DE717465C - Process for the bubble-free coating of metal rollers - Google Patents
Process for the bubble-free coating of metal rollersInfo
- Publication number
- DE717465C DE717465C DEB188894D DEB0188894D DE717465C DE 717465 C DE717465 C DE 717465C DE B188894 D DEB188894 D DE B188894D DE B0188894 D DEB0188894 D DE B0188894D DE 717465 C DE717465 C DE 717465C
- Authority
- DE
- Germany
- Prior art keywords
- coating
- bubble
- metal
- roller
- free coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Verfahren zur blasenfreien Beschichtung von Metallwalzen Die Erfindung bezieht sich auf ein Verfahren zur blasenfreien Beschichtung von Metallwalzen, wie solche z. B. zu Reproduktionszwecken verwendet werden.Process for the bubble-free coating of metal rolls The invention relates to a process for the bubble-free coating of metal rollers, such as such z. B. used for reproduction purposes.
Bei den bekannten Verfahren dieser Art mit erstarrenden, in der Regel hochviscosen Flüssigkeiten, besteht die Gefahr, daß sich durch elektrische Ströme zwischen der Metallwalze und dem Behälter für die Beschichtungsflüssigkeit entstehende Gasbläschen in der aufzutragenden bzw. aufgetragenen Schicht ansetzen und daß dadurch die Gleichmäßigkeit der Beschichtung leidet. Dieser Kachteil muß für viele Velwendiingszi@-eclze vermieden werden, insbesondere wenn es sich um das Aufbringen von lichtempfindlichen Schichten oder von Lackschichten auf Walzen für reproduktionstechnische Zwecke. handelt. D,--r Übelstand tritt besonders auf bei der vorzugsweise angewendeten senkrechten Beschichtung, wenn die zu beschichtende Walze in aufrechter Stellung in ein Gefäß mit- Beschichtungsflüssigkeit gesetzt oder gehängt wird zwecks Erreichung vollkommen nahloser, gleichmäßiger Beschichtung der Walze.In the known process of this type with solidifying, as a rule Highly viscous liquids, there is a risk of electrical currents between the metal roller and the container for the coating liquid Set gas bubbles in the to be applied or applied layer and that thereby the uniformity of the coating suffers. For many Velwendiingszi @ -eclze should be avoided, especially if it is the application of photosensitive Layers or layers of lacquer on rollers for reproduction purposes. acts. D, - r objection occurs particularly with the preferably used vertical Coating when the roller to be coated is in an upright position in a vessel with coating liquid is set or hung in order to achieve perfect seamless, even coating of the roller.
Um diesen Nachteil zii vermeiden, wird nach der Erfindung das Auftreten elektrischer Ströme zwischen Walze und Beschichtungsgefäß vermieden. Dies kann nach der Erfindung dadurch erreicht werden, daß die Walze aus demselben Metall besteht wie die der Walze gegenüberstehnd^n Teile der Vorrichtung, oder auch dadurch, daß alle in der Vorrichtung der Metallwalze gegenüberstehenden Metallteile von der M'alze isoliert sind, oder schließlich dadurch, daß der die Walze umgebende Behälter mit einem elektrisch isolierenden Überzug, z. B. Lack, oder einer Guminierung versehen ist bz«-. selbst aus ein in isolierenden Stoff besteht.In order to avoid this disadvantage zii, according to the invention, the occurrence electrical currents between the roller and coating vessel avoided. This can be done after of the invention can be achieved in that the roller is made of the same metal like that of the roller opposite parts of the device, or also by the fact that all metal parts in the device opposite the metal roller from the M'alze are isolated, or finally by the fact that the container surrounding the roller with an electrically insulating coating, e.g. B. lacquer, or a gum coating is bz «-. itself consists of an insulating material.
Claims (1)