISPOSITIVO PARA EL CONTROL MAGNETICO DEL ARCO, QUE SIN UN TRATAMIENTO TERMICO POSTERIOR, APARECE UNA ESTRUCTURA INCLUSO TAMBIEN EN LA ZONA DE LA COSTURA DE SOLDADURA, QUE PRESENTA UNA RESISTENCIA Y FLEXION CONSIDERABLE, Y QUE ES EVITADA LA PRESENCIA DE MICRO-RECHUPES, CON EL FIN DE PODER APLICAR ESTE PROCEDIMIENTO PARA PIEZAS DE ALTA SEGURIDAD, COMO POR EJEMPLO ARMADURAS DE HIERRO FUNDIDO DE GRAFITO ESFEROIDAL, CON EXTREMOS TUBULARES PRESOLDADOS DE ACERO, LAS TUBERIAS DE LIQUIDO O CONDUCCIONES DE GAS SOMETIDAS A PRESION PUEDEN SER SOLDADOS EN LA OBRA, LAS CARAS FRONTALES A UNIR SON CALENTADAS A UNA TEMPERATURA DE SOLDADURA, SIN PREVIO TRATAMIENTO TERMICO, Y/O LA CARA FRONTAL A UNIR CON AL MENOS UNA DE LAS PIEZAS A SOLDAR, ESTA ANTES DEL PROCESO DE PRENSADO CASI TOTALMENTE LIQUIDA.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
DE4209101A DE4209101C2 (de) | 1992-03-20 | 1992-03-20 | Verfahren zum Verbinden von Sphärogußteilen mit Stahl oder Stahlguß |
Publications (2)
Publication Number | Publication Date |
---|---|
ES2044820T1 ES2044820T1 (es) | 1994-01-16 |
ES2044820T3 true ES2044820T3 (es) | 1995-07-01 |
Family
ID=6454627
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES93102364T Expired - Lifetime ES2044820T3 (es) | 1992-03-20 | 1993-02-16 | Procedimiento para unir piezas de fundicion de hierro nodular con acero o fundicion de acero. |
Country Status (6)
Country | Link |
---|---|
EP (1) | EP0561164B1 (es) |
AT (1) | ATE122594T1 (es) |
DE (2) | DE4209101C2 (es) |
DK (1) | DK0561164T3 (es) |
ES (1) | ES2044820T3 (es) |
GR (2) | GR930300126T1 (es) |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN101400473B (zh) * | 2006-03-16 | 2012-07-18 | 模力斯阿克多有限公司 | 钢铁构件的接合方法 |
DE102007011242B4 (de) | 2006-04-13 | 2019-06-19 | Martin Deibl | Verfahren zum Verbinden von Antriebsstrangteilen |
DE202008005534U1 (de) | 2008-04-21 | 2009-09-17 | Kuka Systems Gmbh | Schweißeinrichtung |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE3924162A1 (de) * | 1988-09-23 | 1990-03-29 | Fischer Ag Georg | Verfahren zum abbrennstumpfschweissen von hochgekohlten werkstoffen, insbesondere gusseisen mit kugelgraphit |
JPH03504695A (ja) * | 1989-01-26 | 1991-10-17 | インスティチュト エレクトロスバルキ イメニ イー.オー.パトナ アカデミイ ナウク ウクラインスコイ エスエスアール | 磁界内を移動するアークを用いて加熱部材を圧接する方法 |
-
1992
- 1992-03-20 DE DE4209101A patent/DE4209101C2/de not_active Expired - Lifetime
-
1993
- 1993-02-16 DK DK93102364.2T patent/DK0561164T3/da active
- 1993-02-16 AT AT93102364T patent/ATE122594T1/de not_active IP Right Cessation
- 1993-02-16 ES ES93102364T patent/ES2044820T3/es not_active Expired - Lifetime
- 1993-02-16 EP EP93102364A patent/EP0561164B1/de not_active Expired - Lifetime
- 1993-02-16 DE DE59300196T patent/DE59300196D1/de not_active Expired - Fee Related
- 1993-12-30 GR GR930300126T patent/GR930300126T1/el unknown
-
1995
- 1995-08-18 GR GR950402264T patent/GR3017156T3/el unknown
Also Published As
Publication number | Publication date |
---|---|
DE59300196D1 (de) | 1995-06-22 |
GR3017156T3 (en) | 1995-11-30 |
EP0561164B1 (de) | 1995-05-17 |
EP0561164A1 (de) | 1993-09-22 |
ES2044820T1 (es) | 1994-01-16 |
DE4209101A1 (de) | 1993-09-23 |
