ES132917A1 - Procedure to increase the corrosion resistance of aluminum alloys with soon 3 to 16 per cent magnesium. - Google Patents
Procedure to increase the corrosion resistance of aluminum alloys with soon 3 to 16 per cent magnesium.Info
- Publication number
- ES132917A1 ES132917A1 ES132917A ES132917A ES132917A1 ES 132917 A1 ES132917 A1 ES 132917A1 ES 132917 A ES132917 A ES 132917A ES 132917 A ES132917 A ES 132917A ES 132917 A1 ES132917 A1 ES 132917A1
- Authority
- ES
- Spain
- Prior art keywords
- soon
- procedure
- increase
- corrosion resistance
- per cent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
ES132917A ES132917A1 (en) | 1933-12-20 | 1933-12-20 | Procedure to increase the corrosion resistance of aluminum alloys with soon 3 to 16 per cent magnesium. |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
ES132917A ES132917A1 (en) | 1933-12-20 | 1933-12-20 | Procedure to increase the corrosion resistance of aluminum alloys with soon 3 to 16 per cent magnesium. |
Publications (1)
Publication Number | Publication Date |
---|---|
ES132917A1 true ES132917A1 (en) | 1934-03-01 |
Family
ID=65588731
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES132917A Expired ES132917A1 (en) | 1933-12-20 | 1933-12-20 | Procedure to increase the corrosion resistance of aluminum alloys with soon 3 to 16 per cent magnesium. |
Country Status (1)
Country | Link |
---|---|
ES (1) | ES132917A1 (en) |
-
1933
- 1933-12-20 ES ES132917A patent/ES132917A1/en not_active Expired
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES132917A1 (en) | Procedure to increase the corrosion resistance of aluminum alloys with soon 3 to 16 per cent magnesium. | |
FR819263A (en) | New aluminum alloy | |
FR804514A (en) | Plated aluminum alloys | |
FR772586A (en) | Aluminum alloys | |
FR782562A (en) | Improved magnesium alloy | |
FR750760A (en) | Improvements to aluminum-based alloys | |
FR807798A (en) | Aluminum alloy | |
FR791803A (en) | Corrosion resistant alloy | |
ES134530A1 (en) | Procedure to ennoble aluminum alloys. | |
ES130445A1 (en) | Procedure to obtain objects of chrome-manganese steel alloys resistant to corrosion. | |
CA331111A (en) | Corrosion resistant alloy | |
FR786592A (en) | Aluminum alloy | |
FR763316A (en) | Improvements to copper-based alloys | |
GB371740A (en) | Improved aluminium alloys | |
FR803522A (en) | Advanced aluminum alloys | |
FR797714A (en) | Advanced aluminum alloy | |
FR44886E (en) | Advanced aluminum alloy | |
FR793084A (en) | Corrosion resistant alloy | |
FR788952A (en) | Application of aluminum alloys | |
FR812438A (en) | Improvements to aluminum-based alloys | |
FR751533A (en) | Improvements relating to ferrous alloys | |
ES121603A3 (en) | Procedure to obtain aluminum alloys. | |
IE12956L (en) | Magnesium alloys | |
FR749609A (en) | Improvements to aluminum and magnesium alloys | |
FR748612A (en) | Improvements to aluminum-based alloys |