GR930300126T1 (en) | 1993-12-30 |
DK0561164T3 (da) | 1995-07-24 |
DE4209101C2 (de) | 1994-05-19 |
ATE122594T1 (de) | 1995-06-15 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES2044820T3 (es) | Procedimiento para unir piezas de fundicion de hierro nodular con acero o fundicion de acero. | |
Wu | Creep properties of 1 Cr 0. 5 Mo steel welded joints with controlled microstructures | |
Knothe | Process for the connection of nodular iron components with steel or cast steel | |
Kuchuk-Yatsenko et al. | Examination of quality of heat-resistant and hardening steel pipe joints, made by press welding with the heating by the magnetically controlled arc | |
Makarov et al. | Preventing hot cracking in end sections of long welds in one‐sided, multi‐arc, submerged‐arc welding | |
KR950000293A (ko) | 순(純) 펄라이트 레일을 중간에 주조 용접하는 방법 | |
Cerjak | Welding of steam turbine components | |
Takahashi et al. | Omission of Intermediate Stress Relief Annealing by Utilizing Low Temperature Postweld Heat Treatment for Welds in Pressure Vessels | |
Semenov et al. | Preheating Temperature Determination for Welding Steel 10 Kh 2 M 1 A-A | |
Metlitskii | Arc welding of austenitic nickel nodular cast iron | |
Heeschen et al. | New results on the formation of residual stresses due to phase transformations in the welded structural steels St 52-3 and StE 690 | |
Ammosov et al. | The Influence of Damages on Crack Initiation in the Overheating Zone of Welded Joints.(Retroactive Coverage) | |
Somsky | Report on the evaluation of twin arc narrow gap process for field welding of rails: Final report | |
Audemar | Choice of Aluminothermic Welding Normal Preheating--Limited Preheating and Recovery | |
Winterstein et al. | Pressure Welding of Cast Iron by the Magnetically Impelled Arc Process | |
Semenov et al. | Preheating Temperature Determination for Welding Steel 10 Kh 2 M 1 A-A[[Previously Titled: Determination of Preheat Temperature inWelding 10 Kh 2 M 1 A-A Steel.]] | |
Steklov et al. | Plasma-Arc Welding of High Silicon Corrosion Resistant 02 Kh 8 N 22 S 6 Steel | |
Minto | Expansion and contraction | |
Gretskii | Mechanism of Crack Formation in the Weld Zone During Welding of Cast Iron With Steel and Ferronickelous Alloys | |
Raboch et al. | Effect of phosphorus and heat treatment on the ductility properties of welded joints in NiCrMoV steel.(MITS WP 1556) | |
Evans et al. | The Effect of Sulphur and Phosphorus on the Microstructure and Properties of C--Mn All-Weld Metal Deposits.(Retroactive Coverage) | |
Morgan | The Weldability of Steels and Its Relationships to Mechanical Properties. II | |
Gretskii | Metal Structure Formation in the Heat-Affected Zone of Carbonitride-Hardened Low-Silicon Steel | |
Velikonja | The Effect of Preliminary Cold Deformation on the Toughness of the Heat Affected Zone of Welded Joints in C 1204 and Nioval 50 Steels.(Retroactive Coverage) | |
Minaeva et al. | Method For Quantitative Estimation of Tendency of Welded Joints to Hot Cracking in Pulsed Laser Welding |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
FG2A | Definitive protection |
Ref document number: 561164 Country of ref document: ES |